8 resultados para Side Vehicle-to-Vehicle Impact Tests.
em Cambridge University Engineering Department Publications Database
Resumo:
We have fabricated self-aligned, side-gated suspended multi-walled carbon nanotubes (MWCNTs), with nanotube-to-gate spacing of less than 10 nm. Evaporated metal forms an island on a suspended MWCNT, the island and the nanotube act as a mask shielding the substrate, and lift-off then removes the metal island, leaving a set of self-aligned side gates. Al, Cr, Au, and Ti were investigated and the best results were obtained with Cr, at a yield of over 90%.
Resumo:
The quasi-static and dynamic responses of laminated beams of equal areal mass, made from monolithic CFRP and Ultra high molecular weight Polyethylene (UHMWPE), have been measured. The end-clamped beams were impacted at mid-span by metal foam projectiles to simulate localised blast loading. The effect of clamping geometry on the response was investigated by comparing the response of beams bolted into the supports with the response of beams whose ends were wrapped around the supports. The effect of laminate shear strength upon the static and dynamic responses was investigated by testing two grades of each of the CFRP and UHMWPE beams: (i) CFRP beams with a cured matrix and uncured matrix, and (ii) UHMWPE laminates with matrices of two different shear strengths. Quasi-static stretch-bend tests indicated that the load carrying capacity of the UHWMPE beams exceeds that of the CFRP beams, increases with diminishing shear strength of matrix, and increases when the ends are wrapped rather than through-bolted. The dynamic deformation mode of the beams is qualitatively different from that observed in the quasi-static stretch-bend tests. In the dynamic case, travelling hinges emanate from the impact location and propagate towards the supports; the beams finally fail by tensile fibre fracture at the supports. The UHMWPE beams outperform the CFRP beams in terms of a lower mid-span deflection for a given impulse, and a higher failure impulse. Also, the maximum attainable impulse increases with decreasing shear strength for both the UHMWPE and CFRP beams. The ranking of the beams for load carrying capacity in the quasi-static stretch-bend tests is identical to that for failure impulse in the impact tests. Thus, the static tests can be used to gauge the relative dynamic performances of the beams. © 2013 Elsevier Ltd. All rights reserved.
Resumo:
The dynamic response of end-clamped sandwich and monolithic beams of equal areal mass subjected to loading via high-velocity slugs of dry and water-saturated sand is measured using a novel laboratory-based method. The sandwich beams comprise aluminium face sheets and an aluminium honeycomb core: the effect of sandwich core strength and beam thickness on the dynamic beam deflection is investigated by varying the orientation and height of the anisotropic aluminium honeycomb core material. High-speed imaging is used to measure the transient transverse deflection of the beams and to record the dynamic modes of deformation. The measurements show that sandwich beams with thick, strong cores are optimal and that these beams significantly outperform monolithic beams of equal mass. The water-saturated sand slugs cause significantly higher deflections compared to the dry sand slugs having the same mean slug velocity and we demonstrate that this enhanced deflection is due to the larger mass of the water-saturated slugs. Finally, we show that the impact of sand slugs is equivalent to the impact of a crushable foam projectile. The experiments using foam projectiles are significantly simpler to perform and thus represent a more convenient laboratory technique. © 2014 Elsevier Ltd. All rights reserved.
Resumo:
This study detailed the structure of turbulence in the air-side and water-side boundary layers in wind-induced surface waves. Inside the air boundary layer, the kurtosis is always greater than 3 (the value for normal distribution) for both horizontal and vertical velocity fluctuations. The skewness for the horizontal velocity is negative, but the skewness for the vertical velocity is always positive. On the water side, the kurtosis is always greater than 3, and the skewness is slightly negative for the horizontal velocity and slightly positive for the vertical velocity. The statistics of the angle between the instantaneous vertical fluctuation and the instantaneous horizontal velocity in the air is similar to those obtained over solid walls. Measurements in water show a large variance, and the peak is biased towards negative angles. In the quadrant analysis, the contribution of quadrants Q2 and Q4 is dominant on both the air side and the water side. The non-dimensional relative contributions and the concentration match fairly well near the interface. Sweeps in the air side (belonging to quadrant Q4) act directly on the interface and exert pressure fluctuations, which, in addition to the tangential stress and form drag, lead to the growth of the waves. The water drops detached from the crest and accelerated by the wind can play a major role in transferring momentum and in enhancing the turbulence level in the water side.On the air side, the Reynolds stress tensor's principal axes are not collinear with the strain rate tensor, and show an angle α σ≈=-20°to-25°. On the water side, the angle is α σ≈=-40°to-45°. The ratio between the maximum and the minimum principal stresses is σ a/σ b=3to4 on the air side, and σ a/σ b=1.5to3 on the water side. In this respect, the air-side flow behaves like a classical boundary layer on a solid wall, while the water-side flow resembles a wake. The frequency of bursting on the water side increases significantly along the flow, which can be attributed to micro-breaking effects - expected to be more frequent at larger fetches. © 2012 Elsevier B.V.
Resumo:
The ballistic performance of equi-mass plates made from (i) stainless steel (SS); (ii) carbon fibre/epoxy (CF) laminate and (iii) a hybrid plate of both materials has been characterised for a spherical steel projectile. The hybrid plate was orientated with steel on the impact face (SSCF) and on the distal face (CFSS). The penetration velocity (V 50) was highest for the SS plate and lowest for the CF plate. A series of double impact tests were performed, with an initial velocity V I and a subsequent velocity V II at the same impact site. An interaction diagram in (V I,V II) space was constructed to delineate penetration from survival under both impacts. The degree of interaction between the two impact events was greater for the CFSS plate than for the SSCF plate, implying that the distal face has the major effect upon the degree of interaction.
Resumo:
As operational impacts from buildings are reduced, embodied impacts are increasing. However, the latter are seldom calculated in the UK; when they are, they tend to be calculated after the building has been constructed, or are underestimated by considering only the initial materials stage. In 2010, the UK Government recommended that a standard methodology for calculating embodied impacts of buildings be developed for early stage design decisions. This was followed in 2011-12 by the publication of the European TC350 standards defining the 'cradle to grave' impact of buildings and products through a process Life Cycle Analysis. This paper describes a new whole life embodied carbon and energy of buildings (ECEB) tool, designed as a usable empirical-based approach for early stage design decisions for UK buildings. The tool complies where possible with the TC350 standards. Initial results for a simple masonry construction dwelling are given in terms of the percentage contribution of each life cycle stage. The main difficulty in obtaining these results is found to be the lack of data, and the paper suggests that the construction and manufacturing industries now have a responsibility to develop new data in order to support this task. © 2013 The Authors. Published by Elsevier B.V. All rights reserved.