226 resultados para UV melting
Resumo:
The PVT data of five kinds of biaxially oriented polypropylene (BOPP) Resins was measured by the PVT-100 apparatus. Thermal expansion coefficients (alpha) and isothermal compressibility (beta) were evaluated from Tait equation in the melting state and then compared with those fitted with the value of experiment. The results showed that it was reasonable to calculate alpha and beta with Tait equation in the melting state. At the same time, it was found that thermal expansion coefficients, isothermal compressibility and the melting temperature (T-m) of one of BOPP melts (S28C) were lower than those of the others in the same test conditions, indicating that the volume deformation of S28C resin is' less so that it could be realized to avoid arising surface defects of the film (biaxially oriented polypropylene film) due to. contracting, thereby decrease damage to the film in the subsequence process. Accordingly superior processing properties of S28C resin are confirmed from PVT. speciality.
Resumo:
After meso-tetra (alpha, alpha, alpha, alpha-O-phenylacetyl benzene)porphyrin combined with McAb 1F2, there was a significant hyperchromic effect, indicating that the combination of porphyrin and antibody is rigid and compact, aromatic amino acids exist at the combining sites of antigen in antibody. These aromatic amino acids are Trys and Trps, but the numbers of Trp are more than that found for Trys. The stochiometric ratio of porphyrin to 1F2 is 1:1, the disassociation constant was determined as(2.084+/-0.216) x 10(-10) mol/L by a method of fluorescence quenching, showing that both have a high affinity.
Resumo:
Nonisothermal crystallization and melting behavior of poly(3-hydroxybutyrate) (PHB) and maleated PHB were investigated by differential scanning calorimetry using various cooling rates. The results show that the crystallization behavior of maleated PHB from the melt greatly depends on cooling rates and its degree of grafting. With the increase in cooling rate, the crystallization process for PHB and maleated PHB begins at lower temperature. For maleated PHB, the introduction of maleic anhydride group hinders its crystallization, causing crystallization and nucleation rates to decrease, and crystallite size distribution becomes wider. The Avrami analysis, modified by Jeziorny, was used to describe the nonisothermal crystallization of PHB and maleated PHB. Double melting peaks for maleated PHB were observed, which was caused by recrystallization during the heating process.
Resumo:
We have employed several techniques, including cyclic voltammetry, UV-Vis spectrometry, small-angle X-ray diffraction, X-ray photoelectron spectroscopy and electrochemical impedance spectroscopy, to characterize the formation processes and interfacial features of ultrathin multilayer films of silicotungstate and a cationic redox polymer on cysteamine-coated Au electrodes self-assembled monolayers. All of these techniques confirm that the multilayer films are built up stepwise as well as uniformly in a layer-by-layer fashion. In particular, the electrochemical impedance spectroscopy is successfully used to monitor the multilayer deposition processes. It has been proved that the electrochemical impedance spectroscopy is a very useful technique in characterization of multilayer films because it provides valuable information about the interfacial impedance features.
Resumo:
In this work, crystallization and melting behavior of metallocene ethylene/alpha-olefin copolymers were investigated by differential scanning calorimetry (DSC) and atomic force microscopy (AFM). The results indicated that the crystallization and melting temperatures for all the samples were directly related to the long ethylene sequences instead of the average sequence length (ASL), whereas the crystallization enthalpy and crystallinity were directly related to ASL, that is, both parameters decreased with a decreasing ASL. Multiple melting peaks were analyzed by thermal analysis. Three phenomena contributed to the multiple melting behaviors after isothermal crystallization, that is, the melting of crystals formed during quenching, the melting-recrystallization process, and the coexistence of different crystal morphologies. Two types of crystal morphologies could coexist in samples having a high comonomer content after isothermal crystallization. They were the chain-folded lamellae formed by long ethylene sequences and the bundlelike crystals formed by short ethylene sequences. The coexistence phenomenon was further proved by the AFM morphological observation.
Resumo:
The local structure and the valences of europium in SrBPO5:Eu prepared in air were checked by means of XAFS at Eu-L-3 edge. From the EXAFS results, it was discovered that the doped europium atoms were nine-coordinated by oxygen atoms and the distances of bond Eu-O were 2.42 Angstrom in the host. From the XANES data, it was found that the divalent and trivalent europium coexisted in the matrix. The emission spectra excited by VUV or UV exhibited a prominent broad band due to the 4f(6)5d-4f(7) transition of Eu2+ ions, which indicated that the trivalent europium ions were reduced in air in the matrix at high temperature by the defects [V-Sr]" formed by aliovalent substitution between Sr2+ and Eu3+ ions. The VUV excitation spectra in 100-200 nm range showed that the matrix had absorption bands with the maxima at about 130 and 150 nm, respectively.
Resumo:
Fe2O3 sol with the particle diameter of 3-5 nm was flocculated by the addition of SDS, and the flocculate formed was redispersed by the further addition of that surfactant. Thus the surfactant bilayer was formed on the surface of Fe2O3. The emulsion polymerization of styrene (St) adsolubilized oil the surfactant adsorbed bilayer was carried out by initiator potassium persulfate (KPS). The UV-Vis and surface photovoltage spectra (SPS) indicate that the Fe2O3 particles were encapsulated in polystyrene(PSt) successfully.
Resumo:
The overall isothermal crystallization kinetics and melting behavior of poly(beta-hydroxybutyrate) (PHB) and maleated PHB with different graft degree were studied by using differential scanning calorimetry (DSC). The Avrami analysis indicates that the introduction of maleic anhydride results in the decrease in the overall crystallization rate of PHB, but does not affect its nucleation mechanism and geometry of crystal growth. The activation energy of the overall crystallization process increases with the increase in graft degree. The phenomenon of multiple melting endotherms is observed, which results from melting and recrystallization during the DSC heating run.
Resumo:
Crystallization and melting behavior of short ethylene sequence of metallocene ethylene/alpha -olefin copolymer with high comonomer content have been studied by standard DSC and modulated-temperature differential scanning calorimetry (M-TDSC) technique. In addition to high temperature endotherm around 120 degreesC, a low temperature endotherm is observed at lower temperatures (40-80 degreesC), depending on time and temperature of isothermal crystallization. The peak position of the low temperature endotherm T-m(low) varies linearly with the logarithm of crystallization time and the slope, D, decreases with increasing crystallization temperature T-c. The T-m(low) also depends on the thermal history before the crystallization at T-c, and an extrapolation of T-m(low) (30.6 degreesC) to a few seconds has been obtained after two step isothermal crystallization before the crystallization at 30 degreesC. The T-m(low) is nearly equal to T-c, and it indicates that the initial crystallization at low temperature is nearly reversible. Direct evidence of conformational. entropy change of secondary crystallization has been obtained by using M-TDSC technique. Both the M-TDSC result and the activation energy analysis of temperature dependence suggest that crystal perfection process and conformational entropy decreasing in residual amorphous co-exist during secondary crystallization.
Resumo:
Electrochemically induced three conformational transitions of calf thymus DNA from B-10.4 to Z(10.2)-DNA and from B-10.2 to B-10.4 and to C-DNA in 10 mM phosphate buffer solution (pH 7.21) at glassy carbon electrode are found and studied by in situ circular dichroism (CD) thin layer spectroelectrochemistry with singular value decomposition least square (SVDLS) analysis. It indicates that the so-called B-10.2 form and the C-form of DNA may be composed of B-10.4 and left-A DNA and of B-10.4 and right-A DNA, respectively. The irreversible electrochemical reduction of adenine and cytosine groups in the DNA molecule is studied by UV-Vis spectroelectrochemistry. Some electrochemical parameters alphan = 0.17, E-0' = -0.70 V (vs. Ag/AgCl), and the standard heterogeneous electron transfer rate constant, k(0) = 1.8 x 10(-5) cm s(-1) are obtained by double logarithmic analysis and non-linear regression. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Multiple melting behavior was observed in the differential scanning calorimetry (DSC) scans for the isothermally crystallized poly(iminosebacoyl iminodecamethylene) (PA1010) samples. Coexistence of crystal populations with different lamellar thickness in PA1010 was discussed by means of DSC, wide-angle X-ray diffraction (WAXD), and small-angle X-ray scattering techniques. During crystallization of the polymer, a major lamellar crystal population developed first, which possessed a higher melting temperature. However, a small fraction of the polymer formed minor crystal population with thinner lamellae, which was metastable and, upon post-annealing, could grow into more stable and thicker lamellae through melting and recrystallization process. Lamellae insertion or stacks would develop during the post-annealing at a lower temperature for the isothermally crystallized samples; thus, multiple crystal populations with different thickness could be produced. It is the multiple distribution of lamella thickness that gives rise to multiple melting behavior of crystalline polymers. (C) 2000 John Wiley & Sons, Inc.
Resumo:
The origins of the single- and double-melting endotherms of isotactic polypropylene crystallized at different temperatures were studied carefully by differential scanning calorimetry, wide-angle X-ray diffraction, and small-angle X-ray scattering. The experimental data show that spontaneous crystallization occurs when the crystallization temperature is lower than 117 degrees C; thus the lamellae formed are imperfect. At a lower heating rate, the recrystallization or reorganization of these imperfect lamellae leads to double endotherms. On the other hand, when the crystallization temperature is higher than 136 degrees C, two major kinds of lamellae with different thickness are developed during the isothermal process, which also results in the double-melting endotherms. In the intermediate temperature range the lamellae formed are perfect, and there is only a single peak in the distribution of lamellar thickness. This explains the origin of the single-melting endotherm. (C) 2000 John Wiley & Sons, Inc.
Resumo:
Phenyl-capped trianiline and tetraaniline in the leucoemeraldine oxidation state were synthesized through a modified-pseudo-high-dilution technique. The chemical oxidation process of these compounds were studied by UV-Vis spectra. It was found that phenyl-capped trianiline in the leucoemeraldine oxidation state was oxidized to its EB form and then decomposed, Phenyl-capped tetraaniline was oxidized to its EB form and then to the pernigraniline oxidation state.
Resumo:
After isothermal crystallization, poly(ethylene terephthalate) (PET) showed double endothermic behavior in the differential scanning calorimetry (DSC) heating scan. During the heating scans of semicrystalline PET, a metastable melt which comes from melting thinner lamellar crystal populations formed between the low and the upper endothermic temperatures. The metastable melt can recrystallize immediately just above the low melting temperature and form thicker lamellae than the original ones. The thickness and perfection depends on the crystallization time and crystallization temperature. The crystallization kinetics of this metastable melt can be determined by means of DSC. The kinetics analysis showed that the isothermal crystallization of the metastable PET melt proceeds with an Avrami exponent of n = 1.0 similar to 1.2, probably reflecting one-dimensional or irregular line growth of the crystal occurring between the existing main lamellae with heterogeneous nucleation. This is in agreement with the hypothesis that the melting peaks are associated with two distinct crystal populations with different thicknesses. (C) 2000 John Wiley & Sons, Inc.
Resumo:
采用高温固相反应法以硅酸为原料合成了等离子显示用荧光体Zn2 SiO4 ∶Mn ,研究了Zn2 SiO4 ∶Mn的VUV和UV光谱特性 ,表明波长小于 2 0 0nm的部分的基质吸收带主要是氧的 2 p轨道到锌的 3d轨道跃迁产生的 ,波长大于 2 0 0nm的部分的基质吸收带是氧的 2 p轨道到硅的 3p轨道跃迁吸收。在VUV和UV激发下 ,Mn2 +的浓度与发射强度的相关性研究表明 ,在不同区域激发时荧光体的发射强度随着Mn2 +的浓度的变化存在明显不同