345 resultados para super-broadband fiber amplifiers
Resumo:
最近,一种新型的掺铋发光材料引起了人们的关注。这种发光材料有长的荧光寿命(τ>200μs),在800nm激光激发下发射波长在1200~1600nm区间的超宽带荧光(荧光半高宽FWHM>200nm),其发光性质与以往文献中报道的Bi^3+或Bi^2+掺杂的发光材料的性质截然不同;光发射截面(σem)是光掺铒光纤放大器玻璃(EDFAG)的2~3倍,其σem×FWHM值是EDFAG的10倍左右,σem×τ值是掺Ti^3+蓝宝石的3倍左右。
Resumo:
The broadband emission in the 1.2 similar to 1.6 mu m region from Li2O-Al2O3-ZnO-SiO2 ( LAZS) glass codoped with 0.01mol.% Cr2O3 and 1.0mol.% Bi2O3 when pumped by the 808nm laser at room temperature is not initiated from Cr4+ ions, but from bismuth, which is remarkably different from the results reported by Batchelor et al. The broad similar to 1300nm emission from Bi2O3-containing LAZS glasses possesses a FWHM ( Full Width at Half Maximum) more than 250nm and a fluorescent lifetime longer than 500 mu s when excited by the 808nm laser. These glasses might have the potential applications in the broadly tunable lasers and the broadband fiber amplifiers. (c) 2005 Optical Society of America.
Resumo:
The broadband luminescence covering 1.2-1.6 mu m was observed from bismuth and aluminum co-doped germanium oxide glasses pumped by 808 nm laser at room temperature. The spectroscopic properties of GeO2:Bi,Al glasses strongly depend on the glass compositions and the pumping sources. To a certain extent, the Al3+ ions play as dispersing reagent for the infrared-emission centers in the GeO2:Bi,Al glasses. The broad infrared luminescence with a full width at half maximum larger than 200 nm and a lifetime longer than 200 mu s possesses these glasses with the potential applications in broadly tunable laser sources and ultra-broadband fiber amplifiers in optical communication field. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
In this paper, we reported on the fabrication of 980 nm InGaAs/InGaAsP strained quantum-well (QW) lasers with broad waveguide. The laser structure was grown by low-pressure metalorganic chemical vapor deposition on a n(+)- GaAs substrate. For 3 mu m stripe ridge waveguide lasers, the threshold current is 30 mA and the maximum output power and the output power operating in fundamental mode are 350 mW and 200 mW, respectively. The output power from the single mode fiber is up to 100 mW, the coupling efficiency is 50%. We also fabricated 100 mu m broad stripe coated lasers with cavity length of 800 mu m, a threshold current density of 170 A/cm(2), a high slope efficiency of 1.03 W/A and a far-field pattern of 40 x 6 degrees are obtained. The maximum output power of 3.5 W is also obtained for 100 mu m wide coated lasers. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Starting from the modeling of isolated ions and ion-clusters, a closed form rate and power evolution equations for high-concentration erbium-doped fiber amplifiers are constructed. Based on the equations, the effects of the fraction of ion-clusters in total ions and the number of ions per cluster on the performance of high-concentration erbium-doped fiber amplifiers are analyzed numerically. The results show that the presence of the ion-clusters deteriorates amplifier performance, such as the signal power, signal gain, the threshold pump power for zero gain, saturated signal gain, and the maximum gain efficiency, etc. The optimum fiber length or other parameters should be modified with the ion-clusters being taken into account for the amplifiers to achieve a better performance. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
An automatic step adjustment (ASA) method for average power analysis (APA) technique used in fiber amplifiers is proposed in this paper for the first time. In comparison with the traditional APA technique, the proposed method has suggested two unique merits such as a higher order accuracy and an ASA mechanism, so that it can significantly shorten the computing time and improve the solution accuracy. A test example demonstrates that, by comparing to the APA technique, the proposed method increases the computing speed by more than a hundredfold under the same errors. By computing the model equations of erbium-doped fiber amplifiers, the numerical results show that our method can improve the solution accuracy by over two orders of magnitude at the same amplifying section number. The proposed method has the capacity to rapidly and effectively compute the model equations of fiber Raman amplifiers and semiconductor lasers. (c) 2006 Optical Society of America
Resumo:
In this paper, we reported on the fabrication of 980 nm InGaAs/InGaAsP strained quantum-well (QW) lasers with broad waveguide. The laser structure was grown by low-pressure metalorganic chemical vapor deposition on a n(+)- GaAs substrate. For 3 mu m stripe ridge waveguide lasers, the threshold current is 30 mA and the maximum output power and the output power operating in fundamental mode are 350 mW and 200 mW, respectively. The output power from the single mode fiber is up to 100 mW, the coupling efficiency is 50%. We also fabricated 100 mu m broad stripe coated lasers with cavity length of 800 mu m, a threshold current density of 170 A/cm(2), a high slope efficiency of 1.03 W/A and a far-field pattern of 40 x 6 degrees are obtained. The maximum output power of 3.5 W is also obtained for 100 mu m wide coated lasers. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Luminescences from bismuth-doped lime silicate glasses were investigated. Luminescences centered at about 400, 650, and 1300 nm were observed, excited at 280, 532 and 808 nm, respectively. These three luminescence bands arise from three different kinds of bismuth ions in the glasses. The visible luminescences centered at 400 and 650 nm arise from Bi3+, and Bi2+, respectively. The infrared luminescences cover the wavelength range from 1000 to 1600 nm when exited by an 808 nm laser diode. The full width at half maximum (FWHM) of the infrared luminescences is more than 205 urn. The intensity of the infrared luminescence decreases with the increment in CaO content. We suggest that the infrared luminescences might arise from Bi+. Such broadband luminescences indicate that the glasses may be potential candidate material for broadband fiber amplifiers and tunable lasers. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
A compact nonporous high silica (SiO2 % > 96%) glass containing 3400 ppm Er3+ ions, which was about ten times higher than that in Er-doped silica fiber amplifier (EDSFA), was synthesized by sintering porous glass immersed into erbium nitrate solution. The 1532 nm fluorescence has a FWHM (Full Width at Half Maximum) of 45 nm wider than that of EDSFA and possesses the glass with potential application in broadband fiber amplifiers. The Judd-Ofelt theoretical analysis reflects that Er3+ ions are located in a higher covalent environment which are comparable to those of aluminosilicate glass. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
A new method was used to prepare erbium-doped high silica (SiO2% > 96%) glasses by sintering nanoporous glasses. The concentration of erbium ions in high silica glasses can be considerably more than that in silica glasses prepared by using conventional methods. The fluorescence of 1532 nm has an FWHM (Full Wave at Half Maximum) of 50 nm, wider than 35 nm of EDSFA (erbium-doped silica fiber amplifer), and hence the glass possesses potential application in broadband fiber amplifiers. The Judd-Ofelt theoretical analysis reflects that the quantum efficiency of this erbium-doped glass is about 0.78, although the erbium concentration in this glass (6 x 103) is about twenty times higher than that in silica glass. These excellent characteristics of Er-doped high silica glass will be conducive to its usage in optical amplifiers and microchip lasers.
Resumo:
Three Er3+-doped tellurite glasses with compositions of 70TeO(2)-30ZnO, 70TeO(2)-20ZnO-10Nb(2)O(5) and 70TeO(2)-20ZnO-5BaO-5Nb(2)O(5) have been investigated for developing fiber and planar broadband amplifiers and lasers. The optical spectroscopic properties and thermal stability of Er3+-doped tellurite glasses have been discussed. The results show that the incorporation of Nb2O5 increases the thermal stability of Er3+-doped tellurite glasses significantly, Er3+-doped niobium tellurite glasses 70TeO(2)-20ZnO-10Nb(2)O(5) and 70TeO(2)-20ZnO-5BaO-5Nb(2)O(5) exhibit the good thermal stability (DeltaT > 150degreesC), the large emission cross-section (>10 x 10(-21) cm(2)) and broad full width at half maximum (similar to65 nm), will be preferable for broadband Er3+-doped fiber amplifiers. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Tellurite glass is proposed as a host for broadband erbium-doped fiber amplifiers because of their excellent optical and chemical properties. A new single mode Er3+/Yb3+ codoped tellurite fiber with D-shape cladding geometry is fabricated in this work. When pumped at 980 nm, a broad erbium amplified spontaneous emission (ASE) nearly 100 nm in the wavelength range of 1450-1650 ran around 1.53 mu m is observed. It was found that the emission spectrum from erbium in tellurite glass fibers is almost twice as broad as the corresponding spectrum in tellurite bulk glass. The changes in ASE with regard to fiber lengths and pumping power were measured and discussed. The output of about 2.3 mW from Er3+/Yb3+ codoped tellurite fiber ASE source is obtained under the pump power of 700 mW. The broad 1.53 mu m emission of Er3+ in Er3+/Yb3+ codoped tellurite glass fiber can be used as host material for potential broadband optical amplifier and tunable fiber lasers. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
In this paper, we present the broadband optical amplification in bismuth-doped germanate glass, at the second telecommunication window when excited with 808 nm and 980 nm laser diodes, respectively. The amplification range is from 1272 nm to 1348 nm wavelength, which is within the O-band of silica fiber communication. This bismuth-doped glass can be used as ultra broadband amplification material for wavelength-division-multiplexing (WDM) at the second telecommunication window.
Resumo:
Tellurite glass is proposed as a host for broadband erbium-doped fiber amplifiers because of their excellent optical and chemical properties. A single-mode Er3+-doped tellurite glass fiber with D-shape cladding was fabricated in this work. The characterization of amplified spontaneous emission (ASE) from this newly fabricated Er3+-doped tellurite fibers are exhibited. When pumped at 980 nm, a very broad erbium ASE nearly 150 nm around 1.53 mum is observed. The changes in ASE with regard to fiber lengths and pumping power were measured and discussed. The output of 2 mW from Er3+-doped tellurite fiber ASE source was obtained under the pump power of 660 mW. The broad 1.53 mum emission of Er3+ in tellurite glass fiber can be used as host material for potential broadband optical amplifier and tunable fiber lasers. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
This paper reports on the optical spectroscopic properties and thermal stability of Er3+-doped TeO2-BaO (Li2O,NaO)-La2O3 glasses for developing 1.5-mu m fiber amplifiers. Upon excitation at 977 nm laser diode, an intense 1.53-mu m infrared fluorescence has been observed with a broad full width at half maximum (FWHM) of about 60 nm for the Er3+-doped TeO2-BaO (Li2O, Na2O)-La2O3 glass with 10 mol% of BaO. The calculated fluorescence lifetime and the emission cross-sections of the 1.53-mu m transition are 2.91 ms and similar to 9.97 x 10(-21) cm(2), respectively. It is noted that the gain bandwidth, a, x FWHM, of the TeO2-BaO-La2O3Er2O3 glass is about 600, which is significantly higher than that in silicate and phosphate glasses. Meanwhile, it is interesting to note that the TeO2-BaO-La2O3-Er2O3 glass has shown a high glass thermal stability and good infrared transmittance. As a result, TeO2-BaO (Li2O, Na2O)-La2O3 glass with 10 mol% of BaO has been considered to be more useful as a host for broadband optical fiber amplifier. (c) 2005 Elsevier B.V. All rights reserved.