265 resultados para Cong bu


Relevância:

10.00% 10.00%

Publicador:

Resumo:

间同1,2-聚丁二烯(s-PB)由丁二烯用Fe(2-EHA)3/Al(i-Bu)3/DEP作催化剂,在己烷溶剂中50℃下聚合制备.用13C NMR谱方法测定的1,2-结构含量为89.3%,间同结构为86.5%;X射线测得聚合物的结晶度约为68%.非等温结晶动力学研究采用DSC方法,改进的Avrami方程可以很好地分析s-PB非等温结晶过程的主期结晶,表明其结晶过程是自成核,三维球形生长.Ozawa方程不适合分析s-PB非等温结晶动力学;Avrami和Ozawa方程结合的方法可以很好地描述s-PB非等温结晶过程,指数a为1.138,F(θ)随着结晶度的提高而增大;并计算了s-PB的结晶活化能.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A series of monodisperse oligo(9,9-di-n-octylfluorene-co-bithiophene)s (OFbTs) with molecular lengths of up to 19.5 nm and molecular weights up to 7025 g mol(-1) has been synthesized by a divergent/convergent approach involving Stille coupling reactions. Stille coupling is quite efficient in preparing this class of oligomers, and even the molecule with nine fluorene units and eight bithiophene units (F9Th16) can be synthesized in a yield as high as 70%. Because of easy functionalization of the thiophene ring at its alpha position, no additional protecting group allowing activation for further reaction is necessary. However, the synthetic routes must be optimized to eliminate contamination of the targeting compounds with the homocoupling product of the organotin reagents. Synthesis of the longest oligomer F13Th24 in a relative large quantity is limited by its low yield due to the pronounced ligand-exchange side reactions of the starting materials and reaction intermediates. All oligomers longer than F4Th6 are nematic mesomorphs and exhibit enhanced glass transition temperature and clearing point with increasing molecular length, as revealed by differential scanning calorimetry and polarizing optical microscopy.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Monodispersed nanoparticles of Ag(I)-polymer hybrids have been prepared by using designed crown-ether-centred two-armed copolymers to chelate Ag+ ions at the interface of organic-aqueous solutions. The copolymer-Ag+ complex nanoparticles, as well as the reduced copolymer-Ag nanoparticles, have been characterized by transmission electron microscopy (TEM), atomic force microscopy (AFM), and x-ray photoelectron spectroscopy (XPS). The particle size can be varied by simply changing the polymer concentration, the monomers, and/or the molecular weight. The copolymer-Ag(I) hybrids exhibit weak photoluminescence, which was substantially enhanced after the hybrids were reduced to copolymer-silver nanoparticles with UV irradiation.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Four single polymers with two kinds of attachment of orange chromophore to blue polymer host for white electroluminescence (EL) were designed. The effect of the side-chain attachment and main-chain attachment on the EL efficiencies of the resulting polymers was compared. The side-chain-type single polymers are found to exhibit more efficient white EL than that of the main-chain-type single polymers. Based on the side-chain-type white single polymer with 4-(4-alkyloxy-phenyl)-7-(4-diphenylamino-phenyl)-2,1,3-benzothiadiazoles as the orange-dopant unit and polyfluorene as the blue polymer host, white EL with simultaneous orange (lambda(max) = 545 nm) and blue emission (lambda(max) = 432 nm/460 nm) is realised. A single-layer device (indium tin oxide/poly(3,4-ethylenedioxythiophene)/polymer/Ca/Al) made of these polymers emits white light with the Commission Internationale de l'Eclairage coordinates of (0.30,0.40), possesses a turn-on voltage of 3.5 V, luminous efficiency of 10.66 cd A(-1), power efficiency of 6.68 lm W-1, and a maximum brightness of 21240 cd m(-2).

Relevância:

10.00% 10.00%

Publicador:

Resumo:

By incorporating 4,7-diphenyl- 2,1,3 benzothiadiazole instead of 2,1,3-benzothiadiazole into the backbone of polyfluorene, we developed a novel series of green light- emitting polymers with much improved color purity. Compared with the state-of-the-art green light-emitting polymer, poly(fluorene-co-benzothiadiazole) (lambda max = 537 nm), the resulting polymers (lambda(max) = 521 nm) showed 10-20 nm blueshifted electroluminescence (EL) spectra and greatly improved color purity because the insertion of two phenylene units between the 2,1,3-benzothiadiazole unit and the fluorene unit reduced the effective conjugation length in the vicinity of the 2,1,3-benzothiadiazole unit. As a result, the resulting polymers emitted pure green light with CIE coordinates of (0.29, 0.63), which are very close to (0.26, 0.65) of standard green emission demanded by the National Television System Committee (NTSC). Moreover, the insertion of the phenylene unit did not affect the photoluminescence (PL) and EL efficiencies of the resulting polymers. PL quantum efficiency in solid films up to 0.82 was demonstrated. Single-layer devices (ITO/PEDOT/ polymer/Ca/Al) of these polymers exhibited a turn-on voltage of 4.2 V, luminous efficiency of 5.96 cd A(-1) and power efficiency of 2.21 lm W-1. High EL efficiencies and good color purities made these polymers very promising for display applications.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Five zinc (II) complexes (1-5) with 4 '-phenyl-2,2 ':6 ',2 ''-terpyridine (ptpy) derivatives as ligands have been synthesized and fully characterized. The para-position of phenyl in ptpy is substituted by the group (R), i.e. tert-butyl (t-Bu), hexyloxy (OHex), carbazole-9-yl (Cz), naphthalen-1-yl-phenyl-amine-N-yl (NPA) and diphenyl amine-N-yl (DPA), with different electron-donating ability. With increasing donor ability of the R, the emission color of the complexes in film was modulated from violet (392 nm) to reddish orange (604 nm). The photoexcited luminescence exhibits significant solvatochromism because the emission of the complexes involves the intra-ligand charge transfer (ILCT) excited state. The electrochemical investigations show that the complexes with stronger electro-donating substituent have lower oxidation potential and then higher HOMO level. The electroluminescence (EL) properties of these zinc (II) complexes were studied with the device structure of ITO/PEDOT/Zn (II) complex: PBD:PMMA/BCP/AlQ/ LiF/Al. Complexes 3, 4 and 5 exhibit EL wavelength at 552, 600 and 609 nm with maximum current efficiency of 5.28, 2.83 and 2.00 cd/A, respectively.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The crystalline syndiotatic 1,2-polybutadiene was synthesized with a catalyst consisting of iron acetylacetonate (Fe(acac)(3))-triisobutylaluminum (Al(i-Bu)(3))-diethyl phosphite (DEP), and the effects of crystal growth conditions on morphology of thin films of the polymer were investigated by transmission electron microscopy (TEM) and electron diffraction (ED) techniques. The polymer with melting point 179 degreesC was found to have 89.3% 1,2-content and 86.5% syndiotacticity by C-13 NMR measurement. The results of electron microscopic studies indicate that the solution-cast thin films of the syndiotatic 1,2-polybutadiene consist of lath-like lamellae with the c-axis perpendicular to the film plane, while a- and b-axes are in the film plane. The morphology of isothermally crystallized thin films of the polymer is temperature dependent. At lower crystallization temperatures (130 degreesC), a spherulitic structure consisting of flat-on lamellae is formed. With an increase in the crystallization temperature (e.g., at 140 degreesC), the spherulites and single faceted crystals coexist. At higher crystallization temperatures (150 degreesC), single crystals with a hexagonal prismatic shape are produced.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We have investigated systematically the morphology of thin films spin-coated from solutions of a semicrystalline diblock copolymer, poly(L-lactic acid)-block-polystyrene (PLLA-b-PS), in solvents with varying selectivity. In neutral solvents (chloroform and tetrahydrofuran (THF)), a spinodal-like pattern was obtained and the pattern boundary was sharpened by diluting the solution. Meanwhile, loose spherical associates, together with larger aggregates composed of these associates by unimer bridges, formed partly due to crystallization of the PLLA blocks in relatively concentrated solutions. In slightly PS-selective solvent (e.g., benzene), both loose and compact spherical micelles were obtained, depending on the polymer concentration, coexisting with unimers. When enhancing the selectivity with mixed solvents, for example, mixing the neutral solvent and the slightly selective solvent with a highly PS-selective solvent, CS2, loose assemblies (nanorods in CS2/THF mixtures and polydisperse aggregates in CS2/benzene mixtures) and well-developed lamellar micelles were obtained.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We have investigated the hole nucleation and growth induced by crystallization of thin crystalline-coil diblock copolymer films. Semicrystalline rodlike assemblies from neutral/selective binary solvent are used as seeds to nucleate crystallization at temperatures above the glass transition temperature (T-g) but below melting point (T-m). The crystallization of nanorods drives neighboring copolymer chains to diffuse into the growing nanorods. Depletion of copolymer chains yields hole nucleation and growth at the edge of the nanorods. Simultaneously, the polymer chains unassociated into the nanorods were oriented by induction from the free surface and the substrate, leading to limitation of the hole depth to the lamellar spacing, similar to20 nm. The holes, as well as the nanorods, grow as t(alpha), where t is the annealing time and a crossover in the exponent a. is found. The orientation and stretching of the copolymer chains by the surface and interface are believed to accelerate the crystallization, and in turn, the latter accelerates the growth rate of the holes. At T > T-m, the grains melt and the copolymer chains relax and flow into the first layer of the film.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Reversibly strain-tunable polymeric photonic crystals made of thermoplastic polyester elastomer (TPEE) were fabricated by using the self-assembled silica opals as templates. The stop band of the polymeric photonic crystal locates at the near infrared (IR) regime in its transmission spectrum, and exhibits a blue shift with the increase of the incident angle. Because of the elasticity of the TPEE, the stop band of the TPEE photonic crystal can also be reversibly tuned at ambient temperature through to and fro uniaxially or biaxially stretching and recovering by changing the lattice spacing and the symmetry of the crystal along (1 1 1) plane.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Highly ordered honeycomb-like macroporous films were obtained via self-assembly of a two-armed polymer with a crown ether core under controlled conditions. A possible mechanism is speculated, primarily based on the strong affinity between the crown ether cores. The pore size and arrangement are sensitive to the solvent evaporation rate and the solution concentration. Upon spontaneous drying, the pore diameter (D) depends on the concentration (c) by a relation of D=518c(-0.610).

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Patterned self-adaptive PS/P2VP mixed polymer brushes were prepared by "grafting to" approach combining with microcontact printing (muCP). The properties of the patterned surface were investigated by lateral force microscopy (LFM), XPS and water condensation figures. In the domains with grafted P2VP, the PS/P2VP mixed brushes demonstrated reversible switching behavior upon exposure to selective solvents for different components. The chemical composition of the top layer as well as the surface wettability can be well tuned due to the perpendicular phase segregation in the mixed brushes. While in the domains without grafted P2VP, the grafted PS did not have the capability of switching. The development and erasing of the pattern is reversible under different solvent treatment.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A series of neutral nickel complexes [Ni(Ph)(PPh3)(N, O)] with Schiff-base ligands (N, O) [N, O = 5-Me-3-tert-Bu-(Ar-N=CH)C6H2O (1, Ar = 2,6-Me2C6H3; 2, Ar = 2,6-i-Pr2C6H3)], [Ni(Ph)(PPh3)(N,O)1, with beta-ketiminato ligands (N, O) [N, O = CH3COCHC=(CH3)N-Ar (3, Ar = 2,6-Me2C6H3; 4, Ar = 2,6-i-Pr2C6H3)] and [Ni(N, N)(PPh3)], and with beta-diketiminato ligands (N, N) [5, N, N = [2,6-i-Pr-2(C6H3)N=C(CH3)](2)CH] have been synthesized and characterized. The molecular structures of complexes 1, 4, and 5 have been confirmed by X-ray single-crystal analyses. Although their ligands have similar structures, complex 4 possesses a structure similar to that of four-coordination nickel with complex 1, while complex 5 reveals a rare three-coordination nickel geometry. These compounds show high catalytic activities of up to 3.16 x 10(7) g PNB mol(-1) Ni h(-1) for the addition polymerization of norbornene in the presence of modified methylaluminoxane (MMAO) as cocatalyst. Catalytic activities, polymer yield, molecular weights, and molecular weight distributions of polyborbornene have been investigated under various reaction conditions.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Metallocene complex (Cp2ZrCl2)-Zr-tt (Cp-tt = eta(5)-1,3-(Bu2C5H3)-Bu-t) (1) has been prepared from the reaction of LiCptt with ZrCl4 in good yield. Reactions of 1 with dilithium dichalcogenolate o-carboranes afforded new type of half-sandwich compounds with dichalcogenolate o-carboranyl ligands [Li(THF)(4)][(CpZr)-Zr-tt(E2C2B10H10)(2)] (E = S, 2a; E = Se, 2b) in which only one cyclopentadienyl ring ligand existed. Complexes 1 and 2a were structurally characterized by X-ray analyses. In complex 2a, the Zr(IV) ion is eta(5)-bound to one 1,3-di-tert-cyclopentadienyl ring and a-bound to four mu(2)-sulfur atoms of two dithio-carboranes. The zirconium atom and four sulfur atoms form a distorted pyramid. The coordination sphere around the zirconium atom resembles in a piano stool structure with four legs of sulfur atoms and the fulcrum at the zirconium atom.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We report the multiple morphologies and their transformation of polystyrene-block-poly(4-vinylpyridine) (PS-b-P4VP) in low-alkanol solvents. In order to improve the solubility of polystyrene block in alcohol solvents, the solution of block copolymer sample was treated at a higher temperature, and then the influence of rate of decreasing temperature on multiple morphologies (including spheres, rods, vesicles, porous vesicles, large compound vesicles, and large compound micelles) was observed. The transformation of spheres to rods, to tyre-shaped large compound micelles, and to sphere-shaped large compound micelles was also realized. The formation mechanisms of the multiple morphologies and their transformation are discussed briefly.