540 resultados para Er:Yb:glass


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Spherical nano-indentations of Cu46Zr54 bulk metallic glass (BMG) model systems were performed using molecular dynamics (MD) computer simulations, focusing specifically on the physical origin of serrated plastic flow. The results demonstrate that there is a direct correlation between macroscopic flow serration and underlying irreversible rearrangement of atoms, which is strongly dependent on the loading (strain) rate and the temperature. The serrated plastic flow is, therefore, determined by the magnitude of such irreversible rearrangement that is inhomogeneous temporally. A dimensionless Deborah number is introduced to characterize the effects of strain rate and temperature on serrations. Our simulations are shown to compare favorably with the available experimental observations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report an intriguing observation that the interaction of brittle nanoscale periodic corrugations (NPCs) can lead to the formation of ductile dimples on the dynamic fracture surface of a tough Vit 1 bulk metallic glass (BMG) under high-velocity plate impact. A “beat” phenomenon due to superposition of simple harmonic vibrations, approximately characterizing NPCs, is proposed to explain this unusual brittle-to-ductile transition. The present results agree well with our previously revealed energy dissipation mechanism in the fracture of BMGs.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Zr-based bulk metallic glass matrix composites with the composition of Zr56.2Ti13.8Nb5.0Cu6.9Ni5.6Be12.(5) were synthesized by the copper-mould suction casting and the Bridgman solidification. The composite, containing a well-developed flowery beta-Zr dendritic phase, was obtained by the Bridgman solidification with the withdrawal velocity of 0.8 mm/s and the temperature gradient of 45 K/mm, and the ultimate strength of 2050 MPa and fracture plastic strain of 14.6% of the composite were achieved, which was mainly interpreted by the homogeneous dispersion of bcc beta-Zr phase in the glass matrix. Crown Copyright (C) 2008 Published by Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report on the conversion of near-ultraviolet radiation of 250-350 nm into near-infrared emission of 970-1100 nm in Yb3+-doped transparent glass ceramics containing Ba2TiSi2O8 nanocrystals due to the energy transfer from the silicon-oxygen-related defects to Yb3+ ions. Efficient Yb3+ emission (F-2(5/2)-> F-2(7/2)) was detected under the excitation of defects absorption at 314 nm. The occurrence of energy transfer is proven by both steady state and time-resolved emission spectra, respectively, at 15 K. The Yb2O3 concentration dependent energy transfer efficiency has also been evaluated, and the maximum value is 65% for 8 mol % Yb2O3 doped glass ceramic. These materials are promising for the enhancement of photovoltaic conversion efficiency of silicon solar cells via spectra modification.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We investigate the laser actions of 5at.% Yb:Gd2xY2(1-x)SiO5 (Yb:GYSO; x = 0.1) crystals with different cutting directions, parallel and vertical to the growth axis. Our results show that the cutting direction of the sample plays an astonished role in the laser operation. The sample cut vertically to the growth axis possesses the favourable lasing characteristics. Its output power reaches 3.13W at 1060nm with a slope efficiency of 44.68% when the absorbed pump power is 8.9 W. In contrast, the sample cut parallel reaches only 1.65 W at 1044 nm with a slope elLiciency of 33.76% with absorbed pump power of 7.99 W. The absorption and emission spectra of the two samples are examined and the merit factor M is calculated. Our analysis is in agreement well with the experimental results. The wavelength tuning range of the superior sample covers from 1013.68 nm to 1084.82 nm.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We investigate the mechanism of selective metallization on glass surfaces with the assistance of femtosecond laser irradiation followed by electroless plating. Irradiation of femtosecond laser makes it possible to selectively deposit copper microstructures in the irradiated area on glass surfaces coated with silver nitrate films. The energy-dispersive X-ray (EDX) analyses reveal that silver atoms are produced on the surface of grooves formed by laser ablation, which serve as catalysis seeds for subsequent electroless copper plating. (C) 2008 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report a new pulse cleaning technique to enhance the contrast ratio of intense ultra-short laser pulses. A pulse temporal cleaner based on nonlinear ellipse rotation by using BK7 glass plate is developed, and a contrast ratio improvement of two orders of magnitude for the milli-joule level femtosecond input pulses is demonstrated, the total transmission efficiency of the pulse cleaner is 16.7%.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report micromodification of Eu element distribution in a silicate glass with femtosecond laser irradiation. Elemental analysis shows that the content of Eu decreased at the focal point and increased in a ring-shaped region around the focal point, which indicates migration of Eu ions has been induced by the femtosecond laser irradiation. Confocal fluorescence spectra demonstrate that the fluorescence intensity of Eu3+ ions increased by 20% in the laser-induced, Eu-enriched, ring-shaped region compared with that for nonirradiated glass. The mechanism for the laser induced change in fluorescence properties of Eu3+ has been investigated. (C) 2009 Optical Society of America

Relevância:

20.00% 20.00%

Publicador:

Resumo:

研究了国产Yb:YAG陶瓷的激光输出特性。激光器采用激光二极管(LD)纵向同轴抽运Yb:YAG陶瓷样品,样品的掺杂原子数分数为1%,一端面镀940 nm和1030 nm双增透膜,另一端面镀1030 nm增透膜,激光器在1031 nm处获得了近红外激光输出。实验中分别测试了Yb:YAG陶瓷在不同输出透射率(T=4%,8%,10%)条件下的激光输出特性。整个实验过程中,激光器维持基横模运转。当输出透射率为10%,吸收的抽运功率为9 W时,激光器获得最大的激光输出功率为1.63 W,相应的斜率效率为23.2%。

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Diode-pumped passively mode-locked laser operation of Yb3+,Na+:CaF2 single crystal has been demonstrated for the first time. By using a SESAM ( semiconductor saturable mirror), simultaneous transform-limited 1-ps passively mode-locked pulses, with the repetition rate of 183MHz, were obtained under the self-Q-switched envelope induced by the laser medium. The average output power of 360mW was attained at 1047nm for 3.34W of absorbed power at 976nm, and the corresponding pulse peak power arrived at 27kW, indicating the promising application of Yb3+,Na+-codoped CaF2 crystals in achieving ultra-short pulses and high pulse peak power. (c) 2005 Optical Society of America.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We investigated the effect of cerium oxide on the precipitation of Ag nanoparticles in silicate glass via a femtosecond laser irradiation and successive annealing. Absorption spectra show that Ce3+ ions may absorb part of the laser energy via multiphoton absorption and release free electrons, resulting in an increase of the concentration of Ag atoms and a decrease of the concentration of hole-trapped color centers, which influence precipitation of the Ag nanoparticles. In addition, we found that the formed Ag-0 may reduce Ce4+ ions to Ce3+ ions during the annealing process, which inhibits the growth of the Ag nanoparticles.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An erratum is presented to correct the propagation loss of the freestanding optical fibers fabricated in glass chip. (c) 2006 Optical Society of America.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Multiple refocusing of a tightly focused femtosecond laser due to the dynamic transformation between self-focusing and self-defocusing is employed to provide a novel method to produce quasi-periodic voids in glass. It is found that the diameter or the interval of the periodic voids increases with the increasing pulse energy of the laser. The detailed course for producing periodic voids is discussed by analysing the damaged track induced by the tightly focused femtosecond laser pulses. It is suggested that this periodic structure has potential applications in fabrication of three-dimensional optical devices.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We investigate the mechanism of formation of periodic void arrays inside fused silica and BK7 glass irradiated by a tightly focused femtosecond (fs) laser beam. Our results show that the period of each void array is not uniform along the laser propagation direction, and the average period of the void array decreases with increasing pulse number and pulse energy. We propose a mechanism in which a standing electron plasma wave created by the interference of a fs-laser-driven electron wave and its reflected wave is responsible for the formation of the periodic void arrays.