Absorption spectrum from 400 to 2000 run and upconversion fluorescence spectra under 940 nm pumping of YAG single crystal codoped with 5 at.% Yb3+ and 4 at.% Tm3+ were studied at room temperature. The blue upconversion emission centered at 483 nm corresponds to the transition (1)G(4) -> H-3(6), the emission band around 646 nm corresponds to the transition (1)G(4) -> F-3(4) of Tm3+. Energy transfer from Yb3+ to Tm3+ is mainly nonradiative and the transfer efficiency was experimentally assessed. The line strengths, transition probabilities and radiative lifetimes of (1)G(4) level were calculated by using Judd-Ofelt theory. Gain coefficient calculated from spectra shows that the upconversion corresponding with transitions (1)G(4) -> H-3(6) in YAG doped with Yb3+ and Tm3+ is potentially useful for blue light Output. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report both continuous-wave and passively mode-locked laser actions in a Yb3+-doped gadolinium yttrium oxyorthosilicate Yb:GdySiO(5) (Yb:GYSO) crystal. Continuous-wave (CW) laser operations were compared under different pump conditions with high-power diodes of different wavelengths and fiber cores. CW mode-locking was obtained with a semiconductor saturable absorber mirror.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An Ho3+-doped YAlO3 (Ho : YAP) single crystal has been grown by the Czochralski technique. The polarized absorption spectra, polarized fluorescence spectra and fluorescence decay curve of the crystal are measured at room temperature. The spectroscopic parameters are calculated based on Judd-Ofelt theory, and the effective phenomenological intensity parameters Omega(2,eff), Omega(4,eff) and Omega(6,eff) are obtained to be 2.89 x 10(-20), 2.92 x 10(-20) and 1.32 x 10(-20) cm(2), respectively. The room-temperature fluorescence lifetime of the Ho3+ 5I(7) -> I-5(8) transition is measured to be 8.1 ms. Values of the absorption and emission cross-sections with different polarizations are presented for the I-5(7) manifold, and the polarized gain cross-section curves are also provided and discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

There are two different effects to generate group delay dispersion by multilayer thin film mirrors: chirper effect and Gires-Tournois effect. Both effects are employed to introduce desired dispersion in the designed mirror. Thus the designed mirror provides large dispersion throughout broad waveband. Such mirror can be used for dispersion compensation in Ti:sapphire femtosecond lasers. Most group delay dispersion of a 5-mm Ti:sapphire crystal can be compensated perfectly with only four bounces of the designed mirror.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We design and experimentally demonstrate some negative dispersion mirrors with optimized Gires-Tournois interferometers. The mirror structure is composed of 38 alternating Ta2O5 and SiO2 layers and could be regarded as two sections: high-reflectivity section consisting of a series of quarter-wavelength optical thickness stacks and negative-dispersion section consisting of only 13 layers. The designed mirrors exhibit the expected performance. These mirrors were fabricated by using ion beam sputtering. By adopting such mirrors, dispersion of a mode-locked femtosecond Ti:sapphire laser has been compensated for mostly. With two series of the mirrors, 32 fs and 15 fs pulses have been obtained respectively.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

TiO2 and ZrO2 films are deposited by electron-beam (EB) evaporation and by sol-gel process. The film properties are characterized by visible and Fourier-transform infrared spectrometry, x-ray diffraction analysis, surface roughness measure, absorption and laser-induced damage threshold (LIDT) test. It is found that the sol-gel Elms have lower refractive index, packing density and roughness than EB deposited films due to their amorphous structure and high OH group concentration in the film. The high LIDT of sol-gel films is mainly due to their amorphous and porous structure, and low absorption. LIDT of EB deposited film is considerably affected by defects in the Elm, and LIDT of sol-gel deposited film is mainly effected by residual organic impurities and solvent trapped in the film.