454 resultados para Molecular weight hyaluronan
Resumo:
The tribological properties of the high-strength and high-modulus ultrahigh molecular weight polyethylene (UHMWPE) film and the UHMWPE composites reinforced by multiwalled carbon nanotubes (MWCNT/UHMWPE) were investigated using a nanoindenter and atomic force microscope (AFM). The MWCNT/UHMWPE composites films exhibited not only high wear resistance but also a low friction coefficient compared to the pure UHMWPE films. We attribute the high wear resistance to the formation of the new microstructure in the composites due to the addition of MWCNTs.
Resumo:
A hemorrhagic proteinase, jerdohagin, was purified from Trimeresurus jerdonii venom by gel filtration and ion-exchange chromatographies. It was a single chain polypeptide with an apparent molecular weight of 96 kDa as estimated by SDS-PAGE under the non-reducing and reducing conditions. Internal peptide sequencing indicated that it consisted of metalloproteinase, disintegrin-like and cysteine-rich domains and belonged to the class III snake venom metalloproteinases (class P-III SVMPs). Like other typical metalloproteinases, hemorrhagic activities of jerdohagin were completely inhibited by EDTA, but not by PMSF. Jerdohagin preferentially degraded a-chain of human fibrinogen. Interestingly, jerdohagin did not activate human prothrombin, whereas it cleaved human prothrombin and fragment F1 of activated human prothrombin. (C) 2004 Elsevier Ltd. All rights reserved.
An improved method for the extraction of low molecular weight organic acids in variable charge soils
Resumo:
Due to specific adsorption to variable charge soils, low molecular weight organic acids (LMWOAs) have not been sufficiently extracted, even if common extractants, such as water and 0.1 M sodium hydroxide (NaOH), were employed. In this work, the method for extracting LMWOAs in soils with 0.1 M NaOH was improved for variable charge soils; e.g. 1.0 M potassium fluoride (KF) with pH 4.0 was applied as an extractant jointed with 0.1 M NaOH based on its stronger ability to change the electrochemical properties of variable charge soils by specific adsorption. With the proposed method, the recoveries of oxalic, tartaric, malic, citric and fumaric acids were increased from 83 4, 93 1, 22 2, 63 +/- 5 and 84 +/- 3% to 98 +/- 2, 100 +/- 2, 85 +/- 2, 90 +/- 2 and 89 +/- 2%, respectively, compared with NaOH alone. Simultaneously, the LMWOAs in Agri-Udic Ferrosol with field moisture were measured with a satisfactory result.
Resumo:
RP-HPLC analysis for low molecular weight organic acids in soil solution has been optimized. An Atlantis (TM) C-18 column was used for the analyses. An optimal determination for eleven organic acids in soil solution was found at room temperature (25 degrees C) and 220 nm detection wavelength, with a mobile phase of 10 mM KH2PO4 -CH3OH (955, pH 2.7), a flow rate of 0.8 mL/min and 10 mu L sample size. The detection limits ranged 3.2-619 ng/mL, the coefficients of variation ranged 1.3-4.6%, and the recoveries ranged 95.6-106.3% for soil solution with standard addition on the optimal conditions proposed.
Effects of low-molecular-weight organic acids on Cu(II) adsorption onto hydroxyapatite nanoparticles
Resumo:
Molecular weight dependence of phase separation behavior of the Poly (ethylene oxide) (PEO)/Poly(ethylene oxide-block-dimethylsiloxane) (P(EO-b-DMS)) blends was investigated by both experimental and theoretical methods. The cloud point curves of PEO/P(EO-b-DMS) blends were obtained by turbidity method. Based on Sanchez-Lacombe lattice fluid theory (SLLFT), the adjustable parameter, epsilon*(12)/k (quantifying the interaction energy between different components), was evaluated by fitting the experimental data in phase diagrams. To calculate the spinodals, binodals, and the volume changes of mixing for these blends, three modified combining rules of the scaling parameters for the block copolymer were introduced.
Resumo:
Well-defined polyacrylonitrile with a higher number-average molecular weight (R.) up to 200,000 and a lower polydispersity index (PDI, 1.7-2.0) was firstly obtained via reversible addition-fragmentation chain transfer (RAFT) process. This was achieved by selecting a stable, easy way to prepare disulfide compound intermediates including bis(thiobenzoyl) disulfide (BTBDS) and bis(thiophenylacetoyl) disulfide (BTPADS) to react with azobis(isobutyronitrile) to directly synthesize RAFT agents in situ.
Resumo:
Lewis base modification strategy on rare earth ternary catalyst was disclosed to enhance nucleophilic ability of active center during copolymerization of carbon dioxide and propylene oxide (PO), poly(propylene carbonate) (PPC) with H-T linkages over 83%, and number-average molecular weight (M-n) up to 100 kg/mol was synthesized at room temperature using Y(CCl3OO)(3)-ZnEt2-glycerine catalyst and 1,10-phenanthroline (PHEN) cocatalyst. Coordination of PHEN with active Zinc center enhanced the nucleophilic ability of the metal carbonate, which became more regio-specific in attacking carbon in PO, leading to PPC with improved H-T linkages.
Resumo:
Cobalt porphyrin complex ((TPPCoX)-X-III) (TPP = 5, 10, 15, 20-Tetraphenylporphyrin; X = halide) in combination with ionic organic ammonium salt was used for the regio-specific copolymerization of propylene oxide and carbon dioxide. A turnover frequency of 188 h(-1) was achieved after 5 h, and the byproduct propylene carbonate was successfully controlled to below 1%, where the obtained poly(propylene carbonate) (PPC) showed number average molecular weight (M-n) of 48 kg/mol, head-to-tail content of 93%, and carbonate linkage of over 99%.
Resumo:
The reversible addition-fragmentation chain transfer (RAFT) polymerization of acrylonitrile (AN) mediated by 2-cyanoprop-2-yl dithiobenzoate was first applied to synthesize polyacrylonitrile (PAN) with a high molecular weight up to 32,800 and a polydispersity index as low as 1.29. The key to success was ascribed to the optimization of the experimental conditions to increase the fragmentation reaction efficiency of the intermediate radical. In accordance with the atom transfer radical polymerization of AN, ethylene carbonate was also a better solvent candidate for providing higher controlled/living RAFT polymerization behaviors than dimethylformamide and dimethyl sulfoxide. The various experimental parameters, including the temperature, the molar ratio of dithiobenzoate to the initiator, the molar ratio of the monomer to dithiobenzoate, the monomer concentration, and the addition of the comonomer, were varied to improve the control of the molecular weight and polydispersity index. The molecular weights of PANS were validated by gel permeation chromatography along with a universal calibration procedure and intrinsic viscosity measurements. H-1 NMR analysis confirmed the high chain-end functionality of the resultant polymers.
Resumo:
Poly(ethylene glycol) (PEG) networks were synthesized by gamma-irradiation. The crystalline behavior of PEG was investigated by differential scanning calorimetry (DSC) and wide-angle X-ray diffraction (WAXD). It was shown that the crystallinity of PEG is dramatically lower in the cross-linked, networks than in pure PEG. When the molecular weight of PEG in the networks decreased to 1000, it could not crystallize at all. Moreover, we also found that the melting temperature of PEG is greatly affected by the presence of a cross-linked network.
Resumo:
Surface morphology of polystyrene (PS) films on different substrates by spin-coating before and after annealing was observed using atomic force microscopy (AFM). The effects of polymer molecular weight, substrates, solvents, and annealing conditions on the morphology of the films were investigated. Before annealing, the grain height decreases, and simultaneously the grain diameter increases with molecular weight (M-w) within the measured molecular weight. After annealing. the situation is opposite, i.e., the grain height increases while the grain diameter decreases with M-w. Furthermore, after annealing the smaller surface roughness (Ra) was obtained. It was also found that film surface roughness (Ra) depends on the vapor pressure and dipole moment of different used solvents as well as the substrates. The experimental results show that when the used solvents have similar dipole moment but different vapor pressure, the Ra of PS film decreased with the decreasing vapor pressure of solvents whether on silicon or on mica. And when the used solvents have close vapor pressure but different dipole moment, the Ra decreased with the increasing of solvent dipole moments on both substrates.
Microwave-assisted synthesis of high-molecular-weight poly(ether imide)s by phase-transfer catalysis
Resumo:
A facile and rapid polycondensation reaction of disodium bisphenol A with bis(chlorophthalimide)s was preformed with a domestic microwave oven in o-dichlorobenzene by phase-transfer catalysis. The polymerization reactions, in comparison with conventional heating polycondensation, proceeded rapidly and were completed within 25 min. The polymerizations gave the corresponding poly(ether imide)s with inherent viscosities of 0.55-0.92 dL g(-1). The effects of various factors on the polymerization, such as the amount of the catalyst, the reaction time, and the microwave power were studied. The properties of the polymers were briefly characterized.