30 resultados para BRANCHED POLYETHYLENE
em Cambridge University Engineering Department Publications Database
Resumo:
In this paper, we present the analysis of electroosmotic flow in a branched -turn nanofluidic device, which we developed for detection and sorting of single molecules. The device, where the channel depth is only 150 nm, is designed to optically detect fluorescence from a volume as small as 270 attolitres (al) with a common wide-field fluorescent setup. We use distilled water as the liquid, in which we dilute 110 nm fluorescent beads employed as tracer-particles. Quantitative imaging is used to characterize the pathlines and velocity distribution of the electroosmotic flow in the device. Due to the device's complex geometry, the electroosmotic flow cannot be solved analytically. Therefore we use numerical flow simulation to model our device. Our results show that the deviation between measured and simulated data can be explained by the measured Brownian motion of the tracer-particles, which was not incorporated in the simulation.
Resumo:
The quasi-static and dynamic behaviour of Linear Low Density Polyethylene (LLDPE) and two LLDPE nanocomposites were studied. Nanocomposites consisting of LLDPE filled with 1% carbon black and 0.5% nanoclay fillers, by weight, were considered. Under quasi-static tensile loading, an improvement in the energy absorbing capability was achieved by adding 1% carbon black fillers. However, during quasi-static puncture and dynamic impact loading, the advantage provided by the fillers was lost. Thermal softening due to adiabatic heating under high strain rate deformation and difference s in the state of stress are considered as reasons for this reduction. © 2011 Published by Elsevier Ltd.
Resumo:
The effect of strain rate upon the uniaxial response of Ultra High Molecular-weight Polyethylene (UHMWPE) fibres, yarns and laminates of lay-up [0/90]48 has been measured in both the 0/90 and ±45 configurations. The tensile strength of the matrix-dominated ±45 laminate is two orders of magnitude less than that of the fibre-dominated 0/90 laminate, and is more sensitive to strain rate. A piezoelectric force sensor device was developed to obtain the high strain rate data, and this achieved a rise time of less than 1 μs. It is found that the failure strength (and failure strain) of the yarn is almost insensitive to strain rate within the range (10 -1-103 s-1). At low strain rates (below 10 -1 s-1), creep of the yarn dominates and the failure strain increases with diminishing strain rate. The tensile strength of the dry yarn exceeds that of the laminate by about 20%. Tests on single fibres exceed the strength of the yarn by 20%. © 2013 Elsevier Ltd. All rights reserved.
Resumo:
Hot-pressed laminates with a [0/90]48 lay-up, consisting of 83% by volume of ultra high molecular-weight polyethylene (UHMWPE) fibres, and 17% by volume of polyurethane (PU) matrix, were cut into cantilever beams and subjected to transverse end-loading. The collapse mechanisms were observed both visually and by X-ray scans. Short beams deform elastically and collapse plastically in longitudinal shear, with a shear strength comparable to that observed in double notch, interlaminar shear tests. In contrast, long cantilever beams deform in bending and collapse via a plastic hinge at the built-in end of the beam. The plastic hinge is formed by two wedge-shaped microbuckle zones that grow in size and in intensity with increasing hinge rotation. This new mode of microbuckling under macroscopic bending involves both elastic bending and shearing of the plies, and plastic shear of the interface between each ply. The double-wedge pattern contrasts with the more usual parallel-sided plastic microbuckle that occurs in uniaxial compression. Finite element simulations and analytical models give additional insight into the dominant material and geometric parameters that dictate the collapse response of the UHMWPE composite beam in bending. Detailed comparisons between the observed and predicted collapse responses are used in order to construct a constitutive model for laminated UHMWPE composites. © 2013 Elsevier Ltd.
Resumo:
The objective of this study was to compare the life-cycle environmental impacts of changed production structures for two consumer goods (high-density polyethylene (HDPE) shopping bags and beds) in Jamaica. A scenario technique was used to construct three alternative production structures for each product; each scenario reflecting an increase in local production in Jamaica which depended on an increased supply of input materials which may be sourced: (1) externally from overseas suppliers, (2) from post-consumer recycling, and (3) locally on the island of Jamaica. These three constructed scenarios were then compared to the existing supply chain or reference scenarios of the products. The results showed that for both case products the recycling scenario was most preferable for localising production, resulting in the lowest environmental impact. This was because the production of raw materials accounted for the largest effect on total environmental impact. As such, the most immediate environmental improvements were realised by lowering the production of virgin materials. © 2007 Elsevier Ltd. All rights reserved.