367 resultados para Polyethylene- Starch Blends


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nylon 6/poly(acrylonitrile-butadiene-styrene)(ABS) blends were prepared in the molten state by a twin-screw extruder. Maleic anhydride-grafted polypropylene (MAP) and solid epoxy resin (bisphenol type-A) were used as compatibilizers for these blends. The effects of compatibilizer addition to the blends were studied via tensile, torque, impact properties and morphology tests. The results showed that the additions of epoxy and MA copolymer to nylon 6/ABS blends enhanced the compatibility between nylon 6 and ABS, and this lead to improvement of mechanical properties of their blends and in a size decrease of the ABS domains.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Macrokinetic models, namly the modified Avrami, Ozawa and Zibicki models, were applied to study the non-isothermal melt crystallization process of PET/PEN/DBS blends by DSC measurement. The modified Avrami model was found to describe the experimental data fairly well. With the cooling rates in the range from 5 to 20 K/min, Ozawa model could be well used to describe the early stages of crystallization. However, Ozawa model did not fit the polymer blends during the late stages of crystallization, because it ignored the influence of secondary crystallization. The crystallization ability of the blends decreases with increasing the DBS content from analysis by using Ziabicki kinetic model, which is similar to the results based on calculation of the effective energy barrier of the blends.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The isothermal crystallization and melting behaviors of poly(propylene carbonate) end-capped with benzenesulfonyl/poly (vinyl alcohol) (PPC-BS/PVA) blends over rich PVA composition range were first investigated by differential scanning calorimetry (DSC). PPS-BS/PVA interaction parameter, chi(12), calculated from equilibrium melting temperature depression was -0.44, revealing miscibility of PPC-BS with PVA in the melt and favorable interactions. The temperature dependence of crystallization rate constant at initial crystallization stage was analyzed using the modified Lauritzen-Hoffman expression. The chain width, a(0), the thickness of a monomolecular layer, b(0), the fold and lateral surface-free energies, sigma(e) and sigma, and the work of chain folding, q, for neat PVA were first reckoned to be 4.50 Angstrom, 4.78 Angstrom, 76.0 erg.cm(-2), and 4.70 kcal.mol(-1), respectively. The values of sigma(e) and q for PVA in PPC-BS/PVA blends exhibited a maximum in the neighborhood of 10/90 PPC-BS/PV, respectively.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

FTIR spectroscopy was used to verify the presence of intermolecular hydrogen bond (inter-H-bond) between poly-(3-hydroxybutyrate co-3-hydroxyvalerate) (PHBV) and bisphenol A (BPA). By monitoring the spectral changes during PHBV crystallization and blends dissociation, the absorptivity ratio of C=O bonds in crystalline and amorphous regions in PHBV and that of H-bonded and free C=O in PHBV/BPA blends were experimentally determined as 1.40 and 1.68, respectively. Using curve-fitting program, the C=O absorptions in spectra of blends were ascribed to three types of bonds: amorphous, crystalline and H-bonded C=O. The crystallinity of PHBV and the fraction of H-bonded C=O were calculated. These results indicated that the H-bond clearly suppressed the PHBV crystallization. Furthermore, the fraction of BPA molecules that simultaneously formed two hydrogen bonds (H-bonds) with C=O was estimated. It revealed that there existed a H-bond network in PHBV/BPA blends. This network was compared with the covalent network by estimating the number of atoms between every two adjacent crosslink points in chain. Up to the high density of H-bond discussed in this paper, there was always a certain part in PHBV that crystallized due to the dynamic character of hydrogen bonds; however, the hydrogen bonds significantly reduced the crystallization rate of PHBV.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Isothermal crystallization behavior of poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) was investigated by means of differential scanning calorimetry and polarized optical microscopy (POM). The Avrami analysis can be used successfully to describe the isothermal crystallization kinetics of PHBV, which indicates that the Avrami exponent n = 3 is good for all the temperatures investigated. The spherulitic growth rate, G, was determined by POM. The result shows that the G has a maximum value at about 353 K. Using the equilibrium melting temperature (448 K) determined by the Flory equation for melting point depression together with U-* = 1500 cal mol(-1), T-infinity = 30 K and T-g = 278 K, the nucleation parameter K-g was determined, which was found to be 3.14+/-0.07 x 10(5) (K-2), lower than that for pure PHB. The surface-free energy sigma = 2.55 x 10(-2) J m(-2) and sigma(e) = 2.70+/-0.06 x 10-2 J m(-2) were estimated and the work of chain-folding (q = 12.5+/-0.2 kJ mol(-1)) was derived from sigma(e), and found to be lower than that for PHB. This implies that the chains of PHBV are more flexible than that of PHB.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

IntroductionConventional polymers such as polyethyleneand polypropylene persistfor many years after landdisposal.Furthermore,plastics are often soiled byfood and other biological substances,making phys-ical recycling of those materials impractical andgenerally undesirable. In contrast,biodegradablepolymers disposed in bioactive environment are de-graded by the enzymatic action of microorganismssuch as bacteria,fungi,and algae.The worldwideconsumption of biodegradable polymers increasedfrom1.4×107kg in ...

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A kind of full-biodegradable film material is discussed in this article. The film material is composed of starch, PVA, degradable polyesters(PHB, PHB-V, PCL) with built plasticizer, a cross-linking reinforcing agent and a wet strengthening agent. It contains a high percentage of starch, costs cheap and is excellent in weather fastness, temperature resistance and waterproof and it could be completely biodegraded. The present paper deals mainly with a new technical route using a new type of electromagnetic dynamic blow molding extruder and some effects on mechanical properties of the system.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Blends of synthetic poly(propylene carbonate) (PPC) with a natural bacterial copolymer of 3-hydroxybutyrate with 3-hydroxyvalerate (PHBV) containing 8 mol % 3-hydroxyvalerate units were prepared with a simple casting procedure. PPC was thermally stabilized by end-capping before use. The miscibility, morphology, and crystallization behavior of the blends were investigated by differential scanning calorimetry, polarized optical microscopy, wide-angle X-ray diffraction (WAXD), and small-angle Xray scattering (SAXS). PHBV/PPC blends showed weak miscibility in the melt, but the miscibility was very low. The effect of PPC on the crystallization of PHBV was evident. The addition of PPC decreased the rate of spherulite growth of PHBV, and with increasing PPC content in the PHBV/PPC blends, the PHBV spherulites became more and more open. However, the crystalline structure of PHBV did not change with increasing PPC in the PHBV/PPC blends, as shown from WAXD analysis. The long period obtained from SAXS showed a small increase with the addition of PPC.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effects of the chain structure and the intramolecular interaction energy of an A/B copolymer on the miscibility of the binary blends of the copolymer and homopolymer C have been studied by means of a Monte Carlo simulation. In the system, the interactions between segments A, B and C are more repulsive than those between themselves. In order to study the effect of the chain structure of the A/B copolymer on the miscibility, the alternating, random and block copolymers were introduced in the simulations, respectively. The simulation results show that the miscibility of the binary blends strongly depends on the intramolecular interaction energy ((ε) over bar (AB)) between segments A and B within the A/B copolymers. The higher the repulsive interaction energy, the more miscible the A/B copolymer and homopolymer C are. For the diblock copolymer/homopolymer blends, they tend to form micro phase domains. However, the phase domains become so small that the blend can be considered as a homogeneous phase for the alternating copolymer/ homopolymer blends. Furthermore, the investigation of the average end-to-end distance ((h) over bar) in different systems indicates that the copolymer chains tend to coil with the decrease Of (ε) over bar (AB) whereas the (h) over bar of the homopolymer chains depends on the chain structure of the copolymers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The electrochemical behavior of alpha-Keggin-type nanoparticles, Co(en)(3)(PMo12O40) (abbreviated as PMo12-Co), have been studied in poly(ethylene glycol) for four different molecular weights (PEG, average MW 400, 600, 1000, and 2000 g mol(-1)) and containing LiClO4 (O/Li=100/1) supporting electrolyte. The diffusion coefficients of the PMo12-Co nanoparticles were determined using a microelectrode by chronoamperometry for PEG of different molecular weights that were used to describe the diffusion behavior of PMo12-Co nanoparticles in different phase states. Moreover, the conductivity of the composite system increases upon addition of PMo12-Co nanoparticles, which was measured by an a.c. impedance technique. FT-IR spectra and DSC were used to follow the interactions of PEG-LiClO4-PMo12-Co, and well described the reason that the PMo12-Co nanoparticles could promote the conductivity of the PEG-LiClO4-PMo12-Co system.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The thin films of poly(methyl methacrylate) (PMMA), poly(styrene-co-acrylonitrile) (SAN) and their blends were prepared by means of spin-coating their corresponding solutions onto silicon wafers, followed by being annealed at different temperatures. The surface phase separations of PMMA/SAN blends were characterized by virtue of atomic force microscopy (AFM). By comparing the tapping mode AFM (TM-AFM) phase images of the pure components and their blends, surface phase separation mechanisms of the blends could be identified as the nucleation and growth mechanism or the spinodal decomposition mechanism. Therefore, the phase diagram of the PMMA/SAN system could be obtained by means of TM-AFM. Contact mode AFM was also used to study the surface morphologies of all the samples and the phase separations of the blends occurred by the spinodal decomposition mechanism could be ascertained. Moreover, X-ray photoelectron spectroscopy was used to characterize the chemical compositions on the surfaces of the samples and the miscibility principle of the PMMA/SAN system was discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The pressure-dependent glass-transition temperatures (T-g's) of poly(methyl methacrylate) (PMMA)/poly(styrene-co-acrylonitrile) (SAN) blends were determined by pressure-volume-temperature (PVT) dilatometry via an isobaric cooling procedure. The Gordon-Taylor and Fox equations were used to evaluate the relationships between the T-g's and compositions of the PMMA/SAN system at different pressures. The relationships were well fitted by the Gordon-Taylor equation, and the experimental data for T-g positively deviated from the values calculated with the Fox equation. Also, the influence of the cooling rate (during the PVT measurements) on T-g was examined.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Reactive compatibilization of ethylene-propylene copolymer functionalized with allyl (3-isocyanato-4-tolyl) carbamate (TAI) isocyanate (EPM-g-TAI) and polyamide 6 (PA6) was investigated in this paper, FTIR analysis revealed the evidence of a chemical reaction between the end groups of PA6 and EPM-g-TAI. Thermal, rheological, morphological, and mechanical properties of the resultant system were examined, DSC analysis indicated that the crystallization of PA6 in Pa6/EPM-g-TAI blends was inhibited, due to the chemical reaction that occurs at the interface of PA6 and EPM-g-TAI. Rheological measurement showed that complex viscosity and storage modulus of PA6/EPM-g-TAI were both dramatically enhanced compared to those of PA6/EPM at the same blending composition. After examining the morphology of both blending systems, smaller particile sizes, more homogeneous distribution of domains and improved interfacial adhesion between matrix and domains were observed in the compatibilized system. Mechanical properties such as tensile strength. Young's modulus, flexural strength and modulus, as well as notched and un-notched impact strength of PA6/EPM-g-TAI blends were also found to improve gradually with increasing the content of grafted TAI.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Polyethylene (PE)/montmorillonite (MMT) nanocomposites were prepared by in situ coordination polymerization using a MMT/MgCl2/TiCl4 catalyst activated by AI(Et),. The catalyst was prepared by first diffusing MgCl2 into the swollen MMT layers, followed by loading TiCl4 on the inner/outer layer surfaces of MMT where MgCl2 was already deposited. The intercalation of MMT layers by MgCl2 and TiCl, was demonstrated by the enlarged interlayer spacing determined by WAXD. The nanoscale dispersion of MMT layers in the polyethylene matrix was characterized by WAXD and TEM. As a consequence, the crystallinity of the nanocomposite decreased sharply, whereas the tensile strength was significantly improved compared to that of virgin polyethylene of comparable molecular weight. The confinement of the nanodispersed MMT layers to molecular chain and the strong interaction between the nanoscale MMT layers and the resin matrix were thought to account for the decrease of crystallinity and the remarkable enhancement of strength.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An ethylene-propylene copolymer (EPM) was functionalized with an iso cyanate-bearing unsaturated monomer, allyl(3-isocyanate-4-tolyl) carbamate (TAI), with dicumyl peroxide as an initiator in a xylene solution. Fourier transform infrared (FTIR) was used to confirm the formation of EPM-g-TAI. The peak at 2273 cm(-1), characteristic of -NCO groups in EPM-g-TAI, revealed evidence of grafting. The grafting degree was determined with both chemical titration and FTIR. The grafting degree could be adjusted, and the maximum was over 6 wt % without any gelation. The molar mass distribution of EPM-g-TAI was narrower than that of EPM. The rheological behavior of both EPM-g-TAI and EPM was investigated with a rotational rheometer. The apparent viscosity of EPM-g-TAI was higher than that of EPM and increased with an increasing grafting degree of TAI. Surface analysis by contact-angle measurements showed that contact angles of EPM-g-TAI samples to a given polar liquid decreased with an increasing grafting degree of TAI. We also obtained the dispersion component of the surface free energy (gamma(S)(d)), the polar component of the surface free energy (gamma(S)(d)), and the total surface free energy (gamma(S) = gamma(S)(d) + gamma(S)(p)) of the grafted EPM. These parameters increased with the enhancement of the grafting degree, which gave us a quantitative estimation of the polar contribution of the grafted TAI to the total surface free energy of EPM-g-TAI.