375 resultados para POLYMER-POLYMER INTERFACE


Relevância:

50.00% 50.00%

Publicador:

Resumo:

The dewetting process of thin polystyrene (PS) film on flat and stripe-patterned substrates is presented. Different dewetting processes were observed when the thin PS films annealed at above the glass transition temperature on these different kinds of substrates. The final dewetting on the flat substrate led to formation of polygonal liquid droplets, while on the stripe-patterned substrate, the droplets were observed to align at the centers of the stripes. A possible explanation for the dewetting process on the stripe-patterned substrate is proposed.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

This paper deals with the dynamic rheological behavior of polypropylene/polyamide6 (PP/PA6) uncompatibilized blends and those compatibilized with a maleic anhydride grafted PP (PP/PP-g-MAH/PA6). The terminal relaxation times of the blends predicted by the Palierne emulsion model were compared with those obtained from experimental relaxation time spectra. The Palierne model succeeded well in describing PP/PA6 uncompatibilized blends with relatively low dispersed phase contents (10 wt%) and failed doing so for those of which the dispersed contents were high (30 wt%). It also failed for the compatibilized ones, irrespective of the dispersed phase content (10 or 30 wt%) and whether or not interface relaxation was taken into consideration. In the case of the uncompatibilized blend with high dispersed-phase content, interconnections among inclusions of the dispersed phase were responsible for the failure of the Palierne model. As for the compatiblized blends, in addition to particle interconnections, the existence of emulsion-in-emulsion (EE) structures was another factor responsible for the failure of Palieme model.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

The effects of the molecular weights (molecular weight of polystyrene, M-w,M-PS, varying from 2.9 to 129 k) on the surface morphologies of spin-coated and annealed polystyrene/poly (methyl methacrylate) (PS/PMMA = 50/50, w/w) blend films were investigated by atomic force microscopy and X-ray photoelectron spectroscopy. For the spin-coated films, when the M-w,M-PS varied from 2.9 to 129 k, three different kinds of surface morphologies (a nanophase-separated morphology, a PMMA cellular or network-like morphology whose meshes filled with PS, a sea-island like morphology) were observed and their formation mechanisms are discussed, respectively. Upon annealing, two different morphology-evolution processes were observed. It is found that a upper PS-rich phase layer is formed when M-w,M-PS < 4 k, and this behavior is mainly attributed to the low interfacial tension between PS and PMMA component. When M-w,M-PS > 4 k, the PS-rich phase forms droplets on top of the PMMA-rich phase layer which wets the SiOx substrate. These results indicate that the surface morphology of the polymer blend films can be controlled by the polymer molecular weight and annealing conditions.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

Stable monolayer of polyaniline doped with camphor sulfonic acid at the air-water interface has been obtained and has been successfully deposited by Langmuir-Blodgett technique onto CaF2 substrate. IR and UV-Vis-NIR spectra show that the doped molecules dedoped partially from the PANI backbone during the monolayer compression or deposition. Gas-sensing measurement indicates that the doped polyaniline LB film was sensitive to ethanol vapor at room temperature.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

Individual hydrophobically modified ethyl hydroxyethyl cellulose (HM-EHEC) molecules under different conditions were elongated using a new atomic force microscope (AFM) based technique-single-molecule force spectroscopy (SMFS). The critical concentration of HM-EHEC for micelle-like clusters at a solid/liquid interface was around 0.8 wt %, which is lower than that in solution. The different mechanical properties of HM-EHEC below and above the critical concentration were displayed on force-extension curves. Through a comparison with unmodified hydroxyethyl cellulose, substituent-induced effects on nanomechanical features of HM-EHEC were investigated. Because of hydrophobic interactions and cooperative binding with the polymer, surfactants such as sodium dodecyl sulfate (SDS) dramatically influence the elastic properties of HM-EHEC below the critical concentration, and further addition of SDS reduces the interactions between the hydrophobic groups and the surfactant.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

A composite solid polymer electrolyte (SPE) of (PEO)(10)LiClO4-Al2O3 was prepared and Pt and stainless steel(SS) blocking electrodes were used for an impedance study. It was found that the semicircle in the high frequency range and the straight line in the low frequency range depend upon different blocking electrodes and polarization potentials applied in the experiments. In the equivalent circuit. two constant phase elements (CPE) have been used instead of the pure geometrical and double layer capacitances. respectively. A theoretical line calculated from their estimated values has a good correlation with the experiment data. Moreover. the equivalent circuit also can be used to explain the impedance properties of Pt and stainless steel (SS) blocking electrodes both in the high and the low frequency ranges. (C) 2001 Elsevier Science Ltd. All rights reserved.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

This paper presents a microelectrode voltammetric determination of heterogeneous electron transfer rate constants (k(s)) and diffusion coefficients (D) of 7,7,8',8 '-tetracyanoquinodimethane (TCNQ) in polyelectrolytes. The diffusion coefficients are estimated using cyclic voltammetry under linear diffusion conditions, and the heterogeneous electron transfer rate constants are obtained under mixed linear and radial diffusion in the polyelectrolyte. k(s) and D increase with increasing temperature, and the activation barriers of the electrode reaction for reduction of TCNQ are obtained. On the other hand, the dependencies of D and k(s) of TCNQ on the size and charge of the counterion are compared in the polyelectrolyte. (C) 1998 Elsevier Science Ltd. All rights reserved.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

The heterogeneous electron transfer rate constants (k(s)) of seven ferrocene derivatives were estimated using cyclic voltammograms under mixed spherical/semi-infinite linear diffusion and steady-state voltammetry at a microdisk electrode in polymer electrolyte. The k(s) and diffusion coefficient (D) are both 100 to 1000-fold smaller in polymer solvent than in monomeric solvents, and the D and k(s) decrease with increasing polymer chain length. The results conform to the difference of viscosity (eta) or relaxation time (tau(L)) for these different solvents. The k(s) and D increase with increasing temperature, and the activation barriers of the electrode reaction are obtained. The influences of the substituting group in the ferrocene ring on k(s) and D are discussed. The k(s) are proportional to the D of the ferrocene derivatives, which indicates that solvent dynamics control the electrode reaction. (C) 1998 Elsevier Science S.A.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

compatibilizing effect of graft copolymer, linear low density polyethylene-g-polystyrene (LLDPE-g-PS), on immiscible blends of LLDPE with styrene-butadiene-styrene triblock copolymer (SBS) has been investigated by means of C-13 CPMAS n.m.r. and d.s.c. techniques. The results indicate that LLDPE-g-PS is an effective compatibilizer for LLDPE/SBS blends. It was found that LLDPE-g-PS chains connect two immiscible components, LLDPE and SBS, through solubilization of chemically identical segments of LLDPE-g-PS into the amorphous region of LLDPE acid PS block domain of SBS, respectively. It was also found that LLDPE-g-PS chains connect the crystalline region of LLDPE by isomorphism, with serious effects on the supermolecular structure of LLDPE. The effect of LLDPE-g-PS on the supermolecular structure of LLDPE in the LLDPE/SBS blends obviously depends on the composition of the blends, but has little dependence on the PS grafting yields of LLDPE-g-PS. (C) 1998 Elsevier Science Ltd. All rights reserved.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

The compatibilizing effect of graft copolymer, linear low density polyethylene-g-polystyrene (LLDPE-g-PS), on immiscible LLDPE/PS blends has been studied by means of C-13 CP-MAS NMR and DSC techniques. The results indicate that LLDPE-g-PS is an effective compatibilizer for LLDPE/PS blends, and the compatibilizing effect of LLDPE-g-PS on LLDPE/PS blends depends on the PS grafting yield and molecular structure of the compatibilizers and also on the composition of the blends. It was found that LLDPE-g-PS chains connect two immiscible components, LLDPE and PS, through solubilization of chemically identical segments of LLDPE-g-PS into the noncrystalline region of the LLDPE and PS domain, respectively. Meanwhile, LLDPE-g-PS chains connect the crystalline region of LLDPE by isomorphism, resulting in an obvious change in the crystallization behavior of LLDPE. (C) 1996 John Wiley & Sons, Inc.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

In order to characterize the interface in polymer blends, a new method is suggested, in which the interface is exposed by selectively dissolving in solvent. By means of X-ray photoelectron spectrometry, we studied the molecular state in the interfacial ar

Relevância:

50.00% 50.00%

Publicador:

Resumo:

The ultra-thin modified PEO (polyethylene oxide)-LiClO4 polymer electrolyte film (50-mu-m) was obtained by solution-casting technique. Impedance spectra were taken on the cells consisting of above PEO film electrolyte and ion-blocking or nonblocking electrodes. The ambient conductivity as high as 1.33 X 10(-4)S cm-1 could be achieved for PEO electrolyte modified by the crosslinking. It was shown that the resistance at the interface between solid polymer electrolyte and lithium electrode is growing with increasing the storage time. At high temperature, as 96-degrees-C, the ionic transport is clearly controlled by diffusion.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

We present a good alternative method to improve the tribological properties of polymer films by chemisorbing a long-chain monolayer on the functional polymer surface. Thus, a novel self-assembled monolayer is successfully prepared on a silicon substrate coated with amino-group-containing polyethyleneimine (PEI) by the chemical adsorption of stearic acid (STA) molecules. The formation and structure of the STA-PEI film are characterized by means of contact-angle measurement and ellipsometric thickness measurement, and of Fourier transformation infrared spectrometric and atomic force microscopic analyses. The micro- and macro-tribological properties of the STA-PEI film are investigated on an atomic force microscope (AFM) and a unidirectional tribometer, respectively. It has been found that the STA monolayer about 2.1-nm thick is produced on the PEI coating by the chemical reaction between the amino groups in the PEI and the carboxyl group in the STA molecules to form a covalent amide bond in the presence of N,N'-dicyclohexylcarbodiimide (DCCD) as a dehydrating regent. By introducing the STA monolayer, the hydrophilic PEI polymer surface becomes hydrophobic with a water contact angle to be about 105degrees. Study of the time dependence of the film formation shows that the adsorption of PEI is fast, whereas at least 24 h is needed to generate the saturated STA monolayer. Whereas the PEI coating has relatively high adhesion, friction, and poor anti-wear ability, the STA-PEI film possesses good adhesive resistance and high load-carrying capacity and anti-wear ability, which could be attributed to the chemical structure of the STA-PEI thin film. It is assumed that the hydrogen bonds between the molecules of the STA-PEI film act to stabilize the film and can be restored after breaking during sliding. Thus, the self-assembled STA-PEI thin film might find promising application in the lubrication of micro-electromechanical systems (MEMS).

Relevância:

40.00% 40.00%

Publicador:

Resumo:

In this paper, the rigid particle filled polymer is studied in the hope to understand the real damage mechanisms. Two damage parameters were introduced and measured. One is the macro-damage of the materials calculated from the modulus measured, another is micro-damage describing the interfacial debonding or the percentage of the particle debonded from the matrix. The damage rate of the macro damage decreases, while the micro damage increases with the applied stress.