Displacement estimation is a key step in the evaluation of tissue elasticity by quasistatic strain imaging. An efficient approach may incorporate a tracking strategy whereby each estimate is initially obtained from its neighbours' displacements and then refined through a localized search. This increases the accuracy and reduces the computational expense compared with exhaustive search. However, simple tracking strategies fail when the target displacement map exhibits complex structure. For example, there may be discontinuities and regions of indeterminate displacement caused by decorrelation between the pre- and post-deformation radio frequency (RF) echo signals. This paper introduces a novel displacement tracking algorithm, with a search strategy guided by a data quality indicator. Comparisons with existing methods show that the proposed algorithm is more robust when the displacement distribution is challenging.
Resumo:
An 80 GSPS photonic ADC system is demonstrated, using broadband MLL and dispersive fibre to form a continuous waveform with time-wavelength mapping, and AWG to channelise. Tests are carried out for RF signals up to 10GHz. © 2005 Optical Society of America.
Resumo:
The addition of silicon to hydrogenated amorphous carbon can have the advantageous effect of lowering the compressive stress, improving the thermal stability of its hydrogen and maintaining a low friction coefficient up to high humidity. Most experiments to date have been on a-C1-xSix:H alloys deposited by RF plasma enhanced chemical vapour deposition (PECVD). This method gives alloys with considerable hydrogen content and only moderate hardness. Here, we use a high plasma density source, the electron cyclotron wave resonance (ECWR) source, to prepare films with a high deposition rate. The composition and bonding in the alloys is determined by XPS, visible and UV Raman and FTIR spectroscopy. We find that it is possible to produce hard, low stress, low friction, almost humidity insensitive a-C1-xSix:H alloys with a good optical transparency and a band gap over 2 eV.
Resumo:
The addition of silicon to hydrogenated amorphous carbon can have the advantageous effect of lowering the compressive stress, improving the thermal stability of its hydrogen, and maintaining a low friction coefficient up to high humidity. Most experiments to date have been on hydrogenated amorphous carbon-silicon alloys (a-C1-xSix:H) deposited by rf plasma enhanced chemical vapor deposition. This method gives alloys with sizeable hydrogen content and only moderate hardness. Here we use a high plasma density source known as the electron cyclotron wave resonance source to prepare films with higher sp3 content and lower hydrogen content. The composition and bonding in the alloys is determined by x-ray photoelectron spectroscopy, Rutherford backscattering, elastic recoil detection analysis, visible and ultraviolet (UV) Raman spectroscopy, infrared spectroscopy, and x-ray reflectivity. We find that it is possible to produce relatively hard, low stress, low friction, almost humidity insensitive a-C1-xSix:H alloys with a good optical transparency and a band gap well over 2.5 eV. The friction behavior and friction mechanism of these alloys are studied and compared with that of a-C:H, ta-C:H, and ta-C. We show how UV Raman spectroscopy allows the direct detection of Si-C, Si-Hx, and C-Hx vibrations, not seen in visible Raman spectra. © 2001 American Institute of Physics.
Resumo:
Structural changes induced by the incorporation of nitrogen into ta-C : H films have been studied by Electron Energy Loss Spectroscopy, X-Ray Photoelectron Spectroscopy, Fourier Transformed Infrared Spectroscopy and Ultraviolet-Visible Spectroscopy. ta-C:H films have been synthesised using a low pressure Electron Cyclotron Wave Resonance (ECWR) source which provides a plasma beam with a high degree of ionisation and dissociation. Nitrogen was incorporated by adding N2 to the C2H2 plasma used for the deposition of ta-C : H films. The N/C atomic ratio in the films rises rapidly until the N2/C2H2 gas ratio reaches three, and then increases more gradually, while the deposition rate decreases steeply. Chemical sputtering of the forming films and the formation of molecular nitrogen within the films limit the maximum nitrogen content to about N/C = 0.6. For low nitrogen content the films retain their diamond-like properties, however as N/C atomic ratio increases, a polymeric-like material is formed, with >C=N- structures and terminating C=N and NH groups that decrease the connectivity of the network.
Resumo:
In this study, a micro-pump unit based on surface acoustic wave (SAW) on piezoelectric ZnO film is designed and fabricated as a micro-fluidic device. It employs a mechanical wave, which is generated electrically using an aluminum interdigital transducer (IDT), and propagates on the surface of the ZnO film. The ZnO film was used in this study because it has a high electromechanical coefficient and an excellent bonding with various substrate materials, in particular silicon. The sputtering parameters for ZnO film deposition have been optimized, and the ZnO films with different thickness from 1 micron to 5.5 microns were prepared. The film properties have been characterized using different methods, such as scanning electron microscopy, X-ray diffraction and atomic force microscopy. Aluminum IDT with a finger width and spacing of 8 microns was patterned on the ZnO film using a lift-off process. The frequency generated was measured using a network analyzer, and it varies from 130 MHz to 180 MHz as a function of film thickness. A signal generator was used to generate the frequency with a power amplifier to amplify the signal, which was then applied to aluminum IDT to generate the surface acoustic wave. If a liquid droplet exists on the surface carrying the acoustic wave, the energy and the momentum of the SAW will be coupled into the fluid, causing the liquid to vibrate and move on film surface. The strength of this movement is determined by the applied voltage and frequency. The volume of the liquid drop loaded on the SAW device in this study is of several hundreds of nanoliters. The movement of the liquid inside the droplet and also on the ZnO film surface can be demonstrated. The performance of ZnO SAW device was characterized as a function of film thickness. © 2007 IOP Publishing Ltd.
Resumo:
This paper presents a method for the fast and direct extraction of model parameters for capacitive MEMS resonators from their measured transmission response such as quality factor, resonant frequency, and motional resistance. We show that these parameters may be extracted without having to first de-embed the resonator motional current from the feedthrough. The series and parallel resonances from the measured electrical transmission are used to determine the MEMS resonator circuit parameters. The theoretical basis for the method is elucidated by using both the Nyquist and susceptance frequency response plots, and applicable in the limit where CF > CmQ; commonly the case when characterizing MEMS resonators at RF. The method is then applied to the measured electrical transmission for capacitively transduced MEMS resonators, and compared against parameters obtained using a Lorentzian fit to the measured response. Close agreement between the two methods is reported herein. © 2010 IEEE.
Resumo:
Capacitive parasitic feedthrough is an impediment that is inherent to all electrically interfaced micron scale resonant devices, resulting in increased challenges to their integration in more complex circuits, particularly as devices are scaled to operate at higher frequencies for RF applications. In this paper, a technique to cancel the undesirable effects of capacitive feedthrough that was previously proposed is here developed for an on-chip implementation. The method reported in this paper benefits from the simplicity of its implementation, and its effectiveness is demonstrated in this paper. This technique is demonstrated for two disk-plate resonators that have been excited in the wine glass mode at 5.4 MHz, though applicable to almost any electrically interfaced resonator. Measurements of the electrical transmission from these resonators show that the magnitude of the frequency response of the system is enhanced by up to 19 dB, while the phase is found to shift through a full 180° about the resonant frequency. This method is proposed as a useful addition to other techniques for enhancing the measured response of electrostatic micromechanical resonators. © 2009 Elsevier B.V. All rights reserved.