The present study investigates the potential use of non-catalyzed water-soluble blocked polyurethane prepolymer (PUP) as a bifunctional cross-linker for collagenous scaffolds. The effect of concentration (5, 10, 15 and 20%), time (4, 6, 12 and 24 h), medium volume (50, 100, 200 and 300%) and pH (7.4, 8.2, 9 and 10) over stability, microstructure and tensile mechanical behavior of acellular pericardial matrix was studied. The cross-linking index increased up to 81% while the denaturation temperature increased up to 12 °C after PUP crosslinking. PUP-treated scaffold resisted the collagenase degradation (0.167 ± 0.14 mmol/g of liberated amine groups vs. 598 ± 60 mmol/g for non-cross-linked matrix). The collagen fiber network was coated with PUP while viscoelastic properties were altered after cross-linking. The treatment of the pericardial scaffold with PUP allows (i) different densities of cross-linking depending of the process parameters and (ii) tensile properties similar to glutaraldehyde method.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The reinforcing effect of inorganic fullerene-like tungsten disulfide (IF-WS2) nanoparticles in two different polymer matrices, isotactic polypropylene (iPP) and polyphenylene sulfide (PPS), has been investigated by means of dynamic depth-sensing indentation. The hardness and elastic modulus enhancement upon filler addition is analyzed in terms of two main contributions: changes in the polymer matrix nanostructure and intrinsic properties of the filler including matrix-particle load transfer. It is found that the latter mainly determines the overall mechanical improvement, whereas the nanostructural changes induced in the polymer matrix only contribute to a minor extent. Important differences are suggested between the mechanisms of deformation in the two nanocomposites, resulting in a moderate mechanical enhancement in case of iPP (20% for a filler loading of 1%), and a remarkable hardness increase in case of PPS (60% for the same filler content). The nature of the polymer amorphous phase, whether in the glassy or rubbery state, seems to play here an important role. Finally, nanoindentation and dynamic mechanical analysis measurements are compared and discussed in terms of the different directionality of the stresses applied.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The objective of the present study is to develop fully renewable and environmentally benign techniques for improving the fire safety of flexible polyurethane foams (PUFs). A multilayered coating made from cationic chitosan (CS) and anionic alginate (AL) was deposited on PUFs through layer-by-layer assembly. This coating system exhibits a slight influence on the thermal stability of PUF, but significantly improves the char formation during combustion. Cone calorimetry reveals that 10 CS-AL bilayers (only 5.7% of the foams weight) lead to a 66% and 11% reduction in peak heat release rate and total heat release, respectively, compared with those of the uncoated control. The notable decreased fire hazards of PUF are attributed to the CS-AL coatings being beneficial to form an insulating protective layer on the surface of burning materials that inhibits the oxygen and heat permeation and slows down the flammable gases in the vapor phase, and thereby improves the flame resistance. This water-based, environmentally benign natural coating will stimulate further efforts in improving fire safety for a variety of polymer substrates.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Using inorganic fullerene-like (IF) nanoparticles and inorganic nanotubes (INT) in organic-inorganic hybrid composite, materials provide the potential for improving thermal, mechanical, and tribological properties of conventional composites. The processing of such high-performance hybrid thermoplastic polymer nanocomposites is achieved via melt-blending without the aid of any modifier or compatibilizing agent. The incorporation of small quantities (0.1-4 wt.%) of IF/INTs (tungsten disulfide, IF-WS2 or molybdenum disulfide, MoS2) generates notable performance enhancements through reinforcement effects and excellent lubricating ability in comparison with promising carbon nanotubes or other inorganic nanoscale fillers. It was shown that these IF/INT nanocomposites can provide an effective balance between performance, cost effectiveness, and processability, which is of significant importance for extending the practical applications of diverse hierarchical thermoplastic-based composites.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This article reviews recent literature on hierarchical thermoplastic-based composites that simultaneously incorporate carbon nanotubes (CNTs) and conventional microscale fibers, and discusses the structure?property relationships of the resulting hybrids. The mixing of multiple and multiscale constituents enables the preparation of materials with new or improved properties due to synergistic effects. By exploiting the outstanding mechanical, thermal and electrical properties of CNTs, a new generation of multifunctional high-performance composites suitable for a wide variety of applications can be developed.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

One of the most used methods in rapidprototyping is Fused Deposition Modeling (FDM), which provides components with a reasonable strength in plastic materials such as ABS and has a low environmental impact. However, the FDM process exhibits low levels of surface finishing, difficulty in getting complex and/or small geometries and low consistency in “slim” elements of the parts. Furthermore, “cantilever” elements need large material structures to be supported. The solution of these deficiencies requires a comprehensive review of the three-dimensional part design to enhance advantages and performances of FDM and reduce their constraints. As a key feature of this redesign a novel method of construction by assembling parts with structuraladhesive joints is proposed. These adhesive joints should be designed specifically to fit the plastic substrate and the FDM manufacturing technology. To achieve this, the most suitable structuraladhesiveselection is firstly required. Therefore, the present work analyzes five different families of adhesives (cyanoacrylate, polyurethane, epoxy, acrylic and silicone), and, by means of the application of technical multi-criteria decision analysis based on the analytic hierarchy process (AHP), to select the structuraladhesive that better conjugates mechanical benefits and adaptation to the FDM manufacturing process

Relevância:

10.00% 10.00%

Publicador:

Resumo:

En este trabajo se llevó a cabo el tratamiento de vinazas mediante dos tecnologías anaerobias. Se dividió en cuatro estudios técnicos. El primero fue el arranque y estabilización del reactor UASB (Upflow Anaerobic Sludge Blanket), en dónde se evaluó la estabilización mediante la eficiencia de remoción de DQO y la granulación del lodo. El segundo estudio evaluó el rendimiento del reactor UASB frente a diferentes Cva. El tercer estudio evaluó el efecto del TRH sobre la eficiencia del reactor UASB, y el cuarto de ellos fue evaluar el rendimiento del RABF (Reactor Anaerobio de Biomasa Fija). El reactor UASB de 2,6 L de capacidad, fue arrancado por lotes, con seis ensayos utilizando vinaza como sustrato. Se obtuvieron eficiencias de remoción en DQO en un rango de 79-91%, en los seis lotes. Se obtuvo formación de gránulos con diámetro (Ø) de 0,85-1,15 mm y un coeficiente de esfericidad (Є) de 0,7-0,77. Se logró la granulación de lodos tras 2 meses de operación. Alcanzada la estabilización del reactor UASB, se siguió una operación en flujo continuo. Las Cva probadas de 1, 2, 4 y 6 gDQO/L.d para el reactor UASB dan una respuesta bastante favorable con respecto al rendimiento del reactor, ya que presento eficiencias de remoción de DQOs del 51 hasta el 76%, eficiencias similares a los reportados por la literatura. En el estudio de TRH se operó con Cva de 6 gDQO/L.d y los TRH fueron de 24, 12 ,5 ,3 y 1 día. El % de eliminación de DQO fue de 51, 60, 57, 60 y 63 % remoción en DQOsoluble, respectivamente. Se alcanzó una producción de biogás máximo de 5.283 ml/d, pero al reducir el TRH se observó una reducción proporcional del volumen total de biogás. El %CH4 contenido en el biogás aumento al disminuir el TRH, reflejando valores de 80 al 92 % de CH4. El RABF con un volumen de 8,2 L, utilizo tubos de plástico corrugado como medio de soporte para las bacterias. Se aplicaron las siguientes Cva; 0,5, 1, 3 y 6 gDQO/L.d. El reactor RABF presento una excelente remoción de la materia orgánica (80% DQOs), una producción de biogás estable, y un contenido en CH4 del biogás muy interesante. Sin embargo, para una Cva superior a 3 gDQO/L.d empezó un comportamiento inesperado de reducción de capacidad. Las condiciones hidrodinámicas del reactor UASB son decisivas para la formación de los gránulos, condición previa para iniciar el flujo continuo. Al operar el reactor UASB en modo continuo, se pudo evaluar las mejores condiciones de operación para este tipo de residuo (vinaza). La Cva de 6 gDQO/L.d para el reactor UASB alimentado con vinaza bruta representa el límite de su capacidad. Sin embargo, al aumentar la Cva se genera una mayor producción de biogás y metano. La eficiencia de remoción de la DQO soluble es independiente del TRH, para una Cva de 6 g DQO/L•d y las condiciones de TRH probadas (24, 12, 5, 3 y 1 días). Los valores de remoción de DQO alcanzados son un poco superior a los valores de biodegradabilidad anaerobia de la vinaza observados de 50 %. De manera general, la reducción del TRH o bien la dilución de la vinaza no presenta un efecto significativo sobre la remoción de la materia orgánica soluble, pero si lo presenta en la remoción de sulfatos reduciendo indirectamente su toxicidad. El soporte termoplástico inoculado en el RABF y alimentado con vinaza bruta, actuó como un filtro, además de obtener buenos resultados en eliminación de DQO, pero dada las dimensiones y la altura del relleno se frena la evacuación del metano. This work was carried out by treatment vinasses with two anaerobic technologies. It was divided into four technical studies. The first was the start up and stabilization Upflow Anaerobic Sludge Blanket (UASB) reactor, where the stability was evaluated by the removal efficiency of COD and sludge granulation. The second study evaluated the performance of the UASB reactor against different OLR. The third study evaluated the effect of HRT on the efficiency of the UASB reactor, and the fourth of which was evaluate the performance Fixed Biomass Anaerobic (FBA) reactor. The UASB reactor of 2,6 L capacity, was started in batch, with six assays using vinasse as substrate. Were obtained removal efficiencies of COD in the range of 79- 91% in the six batches. Forming granules were obtained with a diameter (Ø) of 0,85- 1,15 mm and sphericity coefficient (Є) of 0,7 to 0,77. Sludge granulation was achieved after 2 months of operation. Once stabilization is achieved of the UASB reactor, it was followed by a continuous flow operation. The OLR tested 1, 2, 4 and 6 gCOD/L.d for UASB reactor gives a very favorable response regarding the performance of the reactor, as presented COD5 removal efficiencies of 51 to 76%, similar efficiencies those reported in the literature The HRT study was operated with an OLR of 6 gCOD/L.d and HRT were 24, 12, 5, 3 and 1 day. The removal efficiency was 51, 60, 57, 60 and 63% in soluble COD, respectively. It reached a maximum biogas production of 5.283 ml / d, but by reducing the HRT showed a proportional reduction in the total volume of biogas. The %CH4 content in the biogas increased with decreasing TRH, reflecting values of 80 to 92% of CH4. The FBA reactor with a volume of 8,2 L, used corrugated plastic tubes as carrier for bacteria transportation. The following OLR was applied, 0,5, 1, 3 and 6 gCOD/L.d. The FBA reactor showed an excellent removal of organic matter (80% CODS), a stable biogas production, and CH4 content very interesting. However, for more than 3 gCOD/L.d OLR began with unexpected behavior of capacity reduction. The UASB reactor hydrodynamic conditions are decisive for the formation of the granules, precondition to start the continuous flow. By operating the UASB reactor in continuous mode, it was possible to evaluate the best operating conditions for this type of waste (vinasse). The OLR of 6 gCOD/L.d for the UASB reactor fed with raw vinasse represents the limit of its capacity. However, with increasing OLR creates increased biogas production and methane. The removal efficiency of soluble COD is independent of HRT for OLR of 6 gCOD/L.d and HRT conditions tested (24, 12, 5, 3 and 1 day). COD Removal values achieved are slightly higher than the values of the vinasse anaerobic biodegradability of observed at 50%. Generally, reduction of HRT or vinasse dilution does not present a significant effect on the removal of the soluble organic matter; however if it occurs in the removal of sulfate reducing indirectly its toxicity. The thermoplastic support inoculated in FBA reactor and fed with raw vinasse, acted as a filter, in addition to obtaining good results in COD removal, but given the size and height of the filling slows evacuation of methane.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The adhesives used for applications in marine environments are subject to particular chemical conditions, which are mainly characterised by an elevated chlorine ion content and intermittent wetting/drying cycles, among others.These conditions can limit the use of adhesives due to the degradation processes that they experience. In this work, the chemical degradation of two different polymers, polyurethane and vinylester, was studied in natural seawater under immersion for different periods of time.The diffusion coefficients and concentration profiles of water throughout the thickness of the adhesiveswere obtained.Microstructural changes in the polymer due to the action of water were observed by SEM, and the chemical degradation of the polymer was monitored with the Fourier transform infrared spectroscopy (FTIR) and differential scanning calorimetry (DSC). The degradation of the mechanical properties of the adhesive was determined by creep tests withMixed Cantilever Beam (MCB) specimens at different temperatures. After 180 days of immersion of the specimens, it was concluded that the J-integral value (depending on the strain) implies a loss of stiffness of 51% and a decrease in the failure load of 59% for the adhesive tested.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The end-notched flexure (ENF) test calculates the value of mode II fracture energy in adhesive bonding between the substrates of same nature. Traditional methods of calculating fracture energy in the ENF test are not suitable in cases where the thickness of the adhesive is non-negligible compared with adherent thicknesses. To address this issue, a specific methodology for calculating mode II fracture energy has been proposed in this paper. To illustrate the applicability of the proposed method, the fracture energy was calculated by the ENF test for adhesive bonds between aluminium and a composite material, which considered two different types of adhesive (epoxy and polyurethane) and various surface treatments. The proposed calculation model provides higher values of fracture energy than those obtained from the simplified models that consider the adhesive thickness to be zero, supporting the conclusion that the calculation of mode II fracture energy for adhesives with non-negligible thickness relative to their adherents should be based on mathematical models, such as the method proposed in this paper, that incorporate the influence of this thickness.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Novel carbon fiber (CF)-reinforced poly(phenylene sulphide) (PPS) laminates incorporating inorganic fullerene-like tungsten disulfide (IF-WS2) nanoparticles were prepared via melt-blending and hot-press processing. The influence of the IF-WS2 on the morphology, thermal, mechanical and tribological properties of PPS/CF composites was investigated. Efficient nanoparticle dispersion within the matrix was attained without using surfactants. A progressive rise in thermal stability was found with increasing IF-WS2 loading, as revealed by thermogravimetric analysis. The addition of low nanoparticle contents retarded the crystallization of the matrix, whereas concentrations equal or higher than 1.0 wt% increased both the crystallization temperature and degree of crystallinity compared to those of PPS/CF. Mechanical tests indicated that with only 1.0 wt% IF-WS2 the flexural modulus and strength of PPS/CF improved by 17 and 14%, respectively, without loss in toughness, ascribed to a synergistic effect between the two fillers. A significant enhancement in the storage modulus and glass transition temperature was also observed. Moreover, the wear rate and coefficient of friction strongly decreased, attributed to the lubricant role of the IF-WS2 combined with their reinforcing effect. These inorganic nanoparticles show great potential to improve the mechanical and tribological properties of conventional thermoplastic/CF composites for structural applications.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The rheological and tribological properties of single-walled carbon nanotube (SWCNT)-reinforced poly(phenylene sulphide) (PPS) and poly(ether ether ketone) (PEEK) nanocomposites prepared via melt-extrusion were investigated. The effectiveness of employing a dual-nanofiller strategy combining polyetherimide (PEI)-wrapped SWCNTs with inorganic fullerene-like tungsten disulfide (IF-WS2) nanoparticles for property enhancement of the resulting hybrid composites was evaluated. Viscoelastic measurements revealed that the complex viscosity ?, storage modulus G?, and loss modulus G? increased with SWCNT content. In the low-frequency region, G? and G? became almost independent of frequency at higher SWCNT loadings, suggesting a transition from liquid-like to solid-like behavior. The incorporation of increasing IF-WS2 contents led to a progressive drop in ? and G? due to a lubricant effect. PEEK nanocomposites showed lower percolation threshold than those based on PPS, ascribed to an improved SWCNT dispersion due to the higher affinity between PEI and PEEK. The SWCNTs significantly lowered the wear rate but only slightly reduced the coefficient of friction. Composites with both nanofillers exhibited improved wear behavior, attributed to the outstanding tribological properties of these nanoparticles and a synergistic reinforcement effect. The combination of SWCNTs with IF-WS2 is a promising route for improving the tribological and rheological performance of thermoplastic nanocomposites.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Novel poly(phenylene sulphide) (PPS) nanocomposites reinforced with an aminated derivative (PPS-NH2) covalently attached to acid-treated single-walled carbon nanotubes (SWCNTs) were prepared via simple melt-blending technique. Their morphology, viscoelastic behaviour, electrical conductivity, mechanical and tribological properties were investigated. Scanning electron microscopy revealed that the grafting process was effective in uniformly dispersing the SWCNTs within the matrix. The storage and loss moduli as a function of frequency increased with the SWCNT content, tending to a plateau in the low-frequency regime. The electrical conductivity of the nanocomposites was considerably enhanced in the range 0.1?0.5 wt% SWCNTs; electrical and rheological percolation thresholds occurred at similar nanotube concentrations. Mechanical tests demonstrated that with only 1.0 wt% SWCNTs the Young's modulus and tensile strength of the matrix improved by 51 and 37%, respectively, without decrement in toughness, ascribed to a very efficient load transfer. A moderate decrease in the friction coefficient and a 75% reduction in wear rate were found for the abovementioned nanotube loading, indicating that PPS-NH2-g-SWCNTs are good tribological additives for thermoplastic polymers. Based on the promising results obtained in this work, it is expected that these nanofillers will be used to develop high-performance thermoplastic/CNT nanocomposites for structural applications.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Las uniones estructurales mecánicas y adhesivas requieren la combinación de un número importante de parámetros para la obtención de la continuidad estructural que exigen las condiciones de diseño. Las características de las uniones presentan importantes variaciones, ligadas a las condiciones de ejecución, tanto en uniones mecánicas como especialmente en uniones adhesivas y mixtas (unión mecánica y adhesiva, también conocidas como uniones híbridas). Las propiedades mecánicas de las uniones adhesivas dependen de la naturaleza y propiedades de los adhesivos y también de muchos otros parámetros que influyen directamente en el comportamiento de estas uniones. Algunos de los parámetros más significativos son: el acabado superficial de los materiales, área y espesor de la capa adhesiva, diseño adecuado, secuencia de aplicación, propiedades químicas de la superficie y preparación de los sustratos antes de aplicar el adhesivo. Los mecanismos de adhesión son complejos. En general, cada unión adhesiva solo puede explicarse considerando la actuación conjunta de varios mecanismos de adhesión. No existen adhesivos universales para un determinado material o aplicación, por lo que cada pareja sustrato-adhesivo requiere un particular estudio y el comportamiento obtenido puede variar, significativamente, de uno a otro caso. El fallo de una junta adhesiva depende del mecanismo cohesión-adhesión, ligado a la secuencia y modo de ejecución de los parámetros operacionales utilizados en la unión. En aplicaciones estructurales existen un número muy elevado de sistemas de unión y de posibles sustratos. En este trabajo se han seleccionado cuatro adhesivos diferentes (cianoacrilato, epoxi, poliuretano y silano modificado) y dos procesos de unión mecánica (remachado y clinchado). Estas uniones se han aplicado sobre chapas de acero al carbono en diferentes estados superficiales (chapa blanca, galvanizada y prepintada). Los parámetros operacionales analizados han sido: preparación superficial, espesor del adhesivo, secuencia de aplicación y aplicación de presión durante el curado. Se han analizado tanto las uniones individuales como las uniones híbridas (unión adhesiva y unión mecánica). La combinación de procesos de unión, sustratos y parámetros operacionales ha dado lugar a la preparación y ensayo de más de mil muestras. Pues, debido a la dispersión de resultados característica de las uniones adhesivas, para cada condición analizada se han ensayado seis probetas. Los resultados obtenidos han sido: El espesor de adhesivo utilizado es una variable muy importante en los adhesivos flexibles, donde cuanto menor es el espesor del adhesivo mayor es la resistencia mecánica a cortadura de la unión. Sin embargo en los adhesivos rígidos su influencia es mucho menor. La naturaleza de la superficie es fundamental para una buena adherencia del adhesivo al substrato, que repercute en la resistencia mecánica de la unión. La superficie que mejor adherencia presenta es la prepintada, especialmente cuando existe una alta compatibilidad entre la pintura y el adhesivo. La superficie que peor adherencia tiene es la galvanizada. La secuencia de aplicación ha sido un parámetro significativo en las uniones híbridas, donde los mejores resultados se han obtenido cuando se aplicaba primero el adhesivo y la unión mecánica se realizaba antes del curado del adhesivo. La aplicación de presión durante el curado se ha mostrado un parámetro significativo en los adhesivos con poca capacidad para el relleno de la junta. En los otros casos su influencia ha sido poco relevante. El comportamiento de las uniones estructurales mecánicas y adhesivas en cuanto a la resistencia mecánica de la unión puede variar mucho en función del diseño de dicha unión. La resistencia mecánica puede ser tan grande que falle antes el substrato que la unión. Las mejores resistencias se consiguen diseñando las uniones con adhesivo cianoacrilato, eligiendo adecuadamente las condiciones superficiales y operacionales, por ejemplo chapa blanca aplicando una presión durante el curado de la unión. La utilización de uniones mixtas aumenta muy poco o nada la resistencia mecánica, pero a cambio proporciona una baja dispersión de resultados, siendo destacable para la superficie galvanizada, que es la que presenta peor reproducibilidad cuando se realizan uniones sólo con adhesivo. Las uniones mixtas conducen a un aumento de la deformación antes de la rotura. Los adhesivos dan rotura frágil y las uniones mecánicas rotura dúctil. La unión mixta proporciona ductilidad a la unión. Las uniones mixtas también pueden dar rotura frágil, esto sucede cuando la resistencia del adhesivo es tres veces superior a la resistencia de la unión mecánica. Las uniones híbridas mejoran la rigidez de la junta, sobre todo se aprecia un aumento importante en las uniones mixtas realizadas con adhesivos flexibles, pudiendo decirse que para todos los adhesivos la rigidez de la unión híbrida es superior. ABSTRACT The mechanical and adhesive structural joints require the combination of a large number of parameters to obtain the structural continuity required for the design conditions. The characteristics of the junctions have important variations, linked to performance conditions, in mechanical joints as particular in mixed adhesive joints (mechanical and adhesive joints, also known as hybrid joints). The mechanical properties of the adhesive joints depend of the nature and properties of adhesives and also of many other parameters that directly influence in the behavior of these joints. Some of the most significant parameters are: the surface finished of the material, area and thickness of the adhesive layer, suitable design, and application sequence, chemical properties of the surface and preparation of the substrate before applying the adhesive. Adhesion mechanisms are complex. In general, each adhesive joint can only be explained by considering the combined action of several adhesions mechanisms. There aren’t universal adhesives for a given material or application, so that each pair substrate-adhesive requires a particular study and the behavior obtained can vary significantly from one to another case. The failure of an adhesive joint depends on the cohesion-adhesion mechanism, linked to the sequence and manner of execution of the operational parameters used in the joint. In the structural applications, there are a very high number of joining systems and possible substrates. In this work we have selected four different adhesives (cyanoacrylate, epoxy, polyurethane and silano modified) and two mechanical joining processes (riveting and clinching). These joints were applied on carbon steel with different types of surfaces (white sheet, galvanized and pre-painted). The operational parameters analyzed were: surface preparation, thickness of adhesive, application sequence and application of pressure during curing. We have analyzed individual joints both as hybrid joints (adhesive joint and mechanical joint). The combination of joining processes, substrates and operational parameters has resulted in the preparation and testing of over a thousand specimens. Then, due to the spread of results characteristic of adhesive joints, for each condition analyzed we have tested six samples. The results have been: The thickness of adhesive used is an important variable in the flexible adhesives, where the lower the adhesive thickness greater the shear strength of the joint. However in rigid adhesives is lower influence. The nature of the surface is essential for good adherence of the adhesive to the substrate, which affects the shear strength of the joint. The surface has better adherence is preprinted, especially when there is a high compatibility between the paint and the adhesive. The surface which has poor adherence is the galvanized. The sequence of application has been a significant parameter in the hybrid junctions, where the best results are obtained when applying first the adhesive and the mechanical joint is performed before cured of the adhesive. The application of pressure during curing has shown a significant parameter in the adhesives with little capacity for filler the joint. In other cases their influence has been less relevant. The behavior of structural mechanical and adhesive joints in the shear strength of the joint can vary greatly depending on the design of such a joint. The shear strength may be so large that the substrate fails before the joint. The best shear strengths are achieved by designing the junctions with cyanoacrylate adhesive, by selecting appropriately the surface and operating conditions, for example by white sheet applying a pressure during curing of the joint. The use of hybrid joints no increase shear strength, but instead provides a low dispersion of results, being remarkable for the galvanized surface, which is the having worst reproducibility when performed bonded joints. The hybrid joints leading to increased deformation before rupture. The joints witch adhesives give brittle fracture and the mechanics joints give ductile fracture. Hybrid joint provides ductility at the joint. Hybrid joint can also give brittle fracture, this happens when the shear strength of the adhesive is three times the shear strength of the mechanical joint. The hybrid joints improve stiffness of joint, especially seen a significant increase in hybrid joints bonding with flexible adhesives, can be said that for all the adhesives, the hybrid junction stiffness is higher.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The thermal and thermomechanical properties of poly(phenylene sulphide) (PPS) based nanocomposites incorporating a polymer derivative covalently anchored onto single-walled carbon nanotubes (SWCNTs) were investigated. The grafted fillers acted as nucleating agents, increasing the crystallization temperature and degree of crystallinity of the matrix. They also enhanced its thermal stability, flame retardancy, glass transition (Tg) and heat deflection temperatures while reduced the coefficient of thermal expansion at temperatures below Tg. A strong rise in the thermal conductivity, Young?s modulus and tensile strength was found with increasing filler loading both in the glassy and rubbery states. All these outstanding improvements are ascribed to strong matrix-filler interfacial interactions combined with a compatibilization effect that results in very homogeneous SWCNT dispersion. The results herein offer useful insights towards the development of engineering thermoplastic/CNT nanocomposites for high-temperature applications.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Carbon fiber (CF)-reinforced high-temperature thermoplastics such as poly(phenylene sulphide) (PPS) are widely used in structural composites for aerospace and automotive applications. The porosity of CF-reinforced polymers is a very important topic for practical applications since there is a direct correlation between void content and mechanical properties. In this study, inorganic fullerene-like tungsten disulphide (IF-WS2) lubricant nanoparticles were used to manufacture PPS/IF-WS2/CF laminates via melt-blending and hot-press processing, and the effect of IF-WS2 loading on the quality, thermal and mechanical behaviour of the hybrid composites was investigated. The addition of IF-WS2 improved fiber impregnation, resulting in lower degree of porosity and increased delamination resistance, compression and flexural properties; their reinforcement effect was greater at temperatures above the glass transition (Tg). IF-WS2 contents higher than 0.5 wt % increased Tg and the heat deflection temperature while reduced the coefficient of thermal expansion. The multiscale laminates exhibited higher ignition point and notably reduced peak heat release rate compared to PPS/CF. The coexistence of micro- and nano-scale fillers resulted in synergistic effects that enhanced the stiffness, strength, thermal conductivity and flame retardancy of the matrix. The results presented herein demonstrate that the IF-WS2 are very promising nanofillers to improve the thermomechanical properties of conventional thermoplastic/CF composites.