107 resultados para ISOTHERMAL TUBES
Isothermal Kinetics Modelling of the Fischer-Tropsch Synthesis over the Spray-Dried Fe-Cu-K Catalyst
Resumo:
A method of loop-mediated isothermal amplification (LAMP) was employed to develop a rapid and simple detection system for porcine circovirus type 2 (PCV2). The amplification could be finished in 60 min under isothermal condition at 64 degrees C by employing a set of four primers targeting the cap gene of PCV2. The LAMP assay showed higher sensitivity than the conventional PCR, with a detection limit of five copies per tube of purified PCV2 genomic DNA. No cross-reactivity was observed from the samples of other related viruses including porcine circovirus type 1 (PCV1), porcine parvovirus (PPV), porcine pseudorabies virus (PRV) and porcine reproductive and respiratory syndrome virus (PRRSV). The detection rate of PCV2 LAMP for 86 clinical samples was 96.5% and appeared greater than that of the PCR method. The LAMP assay reported can provide a rapid yet simple test of PCV2 suitable for laboratory diagnosis and pen-side detection due to ease of operation and the requirement of only a regular water bath or heat block for the reaction. (c) 2008 Elsevier B.V. All rights reserved.
Resumo:
The effect of adding internal fins to the injection tube of a storage cell target filled with a polarized atomic beam source has been studied. The tube conductance and the atomic beam intensity at the exit of the injection tube have been measured, observing an unexpectedly large beam loss. Simulations of the atomic beam reproduce the observed attenuation only when the non-zero azimuthal component of the atom's velocity is taken into account.
Resumo:
In order to study the gas-phase chemical behavior of transactinides, an on-line isothermal chromatography apparatus has been developed and applied to separate short-lived technetium isotopes in the form of TcO3 from fission products. The fission products from a Cf-252 source were continuously and rapidly transported through the capillary to the isothermal chromatography apparatus using the N-2/KBr gas-jet techniques. Volatile oxide molecules were formed at the reaction zone kept at 900 degrees C since a trace amount of oxygen existed in the N-2 carrier gas. With the new developed isothermal chromatography apparatus, a selective separation of Tc from fission products was achieved. After isothermal chromatographic separation, Tc-101,Tc-103,Tc-104,Tc-105,Tc-106,Tc-107,Tc-108 were dominantly observed together with their Ru daughters in the gamma-spectrum, The chemical yields of Tc-101, and Tc-104 and Tc-105 isotopes with longer half-lives are about 55-57%, and those of Tc-103, Tc-106 and Tc-108 isotopes with shorter half-lives dropped down to 25-28%. The adsorption enthalpy of the investigated compounds on quartz surfaces was determined to be -150 +/- 5 kJ/mol by fitting the measured retention curves with a Monte Carlo model. The observed species of technetium oxide is attributed to TcO3, which is in good agreement with previous experimental results. That means our system worked properly and it can be used to investigate the gas-phase chemical behavior of transactinides.
Resumo:
We have successfully achieved the integration of isothermal amplification and the subsequent analysis of specific gene fragments on poly(methyl methacrylate) microchips. In our experiments, loop-mediated isothermal amplification, which can offer higher specificity and efficiency than PCR, has been performed at a constant temperature (65 degreesC). After amplification, products could be either examined by the integrated microchip-based electrophoresis or directly observed by naked eye with SYBR Green I added into the reaction solution. By such an integrated microsystem, the amplification and the subsequent analysis of prostate-specific antigen gene with template concentration at 23 fg/muL could be finished within 15 min, which demonstrates its advantages of high specificity, good reproducibility, and fast speed in gene detection.
Resumo:
We produced silver tubes with an outer diameter of 1 mu m, wall thickness of 200 nm, and length of hundreds of micrometers by hydrothermal treatment of aqueous solutions of AgNO3 and hyperbranched polyglycidol (HPG) at 165 degrees C. The surfaces of the silver tubes were chemically modified by HPG, which was confirmed by FTIR of the silver tubes.
Resumo:
Single-crystal tubular products on the millimetre scale have been synthesized from water-soluble calixarene and phenanthroline in the presence of lanthanides by a hydrothermal method, in which the extended structures contain some 1D infinite channels.
Resumo:
The isothermal crystallization behavior of poly(L-lactic acid)/organo-montmorillonite nanocomposites (PLLA/OMMT) with different content of OMMT, using a kind of twice-functionalized organoclay (TFC), prepared by melt intercalation process has been investigated by optical depolarizer. In isothermal crystallization from melt, the induction periods (t(i)) and half times for overall PLLA crystallization (100 degrees C <= T-c <= 120 degrees C) were affected by the temperature and the content of TFC in nanocomposites. The kinetic of isothermal crystallization of PLLA/TFC nanocomposites was studied by Avrami theory. Also, polarized optical photomicrographs supplied a direct way to know the role of TFC in PLLA isothermal crystallization process. Wide angle X-ray diffraction (WAXD) patterns showed the nanostructure of PLLA/TFC material, and the PLLA crystalline integrality was changed as the presence of TFC. Adding TFC led to the decrease of equilibrium melting point of nanocomposites, indicating that the layered structure of clay restricted the full formation of crystalline structure of polymer.
Resumo:
The ageing behavior of an extruded Mg-7Y-4Gd-0.5Zn-0.4Zr alloy during ageing at 250 degrees C has been investigated. Two types of phases have been observed during the ageing process. One is a lamellar phase with a 14H long periodic stacking structure, the other is the beta' phase with an ellipsoidal morphology. The increased mechanical properties of the peak-aged alloy are mainly ascribed to the presence of both of these phases at peak hardness.
Resumo:
A simple way to synthesize beta-Ga2O3 nanoribbons and tubes by electrospinning is introduced. The diameters of the electrospun fibers range from 150 nm to 2.5 mu m and their lengths reach up to several millimeters. The relationship among precursors, precursor concentrations, and crystal growth of beta-Ga2O3 nanoribbons and tubes are discussed. The structures of beta-Ga2O3 fibers have been investigated by various methods such as thermogravimetric (TG) and differential thermal analysis (DTA), X-ray diffraction, FT-IR, Raman spectra, scanning electron micrograph (SEM), and transmission electron micrograph (TEM).
Resumo:
Non-isothermal crystallisation kinetics of a polyamide 6/mesoporous silica nanocomposite (PA6-MS) has been investigated by differential scanning calorimetry (DSC) at different cooling rates. Mandelkern, Jeziorny-Ziabicki and Ozawa methods were applied to describe this crystallisation process. The analyses show that the mesoporous silica particles act as nucleating agents in the composite and that the Avrami exponent n varies from 3.0 to 4.6. The addition of mesoporous silica influenced the mechanism of nucleation and the growth of polyamide 6 (PA6) crystallites.
Resumo:
In this paper, the isothermal crystallization kinetics of polypropylene (iPP) during self-nucleation was studied by means of differential scanning calorimetry(DSC). The iPP was melted at 438 K and then isothermally crystallized in the range of temperature between 421 and 425 K. The mechanism of nucleation and growth of iPP was discussed. The Avrami equation was applied to analyzing the process of isothermal crystallization of iPP from the melt. The average value of Avrami exponent is n=3.01, suggesting that the primary crystallization maybe corresponds to three-dimensional spherulitic growth. The K-g value obtained from Lauritzen-Hoffman equation is 1.128 X 10(5) K-2, which suggests that crystallization species should be regime I. The decrease of crystallization active energy and chain folding work indicates that the self-nucleation can greatly promote the overall crystallization of iPP.