The complex fluoride alpha'-SrAlF5 has been synthesized through hydrothermal and solvothermal methods under mild conditions. The effects of the molar ratio of starting materials, temperature, reaction time and solvents on the synthesis of alpha'-SrAlF5 were discussed. The final products were characterized by XRD and SEM. The rod-like shape of alpha'-SrAlF5 is shown in SEM images.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The complex fluoride LiBaF3 is solvothermally synthesized at 180degreesC and characterized by means of X-ray powder diffraction, scanning electron microscopy, thermogravimetric analysis and infrared spectroscopy. In the solvothermal process, the solvents, mole ratios of initial mixtures and reaction temperature play important roles in the growth of the single crystal.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Tapping mode atomic force microscopy (AFM) was applied to study the adsorption behavior of methanol on mica, highly oriented pyrolytic graphite (HOPG) and indium-tin oxide (ITO) coated glass substrates. On mica and HOPG substrates surfaces, the thin films of methanol with bilayer and multilayer were observed, respectively. The formation of irregular islands of methanol was also found on HOPG surface. On ITO surface only aggregates and clusters of methanol molecules were formed. The influence of sample preparation on the adsorption was discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The oxidation and adsorption of the temperature-denatured DNA at GC electrode are studied by differential pulse voltammetry and in situ FTIR spectroelectrochemistry. The temperature-denatured DNA is adsorbed and formed a DNA multilayer at electrode surface. The temperature-denatured DNA showing partly reversible process was first observed based on the reduction peaks appearing at negative scans and the reversible spectral change. The oxidation product of the temperature-denatured DNA can not diffuse away from the electrode surface easily due to the impediment of the DNA multilayer, so it can be partly reduced.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nanometre-sized poly(vinylidene fluoride) (PVDF) particle domains in a confined space were obtained by blending PVDF with excess poly(methyl methacrylate) (PMMA). When these particles were small enough they showed beta -form structure, which was different from the structure of bigger particles or PVDF bulk. However, the beta -form was thermodynamically metastable because it could eventually be transformed to a more stable phase by annealing at a certain temperature. Larger particle domains were of identical phase to the bulk, indicating that small size favours the formation of the beta -form. (C) 2000 Society of Chemical Industry.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The influence of swelling and stripping acidity on the mass transfer coefficient based on water phase and the inner diameters of membranes were studied with P507-HCl-Sm as working system in the two different kinds of hollow fiber membranes. Effects of extractant concentration, H+ concentration in aqueous phase and Sm3+ concentration on extraction rate were discussed and the corresponding reaction series were obtained. According to the investigations on the interfacial kinetics, the reaction kinetics equation and reaction rate constant were obtained.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The assembly of alternating DNA and positively charged poly(dimethyldiallylammonium chloride) (PDDA) multilayer films by electrostatic layer-by-layer adsorption has been studied. The real-time surface plasmon resonance (BIAcore) technique was used to characterize and monitor the formation of multilayer films in solution in real time continuously. Electrochemical impedance spectroscopy (EIS) and UV-vis absorbance measurements were also used to study the film assembly, and linear film growth was observed. All the results indicate that the uniform multilayer can be obtained on the poly(ethylenimine)- (PEI-) coated substrate surface. The kinetics of the adsorption of DNA on PDDA surface was also studied by the real-time BIAcore technique; the observed rate constant was calculated using a Langmuir model (k(obs) = (1.28 +/- 0.08) x 10(-2) s(-1).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

KMgF3 doped with Eu was synthesized by mild hydrothermal method at 240 degreesC for the first time. The excitation and emission spectra of the KMgF3 : Eu2+ phosphor were measured. Comparing with the sample synthesized through solid state reaction, the variation in the excitation spectra at 360 nm resulted from the existences of V-K color centers; the low emission intensity was due to Eu2+ having transferred part energy to V-K color centers.