217 resultados para SILICA WAVE-GUIDES
Resumo:
We report a new method for fabricating rare-earth-doped silica glasses for laser materials obtained by sintering nanoporous silica glasses impregnated with rare-earth-doped ions. The fabricated materials have no residual pores and show good optical and mechanical properties. Good performance from a Nd3+-doped silica microchip laser operating at 1.064 mum is successfully demonstrated, suggesting that the fabricated silica glasses have potential for use as active materials for high-power solid-state lasers. (C) 2005 Optical Society of America.
Resumo:
We report on room temperature laser actions of a novel thulium-doped crystal Tm center dot Lu2SiO5 (LSO) under diode pumping. An optical optical conversion efficiency of 12% and a slope efficiency of 21% were obtained with the maximum continuous wave (CW) output power of 0.67 W. The emission wavelengths of Tm LSO laser were centered at 2058.4 nm with bandwidth of similar to 13.6 nm.
Resumo:
We report both continuous-wave and passively mode-locked laser actions in a Yb3+-doped gadolinium yttrium oxyorthosilicate Yb:GdySiO(5) (Yb:GYSO) crystal. Continuous-wave (CW) laser operations were compared under different pump conditions with high-power diodes of different wavelengths and fiber cores. CW mode-locking was obtained with a semiconductor saturable absorber mirror.
Resumo:
We demonstrated continuous-wave ( CW) and Q-switched operation of a room-temperature Ho: YAlO3 laser that is resonantly end-pumped by a diode-pumped Tm: YLF laser at 1.91 mu m. The CW Ho: YAlO3 laser generated 5.5 W of linearly polarized (E parallel to c) output at 2118 nm with beam quality factor of M-2 approximate to 1.1 for an incident pump power of 13.8 W, corresponding to optical-to-optical conversion efficiency of 40%. Up to 1-mJ energy per pulse at pulse repetition frequency (PRF) of 5 kHz, and the maximum average power of 5.3-W with FWHM pulse duration of 30.5 ns at 20 kHz were achieved in Q-switched mode. (C) 2008 Optical Society of America.
Resumo:
We report on a diode-pumped, cryogenic and room temperature operation of a Tm,Ho:YAlO3 (c-cut) laser. In a temperature of 77 K, an optical-optical conversion efficiency of 27% and a slope efficiency of 29% were achieved with the maximum continuous-wave (CW) output power of 5.0 W at 2.13 mu m. Acousto-optic switched operation was performed at pulse repetition frequency (PRF) from 1 kHz to 10 kHz, the highest pulse energy of 3.3 mJ in a pulse duration of 40 ns was obtained. In room temperature (RT), the maximum CW power of Tm,Ho:YAlO3 laser was 160 mW with a slope efficiency of 11% corresponding to the absorbed pump power. (C) 2008 Optical Society of America.
Resumo:
Y2O3/SiO2 coatings were deposited on fused silica by electron beam evaporation. A continuous wave CO2 laser was used to condition parts of the prepared samples at different scanning speeds in the air. LAMBDA 900 spectrometer was used to investigate the changes of the transmittance and residual reflection spectrum. A Nomarski microscope under dark field was used to examine the changes of the micro defect density. The changes of the surface roughness and the microstructure of the film before and after conditioning were investigated by AFM and X-ray diffraction, respectively. We found that laser-induced damage threshold (LIDT) of the films conditioning at 30 mm/s scanning speed was increased by more than a factor of 3 over the thresholds of the as-deposited films. The conditioning effect was correlated with an irradiation-induced decrease of the defect density and absorption of the films. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
The high reflection (HR) mirror composed of dielectric stacks with excellent spectrum characteristics and high damage resistant ability is critical for fabricating multilayer dielectric (MLD) grating for pulse compressor. The selection of the SiO2 material as the top layer of the HR mirror for grating fabrication is beneficial for improving the laser-induced damage threshold of MLD grating as well as minimizing the standing-wave effect in the photoresist during the exposure process. Based on an (HLL) H-9 design comprising quarter-waves of HfO2 ( H) and half-waves of SiO2 ( L), we obtain an optimal design of the HR mirror for MLD grating, the SiO2 top layer of which is optimized with a merit function including both the diffraction efficiency of the MLD grating and the electric field enhancement in the grating. Dependence of the performance of the MLD grating on the fabrication error of the dielectric mirror is analysed in detail. The HR mirror is also fabricated by E-beam evaporation, which shows good spectral characteristics at the exposure wavelength of 413 nm and at the operation wavelength of 1053 nm and an average damage threshold of 10 J cm(-2) for a 12 ns pulse.
Resumo:
We report on the design of a high diffraction efficiency multi-layer dielectric grating with wide incident angle and broad bandwidth for 800 nm. The optimized grating can achieve > 95% diffraction efficiency in the first order at an incident angle of 5 degrees from Littrow and a wavelength from 770nm to 830 nm, with peak diffraction efficiency of > 99.5% at 800 nm. The electric field distribution of the optimized multi-layer dielectric grating within the gratings ridge is 1.3 times enhancement of the incidence light, which presents potential high laser resistance ability. Because of its high-efficiency, wide incident, broad bandwidth and potential high resistance ability, the multi-layer dielectric grating should have practical application in Ti:sapphire laser systems.
Resumo:
A new amino silica monolithic column was developed for DNA extraction in a miniaturized format. The monolithic column was prepared in situ by polymerization of tetraethoxysilane (TEOS) and N-(beta-aminoethyl)-gamma-aminopropylmethyldimethoxysilane (AEAPMDMS). DNA was loaded in 50 mM tris(hydroxylmethyl)aminomethane-EDTA buffer at pH 7.0 and eluted with 300 mM potassium phosphate solution at pH 10.0. Under optimal condition, a 6.0-cm monolithic column provided a capacity of 56 ng DNA with an extraction efficiency of 71 +/- 5.2% (X +/- RSD). When the amino silica monolithic column was applied to extract genomic DNA from the whole blood of crucian carp, an extraction efficiency of 52 +/- 5.6% (X +/- SD) was obtained by three extractions. Since the chaotropic-based sample loading and organic solvent wash steps were avoided in this procedure, the purified DNA was suitable for downstream processes such as PCR. This amino silica monolithic column was demonstrated to allow rapid and efficient DNA purification in microscale.
Resumo:
Fifty-one phytoplankton samples were collected from different ecological environments in five provinces located in the central, eastern and southwestern parts of China. 41 taxa of silica-scaled chrysophytes, 8 of them belonging to the Chrysophyceae and 33 to the Synurophyceae, have been identified by means of electron microscopy. Among them, Mallomonas parvula, M. calceolus, M. cyathellata (?), M. costata, M. crassisquama, and Synura echinulata are new to China. The silica-scaled chrysophyte flora and its geographical distribution in this region are analysed and discussed.
Resumo:
The idler is separated from the co-propagating pump in a degenerate four-wave mixing (DFWM) with a symmetrical parametric loop mirror (PALM), which is composed of two identical SOAs and a 70 m highly-nonlinear photonic crystal fiber (HN-PCF). The signal and pump are coupled into the symmetrical PALM from different ports, respectively. After the DFWM based wavelength conversion (WC) in the clockwise and anticlockwise, the idler exits from the signal port, while the pump outputs from its input port. Therefore, the pump is effectively suppressed in the idler channel without a high-speed tunable filter. Contrast to a traditional PALM, the DFWM based conversion efficiency is increased greatly, and the functions of the amplification and the WC are integrated in the smart SOA and HN-PCF PALM. (C) 2008 Elsevier B.V. All rights reserved.