We report a detailed study of surface-bound chemical vapor deposition of carbon nanotubes and nanofibers from evaporated transition metal catalysts exposed to ammonia diluted acetylene. We show that a reduction of the Fe/Co catalyst film thickness below 3 nm results into a transition from large diameter (> 40 nm), bamboo-like nanofibers to small diameter (similar to 5 nm) multi-walled carbon nanotubes. The nanostructuring of ultrathin catalyst films critically depends on the gas atmosphere, with the resulting island distribution initiating the carbon nucleation. Compared to purely thermal chemical vapor deposition, we find that, for small diameter nanotube growth, DC plasma assistance is detrimental to graphitization and sample homogeneity and cannot prevent an early catalyst poisoning. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Lattice-resolved, video-rate environmental transmission electron microscopy shows the formation of a liquid Au-Ge layer on sub-30-nm Au catalyst crystals and the transition of this two-phase Au-Ge/Au coexistence to a completely liquid Au-Ge droplet during isothermal digermane exposure at temperatures far below the bulk Au-Ge eutectic temperature. Upon Ge crystal nucleation and subsequent Ge nanowire growth, the catalyst either recrystallizes or remains liquid, apparently stabilized by the Ge supersaturation. We argue that there is a large energy barrier to nucleate diamond-cubic Ge, but not to nucleate the Au-Ge liquid. As a result, the system follows the more kinetically accessible path, forming a liquid even at 240 degrees C, although there is no liquid along the most thermodynamically favorable path below 360 degrees C.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper we demonstrate how secondary ion mass spectrometry (SIMS) can be applied to ZnO nanowire structures for gold catalyst residue determination. Gold plays a significant role in determining the structural properties of such nanowires, with the location of the gold after growth being a strong indicator of the growth mechanism. For the material investigated here, we find that the gold remains at the substrate-nanowire interface. This was not anticipated as the usual growth mechanism associated with catalyst growth is of a vapour-liquid-solid (VLS) type. The results presented here favour a vapour-solid (VS) growth mechanism instead. Copyright © 2007 John Wiley & Sons, Ltd.