Dry sliding tests were performed on as-cast magnesium alloys Mg97Zn1Y2 and AZ91 using a pin-on-disc configuration. Coefficients of friction and wear rates were measured within a load range of 20-380 and 20-240 N at a sliding velocity of 0.785 m/s. X-ray differactometer, scanning electron microscopy, tensile testing machine were used to characterize the microstructures and mechanical properties of Mg97Zn1Y2 alloy and AZ91 alloy. Worn surface morphologies of Mg97Zn1Y2 and AZ91 were examined using scanning electron microscopy.
Resumo:
Thermal properties and crystallization-behavior of ultrafine fully-vulcanized powdered rubber (UFPR) toughened poly propylene (PP) were studied by Differential scanning calorimetry (DSC) and Wide angle X-ray diffraction (WAXD) measurements. It was found that the fraction of beta-form in the PP crystal increased at first, then sharply deceased up to zero with increasing UFPR content
Resumo:
With the target to design and develop new functionalized green triplet light emitters that possess distinctive electronic properties for robust and highly efficient phosphorescent organic light-emitting diodes (PHOLEDs), a series of bluish-green to yellow-green phosphorescent tris-cyclometalated homoleptic iridium(III) complexes [Ir(ppy-X)(3)] (X=SiPh3, GePh3, NPh2, POPh2, OPh, SPh, SO2Ph, Hppy=2-phenylpyridine) have been synthesized and fully characterized by spectroscopic, redox, and photophysical methods
Resumo:
Lanthanum-zirconium-cerium composite oxide (La-2(Zr0.7Ce0.3)(2)O-7, LZ7C3) coatings were prepared under different conditions by electron beam-physical vapor deposition (EB-PVD). The composition, crystal structure, surface and cross-sectional morphologies, cyclic oxidation behavior of these coatings were studied. Elemental analysis indicates that the coating composition has partially deviated from the stoichiometry of the ingot, and the existence of excess La2O3 is also observed.
Resumo:
The Mg-8Gd-0.6Zr-xHo (x = 1, 3 and 5, mass%) alloys were prepared by casting technology, and structures, aging strengthening mechanism and mechanical properties of the alloys were investigated. The age behaviors and the mechanical properties are improved by adding Ho addition. The structures of the alloys are characterized by the present of rosette-shaped equiaxed grains. The peak hardness value of the Mg-8Gd-0.6Zr-3Ho alloy is 100 Hv, which is about 30% higher than that of Mg-8Gd-0.6Zr alloy.
Resumo:
Self-assembled behavior of rod-terminally tethered three-armed star-shaped coil block copolymer melts was studied by applying self-consistent-field lattice techniques in three-dimensional (3D) space. Similar to rod-coil diblock copolymers, five morphologies were observed, i.e., lamellar, perforated lamellar, gyroidlike, cylindrical and sphericallike structures, while the distribution of the morphologies in the phase diagram was dramatically changed with respect to that Of rod-coil diblock copolymers.
Resumo:
The electrochemical corrosion behavior of Mg-6Al-0.4Mn and Mg-6Al-4RE-0.4Mn (RE = Mischmetal) alloys is investigated in 3.5% NaCl solution. The results of corrosion process, polarization behavior, and electrochemical impedance spectroscopy of the alloys reveal that Mg-6Al-4RE-0.4Mn exhibits enhanced corrosion resistance. The addition of RE stabilizes the solid solution and modifies the passive film through a finer microstructure.
Resumo:
Copolymers of N-vinylformamide and acrylic acid were synthesized by conventional aqueous free-radical polymerization. The phase behavior of the copolymer solutions was investigated through the addition of hydrochloric acid and the variation of the temperature. With a moderate content of N-vinylformamide, the copolymers showed complex phase behaviors. Under low-acidity conditions, a suspending liquid was formed, whereas under high-acidity conditions, the random copolymers could assemble into round nanoparticles with a broad particle size distribution.
Resumo:
Biodegradable poly(e-caprolactone) (PCL) foams with a series of controlled structures were prepared by using chemical foaming method. The cell morphology was detected by scanning electron microscope (SEM). The compressive behavior of the foams was investigated by uniaxial compression test. The effect of density and structural parameters on the foam compressive behavior was analyzed. It was found that the relative compressive modulus has a power law relationship with relative density. Increasing of both the cell wall thickness and the cell density lead to higher compressive modulus of the foam; however, the cell size has no distinct effect on compressive behavior.
Resumo:
Degradation and its temperature dependence of poly(methyl methacrylate) (PMMA) in the blend film of PMMA/SAN were investigated via ire-situ X-ray photoelectron spectroscopy(XPS). The results show that thermal degradation of PMMA takes place at 185, 130, 80 degrees C and even room temperature due to the existence of monochromatic X-ray. Furthermore, the degradation rate depends crucially on the experiment temperature.
Unique electrochemiluminescence behavior of Ru(bpy)(3)(2+) in a gold/Nafion/Ru(bpy)(3)(2+) composite
Resumo:
The unique electrochemiluminescence (ECL) behavior of tris(bipyridine) ruthenium(II) (Ru(bpy)(3)(2+) immobilized in a gold/Nafion/Ru(bpy)(3)(2+) composite material was investigated. In this composite, the Ru(bpy)(3)(2+) ECL was found mainly occurred at 0-0.4 V during the cathodic scan process and the ECL peak was at about 0.1 V, which was quite different to the reported Ru(bpy)(3)(2+) ECL. Similar to the generally observed Ru(bpy)(3)(2+) ECL, the present ECL also could be enhanced by tri-n-propylarnine (TPA). It is also unique that in the presence of TPA, another ECL peak at about 0.38 V occurred.
Resumo:
The phase behavior of symmetric ABA triblock copolymers containing a semiflexible midblock is studied by lattice Monte Carlo simulation. As the midblock evolves from a fully flexible state to a semiflexible state in terms of increase in its persistence length, different phase behaviors are observed while cooling the system from an infinite high temperature to a temperature below T-ODT (order-disorder transition temperature). Within the midblock flexibility range we studied (l(p)/N-c <= 0.105), a lamellar structure is formed at equilibrium state as the situation for fully flexible chains. The fraction of bridge chain is evaluated for the lamellar structures. We find that the increase in midblock rigidity indeed results in the increase in bridge chain fraction within the range from 44.9% to 51.8%.