49 resultados para Stainless steels


Relevância:

20.00% 20.00%

Publicador:

Resumo:

A palladium membrane has been prepared by electroless plating on the surface of a porous stainless steel tube. Since the large surface pores of the tube are obstacle for preparation of a defect-free palladium film on the surface, zirconium oxide particles were deposited inside the pores. The mean thickness of the resulting Pd membrane on the modified tube was ca. 10 mum. It is suggested that the permeability of hydrogen is partly governed by gas diffusion in the pores. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Adoption of a sintered stainless steel fiber felt was evaluated as gas diffusion backing in air-breathing direct methanol fuel cell (DMFC). By using a sintered stainless steel fiber felt as an anodic gas diffusion backing, the peak power density of an air-breathing DMFC is 24 mW cm(-2), which is better than that of common carbon paper. A 30-h-life test indicates that the degraded performance of the air-breathing DMFC is primarily due to the water flooding of the cathode. Twelve unit cells with each has 6 cm(2) of active area are connected in series to supply the power to a mobile phone assisted by a constant voltage diode. The maximum power density of 26 mW cm(-2) was achieved in the stack, which is higher than that in single cell. The results show that the sintered stainless steel felt is a promising solution to gas diffusion backing in the air-breathing DMFC, especially in the anodic side because of its high electronical conductivity and hydrophilicity. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The selective oxidation of cyclohexane to cyclohexanol and cyclohexanone is an important chemical process and it has been paid more attentions recently. In the present work, the stainless steel reactor wall was found to influence the selective oxidation of cyclohexane very significantly, and a quasi-crystalline Ti45Zr35Ni17Cu3 alloy with the similar compositions as the reactor wall was used as a catalyst for the cyclohexane oxidation, as expected, a higher activity was obtained with it. The present results open up a new avenue for developing new catalyst for alkane oxidation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Three kinds of steels were studied using electrically connected hanging specimen in the corrosion simulation device and offshore long scale hanging specimen. The experimental results obtained by the two methods show that the device can better reflect the offshore corrosion environment. A Ni-Cu-P steel specimen was studied through analysis of the specimen's corrosion products and corrosion types. The surface of the samples before and after the removal of the rust layer produced by these two methods were observed and compared after some experiments. The microstructure of the corrosion products under different marine environments were analyzed and compared through IR. It indicated good correlation between the electrically connected hanging specimen method and the long scale hanging specimen method.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect of Cl- on the corrosive wear behaviour of AISI 321 stainless steel in H2SO4 solution was studied via the corrosive wear rate, the load bearing capacity of passive film and the relationship between pitting and corrosive wear. There is a critical load at natural potential, below which the corrosive wear rate is slightly lowered by Cl-, while above which is increased. At natural potential there are more pits at low load than that at a higher one in the wear tracks and the pits are also deeper. The load bearing capacity is lowered by Cl- at passive region and then the corrosive wear rate increased.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The stress corrosion cracking (SCC) of LambdaISI 321 stainless steel in acidic chloride solution was studied by slow strain rate (SSR) technique and fracture mechanics method. The fractured surface was characterized by cleavage fracture. In order to clarify the SCC mechanism, the effects of inhibitor KI on SCC behaviour were also included in this paper. A study showed that the inhibition effects of KI on SCC were mainly attributed to the anodic reaction of the corrosion process. The results of strain distribution in front of the crack tip of the fatigue pre-cracked plate specimens in air, in the blank solution (acidic chloride solution without inhibitor KI) and in the solution added with KI measured by speckle interferometry (SPI) support the unified mechanism of SCC and corrosion fatigue cracking (CFC).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The inhibition effect of nicotinic acid for corrosion of hot dipped Zn and Zn-Al alloy coatings in diluted hydrochloric acid was investigated using quantum chemistry analysis, weight loss test, electrochemical measurement, and scanning electronic microscope (SEM) analysis. Quantum chemistry calculation results showed that nicotinic acid possessed planar structure with a number of active centers, and the populations of the Mulliken charge, the highest occupied molecular orbital (HOMO), and the lowest unoccupied molecular orbital (LUMO) were found mainly focused around oxygen and nitrogen atoms, and the cyclic of the benzene as well. The results of weight loss test and electrochemical measurement indicated that inhibition efficiency (IE%) increased with inhibitor concentration, and the highest inhibition efficiency was up to 96.7%. The corrosion inhibition of these coatings was discussed in terms of blocking the electrode reaction by adsorption of the molecules at the active centers on the electrode surface. It was found that the adsorption of nicotinic acid on coating surface followed Langmuir adsorption isotherm with single molecular layer, and nicotinic acid adsorbed on the coating surface probably by chemisorption. Nicotinic acid, therefore, can act as a good nontoxic corrosion inhibitor for hot dipped Zn and Zn-Al alloy coatings in diluted hydrochloric acid solution. (c) 2007 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The corrosion rate of low alloy steel in different sea zones has close correlation with the content of the alloy element. From the field data of steel corrosion rates in atmospheric zone, splash zone and immersion zone, regression analysis was used to study the correlation between the corrosion rate of steels and the amount of added alloy elements. Three regression equations were obtained in different sea zones. Based on the equations, the anti-corrosion performance of the alloy elements can be deduced which can be used to screen out low alloy steel with good anti-corrosion performance. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The application of hot-dipped zinc and zinc-aluminum alloy coatings were introduced. Exposure tests of the steels with these coatings were conducted in the offshore atmosphere in Qingdao and Xiamen for 12 years separately. Effects of the coating thickness, alloy composition and atmospheric environment on the corrosion performance were studied. Results of the onsite exposure tests were compared with the results of a previous indoor salt spray accelerated corrosion tests. The study supports that zinc-aluminum alloy coatings are useful in providing better corrosion resistance and can be further developed for future applications.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A stainless-steel net is used to support a zeolite NaA membrane synthesized using a 'seeded-growth' method. The zeolite and stainless-steel net are tightly integrated (see Figure), showing large-scale order and high mechanical stability. High oxygen permeance and high permselectivity for O-2 over N-2 (about 7) is demonstrated.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A novel composite coating was synthesized by laser alloying of zirconium nanoparticles on an austenite stainless steel surface using a pulsed Nd:YAG laser. The coating contained duplex microstructures comprising an amorphous phase and an austenitic matrix. A discontinuous zirconium-containing region formed at a depth of 16 mum below the surface. The amorphous phase was present in the zirconium-rich region, with the composition of zirconium ranging from 7.8 to 14.5 at. pet. The formation of the amorphous phase was attributed to the zirconium addition. The hardness, corrosion, and wear-corrosion resistance of the irradiated coating were evidently enhanced compared to those of the stainless steel.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Coatings were synthesized by laser alloying of zirconium (Zr) particles using a pulsed Nd:YAG laser on an austenite stainless steel. The distribution of Zr is uneven, in a depth of 18 mum just below the surface of the pool. The coating consisted of duplex microstructures, i.e. metallic glass (MG) and austenite. The MG formed in Zr-contained regions, with the Zr composition ranging from 7.6 to 16.8 at.%. The formation of the MG was attributed to an increase in glass-forming ability by Zr addition.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The basic remelting and cladding tests with laminar plasma technology on metals have been conducted in order to demonstrate the possibility of the technology applied in material surface modification. The experimental results show that the properties of the modified layers of the cast iron surface can be improved notably by the remelting treatment and those of the stainless steel by the cladding treatment. The related results are also verified by microscopic studies such as scanning electron microscopic (SEM) observations, energy dispersive spectra (EDS) analysis and the Vickers hardness measurements of the surface modified layers.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

采用等离子电弧沉积法在9Cr18钢表面制备了厚约0.5 μm的TiN薄膜,通过显微硬度测试以及纳米压痕和纳米划痕试验,对比考察了9Cr18钢及其表面TiN薄膜的机械和摩擦性能。结果表明,9Cr18钢及其表面TiN沉积膜的纳米硬度分别为8GPa和38GPa,弹性模量分别为250GPa和580 GPa,9Cr18、TiN和有机薄膜的摩擦系数分别为0.40、0.12和、0.10;TiN沉积膜可显著提高基体钢的承载和耐磨能力。