271 resultados para plant resin
Resumo:
Extraction resins, of the type of;levextrel, (which is a collective term for styrene/divinylbenzene based copolymers of predominantly macroporous structure that contain a selective extractant) are important for the recovery and separation of metal ions, as they combine features of solvent extraction and ion exchange resins. This paper presents the results of the adsorption of heavy rare earth ions (Ho(III), Er(III), Tm(III), Yb(III), Lu(III) and Y(III)) from hydrochloric acid solutions at 0.2 mol/L ionic strength and 50 degrees C by the extraction resin containing di (2,4,4-trimethyl pentyl) phosphinic acid (Cyanex 272) and the chromatographic separation of (Er(III), Tm(III) and Yb(III)). Technological separation products, with purity and yield of Tm2O3 >99.97%, >80%, Er2O3 >99.9%, >94% and Yb2O3 >99.8%, >80% respectively, have been obtained from a feed having the composition Tm2O3 60%, Er2O3 10%, and Yb2O3 3%, the others 27%. The distribution coefficients, extraction equilibrium constants and separation factors have been determined as a function of acidity, loading of the resin and rare earths, flow rates and column ratios. The resolutions and efficiencies of separation of Er/Tm/Yb each other have been calculated. The stoichiometry of the extraction of rare earth ions has been suggested as well.
Resumo:
Interpenetrating polymer networks (IPNs) have been synthesized from prepolymers that form miscible blends. All IPNs made from polyacrylate ((polyethylene glycol diacrylate), PEGDA) and epoxy (diglycidyl ether of bisphenol A, DGEBA) can be made in phase separated states by incorporating crosslinks. However, blends of these prepolymers, having a negative Flory-Huggins interaction parameter, are highly miscible. This indicates that formation of IPNs favours phase separation relative to blends. The microphase separation characteristics in the PEGDA/DGEBA IPNs were determined using smalt-angle X-ray scattering (SAXS). The Debye-Bueche and Guinier methods were used to calculate the correlation lengths of the segregated phases existing in the PEGDA/DGEBA IPNs. The results from SAXS showed that the size of the phase segregation zones changed with composition from about 50 to 100 Angstrom.
Resumo:
Three kinds of hydroxy-terminated oligomers were synthesized and characterized by IR, DSC and GPC. The oligomers were crosslinked by melaminealdehyde resin. The orientation and relaxation of the poled and crosslinked polymers were studied by UV-Vis spectra. It was shown that polymers had high orientational stability after corona-poling and crosslinking.
Resumo:
By examining the changes in melting temperature, heat of fusion, tensile strength and ultimate elongation at 150-degrees-C, and weight loss, radiation effects on perfluoroalkoxy resins (PFA) were investigated. The results show that at the temperatures used here the predominant effect caused by radiation on PFA is degradation of the molecular weight. The radiation stability is much better than that of polytetrafluoroethylene, however.
Resumo:
Phenolphthalein poly(ether ether sulphone) (PES-C) was found to be miscible with uncured bisphenol-A-type epoxy resin, i.e. diglycidyl ether of bisphenol A (DGEBA), as shown by the existence of a single glass transition temperature within the whole composition range. Miscibility between PES-C and DGEBA is considered to be due mainly to the entropy contribution. However, dynamic mechanical analysis (d.m.a.) and scanning electron microscopy (SEM) studies revealed that PES-C exhibits different miscibility with four cured epoxy resins (ER). The overall compatibility and the resulting morphology of the cured blends are dependent on the choice of cure agent. For the blends cured with amines (4,4'-diaminodiphenylmethane (DDM) and 4,4'-diaminodiphenylsulphone (DDS)), no phase separation occurs as indicated by either d.m.a. or SEM. However, for the blends cured with anhydrides (maleic anhydride (MA) and phthalic anhydride (PA)), both d.m.a. and SEM clearly show evidence of phase separation. SEM study shows that the two phases interact well in the MA-cured blend while the interface between the phases in the PA-cured blend is poorly bonded. The differences in the overall compatibility and the resulting morphology between the amine-cured and anhydride-cured systems have been discussed from the points of view of both thermodynamics and kinetics.
Resumo:
Dynamic mechanical analysis and scanning electron microscopy were used to study phase separation of three blends of anhydride-cure bisphenol-A-type epoxy resin with phenolphthalein poly(ether ether ketone). Phase separation was observed for all the blends. The overall compatibility and the resulting morphology of the cured blends are dependent on the choice of cure agent. The phenomena have been discussed from the points of view of both thermodynamics and kinetics. The effects of the choice of hardener on phase separation are considered to be primarily due to differences between the chemical natures of the hardeners.
Resumo:
Poly(ethylene oxide) (PEO) was found to be miscible with uncured epoxy resin, diglycidyl ether of bisphenol A (DGEBA), as shown by the existence of a single glass transition temperature (T(g)) in each blend. However, PEO with M(n) = 20 000 was judged to be immiscible with the highly amine-crosslinked epoxy resin (ER). The miscibility and morphology of the ER/PEO blends was remarkably affected by crosslinking. It was observed that phase separation in the ER/PEO blends occurred as the crosslinking progressed. This is considered to be due to the dramatic change in the chemical and physical nature of ER during the crosslinking.
Resumo:
The properties of miscible phenolphthalein poly(ether ether ketone)/phenoxy (PEK-C/phenoxy) blends have been measured by dynamic mechanical analysis and tensile testing. The blends were found to have single glass transition temperatures (T(g)) that vary continuously with composition. The tensile moduli exhibit positive deviations from simple additivity. Marked positive deviations were also observed for tensile strength. The tensile strengths of the 90/10 and 75/25 PEK-C/phenoxy blends are higher than those of both the pure components. Embrittlement, or transition from the brittle to the ductile mode of failure, occurs in the composition range of 50-25 wt% PEK-C. These observations suggest that mixing on the segmental level has occurred and that there is enough interaction between the components to decrease its internal mobility significantly. PEK-C was also found to be miscible with the epoxy monomer, diglycidyl ether of bisphenol A (DGEBA), as shown by the existence of a single glass transition temperature (T(g)) within the whole composition range. Miscibility between PEK-C and DGEBA could be considered to be due mainly to entropy. However, PEK-C was judged to be immiscible with the diaminodiphenylmethane-curved epoxy resin (DDM-cured ER). It was observed that the PEK-C/ER blends have two T(g), which remain invariant with composition and are almost the same as those of the pure components, respectively. Scanning electron microscopy showed that the PEK-C/ER blends have a two-phase structure. The different miscibility with PEK-C between DGEBA and the DDM-cured ER is considered to be due to the dramatic change in the chemical and physical nature of ER after curing.
Resumo:
Jussiaea repens L. (JRL) is an edible medicinal plant and is also used as a vegetable by the local people in southwestern China. The crude extract and its four fractions derived from JRL were evaluated for the 1,1-diphenyl-2-picrylhydrazyl radical-scavenging ability, hydroxyl radical-scavenging capacity and the potassium ferricyanide reduction property. The ethyl acetate-soluble fraction (EAF) and EAF6 (a subfraction derived from EAF) were the most valuable fraction and subfraction, respectively. Furthermore, bioactivity-guided chromatographic fractionation revealed that three pure compounds greatly contributed to the antioxidant activities. Qualitative and quantitative analyses of the major antioxidant constituents in the extract were systematically conducted by NMR, mass spectral analyses and RP-HPLC. The result demonstrated that rosmarinic acid (2.00 mg g(-1) JRL dry weight) quercetin 3-O-beta-D-glucopyranoside (9.88 mg g(-1) JRL dry weight), and kaempferol 3-O-beta-D-glucopyranoside (1.85 mg g(-1) JRL dry weight) were the major antioxidative constituents in JRL. These compounds are reported for the first time from this plant.
Resumo:
Four new (1-4) and seven known (5-11) benzaldehyde derivatives were characterized from the liquid fermentation cultures of Eurotium rubrum, an endophytic fungus that was isolated from the inner tissue of stems of the mangrove plant Hibiscus tiliaceus. The structures of these compounds were determined by extensive analysis of their spectroscopic data. Among these metabolites, compound 1, which was named as eurotirumin, possesses a new carbon skeleton with a cyclopentabenzopyran ring system.