Resumo:

Nano-sized TiNi powder with an average size of 50nm was consolidated using spark plasma sintering (SPS) at 800 °C for 5min. A layer of anatase TiO 2 coating was formed on the sintered TiNi by chemical reaction with a hydrogen peroxide (H2O2) solution at 60 °C followed by heat treatment at 400 °C to enhance the bioactivity of the metal surface. Cell culture using osteoblast cells and a biomimetic test in simulated body fluid proved the biocompatibility of the chemically treated SPS TiNi. © IOP Publishing Ltd.

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Unbiased location- and scale-invariant `elemental' estimators for the GPD tail parameter are constructed. Each involves three log-spacings. The estimators are unbiased for finite sample sizes, even as small as N=3. It is shown that the elementals form a complete basis for unbiased location- and scale-invariant estimators constructed from linear combinations of log-spacings. Preliminary numerical evidence is presented which suggests that elemental combinations can be constructed which are consistent estimators of the tail parameter for samples drawn from the pure GPD family.