146 resultados para Reproductive parameters
Resumo:
Lithium sodium mixed alkali aluminophosphate glasses of the composition xNa(2)O-(15-x)Li2O-4B(2)O(3)-11Al(2)O(3)-5BaO-65P(2)O(5) (where x=0, 3.75, 7.5, 11.25 and 15 mol%) containing 0.5 mol% Er2O3 were prepared by melt quenching. The absorption spectra of Er3+ were studied from the experimental oscillator strengths and the Judd-Ofelt intensity parameters were obtained. The variations of Judd-Ofelt intensity parameters (Omega(2), Omega(4) and Omega(6)), experimental oscillator strengths of certain excited states of Er3+ and hypersensitive band positions with different mixed alkali content have been discussed in detail. It was found that there were similar effects of mixed alkali on both Judd-Ofelt intensity parameter 02 and the experimental oscillator strength of the hypersensitive transition, I-4(15/2) -> H-2(11/2). No shifts in the peak wavelength of the studied transitions were found in different glasses. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
The Er3+/Yb3+ co-doped glasses with compositions of xBi(2)O(3)-(65-x)P2O5-4Yb(2)O(3)-11Al(2)O(3)-5BaO-15Na(2)O (where x = 0, 2.5, 5, 7.5 and 10 mol%) were prepared using the normal melt quench technique. The optical absorption spectra of the glasses were recorded in the wavelength range 300-1700 nm. The effect of Bi2O3 content on the thermal stability and absorption spectra of glasses was investigated. In addition, the Judd-Ofelt parameters and oscillator strengths were calculated by employing Judd-Ofelt theory. It was observed that the positions of the fundamental absorption edge and cut-off wavelength shifted towards red as the content of Bi2O3 increased. However, there were no red shifts found both in the peak wavelength and in the center of mass wavelength of all absorption bands with Bi2O3 content increasing. The results of Judd-Ofelt theory analysis showed that Judd-Ofelt parameters Omega(t), (t = 2, 4, 6) changed sharply when Bi2O3 concentration exceeded 5 mol%. The variation trends of experimental oscillator strength were similar with those of Judd-Ofelt parameters as function of Bi2O3 concentrations. Moreover, differential scanning calorimetry experiments showed that the increases of Bi2O3 content weakened the network structure and then lowered the thermal stability of the glasses. The spontaneous emission probability A(rad), branching ratio beta and the radiative lifetime tau(rad) were also calculated and analyzed. The stimulated emission cross-section of Er3+ was calculated according to the McCumber theory. It was found that the stimulated emission cross-section of Er3+ was monotonically increases with Bi2O3 content increasing. (C) 2006 Elsevier B.V. All rights reserved.
Resumo:
Hybrid TiO2/ormosil waveguiding films have been prepared by the sol-gel method at low thermal treatment temperature of 150° C. The influence of processing parameters including the molar ratios of titanium butoxide (Ti(OBu)(4))/3-glycidoxypropyltrimethoxysilane (GLYMO) and H2O/Ti(OBu)(4) (expressed as R), especially aging of sot on the optical properties was investigated. The optical properties of films were measured with scanning electron microscope (SEM), UV/VIS/NIR spectrophotometer (UV-Vis), m-line and the scattering-detection method. The results indicate that the film thickness increases with the increase of sol aging time, but the variation of refractive index as a function of sot aging time depends on the relative ratios of GLYMO to Ti(OBu)(4). Higher transmittance and lower attenuation of the planar waveguide can be obtained in the sol with lower Ti(OBu)(4) contents and shorter aging time.
Resumo:
Yb: YAlO3 (YAP) (15 at %) and Yb: Y3Al5O12 (YAG)(15 at %) have been grown using the Czochralski method. Their absorption and fluorescence spectra were measured at room temperature and important spectroscopic parameters were calculated. Through the comparison of spectroscopic parameters of Yb:YAP and Yb: YAG, all results indicate that 15 at % Yb:YAP crystal is a potential candidate used for compact, efficient thin chip lasers when the laser output wavelength is 1012 or 103 8 nm. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
We investigate the laser damage behaviour of an electron-beam-deposited TiO2 monolayer at different process parameters. The optical properties, chemical composition, surface defects, absorption and laser-induced damage threshold (LIDT) of Elms are measured. It is found that TiO2 Elms with the minimum absorption and the highest LIDT can be fabricated using a TiO2 starting material after annealing. LIDT is mainly related to absorption and is influenced by the non-stoichiometric defects for TiO2 films. Surface defects show no evident effects on LIDT in this experiment.