113 resultados para Toughness.


Relevância:

20.00% 20.00%

Publicador:

Resumo:

A strong strain-rate and temperature dependence was observed for the fracture toughness of phenolphthalein polyether ketone (PEK-C). Two separate crack-blunting mechanisms have been proposed to account for the fracture-toughness data. The first mechanism involves thermal blunting due to adiabatic heating at the crack tip for the high temperatures studied. In the high-temperature range, thermal blunting increases the fracture toughness corresponding to an effectively higher test temperature. However, in the low-temperature range, the adiabatic temperature rise is insufficient to cause softening and Jic increases with increasing temperature owing to viscoelastic losses associated with the p-relaxation there. The second mechanism involves plastic blunting due to shear yield/flow processes at the crack tip and this takes place at slow strain testing of the single-edge notched bending (SENB) samples. The temperature and strain-rate dependence of the plastic zone size may also be responsible for the temperature and strain-rate dependence of fracture toughness.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The static and impact fracture toughness of phenolphthalein polyether ketone (PEK-C) were studied at different temperatures. The static fracture toughness of PEK-C was evaluated via the linear elastic fracture mechanics (LEFM) and the J-integral analysis. Impact fracture toughness was also analyzed using the LEFM approach. Temperature and strain rate effects on the fracture toughness were also studied. The enhancement in static fracture toughness at 70 degrees C was thought to be caused by plastic crack tip blunting. The increase in impact fracture toughness with temperature was attributed two different mechanisms, namely, the relaxation process in a relatively low temperature and thermal blunting of the crack tip at higher temperature. The temperature-dependent fracture toughness data obtained in static tests could be horizontally shifted to match roughly the data for impact tests, indicating the existence of a time-temperature equivalence relationship. (C) 1995 John Wiley & Sons, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A series of tensile and three-point bending studies was conducted at various temperatures and loading rates using phenolphthalein polyether ketone (PEK-C). Yield stress, Young's modulus, fracture toughness, and crack opening displacement data were obtained for various conditions. In general, both yield stress and Young's modulus increase with decreasing temperature. However, the relationships between fracture toughness, loading rate, and temperature are very complex. This behavior is due to the simultaneous intersection of viscoelasticity and localized plastic deformation. The increased yield stress is the main factor contributing to the reduction in fracture toughness and crack opening displacement. The relationship between fracture toughness and yield stress are discussed. (C) 1995 John Wiley and Sons, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Phenolphthalein poly(ether ketone) (PEK-C) was tested using an instrumented impact tester to determine the temperature effect on the fracture toughness K-c and critical strain energy release rate G(c). Two different mechanisms, namely the relaxation processes and thermal blunting of the crack tip were used to explain the temperature effect on the fracture toughness. Examination of the fracture surfaces revealed the presence of crack growth bands. It is suggested that these bands are the consequence of variations in crack growth along crazes that are formed in the crack tip stress field. As the crack propagates, the stress is relaxed locally, decreasing the growth rate allowing a new bundle of crazes to nucleate along which the crack advances.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fracture toughness values of phenolphthalein poly(ether ketone) (PEK-C) at 190 degrees C were determined by two different methods, i. e. the conventional crack growth method and the crack stress whitening zone method, which show consistent results. This indicates that the crack stress whitening zone method can be used to determine the crack initiation of some polymers for which the blunting line concept is unsuitable.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Blends of a new phenolphthalein poly (ether sulfone) (PES-C) and a thermotropic liquid crystalline polymer (LCP) were prepared by melt-blending in a twin-screw extruder. Rheological properties, fracture toughness, K(IC), and morphology of the blends were

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper deals with the correction of mode II strain energy release rate, G(II), of composite laminates measured with the end-notched flexure (ENF) specimen. A derivation is given of the expressions for compliance and strain energy release rate, in whic

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The use of interlaminar fracture tests to measure the delamination resistance of unidirectional composite laminates is now widespread. However, because of the frequent occurrence of fiber bridging and multiple cracking during the tests, it leads to artificially high values of delamination resistance, which will not represent the behavior of the laminates. Initiation fracture from the crack starter, on the other hand, does not involve bridging, and should be more representative of the delamination resistance of the composite laminates. Since there is some uncertainty involved in determining the initiation value of delamination resistance in mode I tests in the literature, a power law of the form G(IC) = A.DELTA alpha(b) (where G(IC) is mode I interlaminar fracture toughness and DELTA alpha is delamination growth) is presented in this paper to determine initiation value of mode I interlaminar fracture toughness. It is found that initiation values of the mode I interlaminar fracture toughness, G(IC)(ini), can be defined as the G(IC) value at which 1 mm of delamination from the crack starter has occurred. Examples of initiation values determined by this method are given for both carbon fiber reinforced thermoplastic and thermosetting polymers.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

For metal-matrix composites (MMCs), interfacial debonding between the ductile matrix and the reinforcing hard inclusions is an important failure mode. A fundamental approach to improving the properties of MMCs is to optimize their microstructure to achieve maximum strength and toughness. Here, we investigate the flow stress of a MMC with a nanoscale microstructure similar to that of bone. Such a 'biomorphous' MMC would be made of staggered hard and slender nanoparticles embedded in a ductile matrix. We show that the large aspect ratio and the nanometer size of inclusions in the biomorphous MMC lead to significantly improved properties with increased tolerance of interfacial damage. In this case, the partially debonded inclusions continue to carry mechanical load transferred via longitudinal shearing of the matrix material between neighboring inclusions. The larger the inclusion aspect ratio, the larger is the flow stress and work hardening rate for the composite. Increasing the volume concentration of inclusion also makes the biomorphous MMC more tolerant of interfacial damage.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The effects of La2O3 addition on the microstructure and wear properties of laser clad gamma/C(r)7C(3)/TiC composite coatings on gamma-TiAl intermetallic alloy substrates with NiCr-Cr3C2 precursor mixed powders have been investigated by optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction (XRD) and energy-dispersive spectrometer (EDS) and block-on-ring wear tests. The responding wear mechanisms are discussed in detail. The results are compared with that for composite coating without La2O3. The comparison indicates that no evident new crystallographic phases are formed except a rapidly solidified microstructure consisting of the primary hard Cr7C3 and TiC carbides and the gamma/Cr7C3 eutectics distributed in the tough gamma nickel solid solution matrix. Good finishing coatings can be achieved under a proper amount of La2O3-addition and a suitable laser processing parameters. The additions of rare-earth oxide La,03 can refine and purify the microstructure of coatings, relatively decrease the volume fraction of primary blocky Cr7C3 to Cr7C3/gamma eutectics, reduce the dilution of clad material from base alloy and increase the microhardness of the coatings. When the addition of La2O3 is approximately 4 wt.%, the laser clad composite coating possesses the highest hardness and toughness. The composite coating with 4 wt.%La2O3 addition can result the best enhancement of wear resistance of about 30%. However, too less or excessive addition amount of La2O3 have no better influence on wear resistance of the composite coating.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A high toughness wear resistant coating is produced by laser clad Fe-Cr-W-Ni-C alloys. The microstructural and compositional features of the laser-solidified microstructures and phase evolutions occurring during high temperature tempering at 963 K were investigated by using analytical electron microscopy with energy dispersive X-ray analysis. The clad coating possesses the hypereutectic microstructure consisted of M7C3 + (Y + M7C3) Du ring high temperature aging, the precipitation of M23C6 and M2C in austenite and in situ transformation of dendritic M7C3 to M23C6 and eutectic M7C3 to M6C occurred. The laser clad coating reveals an evident secondary hardening and superior impact wear resistance.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In order to study the earthquake recurrence and the characteristics of earthquake series, rupture tests of rock samples and plexiglass samples were made. On rock samples, a number of acoustic emission (AE) and strain measuring points were deployed; the load was one side direct shear. The variation characteristics of AE and strain at different detecting points around the extra large fracture were observed and studied. On plexiglass samples, a series of inclined cracks were prefabricated by a small-scale compressive testing machine. The samples were then loaded on a shockproof platen, when the samples were loaded, the stress intensity factor (SIF) was determined by the laser interferometric technique and shadow optical method of caustics. The fracture conditions such as material toughness around the extra large fracture were also studied. From those experimental results and the theory of fracture mechanics, the earthquake recurrence period and the trend of post-seismic development were studied.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this paper, an accurate formula for calculating the thermal residual stress field in a particle-reinforced composite are presented. Numerical examples are given to show r-variations of the thermal residual stresses. The increase in fracture toughness of matrix predicted by the thermal residual stress field is compared well with the experimentally measured increase.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Essential work of fracture (EWF) analysis is used to study the effect of the silica doping level on fracture toughness of polyimide/silica (PI/SiO2) hybrid films. By using double-edge-notched-tension (DENT) specimens with different ligament lengths, it seems that the introduction of silica additive can improve the specific essential work of fracture (w (e) ) of PI thin films, but the specific non-essential work of fracture (beta w (p) ) will decease significantly as the silica doping level increasing from 1 to 5 wt.%, and even lower than that of neat PI. The failure process of the fracture is investigated with online scanning electron microscope (SEM) observation and the parameters of non-essential work of fracture, beta and w (p) , are calculated based on finite element (FE) method.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Three analytical double-parameter criteria based on a bending model and a two-dimensional finite element analysis model are presented for the modeling of ductile thin film undergoing a nonlinear peeling process. The bending model is based on different governing parameters: (1) the interfacial fracture toughness and the separation strength, (2) the interfacial fracture toughness and the crack tip slope angle, and (3) the interfacial fracture toughness and the critical Mises effective strain of the delaminated thin film at the crack tip. Thin film nonlinear peeling under steady-state condition is solved with the different governing parameters. In addition, the peeling test problem is simulated by using the elastic-plastic finite element analysis model. A critical assessment of the three analytical bending models is made by comparison of the bending model solutions with the finite element analysis model solutions. Furthermore, through analyses and comparisons for solutions based on both the bending model and the finite element analysis model, some connections between the bending model and the finite element analysis model are developed. Moreover, in the present research, the effect of different selections for cohesive zone shape on the ductile film peeling solutions is discussed.