195 resultados para WURTZITE ZNS
Resumo:
Through a facile solvothermal route using zinc chloride and thiourea as reactants, wurtzite ZnS and its precursor ZnS center dot (en)(0.5) (en = ethylenediamine) with various morphologies and sizes were grown, which were characterized by XRD, SEM, TEM and N-2 adsorption and so on. The phase evolution, composition and morphologies of the products are highly dependent on the concentration of en. By keeping the en-water volume ratio at 1/2 to 1, the nanostripes-flower or nanorod-spheric wurtzite ZnS were easily obtained under 120 degrees C for 6-24 h, which possess relatively higher specific surface area and larger total pore volume.
Resumo:
Wurtzite stalactite-like quasi-one-dimensional ZnS nanoarrays with ZnO protuberances were synthesized through a thermal evaporation route. The structure and morphology of the samples are studied and the growth mechanism is discussed. X-ray diffraction (XRD) results show both the ZnS stem and the ZnO protuberances have wurtzite structure and show preferred [001] oriented growth. The photoluminescence and field emission properties have also been investigated. Room temperature photoluminescence result shows it has a strong green light emission, which has potential application for green light emitter. Experimental results also show that the stalactite arrays have a good field emission property, with turn-on field of 11.4 V/mu m, and threshold field of 16 V/mu m. The ZnO protuberances on the ZnS stem might enhance the field emission notably.
Resumo:
Quasi-aligned Eu2+-doped wurtzite ZnS nanowires on Au-coated Si wafers have been successfully synthesized by a vapor deposition method under a weakly reducing atmosphere. Compared with the undoped counterpart, incorporation of the dopant gives a modulated composition and crystal structure, which leads to a preferred growth of the nanowires along the [0110] direction and a high density of defects in the nanowire hosts. The ion doping causes intense fluorescence and persistent phosphorescence in ZnS nanowires. The dopant Eu2+ ions form an isoelectronic acceptor level and yield a high density of bound excitions, which contribute to the appearance of the radiative recombination emission of the bound excitons and resonant Raman scattering at higher pumping intensity. Co-dopant Cl- ions can serve not only as donors, producing a donor-acceptor pair transition with the Eu2+ acceptor level, but can also form trap levels together with other defects, capture the photoionization electrons of Eu2+, and yield long-lasting (about 4 min), green phosphorescence. With decreasing synthesis time, the existence of more surface states in the nanowires forms a higher density of trap centers and changes the crystal-field strength around Eu2+. As a result, not only have an enhanced Eu2+ -4f(6)5d(1)-4f(7) intra-ion transition and a prolonged afterglow time been more effectively observed (by decreasing the nanowires' diameters), but also the Eu2+ related emissions are shifted to shorter wavelengths.
Resumo:
High quality n-type CdS nanobelts (NBs) were synthesized via an in situ indium doping chemical vapor deposition method and fabricated into field effect transistors (FETs). The electron concentrations and mobilities of these CdS NBs are around (1.0x10(16)-3.0x10(17))/cm(3) and 100-350 cm(2)/V s, respectively. An on-off ratio greater than 10(8) and a subthreshold swing as small as 65 mV/decade are obtained at room temperature, which give the best performance of CdS nanowire/nanobelt FETs reported so far. n-type CdS NB/p(+)-Si heterojunction light emitting diodes were fabricated. Their electroluminescence spectra are dominated by an intense sharp band-edge emission and free from deep-level defect emissions. (c) 2006 American Institute of Physics.
Resumo:
ZnO films prepared by the thermal oxidation of the ZnS films through thermal evaporation are reported. The as-deposited ZnS films have transformed to ZnO films completely at 400 degrees C. The 400-700 degrees C annealed films with a preferential c-axis (002) orientation have a hexagonal wurtzite structure. The band gap of ZnO films shifts towards longer wavelength with the increase of the annealing temperature. The relationship between the band gap energy of ZnO films and the grain size is discussed. The shift of the band gap energy can be ascribed to the quantum confinement effect in nanocrystal ZnO films. The photoluminescence spectra of ZnO films show a dominant ultraviolet emission and no deep level or trap state defect emission in the green region. It confirms the absence of interstitial zinc or oxygen vacancies in ZnO films. These results indicate that ZnO film prepared by this simple thermal oxidation method is a promising candidate for optoelectronic devices and UV laser. (c) 2005 Elsevier BN. All rights reserved.
Resumo:
In-situ energy dispersive x-ray diffraction on ZnS nanocrystalline was carried out under high pressure by using a diamond anvil cell. Phase transition of wurtzite of 10 nm ZnS to rocksalt occurred at 16.0 GPa, which was higher than that of the bulk materials. The structures of ZnS nanocrystalline at different pressures were built by using materials studio and the bulk modulus, and the pressure derivative of ZnS nanocrystalline were derived by fitting the equation of Birch-Murnaghan. The resulting modulus was higher than that of the corresponding bulk material, which indicates that the nanomaterial has higher hardness than its bulk materials.
Resumo:
An in situ energy dispersive x-ray diffraction study on nanocrystalline ZnS was carried out under high pressure up to 30.8 GPa by using a diamond anvil cell. The phase transition from the wurtzite to the zinc-blende structure occurred at 11.5 GPa, and another obvious transition to a new phase with rock-salt structure also appeared at 16.0 GPa-which was higher than the value for the bulk material. The bulk modulus and the pressure derivative of nanocrystalline ZnS were derived by fitting the Birch-Murnaghan equation. The resulting modulus was higher than that of the corresponding bulk material, indicating that the nanomaterial has higher hardness than the bulk material.
Resumo:
Optical transmission through flat media should be smaller than 1. However, we have observed optical transmission up to T=1.18. The samples were ZnS-SiO2/AgOx/ZnS-SiO2 sandwiched thin films on glass substrate. The supertransmission could only be observed in the near field. We attribute the supertransmission to the lateral propagation relayed by the laser activated and decomposed Ag nanoparticles. (c) 2006 American Institute of Physics.
Resumo:
使用倾斜角沉积(GLAD)的电子束蒸发技术,制备了倾斜角度在60°~85°之间的ZnS双折射雕塑薄膜(STF)。使用X射线衍射(XRD)和扫描电镜(SEM)检测了ZnS薄膜的结晶状态和断面形貌,使用Lamda-900分光光度计测量了薄膜在不同的偏振光入射时的透过率。研究发现,室温下倾斜沉积ZnS薄膜断面为倾斜柱状结构,且薄膜的结晶程度不高。在相同的监控厚度时,随倾斜角度增大,沉积到基片上的薄膜厚度逐渐变小,但仍然大于余弦曲线显示的理论厚度。根据偏振光垂直入射时薄膜的透过光谱计算了不同角度沉积的薄膜的折射率
Resumo:
The glancing angle deposition (GLAD) technique was used to deposit ZnS films by electron beam evaporation method. The cross sectional scanning electron microscopy (SEM) image illustrated a highly orientated microstructure composed of slanted column. The atomic force microscopy (APM) analysis indicated that incident flux angle had significant effects on the nodule size and surface roughness. Under identical nominal thickness, the actual thickness of the GLAD films is related to the incident flux angle. The refractive index and in-plane birefringence of the GLAD ZnS films were discussed, and the maximum bireffingence Delta n = 0.036 was obtained at incident flux angle of alpha = 80 degrees. Therefore, the glancing angle deposition technique is a promising way to create a columnar structure with enhanced birefringent property. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Chinese Academy of Sciences;National Science Fund for Distinguished Young Scholar 60925016;National High Technology Research and Development program of China 2009AA034101;Postdoctoral Foundation 0971050000
Resumo:
Using the density function theory within the generalized gradient approximation, the band structures of wurtzite ZnO, BeO and MgO have been calculated. The effective-mass parameters are fitted using the calculated eigenvalues. The Dresselhaus spin-orbit effect appears in the k[1 00] direction, and is zero in the high symmetry direction k[00 1]. The orderings of valence band split by the crystal-field and spin-orbit coupling in wurtzite ZnO, BeO and MgO are identified by analyzing the wave function characters calculated by projecting the wave functions onto p-state in the spherical harmonics. For wurtzite ZnO, the ordering of valence band is Still Gamma(7) > Gamma(9) > Gamma(7) due to the negative spin-orbit coupling splitting energy and the positive crystal-field splitting energy. Thus, the Thomas' conclusion is confirmed. For wurtzite BeO and MgO, although their orderings of valence bands are Gamma(7) > Gamma(9) > Gamma(7) too, the origins of their orderings are different from that of wurtzite ZnO. Zn1-x,YxO (Y = Mg, Be) doped with N and P atoms have been studied using first-principles method. The calculated results show that N atom doped in Zn1-x BexO has more shallow acceptor energy level with increasing the concentration of Be atom. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
We investigate the uniaxial strain effect in the c-plane on optical properties of wurtzite GaN based on k center dot p theory, the spin-orbit interactions are also taken into account. The energy dispersions show that the uniaxial strain in the c-plane gives an anisotropic energy splitting in the k(x) - k(y) plane, which can reduce the density of states. The uniaxial strain also results in giant in-plane optical polarization anisotropy, hence causes the threshold carrier density reduced. We clarify the relations between the uniaxial strain and the optical polarization properties. As a result, it is suggested that the compressive uniaxial strain perpendicular to the laser cavity direction in the c-plane is one of the preferable approaches for the effcient improvement of GaN-based laser performance.
Resumo:
The optical properties of the strained wurtzite GaN are investigated theoretically within the nearest neighbor tight-binding method. The piezoelectric effect is also taken into account. The empirical rule has been used in the strained band-structure calculation. The results show that the excitonic transition energies are anisotropic in the c-plane in a high electronic concentration system and have a 60 degrees periodicity, which is in agreement with experiment. (C) 2008 American Institute of Physics. [DOI: 10.1063/1.3001937]