215 resultados para high power induction machine
Resumo:
高功率双包层光纤放大器在光纤传感、光纤通讯、光谱测量和惯性约束聚变等领域有广泛应用。介绍了两种获得放大激光输出的高功率双包层光纤放大器:单频双包层光纤放大器和脉冲双包层光纤放大器。分析了它们的工作原理及关键技术,并对国内外近期进展作了综述。
Resumo:
采用光纤缠绕的方法,来抑制大模场面积(LMA)双包层光纤激光器中的高阶模振荡。将光纤缠绕至两种不同半径,实验测量了相应条件下激光器的输出功率和光束质量因子M2。缠绕半径为165mm时,输出功率为217W,M2为2.96;缠绕半径为52mm时,输出功率为160W,M2为1.38。光纤激光器相应的斜率效率分别为60%和48%。光纤缠绕半径较小时,虽然激光器输出功率减小,但其亮度是大缠绕半径时对应值的3.4倍。
Resumo:
以短的高掺杂浓度的掺铥硅基光纤为增益介质,采用790 nm波长的激光二极管(LD)为抽运源,得到了波长为2 μm的高功率激光输出。当光纤长度为7 cm时,激光器的阈值泵浦功率为135 mW,最大输出功率为1.09 W,斜率效率为9.6%(相对于耦合进光纤的抽运功率)。该激光器的输出稳定性在5%以内。此外,我们还观察分析了工作温度和其他腔结构参量对该激光器工作性能的影响。
Resumo:
尽管双包层光纤激光器的散热性能好于传统的固体激光器的散热性能,光纤激光器中的热沉积仍然是限制提高其输出功率的重要因素.以双端抽运的400W双包层光纤激光器为实例,定量分析了光纤内的热沉积分布.根据所建立的散热模型,为了确保千瓦级双包层光纤激光器安全稳定的运行,抽运端附近的对流换热系数应大于2.8×10-2W·cm-2K-1.据此设计出高功率双包层光纤激光器抽运端冷却装置并成功应用在激光系统中,获得了千瓦级的激光输出.
Resumo:
文中报道了一台采用激光二极管部分边缘泵浦方式的高功率薄片激光器,晶体尺寸是1 mm×10 mm×60 mm。Cr4+:YAG被用来作为被动调Q晶体,在重复频率高于10kHz时,获得了脉宽10ns,平均功率70W,斜线效率为36\%的激光输出。通过控制泵浦光束直径的大小,我们在厚度方向得到了近似衍射极限的光束输出。整个激光器结构紧凑,大小为60 mm×174 mm×150 mm。
Resumo:
采用大功率半导体激光器抽运25m掺Yb双包层光纤,在单程装置中,前向(SPF)和后向(SPB)分别获得了1.46w和1.82w最大超荧光功率,斜度效率分别为23.4%0和29.2%,3dB带宽最大为11nm。采用特定范围波长双色镜作为前腔镜,形成双程前向(DPF)装置,获得最大超荧光输出功率2.12W,此时斜度效率为43.2%,中心波长在1070nm,输出光谱平坦性较好,3dB带宽从单程的11nm提高到42nm。
Resumo:
A high-power ytterbium-doped fiber laser (YDFL) with homemade double-clad fiber (DCF) is introduced in this letter. The geometric parameter and laser characteristics of the fiber have been studied. With one-end-pumping scheme, pumped by a high-power laser diode with launching power of 280 W, a maximum continuous wave (CW) output of 110 W is obtained with an optical-to-optical efficiency of 40%.
Resumo:
Multi-mode rate equations have been developed to investigate mode competition in high-power acousto-optically Q-switched planar waveguide lasers. The mode competition arises from coupling effects and temporal losses in the transform between guided modes and free-space propagation. Pulse-to-pulse instability and temporal beam distortions are enlarged by mode competition when the laser works in the multi-mode regime. The influence of parasitic oscillation is also discussed. A Nd:YAG planar waveguide laser has been established with a folded hybrid/unstable resonator. A maximum average power of 83 W with a beam propagation factor M-x(2) x M-y(2) = 1.2 x 1.4 is obtained. The theoretical simulation agrees well with the experimental observation. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
A high-power Ytterbium-doped fiber laser (YDFL) with homemade double clad fiber (DCF) is introduced in this paper. The output power characteristics of a linear cavity fiber laser have been studied theoretically by solving the rate equations and experimentally tested with single- and double-end-pumping configurations. When both ends of the fiber are pumped by two high-power laser diodes with a launched power of similar to 300 W each, a maximum CW output of 444 W is obtained with a slope efficiency of similar to 75%. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
氟磷酸盐玻璃系统南于其特殊的光学性能和优良的机做与热学性能一直是特种光学玻璃材料领域的一个研究热点。总结了氟磷酸盐玻璃的分类及玻璃组分与其结构的关系,综述了氟磷玻璃在光学器件、高能高功率激光玻璃、光纤激光器、光纤放大器及上转换发光基质材料等领域上的应用,并对其未来的发展进行了展望。
Resumo:
abstract {Silica glass is an attractive host matrix for the emission ions of rare earth and transition metal ions because it has small thermal expansion coefficient, strong thermal resistance, large fracture strength and good chemical durability and so on. However, a major obstacle to using it as the host matrix is a phenomenon of concentration quenching. In this paper, we introduces a novel method to restrain the concentration quenching by using a porous glass with SiO2 content > 95% (in mass) and prepare intense fluorescence high-SiO2 glasses and high-SiO2 laser glass. The porous glass with high-SiO2 content was impregnated with rare-earth and transition metal ions, and consequently sintered into a compact non-porous glass in reduction or oxidization atmospheres. Various intense fluorescence glasses with high emission yields, a vacuum ultraviolet-excited intensely luminescent glass, high silica glass containing high concentration of Er3+ ion, ultrabroad infrared luminescent Bi-doped high silica glass and Nd3+-doped silica microchip laser glass were obtained by this method. The porous glass is also favorable for co-impregnating multi-active-ions. It can bring effective energy transferring between various active ions in the glass and increases luminescent intensity and extend range of excitation spectrum. The luminescent active ions-doped high-SiO2 glasses are potential host materials for high power solid-state lasers and new transparent fluorescence materials.}
Resumo:
Nd-doped and Nd-Al-codoped high silica glasses were obtained by sintering porous glass impregnated with Nd3+ and Al3+ ions. The absorption, fluorescence spectra and fluorescence lifetime of Nd-doped and Nd-Al-codoped high silica glasses were measured. The intensity parameters Omega(1), ( t = 2, 4, 6), fluorescence lifetime, radiative quantum efficiency and stimulated emission cross section were calculated by Judd-Ofelt theory. The effect of aluminum codoping on the fluorescence and structural properties of Nd-doped silica glass has been discussed. By comparing the spectroscopic properties with other Nd-doped oxide glasses and commercial silicate glasses, this Nd-doped high silica glass is likely to be a promising laser material for use in high power and high repetition rate lasers.
Resumo:
高功率脉冲氙灯主要在惯性约束聚变(ICF)研究中用作高功率激光驱动器的抽运光源,其各项性能和使用寿命对高功率激光驱动器的整体工作性能影响很大。在改进制灯材料和管壁结构的基础上,研制了两种不同规格的细长型高功率脉冲氙灯:一种是φm16mm,放电弧长为1140mm;另一种是φm17mm,放电弧长为1270mm。研制的细长型高功率脉冲氙灯,其极限负载能量大、工作寿命长、辐射效率高,工作性能较原先脉冲氙灯有很大的改进和提高。
Resumo:
:为提高大功率脉冲氙灯的封接强度,将微晶玻璃作为封接材料引入到氙灯封接应用中. 以 Bi2O3,ZnO,Al2O3,MgO,CaCO3,SiO2,BaO,H3BO3,P2O5,Na2O 为原料,通过高温熔融制备了大功率脉冲氙灯封接 用微晶玻璃样品. 测试了样品的热膨胀系数,并通过差热分析(Differential Thermal Analysis,DTA)对脉冲氙灯 微晶玻璃的封接温度进行了讨论,用X 射线衍射(X-ray diffraction ,XRD)表征了封接玻璃,并进行了分析. 将 制得的样品磨成玻璃粉末,制成膏剂状玻璃焊料,对大功率脉冲氙灯进行封接,得到大功率脉冲氙灯的微晶 玻璃封接件. 通过氦质谱检漏仪检测,1#、2#、4#封接件气密性良好,达到10-6 Pa.
Resumo:
Bulk-lasses have been prepared in the TeO2-ZnO-ZnCl2 systems. Their characteristic temperatures were determined and analyzed. Raman and FT-IR spectra were used to analyze the effect of ZnCl2 on the structure and spectral properties of tellurite glasses and OH- groups in this glass system. The spectroscopic properties including absorption spectra, emission cross-sections and fluorescence lifetimes of Yb3+ in TeO2-ZnO-ZnCl2 were measured and calculated. It is demonstrated that the progressive replacement less than 20 mol% of TeO2 by ZnCl2 improves the thermal stability, removes the OH- groups, turns TeO4 bipyramidal arrangement into TeO3 (and/or TeO3+1) trigonal pyramids structures and results in the decrease of the symmetry of the structure, which increases the emission cross-sections and lifetimes. But when the content of ZnCl2 up to 30 mol%, the glass system becomes more hygroscopic and introduces more OH- groups, which decrease the emission cross-sections and shorten the lifetimes. The results show that the glass system with (TeO2)-Te-69-(ZnO)-Zn-10-20ZnCl(2)-1Yb(2)O(3) is a desirable component for active laser media for high power generation. (c) 2005 Elsevier B.V. All rights reserved.