Resumo:
Epitaxial YBCO superconducting films were deposited on the single crystal LaAlO3 (001) substrate by metal organic deposition method. All YBCO films were fired at 820 degrees C in humidity range of 2.6%-19.7% atmosphere. Microstructure of YBCO thin films was analyzed by means of X-ray diffraction (XRD) and scanning electron microscopy (SEM). Superconducting properties of YBCO films were measured by four-probe method. XRD results showed that the second phase (such as BaF2)and a-axis-oriented grains existed in the films prepared at 2.6% humidity condition; a-axis-oriented grains increased in the film prepared at higher than 4.2% humidity condition; almost pure c-axias-oriented grains existed in the films fired at 4.2% humidity condition. Morphologies of the YBCO films showed that all films had a smooth and crack-free surface. YBCO film prepared at 4.2% humidity condition showed J(c) value of 3.3 MA/cm(2) at 77 K in self-field.
Resumo:
The transient thermal stress problem of an inner-surface-coated hollow cylinder with multiple pre-existing surface cracks contained in the coating is considered. The transient temperature, induced thermal stress, and the crack tip stress intensity factor (SIF) are calculated for the cylinder via finite element method (FEM), which is exposed to convective cooling from the inner surface. As an example, the material pair of a chromium coating and an underlying steel substrate 30CrNi2MoVA is particularly evaluated. Numerical results are obtained for the stress intensity factors as a function of normalized quantities such as time, crack length, convection severity, material constants and crack spacing. (c) 2005 Elsevier Ltd. All rights reserved.
Resumo:
首次在涂敷PEI的玻璃表面上制备了癸酸及全氟癸酸的单分子层膜。研究了成膜机理及摩擦特性。结果表明。脱水剂DCCD促进了癸酸或全氟癸酸与PEI酞胺化的反应。导致两种羧酸在PEI表面产生了靠化学键(酞胺键)连接的稳定的单分子层膜,摩擦、磨损实验表明。单分子层有机膜的摩擦特性受膜的组成、表面能及有序性和堆积密度的重要影响。表面能越低,有序性和堆积密度越高。摩擦系数越低。与碳氢化合物相比。碳氟化合物形成的有序膜具有更高的强度和抗磨性能。
Resumo:
We present a good alternative method to improve the tribological properties of polymer films by chemisorbing a long-chain monolayer on the functional polymer surface. Thus, a novel self-assembled monolayer is successfully prepared on a silicon substrate coated with amino-group-containing polyethyleneimine (PEI) by the chemical adsorption of stearic acid (STA) molecules. The formation and structure of the STA-PEI film are characterized by means of contact-angle measurement and ellipsometric thickness measurement, and of Fourier transformation infrared spectrometric and atomic force microscopic analyses. The micro- and macro-tribological properties of the STA-PEI film are investigated on an atomic force microscope (AFM) and a unidirectional tribometer, respectively. It has been found that the STA monolayer about 2.1-nm thick is produced on the PEI coating by the chemical reaction between the amino groups in the PEI and the carboxyl group in the STA molecules to form a covalent amide bond in the presence of N,N'-dicyclohexylcarbodiimide (DCCD) as a dehydrating regent. By introducing the STA monolayer, the hydrophilic PEI polymer surface becomes hydrophobic with a water contact angle to be about 105degrees. Study of the time dependence of the film formation shows that the adsorption of PEI is fast, whereas at least 24 h is needed to generate the saturated STA monolayer. Whereas the PEI coating has relatively high adhesion, friction, and poor anti-wear ability, the STA-PEI film possesses good adhesive resistance and high load-carrying capacity and anti-wear ability, which could be attributed to the chemical structure of the STA-PEI thin film. It is assumed that the hydrogen bonds between the molecules of the STA-PEI film act to stabilize the film and can be restored after breaking during sliding. Thus, the self-assembled STA-PEI thin film might find promising application in the lubrication of micro-electromechanical systems (MEMS).
Resumo:
In 0.1 mol/l KH2PO4–Na2HPO4 (pH 7.80) buffer solution, the potential of zero charge (PZC) and the open circuit potential of gold-coated silicon were determined to be about −0.6 and +0.10 V (vs SCE), respectively. The open circuit potential was higher than the PZC, which indicated that the surface of the gold-coated electrode had a positive charge. The ellipsometry experiment showed that the adsorption of fibrinogen onto the gold-coated silicon wafer surface arrived at a saturated state when the adsorption time exceeded 50 min. The percentage of surface without adsorbed protein, θ, was about 63%. This means that the proportion of surface actually occupied by fibrinogen was only about 37% after the adsorption arrived at saturation. The solution/protein capacitance value was determined in an impulse state around −0.59 V (vs SCE) and was stable (4.2×10−5 F) at other potentials.
Resumo:
Anodic bonding with thin films of metal or alloy as an intermediate layer, finds increasing applications in micro/nanoelectromechanical systems. At the bonding temperature of 350 degrees C, voltage of 400 V, and 30 min duration, the anodic bonding is completed between Pyrex glass and crystalline silicon coated with an aluminum thin film with a thickness comprised between 50 and 230 nm. Sodium-depleted layers and dendritic nanostructures were observed in Pyrex 7740 glass adjacent to the bonding interface. The sodium depletion width does not increase remarkably with the thickness of aluminum film. The dendritic nanostructures result from aluminum diffusion into the Pyrex glass. This experimental research is expected to enhance the understanding of how the depletion layer and dendritic nanostructures affect the quality of anodic bonding. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Micro anchor is a kind of typical structures in micro/nano electromechanical systems (MEMS/NEMS), and it can be made by anodic bonding process, with thin films of metal or alloy as an intermediate layer. At the relative low temperature and voltage, specimens with actually sized micro anchor structures were anodically bonded using Pyrex 7740 glass and patterned crystalline silicon chips coated with aluminum thin film with a thickness comprised between 50 nm and 230 nm. To evaluate the bonding quality, tensile pulling tests have been finished with newly designed flexible fixtures for these specimens. The experimental results exhibit that the bonding tensile strength increases with the bonding temperature and voltage, but it decreases with the increase of the thickness of Al intermediate layer. This kind of thickness effect of the intermediate layer was not mentioned in the literature on anodic bonding. (C) 2008 Elsevier Ltd. All rights reserved.
Resumo:
A three-dimensional finite element analysis has been used to determine the internal stresses in a three-phase composite. The stresses have been determined for a variety of interphase properties, the thicknesses of the interphase and the volume fractions of particles. Young's modulus has been calculated from a knowledge of these stresses and the applied deformation. The calculations show that stress distributions in the matrix and the mechanical properties are sensitive to the interphase property in the three-phase composites. The interfacial stresses in the three-dimensional analysis are in agreement with results obtained by an axisymmetric analysis. The predicted bulk modulus in three-dimensional analysis agrees well with the theoretical solution obtained by Qui and Weng, but it presents a great divergence from that in axisymmetric analyses. An investigation indicates that this divergence may be caused by the difference in the unit cell structure between two models. A comparison of the numerically predicted bulk and shear modulus for two-phase composites with the theoretical results indicates that the three-dimensional analysis gives quite satisfactory results.
Resumo:
Anodic bonding with thin films of metal or alloy as an intermediate layer, finds increasing applications in micro/nanoelectromechanical systems. At the bonding temperature of 350 degrees C, voltage of 400 V, and 30 min duration, the anodic bonding is completed between Pyrex glass and crystalline silicon coated with an aluminum thin film with a thickness comprised between 50 and 230 nm. Sodium-depleted layers and dendritic nanostructures were observed in Pyrex 7740 glass adjacent to the bonding interface. The sodium depletion width does not increase remarkably with the thickness of aluminum film. The dendritic nanostructures result from aluminum diffusion into the Pyrex glass. This experimental research is expected to enhance the understanding of how the depletion layer and dendritic nanostructures affect the quality of anodic bonding. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
A method was devised to evaluate the adhesion between a film and a substrate. A front-end coated bullet is accelerated by a gas gun and hits the substrate of the specimen under test. The impact generates a compressive stress pulse that propagates toward the film. After transmission through the interface, part of the pulse is reflected on the free surface of the film, and tensile stress arises at the film-substrate interface, possibly inducing debonding of the film. This dynamic process was demonstrated analytically and simulated numerically by the finite element method. The results validate the initial concept and lay the foundation for further optimization of this method.
Resumo:
A preliminary experiment was carried out to validate the feasibility of the method of impact by a front-end-coated bullet to evaluate the interface adhesion between film and substrate. The theoretical description of the initiation, propagation and evolution of the stress pulse during impact was generalized and formulized. The effects of the crucial parameters on the interface stress were further investigated with FEM. The results found the promising prospect of the application of such a method and provided useful guidance for experimental design.
Resumo:
A dissolved oxygen sensor made of plastic optical fiber as the substrate and dichlorotris (1, 10-phenanthroline) ruthenium as a fluorescence indicator is studied. Oxygen quenching characteristics of both intensity and phase were measured; the obtained characteristics showed deviation from the linear relation described by the Stern-Volmer equation. A two-layer model is proposed to explain the deviation, and main parameters can be deduced with the model. (C) 2009 Optical Society of America
Resumo:
A kind of 1,6,10,15,19,24,28,33-octa-iso-pentyloxy-2,3-metallonaphthalocyanines complexes MNc(iso-PeO)(8) (M = Co, Cu, Pd) are used as spincoating film-forming materials. The surface morphologies of the films prepared were studied first. These films were then used for the experiments of NO2 sensing. The effects of sensing temperature as well as the NO concentration on the sensing properties were studied. The experimental results showed that the three MNc(iso-PeO)(8) films were uniform, smooth and dense. Due to the different metal ions (M) on the center of naphthalocyanine, the CoNc(iso-PeO)(8) film had a higher film resistance and response-recovery rate in the NO2 sensing experiments. On the contrary, the response to NO2 of the PdNc(iso-PeO)(8) and CuNc(iso-PeO)(8) films were superior to that of CoNc(iso-PeO)(8). By varying the sensing temperature, it was found that the elevation of sensing temperature could improve the sensing response, recovery ratio, and sensitivity of the sensing films. At high concentrations of NO2, the response time became shorter. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
The LB films and spin-coated films of tetra-neopentoxy phthalocyanine zinc (TNPPcZn) were prepared and annealed at different temperatures. Their refractive index (n) and extinction coefficient (k) were measured by p-polarized reflectance. The similar value of n and k, as well as similar changing tendency of it and k at varied annealing temperatures, was found between LB films and spin-coated films. In addition, the absorption curves of TNPPcZn LB films and spin-coated films in visible range at different annealing temperature were investigated. The results indicate that the changing tendency of the extinction coefficient of two kinds of TNPPcZn films obtained from two methods mentioned above were coincident. When the annealing temperature increased to 150 degrees C, the monomers of TNPPcZn films transformed to aggregates, n(f) and k(f) of the films increased. Further, n(f) and k(f) decreased as aggregates changed back to monomers again at the annealing temperature of 300 degrees C. The experimental results coincide well with the theoretical analysis. (C) 2004 Elsevier B.V. All rights reserved.