230 resultados para 311-U1325
Resumo:
本文报道了中国纤孔菌属两个新记录种,分别为芮克纤孔菌Inonotus rickii (Pat.) D.A.Reid和杨生纤孔菌Inonotus plorans (Pat.) Bondartsev & Singer。芮克纤孔菌采于海南省保亭县热带植物园,生长在橡胶树上,杨生纤孔菌Inonotus plorans发现于中国西北地区的新疆,生长在杨树上,本文根据中国的材料对这两个种进行了详细描述和显微结构绘图。
Resumo:
作为中国现代社会经济发展的主体发动机,东部沿海地区人地关系的演进状态和趋势不仅决定着地区自身而且决定着整个国家可持续发展的基本取向。有鉴于此,本文试图通过人地关系对应公式进行东部沿海地区人地关系演进状态的总体评价。评价的结果表明:第一,与中西部相比,东部沿海地区人地关系演进的实际紧张状态严峻的多,人地关系演进系数达到了2.13 (表观);第二,在地区人地关系的演进过程中,经济活动和人口集聚起着决定影响,其中尤以经济活动的作用最为关键,其贡献度达到75%;第三,未来人地关系状态的协调和改善主要取决于地区自身资源环境基础的扩展和改造能力。
Resumo:
To clarify the mechanism of organic-inorganic hybrid membrane formation by phase-inversion method, the thermodynamical and theological properties of PSF/TiO2 casting solution were investigated by the viscosity measurement and the triangle phase diagram, respectively. TiO2 introduction decreased the non-solvent tolerance of casting solution with non-solvent 20% ethanol aqueous solution, which caused thermodynamic enhancement of phase separation, and also resulted in the change of theological properties from Newtonian fluid to non-Newtonian fluid and the viscosity increase of casting solution, which induced rheological hindrance in demixing process
Resumo:
Uniform octahedral YVO4:Eu3+ microcrystals have been successfully prepared through a designed two-step hydrothermal conversion method. One-dimensional precursor Y4O(OH)(9)NO3 was first prepared through a simple hydrothermal process without using any surfactant, catalyst or template. Subsequently, well-defined octahedral YVO4 was synthesized at the expense of the precursor during a hydrothermal conversion process. XRD results demonstrate that the diffraction peaks of the final product can be well indexed to the pure tetragonal phase of YVO4.
Resumo:
The hexagonal and monoclinic LaPO4:Eu3+ nanorods can be selectively synthesized through a simple hydrothermal method by only adjusting the reaction temperature. Hexagonal and monoclinic LaPO4:Eu3+ nanorods can be prepared at 120 and 180 degrees C, respectively. The phase conversion of LaPO4:Eu3+ under different temperatures is investigated in detail. Moreover, the influence of the temperature on the intensity and the shift of the peaks of the excitation and emission spectra is discussed, and the decay lifetime of the Eu3+ ions of the sample obtained at different temperature also have been investigated in this paper.
Resumo:
A polymeric gene carrier was developed to deliver vascular endothelial growth factor (VEGF) small interfering RNA (siRNA) for prostate cancer cells in a target-specific manner. Prostate cancer-binding peptide (PCP) was conjugated with polyethylenimine (PEI) via a poly(ethylene glycol) (PEG) linker (PEI-PEG-PCP). The PEI-PEG-PCP conjugate could effectively condense siRNA to form stable polyelectrolyte complexes (polyplexes) with an average diameter of approximately 150 nm in an aqueous solution. VEGF siRNA/PEI-PEG-PCP polyplexes exhibited significantly higher VEGF inhibition efficiency than PCP-unmodified polycationic carriers (PEI-PEG or PEI) in human prostate carcinoma cells (PC-3 cells). The enhanced gene silencing activity of VEGF siRNA/PEI-PEG-PCP was maintained even under serum conditions, owing to the steric stabilization of the polyplexes with hydrophilic PEG grafts. Confocal microscopic studies revealed that the siRNA/PEI-PEG-PCP polyplexes were delivered into PC-3 cells in a PCP ligand-specific manner.
Resumo:
采用紫外可见分光光度法、ESI-MS(电喷雾质谱)与HPLC-UV(高效液相色谱)测定技术分析了等离子体种子处理机处理人参种子对所栽培人参中人参皂苷含量的影响。结果发现,人参种子受到等离子体与梯度磁场综合作用处理后,培育出的人参其总皂苷含量随磁化电流强度的改变呈现近似的正态分布。其中,在磁化线圈电流强度为1.1~1.5 A处理种子后,栽培的人参中总皂苷含量较高。建立了电喷雾质谱分析人参提取物中人参皂苷的半定量方法,方法便捷地反映了未处理及处理后的人参种子所栽培的人参中皂苷成分的含量变化。
Resumo:
High-solids, low-viscosity, stable poly(acrylamide-co-acrylic acid) aqueous latex dispersions were prepared by the dispersion polymerization of acrylamide (AM) and acrylic acid (AA) in an aqueous solution of ammonium sulfate (AS) medium using anionic polyelectrolytes as stabilizers. The anionic polyelectrolytes employed include poly(2-acrylamido-2-methylpropanesulfonic acid sodium) (PAMPSNa) homopolymer and random copolymers of 2-acrylamido-2-methylpropanesulfonic acid sodium (AMPSNa) with methacrylic acid sodium (MAANa), acrylic acid sodium (AANa) or acrylamide (AM). The influences of stabilizer's structure, composition, molecular weight and concentration, AA/AM molar feed ratio, total monomer, initiator and aqueous solution of AS concentration, and stirring speed on the monomer conversion, the particle size and distribution, the bulk viscosity and stability of the dispersions, and the intrinsic viscosity of the resulting copolymer were systematically investigated. Polydisperse spherical as well as ellipsoidal particles were formed in the system. The broad particle size distributions indicated that coalescence of the particles takes place to a greater extent.
Resumo:
We report the electrical characterization of hybrid permeable-base transistors with tris(8-hydroxyquinoline) aluminum as emitter layer. These transistors were constructed presenting an Al/n-Si/Au/Alq(3)/V2O5/Al structure. We investigate the influence of the V2O5 layer thickness and demonstrate that these devices present high common-base and common-emitter current gain, and can be operated at very low driving voltages, lower than 1 V, in both, common-base and common-emitter modes.
Resumo:
Phase separation of bisphenol A polycarbonate (PC) and poly(methyl methacrylate) (PMMA) thin blend film is suppressed by addition of solid epoxy oligomer. Epoxy has strong intermolecular interactions with both PC and PMMA, while PC and PMMA are quite incompatible with each other. Consequently, phase separation in the PC/PMMA blend film pushes epoxy to the interface; at the same time, PC and epoxy react readily at the interface to form a cross-linking structure, binding PMMA chains together. Therefore, the interface between PC and PMMA is effectively reinforced, and the PC/PMMA thin blend film is stabilized against phase separation. On the other hand, only an optimal content of epoxy (i.e., 10 wt %) can serve as an efficient interfacial agent. In contrast to the traditional reactive compatibilization, here we observed that the cross-linking structure along the interface is much more stable than block or graft copolymers. Atomic force microscopy (AFM) is used to characterize the morphological changes of the blend films as a function of annealing time. Two-dimensional fast Fourier transform (2D-FFT) of AFM data allows quantitative investigation of the scaling behavior of phase separation kinetics.
Resumo:
The influences of additive, diluents, temperature, acidity of the aqueous phase on the interfacial behavior of primary amine N1923 in sulfate media have been investigated using the Du Nouy ring method. In addition, the effect of concentration of thorium(IV) loaded in the organic phase on the interfacial tension has also been studied. The interfacial tension isotherms are processed by matching different adsorption equations such as the Gibbs and the Szyszkowski. The surface excess at the saturated interface (Gamma (max)) and the minimum bulk concentration of the extractant necessary to saturate the interface (C-min) under different conditions are calculated according to two adsorption equations to be presented in comprehensive tables and figures. It appears that primary amine N1923 has strong interfacial activity and behaves very differently in various diluents systems. The surface excess at saturated interface increase with the type of diluerits in the following order: chloroform < aromatic hydrocarbons < aliphatic hydrocarbons. The relationship between the interfacial activity and kinetics of thorium extraction by primary amine N1923 has been discussed by considering different factors. However, the interfacial activity of primary amine N1923 is only a qualitative parameter suggesting the interfacial mechanism for thorium extraction, it cannot give strong evidence quantitatively supporting this mechanism.
Resumo:
Ca2Gd8(SiO4)(6)O-2: A(A = Ph2+, Tm3+) phosphors were prepared through the sol-gel process. X-ray diffraction (XRD), scanning electron microseopy(SEM) and photoluminescence spectra were used to characterize the resulting phosphors. The results of XRD indicate that the phosphors crystallized completely at 1000 degreesC. SEM study reveals that the average grain size is 300 similar to 1000 nm. In Ca2Gd8(SiO4)(6)O-2: Tm3+ phosphors, the Tm3+ shows its characteristic blue emission at 456 nm (D-1(2)-F-3(4)) upon excitation into its H-3(6)-D-1(2)(361 nm), with an optimum doping concentration of 1 mol% of Gd3+ in the host lattices. In Ca2Gd8(SiO4)(6)O-2: Pb2+, Tm3+ phosphors, excitation into the Ph2+ at 266 nm (S-1(0)-P-3(1)) yields the emissions of Gd3+ at 311 nm (P-6-S-8) and Tm3+ at 367 nm (D-1(2)-H-3(6)) and 456 our (D-1(2)-F-3(4)), indicating that energy transfer processes of Pb2+-Gd3+ and Ph2+-Tm3+ have occur-red in the host lattices.
Resumo:
A new sensitive assay for aspartate aminotransterase (AST) and alanine aminotransferase (ALT) activities in biofluids was developed, based on the separation and detection of alanine, glutamate, and aspartate using capillary electrophoresis (CE) with electrochemiluminescence (ECL) detection. The three amino acids were separated in 5 mM phosphate of pH 2.1 as background electrolyte, and detected on a 500 mu m platinum disk electrode at 1.2 V (versus Ag/AgCl) in the presence of 10 mM tris(2,2'-bipyridyl)ruthenium(II) dissolved in 80 mM phosphate of pH 10.5. A mass detection limit of 37.3 fmol (or 81.5 fmol) for glutamate, corresponding to the product in the enzyme reaction catalyzed by 1.24 x 10(-9) U AST (or 2.72 x 10(-9) U ALT) in a 30 min reaction period, was achieved. This assay was applied to investigate the cytotoxicity effect of ethanol on HepG2 cells and differentiating nonalcoholic steatohepatitis (NASH) from alcoholic liver disease, indicating that the technique is promising for the application in the cell biological and clinical fields.
Resumo:
A facile method for the synthesis of biphenyl polyimides, which involves the nickel-catalyzed coupling of aromatic dichlorides containing imide structure in the presence of zinc and triphenylphosphine, has been developed. The polymerizations proceeded smoothly under mild conditions and produced biphenyl polyimides with inherent viscosities of 0.13-0.98 dL/g. The polymerizations of bis(4-chlorophthalimide)s with bulky side substituents gave high molecular weight polymers. Low molecular weight polymers from bis(4-chlorophthalimide)s containing rigid diamine moieties and bis(3-chlorophthalimide)s were obtained because of the formations of polymer precipitate and cyclic oligoimides, respectively. The effects of various factors, such as amount of catalyst, solvent volume, ligand, reaction temperature, and time, on the polymerization were studied. The random copolymerization of two bis(chlorophthalimide)s in varying proportions produced medium molecular weight material. The TgS of prepared polyimides were observed at 245-311 degreesC, and the thermogravimetry of polymers showed 10% weight loss in nitrogen at 470-530 degreesC.