110 resultados para CdS
Resumo:
报道了单光束、双光束和三光束飞秒激光在CdS,GaN,SiC样品上诱导形成周期远小于激光波长的纳米周期结构.研究表明,其形成机制不同于入射光与表面散射光干涉的经典机制,二次谐波的产生可能在其中起着重要作用;双光束激光干涉在SiC晶体表面诱导形成二维微米-纳米复合周期结构,干涉花样决定微米长周期结构,长周期结构的烧蚀斑上形成了短周期的自组织纳米结构.在上述研究基础上,初步探索三光束干涉形成二维、三维微米-纳米复合周期结构.
Resumo:
We report an organic/inorganic polymer composite based on the chemically hybridized photoconductor CdS-PVK nanocomposite doped with a new second-order optically nonlinear chromophore 1-n-butoxy-2-methyl-(4-p-nitrophenylazo)benzene (BMNPAB) and plasticizer 9-ethyl-carbazole (ECZ) to manifest a photorefractive (PR) effect. A detailed description of the synthesis and characterization of BMNPAB is presented. The poled film including PVK-10-CdS nanocomposite and BMNPAB exhibits a high second harmonic generation (SHG) coefficient of 31 pm/V The photoconductivity of PVK-CdS nanocomposite also was studied here. Two-beam coupling experiment clearly indicated an asymmetric optical energy exchange between two beams on the polymer composite at zero electrical field, and the two-beam coupling gain of 50.0 cm(-1) and diffraction efficiencv of 4.2% were obtained at 647.1 nm wavelength. (C) 2007 Elsevier Ltd. All rights reserved.
Resumo:
A novel multifunctional inorganic-organic photorefractive (PR) poly(N-vinyl)-3-[p-nitrophenylazolcarbazolyl-CdS nanocomposites with different molar ratios of US to poly(N-vinyl)-3-[p-nitrophenylazo]carbazolyl (PVNPAK) were synthesized via a postazo-coupling reaction and chemically hybridized approach, respectively. The nanocomposites are highly soluble and could be obtained as film-forming materials with appreciably high molecular weights and low glass transition temperature (T,) due to the flexible spacers. The PVNPAK matrix possesses a highest-occupied molecular orbital value of about -5.36 eV determined from cyclic voltammetry. Second harmonic generation (SHG) could be observed in PVNPAK film without any poling procedure and 4.7 pm/V of effective second-order nonlinear optical susceptibility is obtained. The US particles as photosensitizers had a nanoscale size in PVNPAK adopting transmission electron microscopy. The improvement of interface quality between US and polymer matrix is responsible for efficient photoinduced charge generation efficiency in the nanocomposites. An asymmetric optical energy exchange between two beams on the polymer composites PVNPAK-CdS/ECZ has been found even without an external field in two-beam coupling (TBC) experiment, and the TBC gain and diffraction efficiency of 14.26 cm(-1) and 3.4% for PVNPAK-5-CdS/ECZ, 16.43 cm(-1) and 4.4% for PVNPAK-15-CdS/ECZ were measured at a 647.1 nm wavelength, respectively.
Resumo:
鲤科鱼类在东亚的物种多样,分布广泛,物种特征尺寸差异明显,弄清其功能基因的系统演变,对于理解物种分化和功能进化具有重要意义.以具有重要生长调控作用的c-myc基因为标记,通过PCR扩增、克隆和测序,共获得41种鲤科鱼类和外类群c-myc基因全序列,发现并分析了c-myc编码区的两个高变异区.基于c-myc CDS序列,分别采用最大简约法(MP)、最大似然法(ML)和Bayesian法重建了鲤科鱼类的系统发育关系.3种方法所得系统发育关系较为相似.当以亚口鱼科的胭脂鱼(Myxocyprinus asiati
Resumo:
The electronic structure, Zeeman splitting, and g factor of Mn-doped CdS nanowires are studied using the k center dot p method and the mean field model. It is found that the Zeeman splittings of the hole ground states can be highly anisotropic, and so can their g factors. The hole ground states vary a lot with the radius. For thin wire, g(z) (g factor when B is along the z direction or the wire direction) is a little smaller than g(x). For thick wire, g(z) is mcuh larger than g(x) at small magnetic field, and the anisotropic factor g(z)/g(x) decreases as B increases. A small transverse electric field can change the Zeeman splitting dramatically, so tune the g(x) from nearly 0 to 70, in thick wire. The anisotropic factor decreases rapidly as the electric field increases. On the other hand, the Zeeman splittings of the electron ground states are always isotropic.
Resumo:
High quality n-type CdS nanobelts (NBs) were synthesized via an in situ indium doping chemical vapor deposition method and fabricated into field effect transistors (FETs). The electron concentrations and mobilities of these CdS NBs are around (1.0x10(16)-3.0x10(17))/cm(3) and 100-350 cm(2)/V s, respectively. An on-off ratio greater than 10(8) and a subthreshold swing as small as 65 mV/decade are obtained at room temperature, which give the best performance of CdS nanowire/nanobelt FETs reported so far. n-type CdS NB/p(+)-Si heterojunction light emitting diodes were fabricated. Their electroluminescence spectra are dominated by an intense sharp band-edge emission and free from deep-level defect emissions. (c) 2006 American Institute of Physics.
Resumo:
Zeolite Y has been used as the host to generate CdS nanoclusters. The location of CdS nanoclusters inside zeolite hosts was confirmed by the blue-shifted reflection absorption spectra with respect to that of bulk CdS materials. But which kind of cage inside zeolite Y, sodalite cage or supercage, was preferred for the CdS clusters remained unclear. In this paper, we conducted positron annihilation spectroscopy (PAS) measurements for the first time on a series of CdS/Y zeolite samples and concluded that CdS clusters were not located in supercages but in smaller sodalite cages. The stability of CdS clusters inside the sodalite units was due to the coordination of Cd atoms with the framework oxygen atoms of the double six-ring windows. Moreover, PAS revealed some important information of surface states existing on the interfacial layers between CdS clusters and zeolite Y. (C) 2001 Elsevier Science B,V, All rights reserved.
Resumo:
We have studied the hole levels and exciton states in CdS nanocrystals by using the hole effective-mass Hamiltonian for wurtzite structure. It is found that the optically passive P-x state will become the ground hole state for small CdS quantum dots of radius less than 69 Angstrom. It suggests that the "dark exciton" would be more easily observed in the CdS quantum dots than that in CdSe quantum dots. The size dependence of the resonant Stokes shift is predicted for CdS quantum dots. Including the Coulomb interaction, exciton energies as functions of the dot radius are calculated and compared with experimental data.
Resumo:
Manganese doped CdS nanoparticles were synthesized in basic aqueous solution by using mercapto acetate as capping reagents. The nanoparticles were characterized by HRTEM, EPR, photoluminescence and optical absorption measurements. Out of our expectation, doping of Mn2+ ions altered the recombination paths in CdS nanoparticles markedly. The surface stares facilitated PL from Mn2+ doped CdS nanoparticles is reported. A complete suppression of the emission from surface states at room temperature when doping with Mn2+ ions has been observed for the first time. (C) 2000 Elsevier Science Ltd. All rights reserved.
Resumo:
CdSe nanoclusters overcoated with CdS shell were prepared with macapoacetic acid as stabilizer. The optical properties of CdSe nanoclusters and the influence of CdS shell on the electronic structures of CdSe cores were studied by optical absorption, photoluminescence (PL) and photoluminescence excitation (PLE) spectroscopies. Based on PL and PLE results and the theoretical calculation on fine structure of bandedge exciton, a model of formation of excimer within the small clusters was proposed to explain the large Stokes shift of luminescence from absorption edge observed in PL results. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
CdS/ZnS core/shell nanocrystals were prepared from an aqueous/alcohol medium. A red shift of the absorption spectrum and an increase of the room temperature photoluminescence intensity accompanied shell growth.
Resumo:
CdS nanoparticies were prepared in air and their stability by air annealing was studied. A small change in crystal structure and particle size was observed by air annealing, but a rapid reduction in fluorescence was found. Through investigation, it is revealed that it is the surface change or reconstruction rather than the variation of the size or structure that decreases the fluorescence. The emission of the particles consists with two peaks which are dependent on the excitation energy. The two peaks are considered to be arisen from "two" different sizes of nanoparticles and may be explained in terms of selectively excited photoluminescence. Finally we discuss why the discrete state of nanoparticles are able to be resolved in the photoluminescence excitation spectrum, but could not be differentiated in the absorption spectrum.
Resumo:
CdS clusters are formed in the pores of a mesoporous zeolite in which the size of the clusters may be adjusted. The size of the clusters increases as the CdS loading is increased. X-ray diffraction investigation shows that the lattice constants of the clusters contract upon increasing size. This contraction is attributed to an increase of the static pressure exercised by the zeolite framework as the clusters grow bigger. Both the excitonic and trapped emission bands are detected and become more intensive upon decreasing size. Three absorption bands appear in the photoluminescence excitation (PLE) spectra and they shift to the blue as cluster size decreases. Based on the effective-mass approximation, the three bands are assigned to the 1S-1S, 1S-1P and 1S-1D transitions, respectively. The size-dependence of the PLE spectra can also be explained. (C) 1997 Elsevier Science Ltd.
Resumo:
We reported the synthesis of CdS semiconductor nanoparticles using a simple one-pot reaction by thermolysis of cadmium acetylacetonate in dodecanethiol. Optical measurements of the as-obtained CdS nanoparticles revealed that their optical properties were closely related to surface effects. Based upon the cocktail of poly (N-vinylcarbazole) (PVK) and CdS nanoparticles, a bistable device was fabricated by a simple solution processing technique. Such a device exhibited a remarkable electrical bistability, which was attributed to the electric field-assisted charge transfer between PVK and the CdS nanoparticles capped by dodecaethiol. The conduction mechanism changed from an injection-controlled current to a bulk-controlled one during switching from OFF-state to ON-state.