The thermal behaviour and ion-transport properties of a comb polymer electrolyte CP350/LiSCN based on methyl vinyl ether/maleic anhydride copolymer with oligo-oxyethylene side chains were studied by means of DSC and ac impedance method. The two glass transition temperatures which can be attributed to side chains and main chains respectively were found to increase with increasing salt concentration. Conductivities which displayed non-Arrhenius behaviour were analyzed by using Vogel-Tammann-Fulcher equation and interpreted on the basis of the configurational entropy model derived by Gibbs and coworkers. The optimum ionic conductivity at 25 degrees C achieved was 2.19x10(-5)S/cm.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A comb polymer (CP350) with oligo-oxyethylene side chains of the type -(CH2CH2O)(7)CH3 was prepared from methyl vinyl ether/maleic anhydride copolymer and poly(ethylene glycol) methyl ether. The polymer can dissolve LiNO3 salt to form homogeneous amorphous polymer electrolyte. This electrolyte system was first found to have two class glass transitions, and the two T(g)s were observed to increase with increasing salt content. The ionic conduction was measured by using the complex impedance method, and conductivities were investigated as functions of temperature and salt concentration. At 25 degrees C, the ionic conductivity maximum of this system can get to 3.72 X 10(-5) S/cm at the [Li]/ [EO] ratio of 0.057. The appearance of the conductivity maximum has been interpreted as being due to the effect of T-g and the so called physical crosslinks. The temperature dependence of the ionic conductivity displaying non-Arrhenius behaviour can be analyzed using the Vogel-Tammann-Fulcher equation and interpreted on the basis of the configurational entropy model.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A new amorphous comblike polymer (CBP) based on methylvinyl ether/maleic anhydride altering copolymer backbone and on oligooxyethylene side chain was synthesized. The dynamic mechanical properties of CBP and its Li salt complexes were investigated by means of DDV-11-EA type viscoelastic spectrometry. Results showed that there were two glass transitions (alpha-transition and beta-transition) in the temperature range from -100 to 100 degrees C. The beta-transition was assigned to oligo-PEO side chains and the temperature of beta-transition increases with increasing Li salt content. The alpha-transition was assigned to the main chain of CBP. The temperature of the alpha-transition (T-alpha) is also dependent upon the Li-salt content, but not monotonic. The value of T-alpha lies between 30-45 degrees C in the Li salt concentration range studied, near room temperature. It was found that the CBP-Li salt complexes showed an unusual dependence of ionic conductivity on Li salt content. There are two peaks in the plot of the ionic conductivity vs. Li salt concentration, which has been ascribed to the movability of the CBP main chain at ambient temperature. The temperature dependence bf the ionic conductivity indicated that the Arrhenius relationship was not obeyed, and the plot of log sigma against 1/(T - T-0) showed the unusual dual VTF behavior when using side chain glass transition temperature (T-beta) as T-0.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The viscoelastic behavior of phenolphthalein poly(ether ketone) (PEK-C) and its relationship to yielding was studied. The following phenomena were observed: (1) The relaxation behavior at strain near yield closely approximated that at low strain but near the T-g; (2) the temperature and strain rate dependence of yield stress could be modeled by the one-process Eyring theory and the value of the activation volume was the same as that of the glass transition; and (3) according to the Zhurkov-Bueche equation, the cu transition was related to the yield behavior. All these results indicated that the glass transition was the main factor that controlled the yield behavior. (C) 1996 John Wiley & Sons, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Poly(aryl ether ketone ketone)s (PEKK) was a high-performance engineering plastics, By means of Wide Angle X-ray Diffraction (WAXD) and Differential Scanning Calorimetry (DSC) methods, PEKK samples crystallized in solvent induction, from glass state and from melting state were studied, Crystal forms I and II for PEKK were found, The formation of crystal form II was dependent on thermal history and solvent induction, and this form II had melting point 10 degrees C or so lower than that of form I crystallized from glass state, All PEKK samples had low melting peaks which were relevant to the polarization of PEKK molecular chain, while they had nothing to do with thermal history, The heat of fusion for PEKK low melting peaks accounted for,percentage of 2 to 10 or so of the whole heat of fusion, And PEKK has its equilibrium melting point of 409 degrees C.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The microphase separation, glass transition and crystallization of two series of tetrahydrofuran-methyl methacrylate diblock copolymers (PTHF-b-PMMA), one with a given PTHF block of M(n) = 5100 and the other with a given PTHF block of (M) over bar(n) = 7000, were studied in this present work. In the case of solution-cast materials, the microphase separation of the copolymer takes place first, with crystallization then gradually starting in the formed PTHF microphase. The T-g of the PMMA microphase shows a strong dependence on the molecular weight of the PMMA block, while the T-g of the PTHF microphase shows a strong dependence on the copolymer composition. The non-isothermal crystallization temperature (T-c) of the diblock copolymer decreases rapidly and continuously with the increase in the amorphous PMMA weight fraction; the lowest T-c of the copolymer is ca. 35 K lower than the T-c of the PTHF homopolymer. There also exists a T-c dependence on the molecular weight of the PTHF block. In addition, when the major component of the copolymer is PMMA, a strong dependence of the crystallizability of the copolymer on the molecular weight of the PTHF block is observed; the higher the molecular weight, then the stronger its crystallizability. The melting temperature of the block copolymer is dependent on the copolymer composition and the molecular weight of its crystallizable block. Copyright (C) 1996 Elsevier Science Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The change in the microphase separation transition (MST) temperature of a styrene-butadiene-styrene (SBS) triblock copolymer induced by the addition of polystyrene (PS) was investigated by small-angle X-ray scattering. It was found that the transition temperature was determined from the molecular weight (M(H)) Of the added PS in relation to that of the corresponding blocks (M(A)) in the copolymer. The MST temperature decreased with added PS if M(H)/M(A) < 1/4, while it increased with added PS when M(H)/M(A) > 1/4 Analysis of the theoretical expression based on the random phase approximation showed exactly the same tendency of change in the transition temperatures as that observed experimentally. The interaction parameter, chi(SB), obtained by nonlinear fitting of the scattering profiles of SBS/PS blends in the disordered state, was found to be a function of temperature and composition. Composition fluctuations were found to exist in SBS/PS blends, increasing with increasing addition of PS but diminishing with increasing molecular weight of the added PS.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The conformational transition of horse heart cytochrome c induced by bromopyrogal red (BPR) in very low concentration has been firstly investigated by dynamic spectroelectrochemical technique, both at the BPR adsorbed platinum gauze electrode and at a bare platinum gauze electrode in a solution containing BPR. The effect of BPR on the structure of cytochrome c was studied by UV-visible and Fourier transform IR spectroscopy. The unfolded cytochrome c behaves simply as an electron transfer protein with a formal potential of -142 mV vs. a normal hydrogen electrode. The difference between the formal potentials of the native and unfolded cytochrome c is coupled to a difference in conformational energy of the two states of about 40 kJ mol(-1), which agrees well with the result reported. The stability and slow refolding of the unfolded cytochrome c are discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Ln(2)Mo(3)O(12) and Ce2Mo3O12.25 are reduced by hydrogen yielding Mo4+ oxides of the formula Ln(2)Mo(3)O(9) (Ln = La, Ce, Pr, Nd, Sm, Gd and Dy). The new compound Ce2Mo3O9 has the same structure as other Ln(2)Mo(3)O(9) compounds. All of the products are single phase materials and crystallize in a tetragonal scheelite type structure with Mo2O6 clusters. The IR spectra of the Ln(2)Mo(3)O(9) oxides show two absorption bands. These compounds are black n-type semiconductors, and exhibit Curie-Weiss Law behavior from 100K to 250K. Temperature dependence of the electrical properties of these compounds were measured for the first time, and a semiconductor-metal transition was found at about 250 degrees C.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Based on Jeziorny theory, the kinetics of phase transition of poly(ester-imide) has been determined under non-isothermal condition by using differential scanning calorimetry (DSC). Avrami exponent n, kinetic parameters G(c) and rate constant Z(c) were derived and discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effects of metal ions and lanthanide complexes on the gel-to-liquid crystal phase transition temperature T-m of dipalmitoylphosphatidylethanolamine liposomes have been studied by differential scanning calorimetry (DSC) method. The results show that the addition of metal ions to the dipalmitoylphosphatidylethanolamine (DPPE) liposomes dispersions increases the main phase transition temperature T-m in the order of monovalent< divalent< trivalent cations. The enhancement of T-m is not large as increasing the lanthanide ions concentration. The enhancement of Pr3+ is larger than that of La3+. Remarkable differences were observed between La-citrate and La-lactate complexes at different pH solutions. At pH 7.0, La-citrate complex has no effect on the T-m, La-lactate complex, however, increases the T-m value, and the increase is larger than that of free lanthanide ions at the same concentration. The decrease of pH of complexes solutions lowers the phase transition temperature. We have preliminarily discussed the mechanism of the enhancements of lanthanide ions and the synergism of lanthanide ion and lactate ligand follow the ion induced dehydration of lipid and the potential effects of ion-lipid interaction.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

It has been found that the interaction between the two transition metal Mn, Co ions on B-site and their Redox property an the important factors influencing the NO-selectivity in ammonia oxidation. The NO-selectivity is related to the redox ability of Mn3+

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The solid-solid phase transition of [n-C11H23NH3]2ZnCl4 Complex have been studied by Raman spectroscopy. The results show that the occurence of the structural phase transitions mainly related to the change of packing structure and molecular conformation o

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The glass transition behaviour, microphase separation morphology and crystallization of poly(vinyl alcohol)-g-poly(methyl methacrylate) graft copolymers (PVA-g-PMMA) were studied. A lamellar microphase separation morphology was formed, even for a copolyme