257 resultados para High refractive index


Relevância:

80.00% 80.00%

Publicador:

Resumo:

The changes in refractive indices (n(TE) and n(TM)) in a direction normal to the plane of thin films of an organo-soluble polyimide based on 1,4-bis(3,4-dicarboxyphenoxy) benzene dianhydride and 2,2'-dimethyl-4,4'-methylene dianiline were measured by a prism coupler. The results implied that the molecules near the substrate-polyimide interface were much ordered, while those near the polyimide-air interface were less ordered, judging from the variation in the level of negative birefringence with the depth of the films. The molecules are more condensed near the substrate surface, as seen by the average refractive index increasing from the polyimide-air interface to the substrate-polyimide interface, which implies that the condensed states of polyimide molecules change gradually in the depth direction. (C) 1997 Elsevier Science B.V.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Clinopyroxenes of the join CaMgSi2O6(diopside)-NaAlSi2O6 (jadeite) were synthesized in the temperature range 800-1900 degrees C and under varying pressure, 10-55 kbar. The stability regions of various compositions of diopside-jadeite have been established experimentally using different compositions of glass materials: stoichiometric composition NaAlSi2O6, 0.1CaMgSi(2)O(6)-0.9NaAlSi(2)O(6), 0.2CaMgSi(2)O(6)0.8NaAlSi(2)O(6), 0.3CaMgSi(2)O(6)-0.7NaAlSi(2)O(6), and 0.4CaMgSi(2)O(6)-0.6NaAlSi(2)O(6). Unit cell parameters of synthetic clinopyroxenes with the above compositions were determined. The physical properties, such as hardness, toughness, density, and refractive index, etc., were also measured. The results show that synthetic clinopyroxenes have the same properties as the natural one. The gem quality of diopside-jadeite clinopyroxenes was achieved by synthesised on the basis of the above experiments. Various colouring agents, such as Cr2O3, Co2O3, NiO2, Fe2O3, TiO2, MnO, CuO, and their combinations, FeO-Cr2O3, etc., were added to obtain the different colours of gem. In addition, small amounts of the rare-earth oxides, such as CeO2, Nd2O3, Sm2O3, Dy2O3, Eu2O3, Er2O3, Pr6O11, Lu2O3 and CuO-Eu2O3, Co2O3Nd2O3, etc., were also added to produce fluorescent clinopyroxenes for jewellery.