123 resultados para Fabrication technique
Resumo:
High efficiency AlxGa1-xAs/GaAs heteroface solar cells have been fabricated by an improved multi-wafer squeezing graphite boat liquid phase epitaxy (LPE) technique, which enables simultaneous growth of twenty 2.3 X 2.3cm(2) epilayers in one run. A total area conversion efficiency of 17.33% is exhibited (1sun, AM0, 2.0 x 2.0cm(2)). The shallow junction cell shows more resistance to 1 MeV electron radiation than the deep one. After isochronal or isothermal annealing the density and the number of deep level traps induced by irradiation are reduced effectively for the solar cells with deep junction and bombardment under high electron fluences.
Resumo:
Silicon crystal-facet-dependent nanostructures have been successfully fabricated on a (100)-oriented silicon-on-insulator wafer using electron-beam lithography and the silicon anisotropic wet etching technique. This technique takes ad-vantage of the large difference in etching properties for different crystallographic planes in alkaline solution. The mini-mum size of the trapezoidal top for those Si nanostructures can be reduced to less than 10nm. Scanning electron microscopy(SEM) and atomic force microscopy (AFM) observations indicate that the etched nanostructures have controllable shapes and smooth surfaces.
Resumo:
A new technique to fabricate silicon condenser microphone is presented. The technique is based on the use of oxidized porous silicon as sacrificial layer for the air gap and the heavy p~+-doping silicon of approximately 15μm thickness for the stiff backplate. The measured sensitivity of the microphone fabricated with this technique is in the range from -45dB (5.6mV/Pa) to -55dB (1.78mV/Pa) under the frequency from 500Hz to 10kHz, and shows a gradual increase at high frequency. The cut-off frequency is above 20kHz.
Resumo:
In this work, the formation and characterization of nano-sized grains on the modified surfaces of GCr15 and H13 steels have been investigated. The material was processed by pulsed laser surface melting (LSM) under different depths of de-ionized water. The microstructures and phases of the melted zones were examined by x-ray diffraction, environmental field emission scanning electron microscopy and high resolution transmission electron microscopy. The results indicate that LSM under water can successfully fabricate nano-scaled grains on the surfaces of steel, due to the rapid solidification and crystallization by heterogeneous nucleation. The elemental segregation of chromium and activated heterogeneous nucleation mechanism of austenite in liquid metal play a key role in the formation of nano-sized grains at high cooling rates. This one-step technique provides us a new way to prepare uniform nano-scaled grains, and is of great importance for further understanding the growth of nano-materials under extreme conditions.
Resumo:
A novel cemented carbides (W0.7Al0.3)C-0.65-Co with different cobalt contents were prepared by solid-state reaction and hot-pressing technique. Hot-pressing technique as a novel technique was performed to fabricate the bulk bodies of the hard alloys. The novel cemented carbides have superior mechanical properties compared with WC-Co. The density, operate cost of the novel material were lower than WC-Co system. The novel materials were easy to process nanoscale sintering and get the rounded particles in the bulk materials. There is almost no eta-phase in the (W0.7Al0.3)C-0.65-Co cemented carbides system although the carbon deficient get the astonished 35% value.
Resumo:
A novel cemented carbides (W0.5Al0.5)C-0.8-Co with different cobalt contents were prepared by mechanical alloying and hot-pressing technique. Hot-pressing technique as a common technique was performed to fabricate the bulk bodies of the hard alloys. The novel cemented carbides have superior mechanical properties compared to WC-Co. The density, operating cost of the novel material were much lower than WC-Co. There is almost no eta-phase in the (W0.5Al0.5)C-0.8-Co cemented carbides system although the carbon deficient get the value of 20%, and successfully got the nanostructured rounded (W0.5Al0.5)C-0.8 particles.
Resumo:
A method to synthesize Fe3O4 core/Au shell submicrometer structures with very rough surfaces on the nanoscale is reported. The Fe3O4 particles were first modified with uniform polymers through the layer-by-layer technique and then adsorbed a lot of gold nanoseeds for further Au shell formation. The shell was composed of a large number of irregular nanoscale An particles arranged randomly, and there were well-defined boundaries between these Au nanoparticles. The Fe3O4 core/Au shell particles showed strong plasmon resonance absorption in the near-infrared range, and can be separated quickly from solution by an external magnet.
Resumo:
In this article, a novel technique for the fabrication of surface enhanced Raman scattering (SERS) active silver clusters on glassy carbon (GC) has been proposed. It was found that silver clusters could be formed on a layer of positively charged poly(diallyldimethylammonium) (PDDA) anchored to a carbon surface by 4-aminobenzoic acid when a drop containing silver nanoparticles was deposited on it. The characteristics of the obtained silver clusters have been investigated by atomic force microscopy (AFM), SERS and an SERS-based Raman mapping technique in the form of line scanning. The AFM image shows that the silver clusters consist of several silver nanoparticles and the size of the clusters is in the range 80-100 nm. The SERS spectra of different concentrations of rhodamine 6G (R6G) on the silver clusters were obtained and compared with those from a silver colloid. The apparent enhancement factor (AEF) was estimated to be as large as 3.1 x 10(4) relative to silver colloid, which might have resulted from the presence of 'hot-spots' at the silver clusters, providing a highly localized electromagnetic field for the large enhancement of the SERS spectra of R6G. The minimum electromagnetic enhancement factor (EEF) is estimated to be 5.4 x 10(7) by comparison with the SERS spectra of R6G on the silver clusters and on the bare GC surface.
Resumo:
A novel cemented carbides alloy (W0.4Al0.6)C-0.65-Co were prepared by mechanical alloying and hot-pressing sintering in this work. Hot-pressing (HP) as a common technique was performed to fabricate the bulk bodies of the hard alloys. The hardness, bending strength, density of the novel hard alloy are also tested, and it has superior mechanical properties. The hardness of (W0.4Al0.6)C-0.65-Co hard alloy was very high, and the density, operate cost of the novel material were much lower than WC-Co, more important is the aluminum dissolving is not decrease the strength compared with the WC-Co system. There is almost no eta-phase in the (W0.4Al0.6)C-0.65-Co cemented carbides system even the carbon deficient reaches the astonishing value of 35%. This novel property will give us more choice to design and gain new materials that we needed.
Resumo:
X-2-y(2)SiO(5):A (A = Eu3+, Tb3+, Ce3+) phosphor films and their patterning were fabricated by a sol-gel process combined with a soft lithography. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), atomic force microscopy (AFM), scanning electron microscopy (SEM) optical microscopy and photoluminescence (PL) were used to characterize the resulting films. The results of XRD indicated that the films began to crystallize at 900 degreesC with X-1-Y2SiO5, which transformed completely to X-2-Y2SiO5 at 1250 degreesC. Patterned thin films with different band widths (5 pin spaced by 5 pm and 16 pm spaced by 24 pm) were obtained by a soft lithography technique (micromoulding in capillaries, MIMIC). The SEM and AFM study revealed that the nonpattemed phosphor films were uniform and crack free, and the films mainly consisted of closely packed grains with an average size of 350 run. The doped rare earth ions (A) showed their characteristic emissions in X-2-Y2SiO5 phosphor films, i.e., D-5(0)-F-7(J) (J = 0, 1, 2,3,4) for Eu3+, D-5(3), (4)-F-7(J) (J = 6, 5, 4, 3) for Tb3+ and 5d (D-2)-4f (F-2(2/5),(2/7)) for Ce3+, respectively. The optimum doping concentrations for EU3+, Tb3+ were determined to be 13 and 8 mol% of Y3+ in X-2-Y2SiO5 films, respectively.
Resumo:
Three kinds of hybrid organic/inorganic Langmuir-Blodgett films are obtained by the compact organization of poly (1, 2-dihydro-2,2,4-trimethyl)quinoline (abridged as PQ), octadecylamine(abridged as OA) and rare earth-substituted heteropolyanions [abridged as RE(PW11,)(2), RE=Ce-II, Eu-II, Gd-II] using the Langmuir-Blodgett technique. They are characterized by the pi-A isotherms, the absorption spectra, the fluorescence spectra and the atomic force microscope. The scanning tunneling microscopy shows that the conductivity of the hybrid LB films is much better after heteropolyanions having been incorporated in the films.
Resumo:
Three kinds of hybrid Langmuir-Blodgett films are obtained by the organization of poly(1-hydro-2,2,4-trimethyl)quinoline (PQ), stearic acid(SA) and rare earth-substituted heteropolymolybdates (RE(PMo11)(2), RE = Ce-III, Eu-III, La-III) using the Langmuir-Blodgett technique. They are characterized by pi-A isotherms, absorption spectra, fluorescence spectra, IR and atomic force microscope. The absorption spectra indicate that the molecules of PQ and heteropolymolybdates are incorporated into the LB films. The atomic force microscope reveals that heteropolymolybdates aggregate at the surface of the LB film.
Resumo:
Magnetic luminescent nanocomposites were prepared via a layer-by-layer (LbL) assembly approach. The Fe3O4 magnetic nanoparticles of 8.5 nm were used as a template for the deposition of the CdTe quantum dots (QDs)/polyelectrolyte (PE) multilayers. The number of polyelectrolyte multilayers separating the nanoparticle layers and the number of QDs/ polyelectrolyte deposition cycles were varied to obtain two kinds of magnetic luminescent nanocomposites, Fe3O4/PEn/CdTe and Fe3O4/(PE3/CdTe)(n), respectively. The assembly processes were monitored through microelectrophoresis and UV-vis spectra. The topography and the size of the nanocomposites were studied by transmission electron microscopy. The LbL technique for fabricating magnetic luminescent nanocomposites has some advantages to tune their properties. It was found that the selection of a certain number of the inserted polyelectrolyte interlayers and the CdTe QDs loading on the nanocomposites could optimize the photoluminescence properties of the nanocomposites. Furthermore, the nanocomposites could be easily separated and collected in an external magnetic field.
Resumo:
A sol-gel technique was used to prepare Gd2Ti2O7:Eu3+-coated submicron silica spheres (SiO2@Gd2Ti2O7:Eu3+). The resulted SiO2@Gd2Ti2O7:Eu3+ core-shell particles were characterized by x-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), scanning electron microscopy (SEM), energy-dispersive x-ray spectra (EDS), transmission electron microscopy (TEM), photoluminescence (PL) spectra, as well as kinetic decays. The XRD results demonstrate that the Gd2Ti2O7:Eu3+ layers begin to crystallize on the SiO2 spheres after annealing at 800 degrees C and the crystallinity increases with raising the annealing temperature. The obtained core-shell phosphors have perfect spherical shape with narrow size distribution (average size similar to 620 nm), non-agglomeration, and smooth surface. The thickness of the Gd2Ti2O7:Eu3+ shells on the SiO2 cores could be easily tailored by varying the number of deposition cycles (60 nm for four deposition cycles). Under the irradiation of 310 nm ultraviolet, the SiO2@GdTi2O7:Eu3+ samples show strong emission of Eu3+.
Resumo:
Ce3+ and/or Tb3+-doped LaPO4 nanocrystalline thin films and their patterning were fabricated by a sol-gel process combined with soft lithography on silicon and quartz glass substrates. The results of XRD indicated that the films began to crystallize at 700 degreesC. The 1000 degreesC annealed single layer films are transparent by eyes, uniform and crack-free with a thickness of about 200 nm and an average grain size of 100 nm. Patterned thin film with different band widths (5-50 mum) were obtained by micro-molding in capillaries technique. The luminescence and energy transfer properties of Ce3+ and Tb3+ were studied in LaPO4 films.