469 resultados para TUNABLE PHOTOLUMINESCENCE


Relevância:

100.00% 100.00%

Publicador:

Resumo:

LaInO3:Eu3+ phosphors were prepared by a Pechini sol-gel process. X-ray diffraction (XRD), field-emission scanning electron microscopy (FE-SEM), diffuse reflectance, photoluminescence, cathodoluminescence spectra, as well as lifetimes were utilized to characterize the synthesized phosphors. XRD results reveal that the sample begins to crystallize at 600 degrees C and pure LaInO3 phase can be obtained at 800 degrees C. The crystallinity increases upon raising the annealing temperature. The FE-SEM images indicate that LaInO3:Eu3+ phosphors are composed of fine and spherical grains around 40-80 nm in size. Under the excitation of UV light and low-voltage electron-beams, LaInO3:Eu3+ phosphors show the characteristic emissions of the Eu3+ (D-5(J)-F-7(J) J,J(')=0,1,2,3 transitions). The luminescence colors can be tuned from yellowish warm white to red by changing the doping concentration of Eu3+ to some extent. The corresponding luminescence mechanisms have been proposed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Silica xerogels prepared by sol-gel method show blue emission under UV excitation with a smaller Stokes shift. The luminescent properties have been investigated under various preparation conditions and compositions. The silica xerogels show similar luminescent properties when using C2H5OH and N,N-dimethylformamide (DMF) as solvents, which are very different from those when using dimethylsulfoxide (DMSO) as solvent, i.e., a red shift of excitation and emission has been observed in the latter case. The emission intensity of the silica xerogels also depends on the water content and pH of the starting reaction solution. The introduction of organic group (-CH3) in the silica xerogel modifies the network structure and further changes their luminescence properties. Heat treatment results in the decomposition of the organic (-SiCH3) groups, which eliminates the old luminescent centers and produces new luminescent centers in longer wavelength simultaneously. (C) 2000 Elsevier Science B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Many efforts have been devoted to exploring novel luminescent materials that not contain expensive or toxic elements, or do not need a mercury vapor plasma source. In this paper, BPO4 and Li+-doped BPO4 powder samples were prepared by the Pechini-type sol-gel (PSG) process. The structure and optical properties of the resulting samples were characterized by X-ray diffraction (XRD), Fourier transform infrared (FT-IR) spectroscopy, field emission scanning electron microscopy (FESEM), photoluminescence (PL) excitation and emission spectra, kinetic decay, and X-ray photoelectron spectra (XPS), respectively. It was found that PSG -derived Li+-doped BPO4 annealed at 960 degrees C exhibited bright bluish-white emission centered at 416 nm. The luminescence decay curves analysis indicates that each sample has two kinds of lifetimes (5.9 ns and 0.529 ms) and two types of kinetic decay behaviors which can be fitted into a single-exponential function and a double-exponential function, respectively.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

In this paper, BPO4-xSiO(2) (X: SiO2/BPO4 molar ratio, 0-70%) and BPO4-xAl(2)O(3) (X: Al2O3/BPO4 molar ratio, 0-20%) powder samples were prepared by the Pechini-type sol-gel (PSG) process using glycerol and poly(ethylene glycol) as additives. The structure and optical properties of the resulting samples were characterized by X-ray diffraction (XRD), Fourier transform infrared (FT-IR) spectroscopy, field emission scanning electron microscopy (FESEM), diffuse reflection spectra, photoluminescence (PL) excitation and emission spectra, kinetic decay, and X-ray photoelectron spectra (XPS), respectively. It was found that the Pechini-type sol-gel-derived BPO4-xSiO(2) annealed at 1000 degrees C and BPO4-xAl(2)O(3) annealed at 960 degrees C exhibited bright bluish-white emissions centered at 428 and 413 nm, respectively. The luminescence decay curve analysis indicates that each sample has two kinds of lifetimes (more than 0.4 ms and less than 10 ns) and two types of kinetic decay behaviors, which can be fitted into a double-exponential function and a single-exponential function, respectively.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

In this paper, BPO4 and Ba2+-doped BPO4 powder samples were prepared by the sol-gel process using glycerol and poly(ethylene glycol) as additives. The structure and optical properties of the resulting samples were characterized by X-ray diffraction (XRD), Fourier transform infrared (FT-IR) spectroscopy, field emission scanning electron microscopy (FESEM), diffuse reflection spectra, photoluminescence (PL) excitation and emission spectra, quantum yield, kinetic decay, and electron paramagnetic resonance (EPR), respectively. It was found that the undoped BPO4 showed a weak purple blue emission (409 nm, lifetime 6.4 ns) due to the carbon impurities involved in the host lattice. Doping Ba2+ into BPO4 resulted in oxygen-related defects as additional emission centers which enhanced the emission intensity greatly (> 10x) and shifted the emission to a longer-wavelength region (lambda(max) = 434 nm; chromaticity coordinates: x = 0.174, y = 0. 187) with a bluish-white color. The highest emission intensity was obtained ;when doping 6 mol % Ba2+ in BPO4, which has a quantum yield as high as 31%. The luminescent mechanisms of BPO4 and Ba2+-doped BPO4 were discussed in detail according to the existing models for silica-based materials.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

A series of D-pi-A-pi-D type of near-infrared (NIR) fluorescent compounds based on benzobis(thia diazole) and its selenium analogues were synthesized and fully characterized by H-1 and C-13 NMR, high-resolution mass spectrometry, and elemental analysis. The absorption fluorescence, and electrochemical properties were also studied. Photoluminescence of these chromophores ranges from 900 to 1600 nm and their band gaps are between 1.19 and 0.56 eV.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The electronic structure, Zeeman splitting, and g factor of Mn-doped CdS nanowires are studied using the k center dot p method and the mean field model. It is found that the Zeeman splittings of the hole ground states can be highly anisotropic, and so can their g factors. The hole ground states vary a lot with the radius. For thin wire, g(z) (g factor when B is along the z direction or the wire direction) is a little smaller than g(x). For thick wire, g(z) is mcuh larger than g(x) at small magnetic field, and the anisotropic factor g(z)/g(x) decreases as B increases. A small transverse electric field can change the Zeeman splitting dramatically, so tune the g(x) from nearly 0 to 70, in thick wire. The anisotropic factor decreases rapidly as the electric field increases. On the other hand, the Zeeman splittings of the electron ground states are always isotropic.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Rhombohedral-calcite and hexagonal-vaterite types of LuBO:Eu3+ microparticles with various complex self-assembled 3D architectures have been prepared selectively by an efficient surfactant- and template-free hydrothermal process for the first time. X-ray diffraction, scanning electron microscopy, energy-dispersive X-ray spectrometry, transmission electron microscopy, high-resolution transmission electron microscopy, selected area electron diffraction, photoluminescence, and cathodoluminescence spectra as well as kinetic decays were used to characterize the samples.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Tb(1-x)BO3:xEu(3+) (x = 0-1) microsphere phosphors have been successfully prepared by a simple hydrothermal process directly without further sintering treatment. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), thermogravimetric analysis (TGA), scanning electron microscopy (SEM), transmission electron microscopy (TEM), high-resolution transmission electron microscopy (HRTEM), selected area electron diffraction (SAED), photoluminescence (PL), low-voltage cathodoluminescence (CL), and time-resolved emission spectra as well as lifetimes were used to characterize the samples.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this article, monodisperse spherical zirconia (ZrO2) particles with a narrow size distribution were prepared by the controlled hydrolysis of zirconium butoxide in ethanol, followed by heat treatment in air at low temperature from 300 to 500 degrees C. X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy, thermogravimetric and differential thermal analysis (TG/DTA), scanning electron microscopy (SEM), transmission electron microscopy (TEM), photoluminescence (PL) spectra, kinetic decay, and electron paramagnetic resonance were used to characterize the samples. The experimental results indicate that the annealed ZrO2 samples exhibit broad, intense visible photoluminescence. The annealing temperature is indispensable for the luminescence of the obtained ZrO2 particles. The emission colors of the ZrO2 samples can be tuned from blue to nearly white to dark orange by varying the annealing temperature.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

beta-NaYF4 hexagonal microprisms and microrods with different aspect ratios have been prepared via a simple hydrothermal route. X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), and photoluminescence (PL) spectra as well as kinetic decays were used to characterize the samples. The influences of reaction temperature and the molar ratio of NaF to y(3+) on the crystal phases and shapes of final products have been studied in detail. The aspect ratios of products increase gradually with the increase of reaction temperature and NaF/Y3+ molar ratio. The growth mechanisms of crystals prepared under the different conditions are presented systematically. More importantly, the systematical investigation on the luminescence properties of beta-NaYF4:xEu(3+) (x = 0.5, 1, 2, 3, 5, and 10 mol %) with hexagonally microprismatic morphology shows the characteristic emissions of Eu3+ (D-5(J)-F-7(J'), J, J' = 0, 1, 2, 3). Under the excitation of single wavelength light of 397 nm, the luminescence colors of the corresponding products can be tuned feasibly from bluish white to yellow to red by changing the doping concentration of Eu3+.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

CaIn2O4:Eu3+ phosphors were prepared by a Pechini so-gel process. X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), photoluminescence (PL), cathodoluminescence (CL) spectra as well as lifetimes were utilized to characterize the samples. The XRD results reveal that the samples begin to crystallize at 800 degrees C, and the crystallinity increases upon raising the annealing temperature. The FE-SEM images indicate that the CaIn2O4:Eu3+ samples consist of fine and spherical grains with size around 200-400 nm. Under the excitation of ultraviolet light and low-voltage electron beams, the CaIn2O4:Eu3+ phosphors show the characteristic emissions of Eu3+ ((DJ-7FJ ')-D-5 J, J ' = 0, 1, 2, 3 transitions). The luminescence color can be tuned from white to orange to red by adjusting the doping concentration of EU3+. The corresponding luminescence mechanisms have been proposed.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Nanocyrstalline Tb3+-doped LaGaO3 phosphors were prepared through a Pechini-type sol-gel process. X-ray diffraction, field-emission scanning electron microscopy (FESEM), photoluminescence, cathodoluminescence spectra, and lifetimes were utilized to characterize the synthesized phosphors. XRD results reveal that the sample begins to crystallize at 900 degrees C and pure LaGaO3 phase can be obtained at 1000 degrees C. FESEM images indicate that the Tb3+-doped LaGaO3 phosphors are composed of aggregated spherical particles with sizes ranging from 40 to 80 nm. Under the excitation of ultraviolet light and low-voltage electron beams (0.5-3 kV), the Tb3+-doped LaGaO3 phosphors show the characteristic emissions from the LaGaO3 host lattice and the Tb3+ (D-5(3,4)-F-7(6,5,4,3) transitions). The emission colors of Tb3+-doped LaGaO3 phosphors can be tuned from blue to green by changing the excitation wavelength of ultraviolet light and the doping concentration of Tb3+ to some extent. Relevant luminescence mechanisms are discussed.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A series of orange-red to red phosphorescent heteroleptic Cu-I complexes (the first ligand: 2,2 '-biquinoline (bq), 4,4 '-diphenyl2,2 '-biquinoline (dpbq) or 3,3 '-methylen-4,4 '-diphenyl-2,2 '-biquinoline (mdpbq); the second ligand: triphenylphosphine or bis[2-(diphenylphosphino)phenyl]ether (DPEphos)) have been synthesized and fully characterized. With highly rigid bulky biquinoline-type ligands, complexes [Cu(mdpbq)(PPh3)(2)](BF4) and [Cu(mdpbq)(DPEphos)](BF4) emit efficiently in 20 wt % PMMA films with photoluminescence quantum yield of 0.56 and 0.43 and emission maximum of 606 nm and 617 nm, respectively. By doping these complexes in poly(vinyl carbazole) (PVK) or N-(4-(carbazol-9-yl)phenyl)-3,6-bis(carbazol-9-yl) carbazole (TCCz), phosphorescent organic light-emitting diodes (OLEDs) were fabricated with various device structures. The complex [Cu(mdpbq)(DPEphos)](BF4) exhibits the best device performance. With the device structure of ITO/PEDOT/ TCCz:[Cu(mdpbq)(DPEphos)](BF4) (15 wt %)/TPBI/LiF/Al (III), a current efficiency up to 6.4 cd A(-1) with the Commission Internationale de L'Eclairage (CIE) coordinates of (0.61, 0.39) has been realized. To our best knowledge, this is the first report of efficient mononuclear Cu complexes with red emission.