Resumo:
The miscibility, spherulite growth kinetics, and morphology of binary blends of poly(beta-hydroxybutyrate) (PHB) and poly(methyl acrylate) (PMA) were studied with differential scanning calorimetry, optical microscopy, and small-angle X-ray scattering (SAXS). As the PMA content increases in the blends, the glass-transition temperature and cold-crystallization temperature increase, but the melting point decreases. The interaction parameter between PHB and PMA, obtained from an analysis of the equilibrium-melting-point depression, is -0.074. The presence of an amorphous PMA component results in a reduction in the rate of spherulite growth of PRE. The radial growth rates of spherulites were analyzed with the Lauritzen-Hoffman model. The spherulites of PHB were volume-filled, indicating the inclusion of PMA within the spherulites. The long period obtained from SAXS increases with increased PMA content, implying that the amorphous PMA is entrapped in the interlamellar region of PHB during the crystallization process of PHB. All the results presented show that PHB and PMA are miscible in the melt. (C) 2000 John Wiley & Sons, Inc.
Resumo:
Nonisothermal and isothermal melt crystallization kinetics of a novel aryl ether ketone polymer containing meta-phenylene linkages, PEKEKK (T/I), were studied by differential scanning calorimetry (DSC). The Avrami equation modified by Jeziorny and a new approach by combining the Avrami equation with the Ozawa equation could describe the nonisothermal crystallization. Isothermal crystallization could also be described by the Avrami equation. The activation energies were 187 and 159 kJ/mol for nonisothermal and isothermal crystallization, respectively. Using the Hoffman-Weeks method, the equilibrium melting point T-m(o) was estimated as 353 degrees C. From the spherulitic growth equation proposed by Hoffman and Lauritzen, the nucleation parameter K-g of the isothermal melt crystallization was estimated as 5.49 x 10(5) K-2. The crystallization characteristics of PEKEKK (T/I) were compared with those of all-para PEKEKK. The differences were explained by differences in the chain flexibility of the two polymers.
Resumo:
The banded textures in the films of a thermotropic liquid crystalline poly(aryl ether ketone) containing a lateral chloro group have been studied by means of transmission electron microscopy(TEM), electron diffraction(ED) and atomic force microscopy (AFM). The crystallization-induced Landed texture without external shear can be formed when the thin films were annealed at the temperature range(320-330 degrees C) of the liquid crystalline state from the melt, The results show that the banded regions have high orientation of single crystal based on the orthorhombic packing and the growing direction of the Lands is along the b axis of the crystals, This kind of single crystal-like bands is due to the different orientation of the packing molecular chains, The molecular chains of the dark bands in the bright field electron micrograph are perpendicular to the film plane, while the ones of the bright Lands are tilt along the b axis with the tilt angle upto +/-20 degrees.
Resumo:
Crystal and molecular structure of (2.6-dipropylphenylamide) dimethyl (tetra-methyl cyclopentadienyl) silane titanium dichloride (I) was fully characterized by X-ray diffraction. The crystal is obtained from a mixture of ether/hexane as orthorhombic. with a = 12.658 (3) Angstrom. b = 16.62 (3) Angstrom. c = 11.760 (2) Angstrom. V = 2474.2 (9) Angstrom(3). Z = 4, space group Pnma. R = 0.0399; Componud I compose of the pi-bounded ring with its dimethylsilyl-dipropyl phenyl amido group and the two terminal chloride atoms coordinated to central metal to form a so-called constrained geometry catalyst (CGC) structure. The result of molecular mechanics (MM) calculations on compound I shows that bond lengths and bond angles from the MM calculation are comparable to the data obtained from the X-ray diffraction study. The relation of the structure of CGCs and their catalytic activity by MM calculations is also discussed.
Resumo:
Novel poly(aryl ether ketone)s containing a lateral methoxy group were synthesized by nucleophilic substitution reactions of 4,4'-biphenol and methoxyhydroquinone with 1,4-bis(4-fluorobenzoyl)benzene in a sulfolane solvent in the presence of anhydrous potassium carbonate. Their thermotropic liquid crystalline properties were characterized by a variety of experimental techniques, e.g. differential scanning calorimetry (DSC), polarized light microscopy and temperature-dependent FTIR. Thermotropic liquid crystalline behaviour was observed in the copolymers containing 30-80 mol-% mexthoxyhydroquinone. Both melting (T-m) and isotropization (T-i) transitions appeared in the DSC curves. The polarized light microscopy study of the liquid crystalline copolymers suggested their ordered smectic structures. As expected, the copolymers had lower melting transitions than the biphenol-based homopoly(aryl ether ketone)s because of the copolymerization effect of the crystal-disrupting monomer methoxyhydroquinone.
Resumo:
Using poly(styrene-co-maleic anhydride) as the backbone and poly(ethylene glycol) methyl ether as side chains,three kinds of comblike polymers of different side chain length were synthesized. The Li-salt complexes and their firms were prepared. The dynamic mechanical properties were investigated. It was found that the main chain was rigid and the side chain was flexible in this comblike polymer system. Based on the time-temperature equivalence principle, a master curve was constructed. By selecting T-alpha as reference temperature, Arrhenius plots of shift factor and iso-free-volume plots were attained. The values of WLF parameters C-1 and C-2 increase with increasing salt concentration. By reference to T-0 = 50 degrees C, the relation between the average relaxation time 1g tau(c) and Li-salt concentration C is linear. The master curves are displaced progressively to higher frequencies as the M-w of side chains is increased. The relation between the average relaxation time 1g tau(n) and M-w of side chains is also linear. And the master curves are movable with the change of salts. It shows the effect of different kinds of salt on relaxation time.
Resumo:
In this paper, the synthesis and crystallization behavior of poly(ether ether ketone ether ketone) (PEEKEK) are reported. PEEKEK was prepared from 4,4'-bis(p-fluorobenzoyl) diphenyl ether (4,4'-FBDE) and hydroquinone along the nucleophilic substitution route. The thermal properties were investigated by using DSC and TGA. The crystallization behavior of PEEKEK under several conditions, i.e., crystallization from the molten state (melt crystallization), crystallization from a quenched sample (cold crystallization) and crystallization induced by exposing glassy sample to methylene chloride (solvent-induced crystallization) has also been investigated. The results show that crystallization of PEEKEK could be induced by the above methods, and no polymorphism was found. The differences in the crystallization of PEEKEK induced by the above methods are seen in their degree of crystallinity.
Resumo:
Two kinds of novel macrocyclic aryl thioether ether oligomers were synthesized by nucleophilic condensation reaction in high yields under pseudo-high-dilution condition. A combination of H-1 NMR, GPC and MALDI-TOF MS analyses unambiguously confirmed the cyclic nature and their distributions, Macrocyclic thioether ether ketone oligomers can undergo facile melt ring opening polymerization(ROP) initiated by thiyl radical to give a high molecular weight polymer.
Resumo:
In this paper, melt crystallization of poly(ether ether ketone ketone) (PEEKK) under strong electric field was investigated. In the crystal structure of PEEKK, the length of c axis was found to he 1.075 nm, increasing by 7% compared to that of PEEKK crystallized without strong electric field. The molecule chains might take a more extended conformation through the opening of the bridge bond angles by increasing from 124 degrees to 144 degrees under strong electric field in the crystal structure.
Resumo:
The present report deals with some results on phase behavior, miscibility and phase separation for several polymer blends casting from solutions. These blends are grouped as the amorphous polymer blends, blends containing a crystalline polymer or two crystalline polymers. The blends of PMMA/PVAc were miscible and underwent phase separation at elevated temperature, exhibited LCST behavior. The benzoylated PPO has both UCST and LCST nature. For the systems composed of crystalline polymer poly(ethylene oxide) and amorphous polyurethane, of two crystalline polymers poly(epsilon-caprolactone) and poly[3,3,-bis-(chloromethyl) oxetane], appear a single T-g, indicating these blends are miscible. The interaction parameter B's were determined to be -14 J cm(-3), -15 J cm(-3) respectively. Phase separation of phenolphthalein poly(ether ether sulfone)/PEO blends were discussed in terms of thermal properties, such as their melting and crystallization behavior.
Resumo:
The comblike polymers based on poly (styrene-co-maleic anhydride) backbone with poly (ethylene glycol) methyl ether as side chains were synthesized and characterized by H-1 NMR. with the result compared with that of 1R. It is found that it is both feasible and simple to synthesize this kind of compounds with the help of H-1 NMR.
Resumo:
The effect of entanglements on the glass transition and structural relaxation behaviors has been studied for polystyrene (PS) and phenolphthalein poly(ether sulfone) (PES-C) samples by fast evaporation of the solution of concentrations varying from above the overlapping concentration to far below it, and compared to the results we have studied previously in PC. It has been found that for all the polymers we have studied, in the concentrated solution region, the T-g of the samples obtained from solution are independent of the change of concentration and are very close to that of normal bulk samples, whereas in the dilute solution region the T-g of the samples decrease with the logarithm of decreasing concentration. The critical concentrations that divide the two distinct regions for the three polymers are 0.9% g/mL for PC, 0.1% g/mL for PS, and 1% g/mL for PES-C. The decrease of T-g of the samples is interpreted by the decrease of intermolecular entanglements as the isolation of polymer chains, and the entanglement of polymer chains restrained the mobility of the segments. The structural relaxation behavior of the polymers is also found to be different from that of normal bulk samples. The enthalpies of single-chain samples are lower than that of the bulk ones, which correspond to the lower glass transition temperature; the peaks are lower and broader, and the relaxed enthalpy is much lower as compared to that of bulk samples. In the three polymers we have studied, the influence of change of entanglements on both the decrease in glass transition temperature and relaxed enthalpy is the most significant for PS and the least for PES-C. It is indicated that the interactions in the flexible polymers are weak; thus, the restraint of the entanglements on the mobility of the segments plays a more important role in the flexible polymers, and the change of entanglement in the flexible polymers has a more significant influence on the physical properties.
Resumo:
The reaction of NdCl3 with 2 equiv. of Na-(BuC5H4)-C-t in THF(tetrahydrofuran) gives blue crystals [((BUC5H4)-C-t)(2)NdCl](2), C36H52Cl2Nd2(M-r = 844.11) Which crystallizes in the triclinic system with space group
. The crystal data are a=11.978 (1), b=12.671(4), c=12.706(2)Angstrom, alpha=105.47(2), beta=99.38(1)? gamma=93.15 (2)degrees, V=1825 (3) Angstrom(3), Z = 2 , D-c = 1.53g/cm(3), F(000) = 450 , T = 298K , lambda(MoK alpha) = 0.71069 Angstrom, , mu = 14.97cm(-1). Final R = 0.0390, R-w = 0.0376 for 4329 reflections with I greater than or equal to 3 sigma(I-o). The molecule has a dimer structure with two certrosymmetrical chlorine bridges. The structural trend of these analogous complexes is discussed.
Resumo:
The graft copolymerization of butyl acrylate onto poly(vinyl alcohol) with eerie ammonium nitrate as redox initiator in a aqueous medium has been investigated. The formation of graft copolymer was confirmed by means of IR, scanning electron microscopy (SEM), and wide-angle X-ray diffraction (WAXD). The percentage of mononer conversion and percentage of grafting varied with concentrations of initiator, nitric acid, monomer, macromolecular backbone (X-n = 1750, M = 80 000), reaction temperature and reaction time. Some inorganic salts and organic solvents have a great influence upon grafting. The reaction mechanism has been explored, and rate equations for the reaction are established. (C) 2000 John Wiley & Sons, Inc.