332 resultados para Ho:YAG ceramic
Resumo:
Absorption spectrum from 400 to 2000 run and upconversion fluorescence spectra under 940 nm pumping of YAG single crystal codoped with 5 at.% Yb3+ and 4 at.% Tm3+ were studied at room temperature. The blue upconversion emission centered at 483 nm corresponds to the transition (1)G(4) -> H-3(6), the emission band around 646 nm corresponds to the transition (1)G(4) -> F-3(4) of Tm3+. Energy transfer from Yb3+ to Tm3+ is mainly nonradiative and the transfer efficiency was experimentally assessed. The line strengths, transition probabilities and radiative lifetimes of (1)G(4) level were calculated by using Judd-Ofelt theory. Gain coefficient calculated from spectra shows that the upconversion corresponding with transitions (1)G(4) -> H-3(6) in YAG doped with Yb3+ and Tm3+ is potentially useful for blue light Output. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Spectroscopic properties of (Y0.9-xLa0.1Ybx)(2)O-3 transparent ceramic were studied. Two main absorption peaks of the specimen are centered at 940 and 970 nm, which are suitable for InGaAs laser diode pumping. The main emission peaks were located at 1032 and 1075 nm with larger emission cross-section and longer fluorescence lifetime than those of Yb:Y2O3. These properties of (Y0.9-xLa0.1Ybx)(2)O-3 transparent ceramic are favorable to achieve high efficiency and high power laser output. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
Gamma-rays radiation effects on Ce:YAG crystals grown by Czochralski (Cz) and temperature gradient techniques (TGT) have been studied by means of optical absorption and luminescence spectra. Valence of Ce3+ ion changes during the gamma-ray irradiation process and this result indicates Ce4+ ion may exist in both Cz-Ce:YAG and TGT-Ce:YAG crystals. Thermally stimulated luminescence measurements reveal intense thermoluminescence peaks in gamma-irradiated Ce:YAG crystals and trap parameters were calculated by general-order kinetics expression. (C) 2006 Elsevier B.V. All rights reserved.
Resumo:
用温度梯度法生长了直径为75mm大尺寸的Nd:YAG激光晶体,通过退火排除了生长过程中进入晶体的碳原子.用正交偏光显微镜观察了晶体的核心分布以及生长条纹.测试了室温下的吸收谱并利用吸收谱研究了Nd离子在YAG晶体中的分布.比较了温度梯度法与提拉法生长晶体的区别.
Resumo:
YAG单晶是高功率激光的重要材料,近年来高透明度多晶陶瓷作为激光介质引起人们广泛的注意。YAG陶瓷相对单晶具有易制造大尺寸、掺杂浓度高、易批量生产等优点。在Nd:YAG陶瓷获得长足发展的同时,Yb掺杂的陶瓷也得到了越来越多的关注。Yb:YAG陶瓷与Nd:YAG陶瓷相比具有许多优点:Yb掺杂的激光介质无交叉弛豫振荡和激发态吸收,有较宽的吸收带,较长的荧光寿命及较高的量子效率等。因此,高质量的Yb:YAG陶瓷将是非常理想的高功率激光材料。
Resumo:
应用中频感应提拉法生长出掺杂浓度为10 at.-%的Yb:YAG与Yb:YAP晶体,对比了室温下两种晶体的吸收和发射光谱特性。结果表明,Yb:YAG晶体比Yb:YAP晶体有更好的激光性能和低的阈值;同时对比发现,Yb:YAP晶体的吸收截面是Yb:YAG晶体的2.16倍,它容易实现LD泵;由于Yb:YAP晶体的各向异性,它有轴向效应明显,它可以产生偏振激光。
Resumo:
The up-conversion luminescence of Yb3+-doped yttriurn lanthanum oxide transparent ceramic was investigated. It was ascribed to cooperative luminescence originated from the coupled states of the Yb3+ ion pairs. The proper doping of La2O3 can remove the cooperative luminescence of Yb3+ ion. But excessive La2O3 (at least 10 at.%) the cooperative up-conversion of Yb3+:Y2O3 is obtained again, and the intensity of up-conversion luminescence strengthens with the increase of La2O3 content. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
The YAG crystal codoped with Yb3+ and Tm3+ has been grown by Czochralski (Cz) method. The crystal structure of the crystal has been determined by X-ray diffraction analysis. The absorption and emission spectra of Yb,Tm:YAG crystal at room temperature have also been studied. The emission cross-sections have been calculated by Fuechtbauer-Ladenburg formula and reciprocity method. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
We demonstrated continuous-wave ( CW) and Q-switched operation of a room-temperature Ho: YAlO3 laser that is resonantly end-pumped by a diode-pumped Tm: YLF laser at 1.91 mu m. The CW Ho: YAlO3 laser generated 5.5 W of linearly polarized (E parallel to c) output at 2118 nm with beam quality factor of M-2 approximate to 1.1 for an incident pump power of 13.8 W, corresponding to optical-to-optical conversion efficiency of 40%. Up to 1-mJ energy per pulse at pulse repetition frequency (PRF) of 5 kHz, and the maximum average power of 5.3-W with FWHM pulse duration of 30.5 ns at 20 kHz were achieved in Q-switched mode. (C) 2008 Optical Society of America.
Resumo:
We report on a diode-pumped, cryogenic and room temperature operation of a Tm,Ho:YAlO3 (c-cut) laser. In a temperature of 77 K, an optical-optical conversion efficiency of 27% and a slope efficiency of 29% were achieved with the maximum continuous-wave (CW) output power of 5.0 W at 2.13 mu m. Acousto-optic switched operation was performed at pulse repetition frequency (PRF) from 1 kHz to 10 kHz, the highest pulse energy of 3.3 mJ in a pulse duration of 40 ns was obtained. In room temperature (RT), the maximum CW power of Tm,Ho:YAlO3 laser was 160 mW with a slope efficiency of 11% corresponding to the absorbed pump power. (C) 2008 Optical Society of America.
Resumo:
The Ho:YAP crystal is grown by the Czochralski technique. The room-temperature polarized absorption spectra of Ho:YAP crystal was measured on a c-cut sample with 1 at% holmium. According to the obtained Judd-Ofelt intensity parameters Omega(2) = 1.42 x 10(-20) cm(2), Omega(4) = 2.92 x 10(-20) cm(2), and Omega(6) = 1.71 x 10(-20) cm(2), this paper calculated the fluorescence lifetime to be 6 ms for I-5(7) -> I-5(8) transition, and the integrated emission cross section to be 2.24 x 10(-18) cm(2). It investigates the room-temperature Ho:YAP laser end-pumped by a 1.91-mu m Tm:YLF laser. The maximum output power was 4.1 W when the incident 1.91-mu m pump power was 14.4W. The slope efficiency is 40.8%, corresponding to an optical-to-optical conversion efficiency of 28.4%. The Ho:YAP output wavelength was centred at 2118 nm with full width at half maximum of about 0.8 nm.