386 resultados para SOL-GEL CHEMISTRY


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Ternary europium complex with dibenzoylmethane (DBM) and 1,10-phenanthroline (phen) was in-situ synthesized in thin SiO2/polyvinyl butyral (PVB) hybrid films by a two-step sol-gel process and characterized by;means of fluorescence spectroscopy. The luminescence spectra, fluorescence lifetimes and photostability were all investigated. The results showed that the hybrid films exhibited the characteristic emission bands of the Central rare earth Eu3+. In addition, Eu3+ presented longer fluorescence lifetime than in an ethanol solution and the complex had a higher photostability in the hybrid film than in the PVB film containing the corresponding pure complex.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A novel functionalized inorganic-organic hybrid material with cation exchange property was prepared by sol-gel method. The H2O2 biosensor was fabricated by simply dipping the horseradish peroxidase-containing functionalized membrane modified electrode into Meldola's blue (MDB) solution. MDB was adsorbed and firmly immobilized within the membrane. The electrochemical behavior of MDB incorporated in the membrane was more reversible compared with that of the solution species and suitable as mediator for the horseradish peroxidase. The response time was less than 25 s. Linear range is up to 0.6 mM (COH. coeff. 0.9998) with detection Limit of 9 x 10(-7) M. High sensitivity of 75 nA mu M cm(-2) was obtained due to high MDB-loading. The biosensor exhibited a good stability. (C) 1999 Elsevier Science B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In-situ synthesis of terbium complex with salicylic acid (Sal) in silica matrix was made by a two-step sol-gel process. The terbium complex with salicylic acid was formed in sol-gel derived silica gel, and confirmed by the luminescence excitation spectra and infrared(IR) spectra. As compared to the pure terbium complex powder, the silica gel containing terbium complex exhibits its characteristic emission and presents a longer fluorescence lifetime than that for the pure complex. The luminescence properties of the complex containing;silica gel were investigated and compared with that of both terbium doped the silica gel and thp pure complex powder. The reasons leading to the above results were also discussed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In-situ synthesis of europium and terbium complexes with 1,10-phenanthroline (phen) in silica matrix by a two-step sol-gel process has been proposed. The formation of europium and terbium complexes with phen in sol-gel derived silica gel were confirmed by the luminescence excitation spectra. The silica gels that contain in-situ synthesized europium and terbium complex exhibit the characteristic emission bands of the rare earth ions. Furthermore. the rare earth ions present longer fluorescence lifetimes than the comparable pure complex powder and the complexes dissolved in ethanol solutions. The luminescence properties of the silica gels codoped with europium (or terbium) and phen were also investigated with respect to the gels doped with europium (or terbium). (C) 1999 Elsevier Science B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A process for in situ synthesis of terbium complex with salicylic acid by a two-step sol-gel method in silica matrix has been proposed. The luminescence properties of the silica gels codoped with terbium and salicylic acid have also been discussed with respect to that of the gel doped with terbium and that of pure terbium complex with salicylic acid.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

(Y1-xEux)(3)Al5O12 and (Y1-x-yEuxBiy)(3)Al5O12 were prepared by so-gel method. Their structures of the luminophor are similar to that of YAG, which is recorded on the ASTM card and belongs to a cubic system. The luminescent properties show that the reaction temperature of the current sol-gel method is in the range of 400-500 degrees C, which is lower than that of the conventional solid state reaction. The luminophors have the strongest emission intensity when the values of x and y are 0.06 and 0.013, respectively.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Ternary complexes of europium and terbium with paraaminobenzoic acid and 1,10-phenanthroline (Eu(p-ABA)(3). phen . 2H(2)O and Tb(p-ABA)(3). phen . 2H(2)O, where p-HABA = paraaminobenzoic acid and phen = 1,10-phenanthroline) were introduced into a silica matrix by sol-gel method. The luminescence behavior of the complexes in silica gels was studied in comparison with the. corresponding solid-state complexes by means of emission, excitation spectra, and Lifetimes. Within the range of effective dopant concentrations, the luminescence intensities of rare-earth complexes in silica gel increase with the increasing of their dopant concentration. The lifetimes of rare-earth ions (Eu3+ and-Tb3+) in silica gel doped with europium and terbium complexes become longer than those in pure complexes. Very small amounts of rare-earth complexes doped in silica gel matrix can exhibit excellent luminescence properties, (C) 1998 Elsevier Science Ltd.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Europium and terbium complexes with 1,10-phenanthroline were introduced into silica gel by the sol-gel method. The luminescence behavior of the complexes in silica gels was studied compared with the corresponding solid state complexes by means of emission, excitation spectra and lifetimes. (C) 1998 Published by Elsevier Science S.A. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Hybrid materials incorporating poly(ethylene glycol) (PEG) with tetraethoxysilane (TEOS) via a sol-gel process were studied for a wide range of compositions of PEG by DSC and high resolution solid-state C-13- and Si-29-NMR spectroscopy. The results indicate that the microstructure of the hybrid materials and the crystallization behavior of PEG in hybrids strongly depend on the relative content of PEG. With an increasing content of PEG, the microstructure of hybrid materials changes a lot, from intimate mixing to macrophase separation. It is found that the glass transition temperatures (T-g) (around 373 K) of PEG homogeneously embedded in a silica network are much higher than that (about 223 K) of pure PEG and also much higher in melting temperatures T-m (around 323 K) than PEG crystallites in heterogeneous hybrids. Meanwhile, the lower the PEG content, the more perfect the silica network, and the higher the T-g of PEG embedded in hybrids. An extended-chain structure of PEG was supposed to be responsible for the unusually high T-g of PEG. Homogeneous PEG-TEOS hybrids on a molecular level can be obtained provided that the PEG. content in the hybrids is less than 30% by weight. (C) 1998 John Wiley & Sons, Inc.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Ternary complexes of terbium with ortho (and pam) aminobenzoic acid and 1,10-phenanthroline were introduced into silica gel by the sol-gel method. The luminescence behavior of the solid-state samples was studied during the sol-gel aging process by means of emission. excitation spectra, lifetimes and quantum efficiencies.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Y4Al2O9 (YAM) was prepared by a sol-gel process, using yttrium and aluminum citrate complexes as precursors. The sol-gel process produced single-phase YAM at 900 degrees C, as opposed to the conventional solid-state reaction, which led to the formation of other phases, even if at 1600 degrees C. The emission and excitation spectra of Eu3+ and Tb3+ in YAM showed the existence of two luminescence centers, agreeing with the crystal structure of YAM. The spectral properties of the samples are discussed.