307 resultados para Glass-workers
Resumo:
The effects of crystallization temperature (T,), glass bead content and its size on the, formation of beta-crystal and structural stability of originally formed beta-crystal in glass bead filled polypropylene (PP) were examined. The differential scanning calorimetry (DSC) measurements indicated that the amount of beta-phase in PP crystals was a function of the crystallization temperature and glass bead content. For a constant crystallization temperature, it was observed that the amount of beta-crystal initially increased with increase in glass bead content up to 30 wt.%, and then decreased slightly with further increase in the filler content. From the DSC data, a disorder parameter (S) was derived to define the structural stability of originally formed beta-crystals. The structural stability of originally formed beta-crystals was enhanced with increase in either the crystallization temperature or the glass bead content. Also, the influence of glass bead size (4-66 mu m) on the formation and stability of beta-crystals in PP/glass bead blends was studied. Large glass bead particles suppressed the formation and decreased the stability of beta-crystals.
Resumo:
The effects of the glass-bead content and size on the nonisothermal crystallization behavior of polypropylene (PP)/glass-bead blends were studied with differential scanning calorimetry. The degree of crystallinity decreased with the addition of glass bead, and the crystallization temperature of the blends was marginally higher than that of pure PP at various cooling rates. Furthermore, the half-time for crystallization decreased with an increase in the glass-bead content or particle size, implying the nucleating role of the glass beads. The nonisothermal crystallization data were analyzed with the methods of Avrami, Ozawa, and Mo. The validity of various kinetic models for the nonisothermal crystallization process of PP/glass-bead blends was examined. The approach developed by Mo successfully described the nonisothermal crystallization behavior of PP and PP/glass-bead blends. Finally, the activation energy for the nonisothermal crystallization of pure PP and PP/glass-bead blends based on the Kissinger method was evaluated.
Resumo:
Glass beads were used to improve the mechanical and thermal properties of high-density polyethylene (HDPE). HDPE/glass-bead blends were prepared in a Brabender-like apparatus, and this was followed by press molding. Static tensile measurements showed that the modulus of the HDPE/glass-bead blends increased considerably with increasing glass-bead content, whereas the yield stress remained roughly unchanged at first and then decreased slowly with increasing glass-bead content. Izod impact tests at room temperature revealed that the impact strength changed very slowly with increasing glass-bead content up to a critical value; thereafter, it increased sharply with increasing glass-bead content. That is, the lzod impact strength of the blends underwent a sharp transition with increasing glass-bead content. It was calculated that the critical interparticle distance for the HDPE/glass-bead blends at room temperature (25degreesC) was 2.5 mum. Scanning electron microscopy observations indicated that the high impact strength of the HDPE/glass-bead blends resulted from the deformation of the HDPE matrix. Dynamic mechanical analyses and thermogravimetric measurements implied that the heat resistance and heat stability of the blends tended to increase considerably with increasing glass-bead content.
Resumo:
The pressure-dependent glass-transition temperatures (T-g's) of poly(methyl methacrylate) (PMMA)/poly(styrene-co-acrylonitrile) (SAN) blends were determined by pressure-volume-temperature (PVT) dilatometry via an isobaric cooling procedure. The Gordon-Taylor and Fox equations were used to evaluate the relationships between the T-g's and compositions of the PMMA/SAN system at different pressures. The relationships were well fitted by the Gordon-Taylor equation, and the experimental data for T-g positively deviated from the values calculated with the Fox equation. Also, the influence of the cooling rate (during the PVT measurements) on T-g was examined.
Resumo:
Tapping mode atomic force microscopy (AFM) was applied to study the adsorption behavior of methanol on mica, highly oriented pyrolytic graphite (HOPG) and indium-tin oxide (ITO) coated glass substrates. On mica and HOPG substrates surfaces, the thin films of methanol with bilayer and multilayer were observed, respectively. The formation of irregular islands of methanol was also found on HOPG surface. On ITO surface only aggregates and clusters of methanol molecules were formed. The influence of sample preparation on the adsorption was discussed.
Resumo:
Multi-color LLP phenomenon was observed in Mn2+-doped ZnO-B2O3-SiO2 glassceramics after the irradiation of a UV lamp at room temperature. Transparent ZnO-B2O3-SiO2 glass emitted reddish LLP while opaque glass-ceramics prepared by the glass sample after heat treatment emitted yellowish or greenish LLP. The change of the phosphorescence is due to the alteration of co-ordination state of Mn2+. The phosphorescence of the samples was seen in the dark with naked eyes even 12 h after the irradiation with a UV lamp (lambda(max) = 254 nm) for 30 min. Based on the approximative t(-1) decay law of the phosphorescence, we suggest that the LLP is attributed to the thermally assisted electron-hole recombination.
Resumo:
Electrocatalytic reduction of O-2 and H2O2 at the glass carbon electrode modified with microperoxidase-11 immobilized with Nafion film has been studied by means of cyclic voltammetry and rotating disk electrode techniques. The modified electrode shows high catalytic activity toward the reduction of both O-2 and H2O2. The rate constants of Oz and H2O2 reduction at the modified electrode have been measured and compared. It is found that O-2 undergoes a four-electron reduction at the modified electrode and the catalytic activity for the reduction of O-2 is dependent on the pH of the solutions.
Resumo:
The effect of entanglements on the glass transition and structural relaxation behaviors has been studied for polystyrene (PS) and phenolphthalein poly(ether sulfone) (PES-C) samples by fast evaporation of the solution of concentrations varying from above the overlapping concentration to far below it, and compared to the results we have studied previously in PC. It has been found that for all the polymers we have studied, in the concentrated solution region, the T-g of the samples obtained from solution are independent of the change of concentration and are very close to that of normal bulk samples, whereas in the dilute solution region the T-g of the samples decrease with the logarithm of decreasing concentration. The critical concentrations that divide the two distinct regions for the three polymers are 0.9% g/mL for PC, 0.1% g/mL for PS, and 1% g/mL for PES-C. The decrease of T-g of the samples is interpreted by the decrease of intermolecular entanglements as the isolation of polymer chains, and the entanglement of polymer chains restrained the mobility of the segments. The structural relaxation behavior of the polymers is also found to be different from that of normal bulk samples. The enthalpies of single-chain samples are lower than that of the bulk ones, which correspond to the lower glass transition temperature; the peaks are lower and broader, and the relaxed enthalpy is much lower as compared to that of bulk samples. In the three polymers we have studied, the influence of change of entanglements on both the decrease in glass transition temperature and relaxed enthalpy is the most significant for PS and the least for PES-C. It is indicated that the interactions in the flexible polymers are weak; thus, the restraint of the entanglements on the mobility of the segments plays a more important role in the flexible polymers, and the change of entanglement in the flexible polymers has a more significant influence on the physical properties.
Resumo:
Facilitated proton transfer across the water/1,2-dichloroethane (DCE) interface supported on the tips of micro- and nano-pipets by o-phenanthroline (Phen) was studied by using cyclic voltammetry. The formed micro- and nano-liquid/liquid interfaces functioned as micro- and nano-electrodes under certain experimental conditions. The dependence of the half-wave potentials on the aqueous solutions acidities was studied and the ratio of association constants between Phen and proton in the aqueous and DCE phases was calculated by the method proposed by Matsuda et al.. The standard rate constant (k(0)) and the transfer coefficient (alpha) evaluated by using nano-pipets were equal to 0.183 +/- 0.054 cm/s and 0.70 +/- 0.09, respectively.
Resumo:
The toughness of high-density polyethylene (HDPE)/glass-bead blends containing various glass-bead contents as a function of temperature was studied. The toughness of the blends was determined from the notch Izod impact test. A sharp brittle-ductile transition was observed in impact strength-interparticle distance (ID) curves at various temperatures. The brittle-ductile transition of HDPE/glass-bead blends occurred either with reduced ID or with increased temperature. The results indicated that the brittle-ductile-transition temperature dropped markedly with increasing glass-bead content. Moreover, the correlation between the critical interparticle distance (ID.) and temperature was obtained. Similar to the ID, of polymer blends with elastomers, the ID, nonlinearly increased with increasing temperature. However, this was the first observation of the variation of the ID, with temperature for polymer blends with rigid particles. (C) 2001 John Wiley & Sons, Inc. J Polym. Sci Part B: Polym. Phys 39: 1855-1859, 2001.
Resumo:
The glass transition temperatures (T-g) of PS/PPO blends with different compositions were studied under various pressures by means of a PVT-100 analyzer. A general relation of T-g and pressure of the PS/PPO system was deduced by fitting the experimental T-g's. Couchman volume-based equation was testified with the aid of those data. It was found that the experimental T-g's do not obey the Couchman equation of glass transition temperature based on thermodynamic theory. According to our studies, the major reason of the deviation is caused by the neglect of DeltaV(mix). (C) 2001 Published by Elsevier Science Ltd.
Resumo:
The synthesis and characterization of the mesoporous materials FSM-16 (folded sheets mesoporous materials) with highly ordered structure in open-vessel by using cetylpyridium bromide (CPBr) and the single-layered polysilica Kanemite as new template and silicon source, respectively, has been investigated systematically. The hexagonal arrangements of uniformly size pores were characterized by FTIR. XRD. nitrogen adsorption. TG-DTA. SEM and TEM. Especially, the porous products with higher surface areas show remarkable thermal stability up to 1000 C. The potential application as carrier of catalysts or host-guest materials is anticipated. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
We obtained the single-chain polycarbonate sample, by a new fast evaporation method and found that the polycarbonate sample obtained by this method is completely amorphous, while the polycarbonate sample obtained by other methods all have a certain degree of crystallinity. The glass transition temperature (T-g) of the sample decreases with the decreasing of concentration when the concentration of the prepared solution is below the critical value. The critical concentration we obtained from the T-g dependence of concentration is 0.9% g/mL and is in accord with that obtained by viscometry and light scattering methods directly from the solution. The structural relaxation behavior is found also different from that of a normal bulk sample of polycarbonate. The enthalpic peak of the single-chain sample is lower: than that of the bulk one, which corresponds to the lower glass transition temperature. The peak of the single-chain sample is lower and broader, and the relaxed enthalpy is much lower compared with that of the bulk sample. These results have been explained in terms of the effect of entanglement on the mobility of the segments in polymer and the compact conformation in the single-chain sample.