28 resultados para twist of sawn timber

em Universidad Politécnica de Madrid


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Ultrasonic sound velocity measurements with hand-held equipment remain due to their simplicity among the most used methods for non-destructive grading of sawn woods, yet a dedicated normalization effort with respect to strength classes for Spanish species is still required. As part of an ongoing project with the aim of definition of standard testing methods, the effect of the dimensions of commonly tested Scots pine (Pinus sylvestris L.) timbers and equipment testing frequency on ultrasonic velocity were investigated. A dedicated full-wave finite-difference time-domain software allowed simulation of pulse propagation through timbers of representative length and section combinations. Sound velocity measurements vL were performed along the grain with the indirect method at 22 kHz and 45 kHz for grids of measurement points at specific distances. For sample sections larger than the cross-sectional wavelength ?RT, the simulated sound velocity vL converges to vL = (CL/?)0.5. For smaller square sections the sound velocity drops down to vL = (EL/?)0.5, where CL, EL and ? are the stiffness, E-modul and density, respectively. The experiments confirm a linear regression between time of flight and measurement distance even at less than two wavelength menor que2?L distance, the fitted sound speed values increased by 15% between the two tested frequencies.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Large cross section structural timber have been used in many structures over long periods of time and still make up an important part of the market due to its mechanical properties. Furthermore, it is frequent its employment in new construction site. It involves the need for a visual grading standard for timber used in construction according to the quality assessment. The material has to satisfy the requirements according to the currently regulations. UNE 56544 is the Spanish visual grading standard for coniferous structural timber. The 2007 version defined a new visual grade in the standard for large section termed Structural Large Timber (MEG). This research checks the new visual grading and consists of 116 structural size specimens of sawn coniferous timber of Scotch pine (Pinus sylvestris L.) from Segovia, Spain. The pieces had a cross section of 150 by 200 mm. They were visually graded according to UNE 56544:2007. Also, mechanical properties have been obtained according to standard EN 408. The results show very low output with an excessive percentage of rejected pieces (33%). The main reasons for the rejection of pieces are fissures and twist

Relevância:

100.00% 100.00%

Publicador:

Resumo:

El principal objetivo de este estudio es evaluar la influencia de las fendas de secado en las propiedades mecánicas de vigas de madera. Para esto, se utilizan 40 vigas de Pino silvestre (Pinus sylvestris L) de 4200 mm de longitud y 150x200 mm de sección que fueron ensayadas según norma EN 408. Las fendas se registran detalladamente atendiendo a su longitud y posición en cada cara de la viga, y midiendo el espesor y la profundidad cada 100mm a lo largo de la viga. Solo el 10% de la muestra es rechazada por las fendas, según los criterios establecidos por la norma española de clasificación visual UNE 56544. Para evaluar la influencia de las fendas en las propiedades mecánicas, se usan tres parámetros globales basados en el área, el volumen o la profundad de la fenda, y dos locales basados en la profundidad máxima y la profundidad en la zona de rotura. Además se determina la densidad de las piezas. Estos parámetros se comparan con las propiedades mecánicas (tensión de rotura, módulo de elasticidad y energía de rotura) y se encuentra escasa relación entre ellos. Las mejores correlaciones se encuentran entre los parámetros relacionados con la profundidad de las fendas, tanto con el módulo de elasticidad como con la tensión de rotura. The aim of this study is the evaluation of the influence of drying fissures on the mechanical properties of timber beams. For that purpose, 40 sawn timber pieces of Scots pine (Pinus sylvestris L.) with 150x200 mm in cross-section and 4200 mm in length have been tested according to EN 408, obtaining MOR and MOE. The fissures were registered in detail measuring their length and position in each face of the beam, and the thickness and depth every 100 mm in length. Only 10 % of the pieces were rejected because fissures, according to UNE 56544 Spanish visual grading standard. To evaluate the influence of fissures in mechanical properties three global parameters: Fissures Area Ratio or ratio between the area occupied by fissures and the total area in the neutral axis plane of the beam; Fissures Volume Ratio or ratio between volume of fissures and the total volume of the beam; Fissures Average Depth and two local parameters were used: Fissures Maximum Depth in the beam, and Fissures Depth in the broken zone of the beam. Also the density of the beams was registered. These parameters were compared with mechanical properties (tensile strength, elasticity modulus, and rupture energy) and the relationship between them had not been founded. The best relationship was founded between the elasticity modulus y the tensile strength with the parameters which included the depth of the fissures.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Se han clasificado visualmente, según la norma española UNE 56544; 150 piezas de madera aserrada de pino radiata procedentes de Cataluña (España) con una sección de 80x150 mm y una longitud de 2.500 mm. Esta norma establece dos calidades visuales (ME-1 y ME-2) para piezas con grueso menor o igual que 70 mm y una única calidad visual (MEG) para gruesos mayores de 70 mm. Con el fin de conocer el efecto frontera entre la pequeña y la gran escuadría se clasificaron las piezas según ambas categorías. Se determinó la tensión de rotura en flexión, el módulo de elasticidad en flexión y la densidad de cada pieza mediante el ensayo de acuerdo con la norma UNE-EN 408 siguiendo los ajustes definidos en la norma UNE-EN 384. Un 53 % de las piezas se clasificaron como MEG con una resistencia característica a flexión de 28 N/mm2 y un valor medio del módulo de elasticidad de 9.900 N/mm2. Por otra, un 42 % de las piezas se clasificaron como ME-2 y sólo un 3 % como ME-1; en este caso las propiedades mecánicas de la calidad ME-2 no se alejan mucho de las de la calidad MEG. El elevado porcentaje de piezas rechazadas (47 % frente a la MEG) se debe principalmente al defecto de alabeo responsable de un 39 % de rechazo. Si no se considera el alabeo en la clasificación el porcentaje de rechazo desciende al 17 % y las propiedades mecánicas de la calidad MEG presentan un valor característico de resistencia a flexión de 21 N/mm2 y un módulo de elasticidad de 9.100 N/mm2. A sample of 150 pieces of radiata pine sawn timber with 180x120 mm in cross-section and 2.500 mm in length sourcing from Catalonia (Spain) were visually graded according to Spanish standard UNE 56544. This standard establish two visual grades (ME-1 and ME-2) for timber pieces with thickness equal or less than 70 mm, and one grade (MEG) for thickness bigger than 70 mm. In order to know the border effect between small and larger cross-section the pieces were graded in both categories. The modulus of rupture, modulus of elasticity and density were obtained by test according to EN 408 standard and the adjustments of EN 384. A 53 % of pieces were classified as MEG with a characteristic bending strength of 28 N/mm2 and a mean value of MOE of 9.900 N/mm2. On the other hand, a 42 % of pieces were classified as ME-2 and only a 3 % as ME-1; in this case the mechanical properties of ME-2 are not far from MEG properties. The high percentage of rejected pieces (47 % vs MEG) is mainly due to the twist defect with a 39 % of rejected pieces. If twist is not considered in the grading process the reject percentage decreases to 17 % and the mechanical properties of MEG grade present a characteristic value of bending strength of 21 N/mm2 and a MOE of 9.100 N/mm2.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Good results evaluating material properties using non-destructive testing (NDT) techniques have been achieved for decades. Several studies to understand the influence of temperature and moisture content on NDT have concluded different effects. In this study, NDT parameters were measured on the principal structural Spanish sawn timber species, Scots pine (Pinus sylvestris L.). NDT were conducted on 216 specimens of nominal dimensions 20 by 20 by 400 mm. Specimens were divided into several groups and studied at six different temperatures and four different moisture contents. Commercial equipment and techniques applied were Sylvatest Duo (ultrasonic wave technique), Steinkamp BPV (ultrasonic wave technique), and Grindo Sonic Mk5 "Industrial" (vibration analysis technique). Differences in NDT values within specimens at different temperatures and moisture contents were obtained. Main results of this study and relationships that describe changes in NDT values by effect of temperature and moisture content are presented.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The bonding quality of epoxy glued timber and glass fibre reinforced polymers (GFRP) was evaluated by means of compression loading shear test. Three timber species (Radiata pine, Laricio pine and Oak) and two kinds of GFRP (plates and rods made with polyester resin reinforced with mat and roving glass fibre) were glued and tested using three epoxy formulations. The increase in shear strength with age after the setting of epoxy formulations and the effect of surface roughness on timber and GRP gluing (the planing of the surface of timber and the previous sanding of GRP) were studied. It can be concluded that the mechanical properties of these products make them suitable for use in the reinforcement of deteriorated timber structures, and that a rough timber surface is preferable to a planed one, while the previous sanding of GRP surfaces is not advantageous.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Gran parte del patrimonio construido cuenta con edificios cuya estructura está compuesta por elementos de madera. El volumen económico que supone el mantenimiento y renovación de dicho patrimonio es considerable, por ello, es de especial interés el estudio de las diferentes técnicas de refuerzo aplicables a este tipo de estructuras. Las estructuras de madera han sido tradicionalmente reforzadas con piezas del mismo material, aumentando la sección de los elementos dañados, o con acero. La aparición de los materiales compuestos de polímeros reforzados con fibras, y su progresiva aplicación en obras de construcción, hizo que a principios de la década de los noventa se comenzara a aplicar este material en refuerzos de estructuras de madera (Puente de Sins, 1992). La madera es un material natural con una excelente relación entre sus características mecánicas y su peso. Con el uso de materiales compuestos como refuerzo ésta característica se mantiene. En cuanto a su modelo constitutivo, se admite un comportamiento elástico lineal a tracción paralela a la fibra hasta la rotura, mientras que a compresión, se considera un comportamiento lineal elástico inicial, seguido de un tramo plástico. En vigas de madera aserrada sometidas a flexión predomina el modo de fallo por tracción localizándose la fractura frecuentemente en el canto inferior. Los FRP tienen un comportamiento elástico lineal a tracción hasta la rotura y cuentan con excelentes propiedades mecánicas en relación a su peso y volumen. Si se refuerza la viga por el canto inferior se aumentará su capacidad de absorber tracciones y por tanto, es previsible que se produzca un incremento en la capacidad de carga, así como un aumento de ductilidad. En este trabajo se analizan los beneficios que aportan distintos sistemas de refuerzos de materiales compuestos. El objetivo es contribuir al conocimiento de esta técnica para la recuperación o aumento de las propiedades resistentes de elementos de madera sometidos a flexión. Se ha llevado a cabo un estudio basado en datos obtenidos experimentalmente mediante el ensayo a flexión de vigas de madera de pino silvestre reforzadas con materiales compuestos. Las fibras que componen los tejidos utilizados para la ejecución de los refuerzos son de basalto y de carbono. En el caso de los compuestos de fibra de basalto se aplican en distintos gramajes, y los de carbono en tejido unidireccional y bidireccional. Se analiza el comportamiento de las vigas según las variables de refuerzo aplicadas y se comparan con los resultados de vigas ensayadas sin reforzar. Además se comprueba el ajuste del modelo de cálculo no lineal aplicado para predecir la carga de rotura de cada viga reforzada. Con este trabajo queda demostrado el buen funcionamiento del FRP de fibra de basalto aplicado en el refuerzo de vigas de madera y de los tejidos de carbono bidireccionales con respecto a los unidireccionales. ABSTRACT Many of the buildings of the built heritage include a structure composed by timber elements. The economic volume involved in the maintenance and renewal of this built heritage is considerable, therefore, the study of the different reinforcement techniques applicable to this type of structure is of special interest. The wooden structures have traditionally been reinforced either with steel or with pieces of the same material, increasing the section of the damaged parts. The emergence of polymer composites reinforced with fibers, and their progressive use in construction, started to be applied as reinforcement in timber structures at the beginning of the nineties decade in the 20th century (Sins Bridge, 1992). Wood is a natural material with an excellent ratio between its mechanic characteristics and its weight. This feature is maintained with the use of composites as reinforcement. In terms of its constitutive model, linear elastic behavior parallel to the fiber up to fracture is admitted when subjected to tensile stress, while under compression, an initial linear elastic behavior, followed by a section plasticizing, is considered. In sawn timber beams subjected to bending, the predominant failure is mainly due to tensile stress; and frequently the fracture is located at the beam lower face. The FRP have a linear elastic behavior until fracture occurs, and have excellent mechanical properties in relation to their weight and volume. If the beam is reinforced by its lower face, its capacity to absorb tensile stresses will increase, and therefore, an increase in its carrying capacity is likely to be produced, as well as an increase in ductility. This work analyzes the benefits different reinforcement systems of composite materials provide, with the aim of contributing to the knowledge of this technique for recovering or increasing the strength properties of timber elements subjected to bending loads. It is a study based on data obtained experimentally using bending tests of pine timber beams reinforced with composite materials. Fibers used for the execution of the reinforcement are basalt and carbon. Basalt fiber composites are applied in different grammages, whereas with carbon composites, unidirectional and bidirectional fabrics are used. The behavior of the beams was analyzed regarding the reinforcement variables applied, and the results are compared with those of the tested beams without reinforcement. Furthermore it has been proved adjunting the nonlinear calculation model applied to predict the failure load of each reinforced beam. This work proves the good behavior of fiber reinforce plastic (FRP) with basalt fiber when applied to timber beams, and that of bidirectional carbon fabrics as opposed to the unidirectional ones.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

An engineering modification of blade element/momentum theory is applied to describe the vertical autorotation of helicopter rotors. A full non‐linear aerodynamic model is considered for the airfoils, taking into account the dependence of lift and drag coefficients on both the angle of attack and the Reynolds number. The proposed model, which has been validated in previous work, has allowed the identification of different autorotation modes, which depend on the descent velocity and the twist of the rotor blades. These modes present different radial distributions of driven and driving blade regions, as well as different radial upwash/downwash patterns. The number of blade sections with zero tangential force, the existence of a downwash region in the rotor disk, the stability of the autorotation state, and the overall rotor autorotation efficiency, are all analyzed in terms of the flight velocity and the characteristics of the rotor. It is shown that, in vertical autorotation, larger blade twist leads to smaller values of descent velocity for a given thrust generated by the rotor in the autorotational state.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

An engineering modification of blade element/momentum theory is applied to describe the vertical autorotation of helicopter rotors. A full non-linear aerodynamic model is considered for the airfoils, taking into account the dependence of lift and drag coefficients on both the angle of attack and the Reynolds number. The proposed model, which has been validated in previous work, has allowed the identification of different autorotation modes, which depend on the descent velocity and the twist of the rotor blades. These modes present different radial distributions of driven and driving blade regions, as well as different radial upwash/downwash patterns. The number of blade sections with zero tangential force, the existence of a downwash region in the rotor disk, the stability of the autorotation state, and the overall rotor autorotation efficiency, are all analyzed in terms of the flight velocity and the characteristics of the rotor. It is shown that, in vertical autorotation, larger blade twist leads to smaller values of descent velocity for a given thrust generated by the rotor in the autorotational state.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Desde 1995, el derecho internacional se ha integrado en el ordenamiento jurídico español en lo referente a seguridad y salud. Sin embargo, la situación de la seguridad en los aprovechamientos forestales no ha mejorado notablemente, puesto que se detectan frecuentes casos de personal trabajando sin equipo de protección e incumpliendo las instrucciones de trabajo seguro, y son abundantes las referencias a una elevada accidentalidad. Para evaluar estos aspectos, primeramente se han comparado y valorado los datos de accidentalidad de los taladores de una empresa de referencia con los de los sectores agrario y de la construcción a través de las estadísticas nacionales y con los datos depurados del sector forestal a partir de la base de datos de declaración electrónica de accidentes de la C.A. de Castilla y León. En segundo lugar, se han identificado las deficiencias en materia de prevención, diseñando para ello una encuesta que se ha llevado a cabo en 35 aprovechamientos de Castilla y León. Posteriormente, se ha verificado que la reducción de la accidentalidad en la empresa de referencia se debe a la aplicación del plan de prevención. Se han caracterizado los riesgos en los que habían incurrido los taladores y se han descrito las medidas adoptadas para la reducción de los accidentes en la empresa estudiada, lo que ha conducido a una serie de recomendaciones para reducir la accidentalidad. Por otro lado se han analizado las causas de los picos de accidentalidad detectados. Como conclusión, se puede reducir sensiblemente la accidentalidad sólo si la empresa integra la política de prevención como un objetivo más de la gestión empresarial, en todos los niveles de su organización, acompañando las herramientas técnicas con formación temprana y motivación adecuada. Palabras clave: aprovechamientos forestales, riesgos laborales, prevención, trabajador forestal, accidentalidad, incidencia, gravedad. From 1995, Spanish safety legislation has been adapted to the Internationa! framework. However, operationally the situation is not so good, at least in the wood harvesting activity. Some forest workers are still found not wearing the compulsory safety equipment, working without respecting safety rules and references to high accidents rates are frequent. To assess those aspects, firstly some comparisons have been made between the accident records in a reference company and the accident indexes at national and regional level for building and farming activities. Secondly, using a purpose-designed questionnaire applied to 35 logging worksites in Castilla y Leon Region, deficiencies in prevention have been identified. The relation between the accident reduction and the prevention methods used by the reference studied company has been confirmed. Also the main causes and peaks of the accidents have been analyzed. Finally, some recommendations to reduce the risk of accidents in harvesting operations are provided. The main conclusion confirms that the possibility of reducing the accident risk is conditioned to the commitment of all the staff of the timber harvesting company, at every level of responsibility, to search for excellence in safety as one more entrepreneurial goal. This fact should be accompanied by the staff early training and the adequate motivation means. Keywords: logging, labor risk, safety and health, prevention, logging workers, accident incidence, accident severity.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

El proyecto de rehabilitación de una de las naves del complejo fabril de la industria química ?CROS? en Valencia se llevó a cabo con el criterio de mantener, en la medida de lo posible, los elementos estructurales presentes en la nave. Con este objetivo se realizaron una serie de ensayos no destructivos (END) in situ. Estos ensayos permitieron evaluar la calidad de la madera, determinar qué elementos estructurales debían ser sustituidos y comprobar la aptitud de los que iban a ser reutilizados. Los END empleados en este estudio fueron los siguientes: (1) Identificación de la especie por técnicas anatómicas, (2) Clasificación resistente por método visual, (3) Estimación de humedad por la técnica de resistencia eléctrica; (4) Obtención de velocidades de propagación ultrasónicas (5) Resistógrafía y (6) Alteración de la propagación de ondas electromagnéticas por medio de Georradar. Para la calibración de estos END se tomó una muestra de piezas y se hicieron ensayos destructivos bajo condiciones controladas en laboratorio. En el trabajo que aquí se presenta se muestra la metodología empleada durante el proceso de toma de datos, de análisis de resultados y de cruce de la información obtenida a partir de cada uno de los ensayos hasta llegar a un diagnóstico para los elementos analizados. The assessment of structural timber was requested in the rehabilitation project of the Naves of the chemical industry "CROS". The criterion was to maintain as much as possible timber of the structure and to make only partial replacements. In order not to damage the existing structure and to assess the quality of the existing timber, a series of non-destructive testing (NDT) in the entire structure were performed: (1) Identification of the species by anatomical techniques, (2) Strength grading by visual method, (3) Estimation of moisture content by the technique of electrical resistance, (4) Acquisition of ultrasonic propagation velocities (5) Resistography and (6) Record of the propagation of electromagnetic waves by means of Ground-penetrating radar. Following, a sample group was chose to carry out destructive testing in the lab and compare the NDT results with those obtained with the standard UNE-EN408 (modules of strength, stiffness and density). In the present work, the results provided by each of the NDT techniques are detailed and above all, what is more important, the validity of these after they have been contrasted with the destructive standard tests.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

En el presente trabajo se desarrolla una metodología para poder determinar los coeficientes de fricción tanto estático como dinámico aplicable a diferentes especies de madera. Para desarrollar dicha metodología se utilizan las instalaciones que posee la Plataforma de Enxeñería da Madeira Estructural (PEMADE) donde hay una mesa que permite la realización de ensayos de rozamiento. Se realizan ensayos utilizando una especie de madera muy usada en estructuras como es la Picea abies (L) Karst. La humedad de la madera es del 12%, ya que según indica la actual norma UNE-EN 408, los ensayos para la determinación de las propiedades físicas y mecánicas de la madera estructural se deben de hacer con ese contenido de humedad. Finalmente, decir que este trabajo de investigación sienta las bases para realizar posteriores campañas de ensayos con esta base metodológica que permitan, para diferentes especies de madera y humedades, obtener rangos de valores de los coeficientes de rozamiento estático y dinámico para las principales especies de madera de uso estructural. This research develops a methodology to determine the coefficients of both static and dynamic friction apply to different species of wood. To develop such a methodology is used the installations owned by the Plataforma de Enxeñería da Madeira Estructural (PEMADE) where there is a table that allows testing of friction. Tests are carried out using a wood species normally used in structures such as Picea abies (L) Karst. The wood moisture content is 12%, and that, according to the current UNE-EN 408 norm, the tests for determining the physical and mechanical properties of structural timber should do with that moisture content. Finally, it can say that this research provides the basis for subsequent test campaigns with this methodological basis to obtain, for different wood species and moisture, the ranges of values of the coefficients of static and dynamic friction for major wood species for structural use.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

En esta Tesis se cuantifica la variación cromática que producen los barnices en el color de los diferentes tipos de maderas de construcción, obteniendo un modelo matemático de predicción de color de la madera. Se analizan las prestaciones de dieciséis barnices, supuestamente incoloros, aplicados sobre veinte tipos de maderas, angiospermas y gimnospermas, de distintas densidades y latitudes. Ambos materiales son de uso frecuente en el ámbito de la construcción y de fácil localización en las tiendas y almacenes de ambos sectores. Se utilizan técnicas de descomposición cromática, mediante el empleo de microscopio óptico de reflexión, para poder obtener un abanico gráfico de histogramas con valores numéricos de luminosidad y composición cromática, y de esta forma comprobar que los supuestos barnices que se venden como incoloros, no son totalmente incoloros sino que muestran tendencias a virar hacia alguno de los colores básicos. En el proceso experimental de la Tesis, se aplican 16 barnices sobre 20 tipos de maderas, obteniéndose los histogramas de las campañas de fotografías realizadas con cinco años de diferencia, obteniéndose no solo la variación de color que producen los barnices sobre el original de la madera, sino además la influencia de un envejecimiento a los cinco años. La Tesis relaciona el tipo de barniz idóneo para cada tipo de madera, de modo que produzca la menor variación cromática. La Tesis además obtiene un modelo matemático que permite predecir el color final de la madera tratada en función del color inicial de la madera sin barnizar. Se propone en esta Tesis una recomendación de los productos a utilizar en cada uno de los tipos de madera en base a su color inicial. This Thesis quantifies the chromatic variation caused by varnishes in the colour of different types of timbers, obtaining a mathematical model for predicting the timber’s colour. The performance of sixteen varnishes, supposedly colourless, is analysed, applied on twenty types of timber, angiosperms and gymnosperms, of different densities and latitudes. Both materials are of frequent use in the construction field and easily located in the stores and warehouses of both sectors. Chromatic decomposition techniques are used, through the utilization of a reflection optical microscope, in order to obtain a graphic range of histograms with numerical values of luminosity and chromatic composition, and this way confirm that the alleged varnishes sold as colourless are not completely colourless but are prone to shift towards one of the basic colours. During the Thesis’ experimental procedure 16 varnishes are applied on 20 types of timber, obtaining the colour histograms of the photography campaigns carried out with a five years difference, resulting in not only the colour variation caused by the varnishes on the original timber, but also the influence of its ageing five years later. The Thesis links the right type of varnish for each kind of timber, so that as little chromatic variation as possible occurs. The Thesis obtains as well a mathematical model, which makes it possible to predict the final colour of the treated timber depending on the original colour of the timber with no varnish. This Thesis proposes a recommendation of the products to use on each type of timber on the basis of its original colour.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Este proyecto tiene por objetivo la realización de un análisis comparativo de la normativa española existente para el cálculo de la carga de hundimiento de cimentaciones mediante pilotes, viendo el contenido de cada una de ellas y aplicándolo a un caso práctico. Inicialmente se realiza un planteamiento general del modo de cálculo de la carga de hundimiento de los pilotes desde el punto de vista estático. A continuación se recoge la formulación existente en el Código Técnico de la Edificación (CTE), en las Recomendaciones para Obras Marítimas y Portuarios (ROM 05-05) y en la Guía de Cimentaciones en Obras de Carretera (GCOC) viendo de donde se extraen las fórmulas empleadas en ellas. Para pasar a realizar un análisis comparativo de ellas con la ayuda de distintos gráficos y viendo la relación que presentan unos códigos con otros tanto para suelos granulares como cohesivos y pilotes hincados y excavados, que es lo que distinguen los tres códigos generalmente. Por último, se realiza un análisis comparativo de los resultados obtenidos para la cimentación de tres viaductos de la autovía Noroeste de Murcia realizando un análisis económico de esta cimentación. ABSTRACT The aim of this project is to develop a comparative analysis of the actual Spanish regulations for the calculation of sinking’s load of foundation design based on timber piles, observing the contents of each and every one of them an applying it to a real and practical situation. To begin with, a general proposal is made from calculation the sinking load of the timber piles from the static point of view. Next, the actual formulation is gathering in “Código Técnico de la Edificación” (CTE), “Recomendaciones para Obras Marítimas y Portuarias” and “Guía de Cimentaciones en Obras de Carretera”, observing where the applied formulas are calculated from. Thereupon, a coparativeanalysis of them is carry out with the help of different graphics and facing the connections from some codes to anothers, not only for granular but for cohesive surface, and for drilling and digging out piles, that’s what generally distinguishes among for three codes. Finally, a comparative analysis of obtained results is carry out for the foundation of the three viaducts of Murcia’s NorthWest motorway, accomplishing economical analysis of this foundation.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Non-destructive, visual evaluation and mechanical testing techniques were used to assess the structural properties of 374 samples of chestnut (Castanea sativa). The principal components method was applied to establish and interpret correlations between variables obtained of modulus of elasticity, bending strength and density. The static modulus of elasticity presented higher correlation values than those obtained using non-destructive methods. Bending strength presented low correlations with the non-destructive parameters, but there was some relation to the different knot ratios defined. The relationship was stronger with the most widely used ratio, CKDR. No significant correlations were observed between any of the variables and density.