Thiol-functionalized mesoporous ethane-silicas with large pore were synthesized by co-condensation of 1,2-bis(trimethoxy-sily)ethane (BTME) with 3-mercaptopropyltrimethoxysilane (MPTMS) using nonionic oligomeric polymer C1H (OCH(2)-CH(2))(10)OH (Brij-76) or poly(alkylene oxide) block copolymer (P123) as surfactant in acidic medium. The results of powder X-ray diffraction (XRD), nitrogen gas adsorption, and transmission electron microscopy (TEM) show that the resultant materials have well-ordered hexagonal mesoscopic structure with uniform pore size distributions. (29)Si MAS NNR, (13)C CP-MAS NMR. FT-IR, and UV Raman spectroscopies confirm the attachment of thiol functionalities in the mesoporous ethane-sificas. The maximum content of the attached thiol group (-SH) in the mesoporous framework is 2.48mmol/g. The ordered mesoporous materials are efficient Hg(2+) adsorbents with almost every -SH site accessible to Hg(2+). In the presence of various kinds of heavy metal ions such as Hg(2+), Cd(2+), Zn(2+), Cu(2+) and Cr(3+), the materials synthesized using poly(alkylene oxide) block cooollxmier (Pluronic 123) g(2+), as surfactant show almost similar affinity to Hg(2+), Cd(2+), and Cr(3+), while the materials synthesized using ofigomeric polymer C(18)H(37)(OCH(2)CH(2))(10)OH (Brij-76) as surfactant exhibit high selectivity to Hg(2+). (C) 2004 Elsevier Inc. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Two porous zirconium methylphosphonates (designated as ZMPmi and ZMPme respectively) were synthesized by using dibutyl methylphosphonate (DBMP) as a template. Two efficient post-synthetic treatments were developed to remove the incorporated template without destroying the hybrid structures. The materials were characterized by SEM, EPMA, TG, DTA, FTIR, and NMR. Specific surface area and porosity were evaluated by BET, alpha(s)-plots and DFT methods based on N-2 adsorption-desorption isotherms. The specific surface areas of ZMPmi and ZMPme are determined to be 279 and 403 m(2) g(-1) and the maxima of pore size distributions are at 0.7 and 1.3 nm respectively. (c) 2005 Elsevier Inc. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

By using the bifunctional ligand, 8-hydroxyquinoline-functionalized organosilane (Q-Si), the new mesoporous material Q-MCM-41 covalently bonded with 8-hydroxyquinoline was synthesized. Through the ligand exchange reaction, the new near-infrared (NIR) luminescent mesoporous LnQ(3)-MCM-41 (Ln = Er, Nd, Yb) materials were prepared by linking the lanthanide quinolinate complexes to the ordered mesoporous Q-MCM-41 material. The LnQ(3)-MCM-41 materials were characterized by powder X-ray diffraction and N-2 adsorption/desorption, and they all show the characteristic mesoporous structure of MCM-41 with highly uniform pore size distributions.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A novel periodic mesoporous organosilica (PMO) material was synthesized through one-step co-condensation of 1,2-bis(triethoxysilyl)ethane (BTESE) and benzoic acid-functionalized organosilane (BA-Si) using cetyltrimethylammonium bromide (CTAB) as a structure-directing agent under basic conditions. The materials were fully characterized by FTIR, XRD, N-2 adsorption-desorption isotherms and FESEM. FTIR spectra proved that BA-Si was successfully incorporated into the PMO materials (PMOs) via benzyl group as a linker. XRD and N-2 adsorption-desorption isotherms revealed the characteristic mesoporous structure with highly uniform pore size distributions. FESEM confirmed that the morphology of the PMOs was significantly dependent cri the molar ratio of two organosilica precursors.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A mesostructured cellular foam (MCF) with three-dimensional (313) disordered strutlike structure is prepared by using triblock copolymer (poly(styrene-b-butadiene-b-styrene), SBS, M-W = 140K) as template under strong acid conditions. It is the first report to use triblock copolymer with both hydrophobic head and tail groups instead of hydrophilic head and hydrophobic tail copolymers to synthesize siliceous mesostructured cellular foams. The resulted materials have high pore volume (0.92 cm(3)/g) and relatively narrow pore size distributions with a large pore size of 7.9 nm, which will allow for the fixation of large active complexes, reduce diffusional restriction of reactants and enable reactions involving bulky molecules to take place, especially.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Uniformly carbon-covered alumina (CCA) was prepared via the carbonization of sucrose highly dispersed on the alumina surface. The CCA samples were characterized by XRD, XPS, DTA-TG, UV Raman, nitrogen adsorption experiments at 77 K, and rhodamine B (RB) adsorption in aqueous media. UV Raman spectra indicated that the carbon species formed were probably conjugated olefinic or polycyclic aromatic hydrocarbons, which can be considered molecular subunits of a graphitic plane. The N(2) adsorption isotherms, pore size distributions, and XPS results indicated that carbon was uniformly dispersed on the alumina surface in the as-prepared CCA. The carbon coverage and number of carbon layers in CCA could be controlled by the tuning of the sucrose content in the precursor and impregnation times. RB adsorption isotherms suggested that the monolayer adsorption capacity of RB on alumina increased drastically for the sample with uniformly dispersed carbon. The as-prepared CCA possessed the texture of alumina and the surface properties of carbon or both carbon and alumina depending on the carbon coverage.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this study, a novel sol-gel method is used to synthesize amorphous silica-alumina materials with a narrow mesoporous distribution and various Si/Al molar ratios without using any templates and pore-regulating agents. During the preparation procedure, only inexpensive inorganic salts were used as raw materials, instead of expensive and harmful alkoxides. The precursor sol was dried at room temperature in a vacuum box kept at 60 mmHg until it began to form the gel. The results of a nitrogen sorption experiment indicate that the synthesized materials with different Si/Al molar ratios have similar mesoporous distributions (within 2-12 nm). Moreover, it was found that the material's pore size distribution remains at a similar value during the heat treatment from room temperature to 550 degreesC. On the basis of the nitrogen sorption, TEM, and AFM characterization results, a formation mechanism of mesopores which accounts for the experimental data is also suggested. This suggested mechanism involves rearrangement of the primary particles during the drying process to form the precursors of the similarly sized mesopores. The synthesized materials were characterized by XRD, thermal analysis (TG/DTA), Al-27 and Si-29 MAS NMR spectroscopy, SEM, TEM, and AFM. The results of Al-27 and 29Si MAS NMR indicate that the distribution of silicon and aluminum in the synthesized materials is more uniform and homogeneous than that in the mixed oxides prepared via the traditional sol-gel method even at high alumina contents. The type and density of the acid sites were studied using pyridine adsorption-desorption FTIR spectroscopy. It was shown that the acidity of the synthesized materials is higher than that of the silica-alumina materials prepared by conventional methods.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A new mesoporous sphere-like SBA-15 silica was synthesized and evaluated in terms of its suitability as stationary phases for CEC. The unique and attractive properties of the silica particle are its submicrometer particle size of 400 nm and highly ordered cylindrical mesopores with uniform pore size of 12 nm running along the same direction. The bare silica particles with submicrometer size have been successfully employed for the normal-phase electrochromatographic separation of polar compounds with high efficiency (e.g., 210 000 for thiourea), which is matched well with its submicrometer particle size. The Van Deemeter plot showed the hindrance to mass transfer because of the existence of pore structure. The lowest plate height of 2.0 mu m was obtained at the linear velocity of 1.1 mm/s. On the other hand, because of the relatively high linear velocity (e.g., 4.0 mm/s) can be generated, high-speed separation of neutral compounds, anilines, and basic pharmaceuticals in CEC with C-18-modified SBA-15 silica as stationary phases was achieved within 36, 60, and 34 s, respectively.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The size structure of the planktonic community in a Changjiang floodplain lake (Lake Chenhu, Hubei, P. R. China) was described for the inundation period of May through September 1983. The modality of the Sheldon-type size distributions changed hydrographically with the spectral profiles being bimodal during low, rising, mid-high and falling water phases, and trimodal soon after filling and shortly before falling. The modal peaks corresponded respectively to the dominant organisms of chlorophytes and nauplii, while the troughs centered on the bacteria and macrocrustacean size classes in the lake. The slope of the normalized biomass spectrum (an index of plankton size distribution) was less than -1.0 for the filling and falling phases or close to -1.0 for the high water period, indicating that the planktonic biomass tended to decrease or evenly distributes across logarithmically ordered size classes, respectively. This observed variation in the size distribution of the plankton community mainly resulted from changes in water levels and contents of particulate inorganic matter (PIM) in the lake.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

A bar on the Brazos River near Calvert, Texas, has been analyzed in order to determine the geologic meaning of certain grain size parameters and to study the behavior of the size fractions with transport. The bar consists of a strongly bimodal mixture of pebble gravel and medium to fine sand; there is a lack of material in the range of 0.5 to 2 mm, because the source does not supply particles of this size. The size distributions of the two modes, which were established in the parent deposits, are nearly invariant over the bar because the present environment of deposition only affects the relative proportions of the two modes, not the grain size properties of the modes themselves. Two proportions are most common; the sediment either contains no gravel or else contains about 60% gravel. Three sediment types with characteristic bedding features occur on the bar in constant stratigraphic order, with the coarsest at the base. Statistical analysis of the data is based on a series of grain size parameters modified from those of Inman (1952) to provide a more detailed coverage of non-normal size curves. Unimodal sediments have nearly normal curves as defined by their skewness and kurtosis. Non-normal kurtosis and skewness values are held to be the identifying characteristics of bimodal sediments even where such modes are not evident in frequency curves. The relative proportions of each mode define a systematic series of changes in numerical properties; mean size, standard deviation and skewness are shown to be linked in a helical trend, which is believed to be applicable to many other sedimentary suites. The equations of the helix may be characteristic of certain environments. Kurtosis values show rhythmic pulsations along the helix and are diagnostic of two-generation sediments.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

We have synthesized a porous co-polyimide film by coagulating a polyimide precursor in the non-solvent and thermal imidization. Factors affecting the morphology, pore size, porosity, and mechanical strength of the film were discussed. The porous polyimide matrix consists of a porous top layer and a spongy sub-structure with micropores. It is used as a porous matrix to construct sulfonated poly(styrene-ran-ethylene) (SPSE) infiltrated composite membrane for direct methanol fuel cell (DMFC) application. Due to the complete inertness to methanol and the very high mechanical strength of the polyimide matrix, the swelling of the composite membrane is greatly suppressed and the methanol crossover is also significantly reduced, while high proton conductivity is still maintained. Because of its higher proton conductivity and less methanol permeability, single fuel cell performance test demonstrated that this composite membrane outperformed Nafion membrane.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

A new methodology is described for the one-step aqueous preparation of highly monodisperse gold nanoparticles with diameters below 5 nm using thioether- and thiol-functionalized polymer ligands. The particle size and size distribution was controlled by subtle variation of the polymer structure. It was shown that poly(acrylic acid) (PAA) and poly(methacrylic acid) (PMAA) were the most effective stabilizing polymers in the group studied and that relatively low molar mass ligands (similar to 2500 g/mol) gave rise to the narrowest particle size distributions. Particle uniformity and colloidal stability to changes in ionic strength and pH were strongly affected by the hydrophobicity of the ligand end group. "Multidentate" thiol-terminated ligands were produced by employing dithiols and tetrathiols as chain-transfer agents, and these ligands gave rise to particles with unprecedented control over particle size and enhanced colloidal stability. It was found throughout that dynamic light scattering (DLS) is a very useful corroboratory technique for characterization of these gold nanoparticles in addition to optical spectroscopy and TEM.