317 resultados para Nickel Compounds
Resumo:
The effects of both organically modified montmorillonite (OMMT) and Ni2O3 on the carbonization of polypropylene (PP) during pyrolysis were investigated. The results from TEM and Raman spectroscopy showed that the carbonized products of PP were mainly multiwalled carbon nanotubes (MWNTs). Surprisingly, a combination of OMMT and Ni2O3 led to high-yield formation of MWNTs. X-ray powder diffraction (XRD) and GC-MS were used to investigate the mechanism of this combination for the high-yield formation of MWNTs from PP. Bronsted acid sites were created in degraded OMMT layers by thermal decomposition of the modifiers. The resultant carbenium ions play an important role in the carbonization of PP and the formation of MWNTs. The degradation of PP was induced by the presence of carbenium ions to form predominantly products with lower carbon numbers that could be easily catalyzed by the nickel catalyst for the growth of MWNTs. Furthermore, carbenium ions are active intermediates that promote the growth of MWNTs from the degradation products with higher carbon numbers through hydride-transfer reactions. The XRD measurements showed that Ni2O3 was reduced into metallic nickel (Ni) in situ to afford the active sites for the growth of MWNTs.
Resumo:
A novel synthesis of asymmetric bis(chlorophthalimide)s (3,4-BCPIs) has been established. The polymerizations of them produced higher molecular weight (0.38-0.51 dL/g) polyimides containing biphenyl units than those of isomeric polymers derived from symmetric bis(chlorophthalimide)s (4,4'-BCPIs) and 3,3'-BCPIs. The distribution of the formed biphenyl units of head to tail, head to head, and tail to tail in the chain of the polymers was about 58.0:21.0:21.0, determined by C-13 NMR spectra of the polymers. The composition of model compounds, determined by HPLC, was well consistent with the 13C NMR spectrum result. Comparing with polymers derived from 4,4'-BCPIs and 3,3'-BCPIs, the polymers derived from 3,4-BCPIs showed better solubilities in N,N-dimethylacetamide (DMAc), N,N-dimethyl-formamide (DMF), and N-methylpyrrolinone (NMP). Flexible films could be cast from the polymer solution with the inherent viscosities of above 0.35 dL/g. The polymer derived from asymmetric bis(chlorophthimide)s gave the highest T-g among the isomeric polymers.
Resumo:
A series of nickel(II) complexes bearing two nonsymmetric bidentate beta-ketoiminato chelate ligands have been prepared, and the structures of complexes [(2,6-Me2C6H3)NC(CH3)C(H)C(Ph)O](2)Ni (4a) and [(2,6-Me2C6H3)NC(CH3)C(H)C(CF3)O](2)Ni (4c) have been confirmed by X-ray crystallographic analysis. These nickel(II) complexes were investigated as catalysts for the vinylic polymerization of norbornene. Using modified methylaluminoxane (MMAO) as a cocatalyst, these complexes display very high activities and produce high molecular weight polymers. Catalytic activity of up to 1.16 x 10(4) kg/mol(Ni) .h and the viscosity-average molecular 9 weight of polymer of up to 870 kg/mol were observed. Catalyst activity, polymer yield, and polymer molecular weight could be controlled over a wide range by the variation of the reaction parameters such as Al/Ni molar ratio, norbornene/catalyst molar ratio, monomer concentration, polymerization reaction temperature and time.
Resumo:
The RENi3 (RE = La, Ce, Pr, Nd, Sm, Gd, Tb, Dy, Ho, Er, Y) series compounds have been prepared by arc melting constituent elements under Ar atmosphere. X-ray diffraction (XRD) analysis reveals that the as-prepared alloys have different lattice parameters and cell volumes, depending on different rare earth (RE) element. The electrochemical characteristics, including the electrochemical capacity, P-C isotherms, high rate chargeability (HRC) and high-rate dischargeability (HRD), of these alloys have been studied through the charge-discharge recycle testing at different temperatures, charge currents and discharge currents. The results show that YNi3 has the largest cell volume, smallest density, and moreover, it shows more satisfactory electrochemical characteristics than other alloys, including discharge capacity, HRC, HRD and low temperature dischargeablity.
Resumo:
alpha-Diimine nickel catalyst hearing two allyl groups [ArN=C](2)C10H6NiBr2 (Ar = 4-allyl-2,6-(i-Pr)(2)C6H2)] (Cat-I) has been synthesized and characterized. The corresponding polymer-incorporated nickel catalysts PC and the SiO2-supported shell-core structure catalyst SC-1 were obtained by the co-polymerization of the olefin groups of Cat-1 with styrene in the presence of a radical initiator. Radical co-polymerizations with styrene in Solution were investigated in detail, and the compositions and molecular weight of the copolymers were determined. All three types of catalysts (Cat-1, PC and SC-1) have been investigated for ethylene polymerization. These catalysts were found to exhibit high activity in the presence of modified methylaluminoxane (MMAO) as a co-catalyst. Among them, the polymer-incorporated PC and SiO2 shell-core catalyst SC-1 displayed very high activity (similar to2.62 and similar to1.11 kg (mmol Ni)(-1) h(-1), respectively) with product molecular weights (M,) in the range 26 x 10(4) to 47 x 10(4) under 0.1 MPa ethylene pressure. The particle morphology of polyethylene produced by the shell-core structure catalyst SC-1 was improved.
Resumo:
Self-immobilized nickel and iron diimine catalysts bearing one or two allyl groups of [ArN=C](2)(C10H6)NiBr2 [Ar = 4-allyl-2,6-(i-Pr)(2)C6H2] (1), [ArN=C(Me)[Ar'N=C(Me)]C5H3NFeCl2 [Ar = Ar' = 4-allyl-2,6-(i-Pr)(2)C6H3, Ar = 2,6-(i-Pr)(2)C6H3, and Ar' = 4-allyl-2,6-(i-Pr)(2)C6H3] were synthesized and characterized. All three catalysts were investigated for olefin polymerization. As a result, these catalysts not only showed high activities as the catalyst free from the allyl group, such as [ArN=C](2)C10H6,NiBr2 (Ar = 2,6-(i-Pr)(2)C6H2)], but also greatly improved the morphology of polymer particles to afford micron-granula polyolefin. The self-immobilization of catalysts, the formation mechanism of microspherical. polymer, and the influence on the size of the particles are discussed. The molecular structure of self-immobilized nickel catalyst 1 was also characterized by crystallographic analysis.
Resumo:
Ceramic carbon materials were developed as new sorbents for solid-phase extraction of organic compounds using chlorpromazine as a representative. The macroporosity and heterogeneity of ceramic carbon materials allow extracting a large amount of chlorpromazine over a short time. Thus, the highly sensitive and selective determination of chlorpromazine in urine sample was achieved by differential pulse voltammograms after only 1-min extraction. The total analysis time was less than 3 min. In comparison with other electrochemical and electrochemi-luminescent methods following 1-min extraction, the proposed method improved sensitivity by about 2 and 1 order of magnitude, respectively. The fast extraction, diversity, and conductivity of ceramic carbon materials make them promising sorbents for various solid-phase extractions, such as solid-phase microextraction, thin-film microextraction, and electrochemically controlled solidphase extraction. The preliminary applications of ceramic carbon materials in chromatography were also studied.
Resumo:
We report a method for estimating the positions of charge transfer (CT) bands in Eu3+-doped complex crystals. The environmental factor ( he) influencing the CT energy is presented. he consists of four chemical bond parameters: the covalency, the bond volume polarization, the presented charge of the ligand in the chemical bond, and the coordination number of the central ion. These parameters are calculated with the dielectric theory of complex crystals. The relationship between the experimental CT energies and calculated environmental factors was established by an empirical formula. The calculated values are in good agreement with the experimental results. Such a relationship was confirmed by detailed analysis. In addition, our method is also useful to predict the charge-transfer position of any other rare earth ion.
Resumo:
A series of alpha-diimine nickel(II) complexes containing chloro-substituted ligands, [(Ar)N=C(C10H6)C=N(Ar)]NiBr2 (4a, Ar = 2,3-C6H3Cl2; 4b, Ar = 2,4-C6H3Cl2; 4c, Ar = 2,5-C6H3Cl2; 4d, Ar = 2,6-C6H3Cl2; 4e, Ar = 2,4,6-C6H2Cl3) and [(Ar)N=C(C10H6)C=N(Ar)](2)NiBr2 (5a, Ar = 2,3-C6H3Cl2; 5b, Ar = 2,4-C6H3Cl2; 5c, Ar = 2,5-C6H3Cl2), have been synthesized and investigated as precatalysts for ethylene polymerization. In the presence of modified methylaluminoxane (MMAO) as a cocatalyst, these complexes are highly effective catalysts for the oligomerization or polymerization of ethylene under mild conditions. The catalyst activity and the properties of the products were strongly affected by the aryl-substituents of the ligands used. Depending on the catalyst structure, it is possible to obtain the products ranging from linear alpha-olefins to high-molecular weight polyethylenes.
Resumo:
Crystallographic and electrochemical characteristics of ball-milled Ti45Zr35Ni17Cu3 +xNi (x = 0, 5, 10, 15 and 20 mass%) composite powders have been investigated. The powders are composed of amorphous, I- and Ni-phases when x increases from 5 to 20. With increasing x, the amount of Ni-phase increases but the quasi-lattice constant decreases. The maximum discharge capacity first increases as x increases from 0 to 15 and then decreases when x increases further from 15 to 20. The high-rate dischargeability and cycling stability increase monotonically with increasing x. The improvement of the electrochemical characteristics is ascribed to the metallic nickel particles highly dispersed in the alloys, which improves the electrochemical kinetic properties and prevents the oxidation of the alloy electrodes, as well as to the mixed structure of amorphous and icosahedral quasicrystal line phases, which enhances the hydrogen diffusivity in the bulk of the alloy electrodes and efficiently inhibits the pulverization of the alloy particles.
Resumo:
A series of binuclear neutral nickel and palladium complexes [(XC6H2CH=NC6H3-iPr(2))MRL](2) 4b-f (X=NO2, M=Ni, R=Ph, L=PPh3, 4b; X=H, M=Pd, R=Me, L=PPh3,4c; X=H,M=Pd, R=Me, L=Py, 4d; X=NO2,M=Pd, R=Me, L=PPh3, 4e; X=NO2, M=Pd, R=Me, L=Py, 4f) and [(C10H7CH=NC6H3-iPr(2))MRL](2) 8a-c (M=Ni, R=Ph, L=PPh3, 8a; M=Pd, R=Me, L=PPh3, 8b; M=Pd, R=Me, L=Py, 8c) have been synthesized and characterized. The structures of complexes 4e and 8b have also been confirmed by X-ray crystallographic analysis. With modified methylalummoxane (MMAO) as cocatalysts, these complexes and complex [(C6H3CH=NC6H3-iPr(2))NiPh(PPh3)](2) 4a are capable of catalyzing the addition polymerization of norbomene (NBE) with the high activity up to 2.3 x 10(8) g PNBE/(mol(M) h). The structure of complexes affects considerably catalytic activity towards norbomene polymerization. The polymers obtained with nickel complexes are soluble, while those obtained with palladium complexes are insoluble. Palladium complexes 4c, 4e and 8b bearing PPh3 ligands exhibit much higher activities than the corresponding complexes 4d, M and 8c bearing pyridine ligands under the same conditions.
Resumo:
Nickel appears the most promising for the replacement of palladium among the inexpensive transition metals for that it is active for Heck reaction and about 500 times cheaper than palladium. In this article, we describe our recent results in the area of nickel-catalyzed Heck vinylations. Main focus is on the influence of ligand concentration in different organic solvents and the effects of the addition of water. The conversion is high in NMP and increases with increasing of PPh3/Ni ratio; in ethanol and toluene the conversion presents a maximum value on Ni(PPh3)(2). The effect of the addition of water is sensitive to the concentration of PPh3 and the nature of solvent, it was well explained with the formation and transfer of the active species in the different solvent systems.
Resumo:
The activities/properties of two molecules with identical formula but different configuration states of the asymmetric atoms are different. Thus, usually the common topological indices are not suitable. In this study, the chiral topological indices were obtained by extending A(mi) indices suggested by our laboratory and molecular connectivity indices. The modified topologial indices have been used for the studies on D2 for dopamine receptor and a receptor activities of fourteen N-alkylated 3-(3-hydroxypyenyl)-piperidines. It has been observed that selected variables possess low correlations. The results obtained by using multiple regression analysis and artificial neural networks are satisfactory.
Resumo:
Icosahedral quasicrystalline Ti45Zr35Ni17Cu3 alloy powder was ball-milled with 20 mass% Ni, and the effect of the ball-milling time (t) on crystallographic and electrochemical characteristics were investigated. The amounts of icosahedral quasicrystalline and Ni phases decreased when ball-milling time increased from 30 to 180 min. The powder consisted of amorphous and (Ni and Ti) phases after 360 min of ball-milling. The maximum discharge capacity of the powder electrodes first increased from 89 (t = 0 min) to 192 mAh g(-1) (t = 180 min), and then decreased to 138 mAh g(-1) (t = 360 min). The high-rate dischargeability and the discharge capacity after 15 cycles increased with increasing ball-milling time.
Resumo:
This paper presents results concerning structure and electrochemical characteristics of the La0.67Mg0.33 (Ni0.8Co0.1Mn0.1) (x) (x=2.5-5.0) alloy. It can be found from the result of the Rietveld analyses that the structures of the alloys change obviously with increasing x from 2.5 to 5.0. The main phase of the alloys with x=2.5-3.5 is LaMg2Ni9 phase with a PuNi3-type rhombohedral structure, but the main phase of the alloys with x=4.0-5.0 is LaNi(5)phase with a CaCu5-type hexagonal structure. Furthermore, the phase ratio, lattice parameter and cell volume of the LaMg2Ni9 phase and the LaNi5 phase change with increasing x. The electrochemical studies show that the maximum discharge capacity increases from 214.7 mAh/g (x=2.5) to 391.1 mAh/g (x=3.5) and then decreases to 238.5 mAh/g (x=5.0). As the discharge current density is 1,200 mA/g, the high rate dischargeability (HRD) increases from 51.1% (x=2.5) to 83.7% (x=3.5) and then decreases to 71.6% (x=5.0). Moreover, the exchange current density (I-0) of the alloy electrodes first increases and then decrease with increasing x from 2.5 to 5.0, which is consistent with the variation of the HRD. The cell volume reduces with increasing x in the alloys, which is detrimental to hydrogen diffusion and accordingly decreases the low-temperature dischargeability of the alloy electrodes.