160 resultados para Rubber Treatment
Resumo:
The effects of rubber content and temperature on dynamic fracture toughness of ABS materials have been investigated based on the J-integral and crack opening displacement (COD, delta) concepts by an instrumented Charpy impact test. A multiple specimens R-curve method and stop block technique are used. It is shown that the materials exhibit a different toughness behavior, depending on rubber content and temperature. The resistance against stable crack initiation (J(0.2) or delta(0.2)) increases with increasing rubber content. However, J(0.2) first increased with increasing temperature until reaching the maximum value; after that, it decreases with further increasing the temperature. (C) 2000 John Wiley & Sons, Inc.
Resumo:
The graft copolymerization of butyl acrylate onto poly(vinyl alcohol) with eerie ammonium nitrate as redox initiator in a aqueous medium has been investigated. The formation of graft copolymer was confirmed by means of IR, scanning electron microscopy (SEM), and wide-angle X-ray diffraction (WAXD). The percentage of mononer conversion and percentage of grafting varied with concentrations of initiator, nitric acid, monomer, macromolecular backbone (X-n = 1750, M = 80 000), reaction temperature and reaction time. Some inorganic salts and organic solvents have a great influence upon grafting. The reaction mechanism has been explored, and rate equations for the reaction are established. (C) 2000 John Wiley & Sons, Inc.
Resumo:
Controlled cyclization of styrene-butadiene rubber (SBR) was achieved with the aid of cationic catalyst system based on diethylaluminium chloride (AIEt(2)Cl) and benzyl chloride (C6H5CH2Cl) and by working in xylene solution at high temperature (T > 100 degreesC). The main parameters of the cyclization process were investigated. Elastomers with low intrinsic viscosity, ready solubility, free gel were obtained. The products were characterized with IR H-1-NMR, DSC, GPC. The polycyclic structure was determined. (C) 2001 Published by Elsevier Science Ltd.
Resumo:
The fracture behavior of ABS materials with a particle diameter of 110 nm and of 330 nm was studied using instrumented Charpy impact tests. The effects of rubber content and temperature on fracture behavior, deformation mode, stable crack extension, plastic zone size, J-integral value, and crack opening displacement were investigated. In the case of a particle size of 110 nm, the material was found to break in a brittle manner, and the dominant crack mechanism was unstable crack propagation. Fracture toughness increases with increasing rubber content. In the case of a particle size of 330 nm, brittle-to-tough transition was observed. The J-integral value first increases with rubber content, then levels off after the rubber content is greater than 16 wt %. The J-integral value of a particle diameter of 330 nm was found to be much greater than that of 110 nm. The J-integral value of both series first increased with increasing temperature until reaching the maximum value, after which it decreased with further increasing temperature. The conclusion is that a particle diameter of 330 nm is more efficient than that of 110 nm in toughening, but for both series the effectiveness of rubber modification decreases with increasing temperatures higher than 40 degreesC because of intrinsic craze formation in the SAN matrix at temperatures near the glass transition of SAN. (C) 2000 John Wiley & Sons, Inc.
Resumo:
Blends of nylon-6 and epoxidised ethylene propylene diene (eEPDM) rubber were prepared through reactive mixing. It is found that the toughness of nylon-6 can be much improved by this method, and that the particle size of eEPDM is much smaller than that of unexpoxidised EPDM (uEPDM) rubber in a nylon-6 matrix. This indicates that the epoxy group in eEPDM could react with a nylon-6 end group to form a graft copolymer which could act as an interfacial compatibiliser between the nylon-6 and the eEPDM rubber dispersed phase. (C) 1998 Elsevier Science Ltd. All rights reserved.
Resumo:
A super-tough polycarbonate (PC) blend was obtained by using epoxidized ethylene propylene diene (eEPDM) rubber as modifier. The notched Izod impact strength of PC/eEPDM (96/4) blend shows a great improvement, with a value about 25 times of that of pure PC. Finely and homogeneously dispersed rubber particles (0.2-0.8 mu m) in the PC matrix indicated good adhesion between the eEPDM rubber phase and the PC matrix. (C) 1997 Elsevier Science Ltd.
Resumo:
Measurement of iron and manganese is very important in evaluating the quality of natural waters. We have constructed an automated Fe(II), total dissolved iron(TDI), Mn(II), and total dissolved manganese(TDM) analysis system for the quality control of underground drinking water by reverse flow injection analysis and chemiluminescence detection(rFIA-CL), The method is based on the measurement of the metal-catalyzed light emission from luminol oxidation by potassium periodate. The typical signal is a narrow peak, in which the height is proportional to light emitted and hence to the concentration of metal ions. The detection limits were 3 x 10(-6) mu g ml(-1) for Fe(II) and the linear range extents up to 1.0 x 10(-4) and 5 x 10(-6) mu g ml(-1) for Mn(II) cover a linear range to 1.0 x 10(-4) mu g ml(-1). This method was used for automated in-situ monitoring of total dissolved iron and total dissolved in underground water during water treatment. (C) 1997 Elsevier Science B.V.
Resumo:
In this paper, epoxidation of ethylene propylene diene rubber by in situ generated performic acid is discussed. The samples have been characterized by infra-red and H-1-nuclear magnetic resonance analyses. Quantitative analysis of the reaction products is made possible by using the methyl deformation band at 1377 cm(-1) as internal standard. The conversion of double bonds increases rapidly within the first 1 h, then gradually, over 2 h, has only a slight increase. The maximum conversion ratio of double bonds is about 70%. The relative content of epoxy groups has a top value at about 7 h. The side reactions are also discussed. (C) 1997 Elsevier Science Ltd.
Resumo:
Using the wide-angle X-ray diffraction method, the variation of crystallographic parameters of poly(aryl ether ether ketone ketone) (PEEKK) has been studied in different heat treatment temperatures. All the reflections and their intensities as well as their Miller indices are presented in detail according to an orthorhombic system. The investigation indicates that the unit cell parameters a, b, c and the unit cell volume V systematically decrease with increasing heat treatment temperature. This variation is interpreted by the change of conformation of polymer molecular chains during thermal treatment. The results calculated from the formula of degree of crystallinity (W-c,W-x) for PEEKK, which was derived based on X-ray scattering intensity theory and the graphic multipeak resolution method, are compatible with the density measurement (W-c,W-d) and calorimetry (W-c,W-h) values. (C) 1997 Elesevier Science Ltd.