240 resultados para VELOCITY DISPERSION
em Cambridge University Engineering Department Publications Database
Resumo:
The conventional technology for generating ultrashort pulses relies on soliton-like operation based mode-locking. In this regime, the pulse duration is limited by nonlinear optical effects[1]. One method to mitigate these effects is to alternate segments of normal and anomalous group velocity dispersion (GVD) fiber[1]. This configuration is known as dispersion-managed soliton design. It decreases the nonlinear optical effects and reduces the pulse duration[1]. © 2011 IEEE.
Resumo:
We develop two new amphiphilic molecules that are shown to act as efficient surfactants for carbon nanotubes in nonpolar organic solvents. The active conjugated groups, which are highly attracted to the graphene nanotube surface, are based on pyrene and porphyrin. We show that relatively short (C18) carbon tails are insufficient to provide stabilization. As our ultimate aim is to disperse and stabilize nanotubes in siloxane matrix (polymer and cross-linked elastomer), both surfactant molecules were made with long siloxane tails to facilitate solubility and steric stabilization. We show that the pyrene-siloxane surfactant is very effective in dispersing multiwall nanotubes, while the porphyrin-siloxane makes single-wall nanotubes soluble, both in petroleum ether and in siloxane matrix.
Resumo:
Surface coatings and treatments have been used to reduce material loss of components in bubbling fluidized bed combustors (FBCs). The performance of protective coatings in FBC boilers and laboratory simulations is reviewed. Important coating properties to minimize wastage appear to be high hardness, low oxidation rate, low porosity, high adhesion and sufficient thickness to maintain protection for a long period. Economic considerations and criteria for choosing a suitable coating or treatment are discussed for the different types of bubbling FBC. © 1995.
Resumo:
We report on rheological properties of a dispersion of multiwalled carbon nanotubes in a viscous polymer matrix. Particular attention is paid to the process of nanotubes mixing and dispersion, which we monitor by the rheological signature of the composite. The response of the composite as a function of the dispersion mixing time and conditions indicates that a critical mixing time t* needs to be exceeded to achieve satisfactory dispersion of aggregates, this time being a function of nanotube concentration and the mixing shear stress. At shorter times of shear mixing t< t*, we find a number of nonequilibrium features characteristic of colloidal glass and jamming of clusters. A thoroughly dispersed nanocomposite, at t> t*, has several universal rheological features; at nanotube concentration above a characteristic value nc ∼2-3 wt. % the effective elastic gel network is formed, while the low-concentration composite remains a viscous liquid. We use this rheological approach to determine the effects of aging and reaggregation. © 2006 The American Physical Society.
Resumo:
Transport measurements were performed on individual PECVD grown MWCNT nanobridge structures. Temperature dependent conductance measurements show that as the temperature is decreased, the conductance also decreases. The nanotubes were able to carry high current densities with the observed maximum at ∼108 A/cm2. High volatile measurements reveal that the PECVD grown MWCNTs break down in segments of nanotube shells.
Resumo:
Poly-methylmethacrylate suspended dispersion was used to fabricate multiwalled carbon nanotube (MWCNT) bridges. Using this technique, nanotubes could be suspended between metal electrodes without any chemical etching of the substrate. The electrical measurement on suspended MWCNT bridges shows that the room temperature resistance ranges from under a kω to a few Mω.
Resumo:
We report on the electrical characteristics of plasma enhanced chemical vapour deposition (PECVD)-grown, multi-walled carbon nanotube (MWCNT) devices made by a new fabrication method, PMMA suspended dispersion. This method makes it possible to suspend nanotubes between metal electrodes and to remove unwanted nanotubes from the substrate. The measurements show that the MWCNTs are metallic and able to maintain a current density ∼2×106 A/cm2 for more than 15 days with a maximum current density of ∼1.8×107 A/cm2. This high current density and reliability will make PECVD-grown MWCNTs applicable to field emission cathodes. © 2002 Elsevier Science B.V. All rights reserved.
Resumo:
Theoretical predictions of the diameters of continuous ink-jets downstream of long nozzles are generalized to include the important cases of ink-jet fluids and shorter nozzles where the velocity profile at the nozzle exit is undeveloped (non-parabolic). Comparisons of the new predictions with experiments and simulations are made for fairly long nozzles with tapered profiles and short nozzles with conical profiles; experimental and simulated profiles are also compared downstream of the nozzle exit for both industrial and large scale ink-jet print heads. Precise measurements of the un-modulated jet diameters downstream of the nozzle exit can set really useful limits to the possible shapes of the flow profile right at the nozzle exit, and in particular allow some assessment of the axial velocity gradients and fluid shear rates at the nozzle exit where direct speed measurement is usually impractical. Simulations allow further study of the relaxation of the velocity profile downstream of the nozzle exit, and are reported for both un-modulated and modulated CIJ jetting. Implications of this work include speeding up CIJ simulations, absolute calibration of the applied CIJ system modulation, and the likely magnitude of dynamic surface tension effects on observed CIJ satellite speeds.