Resumo:

The Schottky barrier heights of various metals on the high permitivity oxides tantalum pentoxide, barium strontium titanate, lead zirconate titanate, and strontium bismuth tantalate have been calculated as a function of the metal work function. It is found that these oxides have a dimensionless Schottky barrier pinning factor S of 0.28-0.4 and not close to 1 because S is controlled by Ti-O-type bonds not Sr-O-type bonds, as assumed in earlier work. The band offsets on silicon are asymmetric with a much smaller offset at the conduction band, so that Ta2O5 and barium strontium titanate are relatively poor barriers to electrons on Si. © 1999 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Schottky barrier heights of various metals on tantalum pentoxide, barium strontium titanate, lead zirconate-titanate and strontium bismuth tantalate have been calculated as a function of metal work function. These oxides have a dimensionless Schottky barrier pinning factor, S, of 0.28 - 0.4 and not close to 1, because S is controlled by the Ti-O type bonds not Sr-O type bonds, as assumed previously. Band offsets on silicon are asymmetric with much smaller offset at the conduction band, so that Ta2O5 and barium strontium titanate (BST) are relatively poor barriers to electrons on Si.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Thickness of the near-interface regions (NIR) and central bulk ohmic resistivity in lead lanthanum zirconate titanate ferroelectric thin films were investigated. A method to separate the low-resistive near-interface regions (NIRs) from the high-resistive central bulk region (CBR) in ferroelectric thin films was presented. Results showed that the thickness of the NIRs depended on the electrode materials in use and the CBR resistivity depended on the impurity doping levels.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Capacitance-voltage (C-V) characteristics of lead zirconate titanate (PZT) thin films with a thickness of 130 nm were measured between 300 and 533 K. The transition between ferroelectric and paraelectric phases was revealed to be of second order in our case, with a Curie temperature at around 450 K. A linear relationship was found between the measured capacitance and the inverse square root of the applied voltage. It was shown that such a relationship could be fitted well by a universal expression of C/A = k(V+V(0))(-1/2) and that this expression could be derived by expanding the Landau-Devonshire free energy at an effective equilibrium position of the Ti/Zr ion in a PZT unit cell. By using the derived equations in this work, the free energy parameters for an individual material can be obtained solely from the corresponding C-V data, and the temperature dependences of both remnant polarization and coercive voltage are shown to be in quantitative agreement with the experimental data.