2 resultados para thermal effects
Resumo:
We report an experimental study on confined systems formed by butyloxybenzylidene octylaniline liquid crystal (4O.8) + gamma-alumina nanoparticles. The effects of the confinement in the thermal and dielectric properties of the liquid crystal under different densities of nanoparticles is analyzed by means of high resolution Modulated Differential Scanning Calorimetry (MDSC) and broadband dielectric spectroscopy. First, a drastic depression of the N-I and SmA-N transition temperatures is observed with confinement, the more concentration of nanoparticles the deeper this depression is, driving the nematic range closer to the room temperature. An interesting experimental law is found for both transition temperatures. Second, the change in shape of the heat capacity peaks is quantified by means of the full width half maximum (FWHM). Third, the confinement does not noticeably affect the molecular dynamics. Finally, the combination of nanoparticles and the external applied electric field tends to favor the alignment of the molecules in metallic cells. All these results indicate that the confinement of liquid crystals by means of gamma-alumina nanoparticles could be optimum for liquid crystal-based electrooptic devices.
Resumo:
The structure, thermal stability, morphology and ion conductivity of titanium perovskites with the general formula Li3xLn2/3−xTiO3 (Ln = rare earth element; 3x= 0.30) are studied in the context of their possible use as solid electrolyte materials for lithium ion batteries. Materials are prepared by a glycine-nitrate method using different sintering treatments, with a cation-disorder-induced structural transition from tetragonal to cubic symmetry, detected as quenching temperature increases. SEM images show that the average grain size increases with increasing sintering temperature and time. Slightly higher bulk conductivity values have been observed for quenched samples sintered at high temperature. Bulk conductivity decreases with the lanthanide ion size. A slight conductivity enhancement, always limited by grain boundaries, is observed for longer sintering times. TDX measurements of the electrolyte/cathode mixtures also show a good stability of the electrolytes in the temperature range of 30-1100ºC.