243 resultados para erbium-doped fiber laser (EDFL)


Relevância:

100.00% 100.00%

Publicador:

Resumo:

We present a novel 800-nm Bragg-mirror-based semiconductor saturable absorption mirror with low temperature and surface state hybrid absorber, with which we can realize the passive soliton mode locking of a Ti:sapphire laser pumped by 532-nm green laser which produces pulses as short as 37 fs. The reflection bandwidth of the mirror is 30 nm and the pulse frequency is 107 MHz. The average output power is 1.1 W at the pump power of 7.6 W.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

The output spectrum of Yb-doped double-clad fiber superfluorescent source (SFS) is tailored by placing a broadband dichroic mirror in the pump end of conventional single-pass forward configuration, which constitutes double-pass forward configuration. The 3 dB bandwidth is increased from I I to 42 nm. A maximum output SFS power of 2.12 W and a slope efficiency of 43.2% are obtained. The double-clad fiber is 25 in and the pump power is adequate to saturate the fiber as far as the feedback-induced lasing appears. (c) 2004 Elsevier Ltd. All rights reserved.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

The lasing in an end-pumped gain guided index-antiguided (GG-IAG) Yb3+-doped silicate glass fiber with a 200 mu m diameter core is demonstrated. Laser beams with similar beam propagation factors M (2) and mode field diameters W (0) (> 160 mu m) were observed at the output end of the GG-IAG fibers under different pump powers, which indicated that single mode behavior and excellent beam quality were achieved during propagation. Furthermore, the laser amplifier characteristics in the present Yb3+-doped GG-IAG fiber were also evaluated.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

In this paper, we present a simple technique to determine the coupling efficiency between a laser diode and a lensed-tip based on the ABCD transformation matrix method. We have compared our analysis technique to that of previous work and have found that the presented method is reliable in predicting the coupling efficiency of lensed-tip and has the advantage of simplicity of coupling efficiency calculation even by a pocket calculator. The results can be useful for designing coupling optics. (c) 2005 Elsevier GmbH. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

A laser beam at wavelength 647 nm is focused on a sample of 5 mol% MgO-doped lithium niobate crystal for domain inversion by a conventional external electric field. In this case, a reduction of 36% in the electric field required for domain nucleation (nucleation field) is observed. To the best of our knowledge, it is the longest wavelength reported for laser-induced domain inversion. This extends the spectrum of laser inducing, and the experimental results are helpful to understand the nucleation dynamics under laser illumination. The dependence of nucleation fields on intensities of laser beams is analysed in experiments.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

A specklegram in a multimode fiber (MMF) has successfully been used as a sensor for detecting external disturbance. Our experiments showed that the sensitivity in the sensor with a multiple longitudinal-mode laser as its source was much higher than that with a single longitudinal-mode laser. In addition, the near-field pattern observations indicated that the coupling between different transverse modes in the MMF is quite weak. Based on the experimental results, a theoretical model for the speckle formation is proposed, taking a bend-caused phase factor into consideration. It is shown in the theoretical analysis that the interferences between different longitudinal modes make a larger contribution to the specklegram signals. (C) 2007 Optical Society of America.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

A novel method incorporating the shielded method and the post-processing method has been proposed to fabricate the pi-phase-shilted fibre grating. Then an Er-doped pi-phase-shifted distributed feedback fibre grating laser has been fabricated using the grating. The laser threshold is 20 mW. When pumped with 90 mW light at 980 nm, the laser gives an output of 1.1 mW. Its signal-to-noise ratio is better than 60 dB. It is demonstrated that the laser is single mode operation by means of a Fabry-Perot scanning interferometer.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Si:SbOx films have been deposited by reactive dc-magnetron sputtering from a Sb target with Si chips attached in Ar + O-2 with the relative O-2 content 7%. The as-deposited films contained Sb metal, Sb2O3, SiO, Si2O3 and SiO2. The crystallization of Sb was responsible for the changes of optical properties of the films. The results of the blue laser recording test showed that the films had good writing sensitivity for blue laser beam (406.7 nm), and the recording marks were still clear even if the films were deposited in air 60 days, which demonstrated that doping silicon in SbOx films can improve the stability of SbOx films. High reflectivity contrast of about 36% was obtained at a writing power 6 mW and writing pulse width 300 ns. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Fe:BiOx films are fabricated on K9 glass substrates by rf-magnetron sputtering of a BiFeO target under argon atmosphere with increasing sputtering power from 80 to 200 W at room temperature. It is found that the thin films grown at the sputtering power of 160W can be formed at an appropriate deposition rate and have an improved surface morphology. The XPS result reveals that the films investigated are comprised of Bi, Fe and O elements. A typical XRD pattern shows that no phase transition occurs in the films up to 400 degrees C. The results of the blue laser recording test demonstrate that the Fe:BiOx films have good writing sensitivity for blue laser beam (406.7 nm) and good stability after reading 10000 times. The recording marks of 200nm or less are obtained. These results indicate that the introduction of Fe into BiOx films can reduce the mark size and improve the stability of the films.