414 resultados para POLYAMIDE BLENDS


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The decaying of free radicals in the course of heating, trapped in irradiated polyamide 1010 with different crystallinities, were investigated using an ESR technique. The decaying temperature, at which all radicals decay completely, depends on the aggregation of polyamide 1010 prior to radiation. The higher the crystallinity, the higher the temperature at which the radicals disappear. Dynamically speaking, radicals in specimens with higher crystallinity take longer to decay. (C) 1997 Elsevier Science Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The crystallization, miscibility and structure of polyimide PBPI-E/PTI-E blends were studied by DSC, DMA, NMR and fluorescence techniques, where PBPI-E is a biphenyldianhydride-based polyimide, and PTI-E is a polyimide from 4,4'-thiodiphthalic anhydride and 4,4'-oxydianiline. The results obtained show that PBPI-E/PTI-E blends are miscible at a molecular level for all the compositions studied. However, the glass transition temperature of the blends is well below the value predicted by the Fox equation, and the blends are not stable at high temperature, i.e. phase separation will occur when the blends are annealed about T-g. Moreover, the melting point T-m, differential enthalpy Delta H and spin-lattice relaxation time T-l(c) of the blends increase with the annealing time. (C) 1997 Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Radiation-induced crystallization of polyamide-1010 (PA1010) or nylon-1010 containing heterogeneous nuclei (neodymium oxide, Nd2O3) is discussed in this paper by Wide Angle X-ray Diffraction (WAXD) and Differential Scanning Calorimetry (DSC). The results show that at low dosage the crystallinities of the irradiated specimens increase, while crystallite size (L(hkl)) decreases, indicating that some new crystallites are produced in the course of irradiation. The new centers were brought about in the fold surface of the lamellae. Copyright (C) 1997 Elsevier Science Ltd

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Irradiated polyamide-1010 (PA1010) with and without heat treatment after gamma-ray irradiation was compared by wide angle x-ray diffraction (WAXD), differential scanning calorimeter (DSC) and the determination of gel fractions. The results indicate that post radiation effects due to post radiation crosslinking and scissions affect physical properties. Post radiation effects restrain the formation and perfection of the planes (010), and make the crystals imperfect. Post radiation effects change the crystalline structures of polyamide-1010.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Blends of a poly(ether sulfone) (PES) and a polycarbonate (PC) were prepared by melt-mixing and were studied by tensile tests, differential scanning calorimetry, dynamic mechanical analysis, density measurements and transmission electron microscopy (TEM). The blends were found to be two-phase systems and an interfacial layer was presumed to be formed between two phases, which was verified by TEM. A synergism of elongation at break and tensile modulus was shown in PES/PC blends. The effects of the crosshead speed on the mechanical properties were discussed for blends with different PES/PC weight ratios.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Mechanical properties and morphology of blends of polypropylene (PP) with high molecular weight polyethylene (HMWPE) prepared by coprecipitation from xylene solution are investigated. Compared to blends of PP with commercial high-density polyethylene (HDPE), the mechanical properties of the blends of PP/HMWPE are much superior to those of PP/HDPE blends. Not only is the tensile strength stronger, but also the elongation at break is much higher than that of the PP/HDPE blends of the same composition. These differences increase with increasing HMWPE and HDPE content. Scanning electron microscopy of the fracture surface resulting from the tensile tests shows that the compatibility in PP/HMWPE blends is much better than that in PP/HDPE blends. This is most likely attributable to the enhanced chain entanglement of HMWPE with the PP in the amorphous phase due to the lower crystallinity, owing to the high molecular weight of the HMWPE, and a much more flexible chain. The thermal behavior and spherulite morphology of both blends are also investigated.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The miscibility and specific interactions in poly (beta-hydroxybutyrate) (PHB)/poly(p-vinylphenol) (PVPh) blends were studied by differential scanning calorimetry(DSC) , fourier transform infrared(FTIR) spectrometer and high resolution solid state C-13 NMR, A single composition-dependent glass transition temperatures were obtained by DSC which indicate the blends of PHB/PVPh were miscible in the melt state, The experimental glass transition temperatures were fitted quite well with those obtained from Couchman-Karasz equation. The FTIR study shows that the strong intermolecular hydrogen bonding exists in blends of PHB with strong proton acceptor and PVPh with strong proton donor and is the origin of its compatibility. The CPMAS C-13 NMR spectra also show that the strong hydrogen bonding exists in PHB/PVPh blends. From the T-1 rho(H) relaxation time it follows that the blends of PHB/PVPh(40/60, 20/80) studied are completely homogeneous on the scale of about 3.2 nm.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The thermosetting polyimide PMR-I5 and its blends with thermoplastic polyimides have been studied by dynamic mechanical analysis. The results obtained indicate that the level of beta relaxations in PMR-15 are increased with an increase in cross-linking density. This phenomenon is interpreted as a change of chemical structure during the cross-linking process. Addition of thermoplastic polyimide makes the magnitude of beta relaxations increase when PMR-15 is the major component. This might be due to the strong intermolecular charge-transfer interaction between PI and PI or PMR-15 and PMR-15 molecular chains being partly replaced by the weak intermolecular interaction between PI and PMR-15 in PMR-15/PI blends, resulting in some phenylene rings or imide groups in PIs and PMR-15 chains being able to participate in beta relaxation. However, this increment in beta relaxation magnitude can be reduced by heat treatment of the sample, as a result of phase separation. Hence, it is concluded that the beta relaxation magnitude is determined by the number of groups which can participate in relaxation per unit length, i.e. the magnitude of beta relaxation increases with decreasing interaction between the molecular chains. Copyright (C) 1996 Elsevier Science Ltd

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Differential scanning calorimetry (DSC), Fourier-transform infrared spectroscopy (FTIR), scanning electron microscopy (SEM), and X-ray photoelectron spectroscopy (XPS) were used to study the miscibility of blends of a graft copolymer of poly(methyl methacrylate) on linear low density polyethylene (LLDPE-g-PMMA, G-3) with poly(vinylidene fluoride)(b) (PVF2) and the compatibilization of blends of LLDPE/PVF2. The specific interaction between PMMA side chains and PVF2 in G-3/PVF2 binary blends is weaker than that between the homopolymers PMMA and PVF2. There are two states of PVF2 in the melt of a G-3/PVF2 (60/40, w/w) blend, one as pure PVF2 and the other interacting with PMMA side chains. The miscibility between PMMA side chains and PVF2 affects the crystallization of PVF2. LLDPE-g-PMMA was demonstrated to be a good compatibilizer in LLDPE/PVF2 blends, improving the interfacial adhesion and dispersion in the latter. Diffusion of PMMA side chains into PVF2 in the interfacial region reduces the crystallization rate and lowers the melting point (T-m) and the crystallization temperature (T-c) of PVF2 in the blends.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Noncompatibilized and compatibilized blends of nylon 1010/PP blends having five different viscosity ratios were prepared by melt extrusion. Glycidyl methacrylate-grafted-polypropylene (PP-g-GMA) was used as the compatibilizer to enbance the adhesion between the two polymers and to stabilize the blend morphology. The effect of the viscosity ratio on the morphology of nylon 1010/polypropylene blends was investigated, with primary attention to the phase-inversion behavior and the average particle size of the dispersed phase. The relationship between the mechanical properties and the phase-inversion composition was investigated as well. Investigation of the morphology of the blends by microscopy indicated that the smaller the viscosity ratio (eta(PP)/eta(PA)) the smaller was the polypropylene concentration at which the phase inversion took place and polypropylene became the continuous phase. The compatibilizer induced a sharp reduction of particle size, but did not have a major effect on the phase-inversion point. An improvement :in the mechanical properties was found when nylon 1010 provided the matrix phase. (C) 1996 John Wiley & Sons, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The miscibility of blends of poly(styrene-co-acrylonitrile) (SAN) with poly(methyl methacrylate) (PMMA) or poly(ethyl methacrylate) (PEMA) has been investigated by means of NMR and DSC techniques. It is found that there are intermolecular interactions between the phenyl groups in SAN and carbonyl groups in PMMA or PEMA, and the strength of this intermolecular interaction strongly depends on the properties of ester side groups in PEMA or PMMA, composition of the blends and a certain composition of the copolymer. It is this specific interaction instead of the intramolecular repulsion force within the copolymer that plays a key role for the miscibility of SAN/PMMA and SAN/PEMA blends.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The miscibility of blends of poly(vinylidene chloride-co-acrylonitrile) (VDC-AN) and poly(methyl methacrylate) (PMMA) has been studied with DSC, FT-IR, and NMR methods. The results indicate that the VDC-AN/PMMA blends are miscibile on a molecular level, and the dipole-dipole interactions between C=O and C-Cl-2 and/or interpolymer hydrogen bondings between COOCH3 and CN and CCl groups play the role on the miscibility of the blends. It is found that the -CCl2- groups have two different chemical environments in the pure VDC-AN copolymer, which may result from the different configurations of the copolymer, such as -CCl2- groups in the ''alternating'' segments and -CCl2- groups in the ''blocky'' segments as proposed. It is the -CCl2- group in the ''alternating'' segment that takes part in the dipole-dipole interaction with C=O group in PMMA.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The compatibilizing effect of graft copolymer, linear low density polyethylene-g-polystyrene (LLDPE-g-PS), on immiscible LLDPE/PS blends has been studied by means of C-13 CP-MAS NMR and DSC techniques. The results indicate that LLDPE-g-PS is an effective compatibilizer for LLDPE/PS blends, and the compatibilizing effect of LLDPE-g-PS on LLDPE/PS blends depends on the PS grafting yield and molecular structure of the compatibilizers and also on the composition of the blends. It was found that LLDPE-g-PS chains connect two immiscible components, LLDPE and PS, through solubilization of chemically identical segments of LLDPE-g-PS into the noncrystalline region of the LLDPE and PS domain, respectively. Meanwhile, LLDPE-g-PS chains connect the crystalline region of LLDPE by isomorphism, resulting in an obvious change in the crystallization behavior of LLDPE. (C) 1996 John Wiley & Sons, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Poly(ether ether ketone) and poly(ether diphenyl ether ketone) homopolymers are prepared by nucleophilic substitution routes. Miscibility of PEEK/PEDEK blends has been studied by wide-angle X-ray diffraction (WAXD) and differential scanning calorimetry (d.s.c.). The results indicate that for PEEK/PEDEK blends, when the PEDEK content (weight fraction) is greater than 0.20 and less than 0.75, PEEK and PEDEK components form independent crystalline regions, i.e. they are immiscible; when the PEDEK content is in the range W-PEDEK less than or equal to 0.20 or greater than or equal to 0.75, a rich PEEK- or PEDEK-rich content crystallizes from a mixed melt and PEEK and PEDEK are miscible. Copyright (C) 1996 Elsevier Science Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The change in the microphase separation transition (MST) temperature of a styrene-butadiene-styrene (SBS) triblock copolymer induced by the addition of polystyrene (PS) was investigated by small-angle X-ray scattering. It was found that the transition temperature was determined from the molecular weight (M(H)) Of the added PS in relation to that of the corresponding blocks (M(A)) in the copolymer. The MST temperature decreased with added PS if M(H)/M(A) < 1/4, while it increased with added PS when M(H)/M(A) > 1/4 Analysis of the theoretical expression based on the random phase approximation showed exactly the same tendency of change in the transition temperatures as that observed experimentally. The interaction parameter, chi(SB), obtained by nonlinear fitting of the scattering profiles of SBS/PS blends in the disordered state, was found to be a function of temperature and composition. Composition fluctuations were found to exist in SBS/PS blends, increasing with increasing addition of PS but diminishing with increasing molecular weight of the added PS.