202 resultados para (cyst of P. conicum)
Resumo:
The title complex [(VB1)(2)DMFHPMo12O40.5DMF, VB1 = vitamin B-1 (thiamine chloride), DMF = N,N-dimethylformamide] has been synthesized and characterized by elemental analysis, IR, UV-Vis, electron spin resonance, X-ray photoelectron spectroscopy and cyclic voltammetry methods. The X-ray crystal structure revealed that there is one independent molecule in the unit cell of the title complex that contains one mixed-valence heteropolyanion, two VB1+ cations and six DMF molecules. The title complex possesses a centrosymmetrical arrangement in the unit cell, with the P atom at the symmetry center of the heteropolyanion and with eight O atoms surrounding the central P atom, such that two sets of PO4 tetrahedra are formed. The PO4 tetrahedra and MoO66-(7-) octahedra are disordered in the heteropolyanion. The bond distances of P-O-a and Mo=O-d are in the ranges 1.57 (4)-1.70 (4) Angstrom and 1.61 (2)-1.67 (2) Angstrom, respectively.
Resumo:
Layered compound zirconium bis(monohydrogenphosphate)(alpha-ZrP) intercalated with rare earth complex Eu(DBM)(3)phen was prepared. The pre-intercalation of p-methoxyaniline into alpha-ZrP makes the interlayer separation large enough to exchange PMA with europium complex, thus, the luminescent assembly was prepared. This was confirmed by X-ray diffraction, UV-visible spectra and elemental analysis. The fluorescence spectra and lifetime of the assembly were also presented.
Resumo:
The luminescence of unusual divalent bismuth (Bi2+) in BaB8O13 is reported. The emission band with maximum peak at 592 nm corresponds to the P-2(3/2)-->P-2(1/2) transition of Bi2+ in the matrix and the excitation spectrum with two bands peaked at 470 and 580 nm respectively corresponds to two split crystal-field levels of P-2(3/2) state. The small Stokes shift (similar to 350 cm(-1)) reflects the rigid structure of the host for the Bi2+ ions.
Resumo:
The compatibilizing effect and mechanism of poly(styrene-b-4-vinylpyridine) diblock copolymer, P(S-b-4VPy), on the immiscible blend of polystyrene (PS)/zinc salt of sulphonated polystyrene (Zn-SPS) were studied. SEM results show that the domains of the dispersed phase in the blend become finer. DSC experiments reveal that the difference between the two T-g's corresponding to the phases in the blends becomes larger on addition of P(S-b-4VPy), mainly resulting from dissolving of the poly(4-vinylpyridine (P4VPy) block in the Zn-SPS phase. FTIR analysis shows that compatibility of P4VPy and Zn-SPS arises from the stoichiometric coordination of the zinc ions of Zn-SPS and pyridine nitrogens of P4VPy. SAXS analysis indicates the effect of the P(S-b-4VPy) content on the structure of the compatibilized blends. When the content of the block copolymer is lower than 4.1 wt%, the number of ion pairs in an aggregate in the Zn-SPS becomes smaller, and aggregates in ionomer in the blend become less organized with increasing P(S-b-4VPy). When the P(S-b-4VPy) content in the blend is up to 7.4 wt%, a fraction of P(S-b-4VPy) form a separate domain in the blend. (C) 1999 Elsevier Science Ltd. All rights reserved.
Resumo:
Two closely series of poly(ester imide)s had been synthesized by solution polycondensation of p-phenylenebis(trimellitate) dianhydride with aliphatic diamines. The differential scanning calorimetry (DSC) traces of the most poly(ester imide)s exhibited two endotherms representing the solid state to anisotropic phase transition (T-m1) and the anisotropic to isotropic melt transition (T-m2), respectively. Observation under polarizing microscope and wide-angle X-ray diffraction (WAXD) measurements suggested that the anisotropic phase formed above the melting paints (T-m1) had a smectic character. The thermogravimetric analyses (TGA) revealed that the thermal stabilities of the poly(ester imide)s were up to 350 degrees C. (C) 1999 John Wiley & Sons, Inc.
Resumo:
The compatibilization effect of poly(styrene-b-2-ethyl-2-oxazoline) diblock copolymer, P(S-b-EOx), on immiscible blends of poly(2,6-dimethyl-1,4-phenylene oxide) (PPO) and poly(ethylene-co-acrylic acid) (EAA) is examined in terms of phase structure and thermal, rheological and mechanical properties, and its compatibilizing mechanism is investigated by Fourier-transform infrared spectroscopy. The block copolymer, synthesized by a mechanism transformation copolymerization, is used in solution blending of PPO/EAA. Scanning electron micrographs show that the blends exhibit a more regular and finer dispersion on addition of a small amount of P(S-b-EOx). Thermal analysis indicates that the grass transition of PPO and the lower endothermic peal; of EAA components become closer on adding P(S-b-EOx), and the added diblock copolymer is mainly located at the interface between the PPO and EAA phases. The interfacial tension estimated by theological measurement is significantly reduced on addition of a small amount of P(S-b-EOx). The tensile strength and elongation at break increase with the addition of the diblock copolymer for PPO-rich blends, whereas the tensile strength increases but the elongation at break decreases for EAA-rich blends. This effect is interpreted in terms of interfacial activity and the reinforcing effect of the diblock copolymer, and it is concluded that the diblock copolymer plays a role as an effective compatibilizer for PPO/EAA blends. The specific interaction between EAA and polar parts of P(S-b-EOx) is mainly hydrogen bonding. (C) 1998 Elsevier Science Ltd. All rights reserved.
Resumo:
Poly(vinyl acetate-co-vinyl alcohol) copolymers (P(VAc-co-VA)) were synthesized by hydrolysis-alcoholysis of PVAc. The miscibility, crystallization, and morphology of poly(P-hydroxybutyrate) (PHB) and P(VAc-co-VA) blends were studied by differential scanning calorimetry, optical microscopy (OM), and SAXS. It is found that the P(VAc-co-VA)s with vinyl alcohol content of 9, 15, and 22 mol % will form a miscible phase with the amorphous part of PHB in the solution-cast samples. The melting-quenched samples of PHB/P(VAc-co-VA) blends with different vinyl alcohol content show different phase behavior. PHB and P(VAc-co-VA9) with low vinyl alcohol content (9% mel) will form a miscible blend in the melt state. PHB and P(VAc-co-VA15) with 15 mol % vinyl alcohol will not form miscible blends while PHB/P(VAc-co-VA15) blend with 20/80 composition will form a partially miscible blend in the melt state. PHB and P(VAc-co-VA22) with 22 mol % vinyl alcohol are not miscible in the whole composition range. The single glass transition temperature of the blends within the whole composition range suggests that PHB and P(VAc-co-VA9) are totally miscible in the melt. The crystallization kinetics was studied from the whole crystallization and spherulite growth for the miscible blends. The equilibrium melting point of PHB in the PHB/P(VAc-co-VA9) blends, which was obtained from DSC results using the Hoffman-Weeks equation, decreases with the increase in P(VAc-co-VA9) content. The negative value of the interaction parameter determined from the equilibrium melting point depression supports the miscibility between the components. The kinetics of spherulitic crystallization of PHB in the blends was analyzed according to nucleation theory in the temperature range studied in this work. The best fit of the data to the kinetic theory is obtained by employing WLF parameters and the equilibrium melting points obtained by DSC. The addition of P(VAc-co-VA) did not affect the crystalline structure of PHB, as shown by the WAXD results. The long periods of blends obtained from SAXS increase with the increase in P(VAc-co-VA) content. It indicates that the amorphous P(VAc-co-VA) was rejected to interlamellar phase corporating with the amorphous part of PHB.
Resumo:
The blends of poly(beta-hydroxybutyrate-co-beta-hydroxyvalerate) (P(HB-co-HV)/poly(p-vinylphenol)(PVPh) were investigated by differential scanning calorimetry (DSC), Fourier transform IR (FT-IR) spectroscopy and high-resolution solid-state C-13 NMR techniques. Single glass transition temperatures existing in the whole composition range indicates that these blends are miscible. The presence of hydrogen bonding between the hydroxyl of PVPh and carbonyl of P(HB-co-HV), shown by FT-IR spectra, is the origin of the miscibility. Furthermore, results obtained by high-resolution solid-state C-13 NMR give more information about the structure of the blends. (C) 1998 Elsevier Science Ltd. All rights reserved.
Dependence of superconducting temperature on chemical bond parameters in YBa2Cu3O6+delta (delta=0-1)
Resumo:
The chemical bond parameters, that is ionicities and average energy gaps, for all types of chemical bonds in YBa2Cu3O6+delta have been investigated with variation of oxygen content delta (delta = 0.0, 0.35, 0.45, 0.58, 0.64, 0.73, 0.78, 0.81, 0.95, 1.00). The theory used is the complex crystal chemical bond theory, which is the development of P-V-L theory. The two plateaus near 90 K and 60 K in superconducting transition temperatures, and the disappearance of superconductivity with the change of oxygen content, were reasonably explained by chemical bond parameters. The results also showed that the Cu-O chains play a vital role in the transition from non-superconductors to superconductors, and the highest transition temperature occurred when the plane-chain reached a coupling state. (C) 1998 Elsevier Science Ltd. All rights reserved.
Resumo:
Gas transport properties of home- and copolyimides prepared from 3,3',4,4'- and 2,2',3,3'-thiaphthalic dianhydride (p-TDPA and m-TDPA, respectively) with 4,4-oxydianiline (ODA) were investigated. The fractional free volume of m-TDPA-ODA is larger than that of p-TDPA-ODA, and the chain segmental mobility of the former is lower than that of the latter. The permeability coefficients of m-TDPA-ODA to H-2, CO2, and O-2 are more increased by 48, 69 and 75%, at 30 degrees C and 10 atm, respectively, than those of p-TDPA-ODA; but the permselectivities of m-TDPA-ODA for H-2, CO2, and O-2 toward N-2 are more decreased by 33, 77, and 26%, respectively, than those of p-TDPA-ODA. The permeability coefficients and the diffusion coefficients of the copolyimides can be described by the following equations: log P = Phi(p) log P-p + Phi(m), log P-m and log D-a = D-a = Phi(p) log(D-alpha)(p) + Phi(m) log(D-a)(m), respectively. The variation of the permselectivity is controlled predominantly by diffusivity selectivity. These observations are interpreted in terms of variations in the fractional free volume of polyimides. (C) 1997 John Wiley & Sons, Inc.
Resumo:
The cleavage of 3',5'-cAMP, 3',5'-cGMP and 3',5'-dcAMP by lanthanides has been investigated by HPLC and H-1 NMR. Rapid cleavage of cAMP, cGMP and dcAMP by Ce(III) under air at pH 8 and 37 degrees C has been observed. Regioselective cleavage of P-O(5') bond in cAMP, cGMP and dc;aMP tu give the corresponding 3'-AMP, 3'-GMP and 3'-dAMP by lanthanide chlorides has been achieved, and 3'-AMP and 3'-GMP are cleaved to adenosine(A) and guanosine(CT) more slowly, respectively, The notable difference in reactivity between Ce(III) and the other lanthanide ions under air has also been studied. The cleavage is enhanced with the increase in the molar fraction of Ce(IV). The fast cleavage of cAMP by Ce(III) under air at pH 8 is ascribed to the resultant Ce(IV) in the reaction mixture.
Resumo:
The influence of lanthanum ions on the polymorphic phase of egg phosphatidylethanolamine and dielaidoylphosphatidylethanolamine (PE and DEPE) has been investigated by means of P-31-nuclear magnetic resonance (P-31-NMR) and high sensitivity differential scanning calorimetry (DSC) techniques. P-31-NMR experiments show that lanthanum ions promote the formation of the hexagonal II phase at temperatures lower than those of the pure egg PE, DSC results also show that lanthanum ions induce the formation of hexagonal II phase in DEPE liposomes even al very low ion concentration, The effect of lanthanum ions on the polymorphism of PE liposomes is much greater than that of calcium.
Resumo:
A new series of fully aromatic thermotropic liquid crystalline copolyesters were synthesized by thermal polycondensation of p-hydroxybenzoic acid (PHB), terephthalic acid (TPA), resorcinol (RES) and bis (4-hydroxyphenyl) methanone (BHP). The DSC traces of copolyesters exhibited two or three endotherms, the low temperature endotherm(Tm) of which indicated the transition from solid state to anisotropic phase. Observation under polarizing microscope and WAXD measurements suggested that the LC-phase formed immediately above Tm had a nematic character.
Resumo:
A series of thermotropic liquid crystalline copolyesters were synthesized by thermal polycondensation of p-hydroxybenzoic acid, terephthalic acid, bis (4-hydroxyphenyl) methanone and diols. The resulting copolyesters were characterized by WAXD,DSC and PLM. All the copolyesters formed a nematic phase.
Resumo:
Langmuir-Blodgett (LB) films of (p-carboxyphenoxy)-tri(2,4-di-tert-pentyl phenoxy)phthalocyanine copper(II) (asyCuPc) are prepared; the associated forms of the compound in chloroform solution and the particular orientation of asyCuPc molecular macrocycles in LB films is determined by polarized UV-VIS.