15 resultados para Service life (Engineering)

em Universidad Politécnica de Madrid


Relevância:

90.00% 90.00%

Publicador:

Resumo:

Freezing of water or salt solution in concrete pores is a main cause for severe damage and significant reduction of the service life. Most of the freeze-thaw (F-T) accelerated tests measure the scaling of concrete by weighting. This paper presents complementary procedures based on the use of strain gages and ultrasonic pulse velocity (UPV) for measuring the deterioration of concrete due to freezing and thawing. These non-destructive testing (NDT) procedures are applied to two types of concretes, one susceptible to F-T damage and the other does not. The results show a good correlation between scaling and the measurements obtained with NDT. Showing NDT the advantage to detect before the damage and to perform continuous measurement

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Waste produced during the service life of automobiles has received much less attention than end-of-life vehicles themselves. In this paper, we deal with the set up of a reverse logistics system for the collection and treatment of use-phase residues. First, the type of waste arising during vehicles? service life is characterized. Data were collected in collaboration with SIGRAUTO, the product stewardship organization in charge of vehicles? recovery in Spain. Next, three organizational models are proposed. The three alternatives are benchmarked and assessed from a double organizational and operational perspective for the particular case of the Madrid region in Spain

Relevância:

90.00% 90.00%

Publicador:

Resumo:

La mayoría de las estructuras de hormigón pretensadas construidas en los últimos 50 años han demostrado una excelente durabilidad cuando su construcción se realiza atendiendo las recomendaciones de un buen diseño así como una buena ejecución y puesta en obra de la estructura. Este hecho se debe en gran parte al temor que despierta el fenómeno de la corrosión bajo tensión típico de las armaduras de acero de alta resistencia. Menos atención se ha prestado a la susceptibilidad a la corrosión bajo tensión de los anclajes de postensado, posiblemente debido a que se han reportado pocos casos de fallos catastróficos. El concepto de Tolerancia al Daño y la Mecánica de la Fractura en estructuras de Ingeniería Civil ha empezado a incorporarse recientemente en algunas normas de diseño y cálculo de estructuras metálicas, sin embargo, aún está lejos de ser asimilado y empleado habitualmente por los ingenieros en sus cálculos cuando la ocasión lo requiere. Este desconocimiento de los aspectos relacionados con la Tolerancia al Daño genera importantes gastos de mantenimiento y reparación. En este trabajo se ha estudiado la aplicabilidad de los conceptos de la Mecánica de la Fractura a los componentes de los sistemas de postensado empleados en ingeniería civil, empleándolo para analizar la susceptibilidad de las armaduras activas frente a la corrosión bajo tensiones y a la pérdida de capacidad portante de las cabezas de anclajes de postensado debido a la presencia de defectos. Con este objeto se han combinado tanto técnicas experimentales como numéricas. Los defectos superficiales en los alambres de pretensado no se presentan de manera aislada si no que existe una cierta continuidad en la dirección axial así como un elevado número de defectos. Por este motivo se ha optado por un enfoque estadístico, que es más apropiado que el determinístico. El empleo de modelos estadísticos basados en la teoría de valores extremos ha permitido caracterizar el estado superficial en alambres de 5,2 mm de diámetro. Por otro lado la susceptibilidad del alambre frente a la corrosión bajo tensión ha sido evaluada mediante la realización de una campaña de ensayos de acuerdo con la actual normativa que ha permitido caracterizar estadísticamente su comportamiento. A la vista de los resultados ha sido posible evaluar como los parámetros que definen el estado superficial del alambre pueden determinar la durabilidad de la armadura atendiendo a su resistencia frente a la corrosión bajo tensión, evaluada mediante los ensayos que especifica la normativa. En el caso de las cabezas de anclaje de tendones de pretensado, los defectos se presentan de manera aislada y tienen su origen en marcas, arañazos o picaduras de corrosión que pueden producirse durante el proceso de fabricación, transporte, manipulación o puesta en obra. Dada la naturaleza de los defectos, el enfoque determinístico es más apropiado que el estadístico. La evaluación de la importancia de un defecto en un elemento estructural requiere la estimación de la solicitación local que genera el defecto, que permite conocer si el defecto es crítico o si puede llegar a serlo, si es que progresa con el tiempo (por fatiga, corrosión, una combinación de ambas, etc.). En este trabajo los defectos han sido idealizados como grietas, de manera que el análisis quedara del lado de la seguridad. La evaluación de la solicitación local del defecto ha sido calculada mediante el empleo de modelos de elementos finitos de la cabeza de anclaje que simulan las condiciones de trabajo reales de la cabeza de anclaje durante su vida útil. A partir de estos modelos numéricos se ha analizado la influencia en la carga de rotura del anclaje de diversos factores como la geometría del anclaje, las condiciones del apoyo, el material del anclaje, el tamaño del defecto su forma y su posición. Los resultados del análisis numérico han sido contrastados satisfactoriamente mediante la realización de una campaña experimental de modelos a escala de cabezas de anclaje de Polimetil-metacrilato en los que artificialmente se han introducido defectos de diversos tamaños y en distintas posiciones. ABSTRACT Most of the prestressed concrete structures built in the last 50 years have demonstrated an excellent durability when they are constructed in accordance with the rules of good design, detailing and execution. This is particularly true with respect to the feared stress corrosion cracking, which is typical of high strength prestressing steel wires. Less attention, however, has been paid to the stress corrosion cracking susceptibility of anchorages for steel tendons for prestressing concrete, probably due to the low number of reported failure cases. Damage tolerance and fracture mechanics concepts in civil engineering structures have recently started to be incorporated in some design and calculation rules for metallic structures, however it is still far from being assimilated and used by civil engineers in their calculations on a regular basis. This limited knowledge of the damage tolerance basis could lead to significant repair and maintenance costs. This work deals with the applicability of fracture mechanics and damage tolerance concepts to the components of prestressed systems, which are used in civil engineering. Such concepts have been applied to assess the susceptibility of the prestressing steel wires to stress corrosion cracking and the reduction of load bearing capability of anchorage devices due to the presence of defects. For this purpose a combination of experimental work and numerical techniques have been performed. Surface defects in prestressing steel wires are not shown alone, though a certain degree of continuity in the axial direction exist. A significant number of such defects is also observed. Hence a statistical approach was used, which is assumed to be more appropriate than the deterministic approach. The use of statistical methods based in extreme value theories has allowed the characterising of the surface condition of 5.2 mm-diameter wires. On the other hand the stress corrosion cracking susceptibility of the wire has been assessed by means of an experimental testing program in line with the current regulations, which has allowed statistical characterisasion of their performances against stress corrosion cracking. In the light of the test results, it has been possible to evaluate how the surface condition parameters could determine the durability of the active metal armour regarding to its resistance against stress corrosion cracking assessed by means of the current testing regulations. In the case of anchorage devices for steel tendons for prestressing concrete, the damage is presented as point defects originating from dents, scratches or corrosion pits that could be produced during the manufacturing proccess, transport, handling, assembly or use. Due to the nature of these defects, in this case the deterministic approach is more appropriate than the statistical approach. The assessment of the relevancy of defect in a structural component requires the computation of the stress intensity factors, which in turn allow the evaluation of whether the size defect is critical or could become critical with the progress of time (due to fatigue, corrosion or a combination of both effects). In this work the damage is idealised as tiny cracks, a conservative hypothesis. The stress intensity factors have been calculated by means of finite element models of the anchorage representing the real working conditions during its service life. These numeric models were used to assess the impact of some factors on the rupture load of the anchorage, such the anchorage geometry, material, support conditions, defect size, shape and its location. The results from the numerical analysis have been succesfully correlated against the results of the experimental testing program of scaled models of the anchorages in poly-methil methacrylate in which artificial damage in several sizes and locations were introduced.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Engineering of devices and systems such as magnets, fault current limiters or cables, based on High Temperature Superconducting wires requires a deep characterization of the possible degradation of their properties by handling at room temperature as well as during the service life thus establishing the limits for building up functional devices and systems. In the present work we report our study regarding the mechanical behavior of spliced joints between commercial HTS coated conductors based on YBCO at room temperature and service temperature, 77 K. Tensile tests under axial stress and the evolution of the critical current and the electric resistance of the joints have been measured. The complete strain contour for the tape and the joint has been obtained by using Digital Image Correlation. Also, tensile tests under external magnetic field have been performed and the effect of the applied field on the critical current and the electric resistance of the joints has been studied. Finally, a preliminary numerical study by means of Finite Element Method (FEM) of the mechanical behavior of the joints between commercial HTS is presented.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Engineering of devices and systems such as magnets, fault current limiters or cables, based on High Temperature Superconducting wires requires a deep characterization of the possible degradation of their properties by handling at room temperature as well as during the service life thus establishing the limits for building up functional devices and systems. In the present work we report our study regarding the mechanical behavior of spliced joints between commercial HTS coated conductors based on YBCO at room temperature and service temperature, 77 K. Tensile tests under axial stress and the evolution of the critical current and the electric resistance of the joints have been measured. The complete strain contour for the tape and the joints has been obtained by using Digital Image Correlation. Also, tensile tests under external magnetic field have been performed and the effect of the applied field on the critical current and the electric resistance of the joints has been studied. Additionally, fatigue tests under constant cyclic stress and loading-unloading ramps have been carried out in order to evaluate the electromechanical behavior of the joints and the effect of maximum applied stress on the critical current. Finally, a preliminary numerical study by means of the Finite Element Method (FEM) of the electromechanical behavior of the joints between commercial HTS is presented.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Las normativas que regulan la seguridad de las presas en España han recogido la necesidad de conocer los desplazamientos y deformaciones de sus estructuras y cimientos. A día de hoy, son muchas las presas en explotación que no cuentan con un sistema de auscultación adecuado para controlar este tipo de variables, ya que la instalación de métodos clásicos de precisión en las mismas podría no ser viable técnicamente y, de serlo, supondría un coste económico importante y una dudosa garantía del proceso de ejecución de la obra civil correspondiente. Con el desarrollo de las nuevas tecnologías, la informática y las telecomunicaciones, han surgido nuevos sistemas de auscultación de desplazamientos. Los sistemas GPS actuales, diseñados para el control de estructuras, guiado de maquinaria, navegación y topografía, estabilidad de taludes, subsidencias, etc. permiten alcanzar precisiones centimétricas. El sistema de control de movimientos basado en la tecnología DGPS (GPS diferencial) combinada con un filtro estadístico con el que se alcanzan sensibilidades de hasta ±1 mm en el sistema, suficientes para una auscultación normal de presas según los requerimientos de la normativa actual. Esta exactitud se adapta a los desplazamientos radiales de las presas, donde son muy comunes valores de amplitudes en coronación de hasta 15 mm en las de gravedad y de hasta 45 mm en el caso de las presas bóveda o arco. La presente investigación tiene por objetivo analizar la viabilidad del sistema DGPS en el control de movimientos de presas de hormigón comparando los diferentes sistemas de auscultación y su correlación con las variables físicas y las vinculadas al propio sistema GPS diferencial. Ante la necesidad de dar respuesta a estas preguntas y de validar e incorporar a la mencionada tecnología en la ingeniería civil en España, se ha llevado a cabo un estudio de caso en La Aceña (Ávila). Esta es una de las pocas presas españolas que se está controlando con dicha tecnología y de forma simultánea con los sistemas clásicos de auscultación y algunos otros de reciente aplicación La presente investigación se ha organizado con idea de dar respuesta a varias preguntas que el explotador de presas se plantea y que no se analizan en el estado del arte de la técnica: cómo hacer la configuración espacial del sistema y cuáles son los puntos necesarios que se deben controlar, qué sistemas de comunicaciones son los más fiables, cuáles son los costes asociados, calibración del software, vida útil y mantenimientos requeridos, así como la posibilidad de telecontrolar los datos. Entre las ventajas del sistema DGPS, podemos señalar su bajo coste de implantación y posibilidad de controlarlo de forma remota, así como la exactitud y carácter absoluto de los datos. Además, está especialmente indicado para presas aisladas o mal comunicadas y para aquellas otras en las que el explotador no tiene referencia alguna de la magnitud de los desplazamientos o deformaciones propias de la presa en toda su historia. Entre los inconvenientes de cualquier sistema apoyado en las nuevas tecnologías, destaca la importancia de las telecomunicaciones ya sea en el nivel local en la propia presao desde su ubicación hasta el centro de control de la explotación. Con la experiencia alcanzada en la gestión de la seguridad de presas y sobre la base de la reciente implantación de los nuevos métodos de auscultación descritos, se ha podido analizar cada una de sus ventajas e inconvenientes. En el capítulo 5, se presenta una tabla de decisión para el explotador que servirá como punto de partida para futuras inversiones. El impacto de esta investigación se ha visto reflejado en la publicación de varios artículos en revistas indexadas y en el debate suscitado entre gestores y profesionales del sector en los congresos nacionales e internacionales en los que se han presentado resultados preliminares. All regulations on the safety of dams in Spain have collected the need to know the displacements and deformations of the structure and its foundation. Today there are many dams holding not have an adequate system of auscultation to control variables such as the installation of classical methods of precision in the same might not be technically feasible, and if so, would cost important economic and guarantee the implementation process of the dubious civil works. With the development of new technologies, computing and telecommunications, new displacements auscultation systems have emerged. Current GPS systems designed to control structures, machine guidance, navigation and topography, slope stability, subsidence, etc, allow to reach centimeter-level accuracies. The motion control system based on DGPS technology applies a statistical filter that sensitivities are achieved in the system to ± 1 mm, sufficient for normal auscultation of dams as required by current regulations. This accuracy is adapted to the radial displacement of dams, which are common values in coronation amplitudes up to 15 mm in gravity dams and up to 45 mm in arch or arc dams. This research aims to analyze the feasibility of DGPS system in controlling movements of concrete dams, comparing the different systems auscultation and its correlation with physical variables and linked to differential GPS system itself. Given the need to answer this question and to validate and incorporate this technology to civil engineering in Spain, has conducted a case study in real time at the dam La Aceña (Ávila). This dam is one of the few Spanish companies, which are controlling with this technology and simultaneously with the classic auscultation systems and some other recent application. This research has been organized with a view to responding to questions that the dam operator arises and in the state of the art technique not discussed: how to make spatial configuration of the system and what are the necessary control points what communication systems are the most reliable, what are the associated costs, calibration software, service life and maintenance requirements, possibility of monitoring, etc. Among the advantages we can point to its low cost of implementation, the possibility of remote, high accuracy and absolute nature of the data. It could also be suitable for those isolated or poorly communicated dams and those in which the operator has no reference to the magnitude of displacements or deformations own prey in its history. The disadvantages of any system based on the new technologies we highlight the importance of telecommunications, either locally or from this dam control center of the farm. With the experience gained in the management of dam safety and based on the recent introduction of new methods of auscultation described, it has been possible to analyze each of their advantages and disadvantages. A decision table for the operator, which will serve as a starting point for future investments is presented. The impact of research, has been reflected in the publication of several articles in refereed journals and discussion among managers and professionals in national and international conferences in which they participated.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

La durabilidad de las estructuras de hormigón armado no es ilimitada, en especial en determinados ambientes. El ingreso de agentes agresivos en el hormigón, fundamentalmente dióxido de carbono e iones cloruros, rebasando el espesor del recubrimiento y alcanzando las armaduras, reducen el alto pH del hormigón hasta alcanzar un umbral crítico, por debajo del cual, el acero queda despasivado. Posteriormente, si existe el suficiente aporte de humedad y oxígeno, el acero se corroe, lo que supone drásticas reducciones de la vida de servicio de estas estructuras y su inevitable reparación. La utilización de armaduras de acero inoxidable es una alternativa que está recibiendo cada vez más consideración. Su resistencia a la corrosión en los ambientes más agresivos, incluso con ataque de cloruros, lo convierte en el material idóneo para prolongar de forma muy considerable la vida útil de la estructura. En este trabajo se ha evaluado el comportamiento mecánico y estructural, y de resistencia a la corrosión, de un nuevo acero inoxidable dúplex de bajo contenido en níquel, el EN 1.4482 (AISI 2001), y se ha comparado con el inoxidable austenítico más utilizado, el EN 1.4301 (AISI 304), con el dúplex EN 1.4362 (AISI 2304) y con el tradicional acero al carbono B-500-SD. El estudio mecánico y estructural se ha realizado en tres niveles diferentes: a nivel de barra, estudiando las propiedades mecánicas y de ductilidad de los cuatro aceros citados; a nivel de sección, estudiando su comportamiento a flexión con diferentes cuantías de armado por medio de los diagramas momento-curvatura; y a nivel de pieza, ensayando una serie de vigas armadas con diferentes aceros y cuantías, y comprobando su comportamiento a desplazamiento y resistencia por medio de los diagramas carga-desplazamiento. El estudio de resistencia a la corrosión se ha realizado embebiendo barras corrugadas, de los tres aceros inoxidables mencionados, en probetas de mortero contaminadas con diferentes cantidades de cloruros, y realizando mediciones electroquímicas durante un periodo de al menos un año. Se han preparado probetas de mortero para dos comparativas diferentes. La primera, manteniendo las probetas en un desecador con el 95 % de humedad relativa durante todo el periodo de mediciones. La segunda, sumergiendo parcialmente las probetas en una solución tampón para carbonatar el mortero. Los resultados de los ensayos mecánicos han demostrado dos aspectos diferentes. Uno, que las armaduras de acero inoxidable tienen un comportamiento muy similar a las de acero al carbono en lo referente a las resistencias alcanzadas, en el límite elástico y en rotura, pero distinto en cuanto al módulo de deformación longitudinal, cuyo valor es claramente inferior al del acero al carbono, por lo que su utilización en las estructuras de hormigón necesita tener en cuenta ese dato en los análisis lineales de cálculo. El segundo aspecto es que las armaduras de acero inoxidable laminadas en caliente presentan una ductilidad muy superior a las de acero al carbono, por lo que ofrecen una mayor seguridad frente a su rotura o al colapso de la estructura, lo que se debe tener en cuenta en el análisis de cálculo plástico. En cambio, las armaduras de acero inoxidable laminadas en frío sólo cumplen con los límites mínimos de ductilidad establecidos en la instrucción EHE-08 para los aceros soldables, y no para los aceros con características especiales de ductilidad. El estudio a nivel de sección refleja la paradoja de obtener secciones menos dúctiles con las armaduras de acero inoxidable laminadas en caliente que con las armaduras de acero al carbono. Para subsanarlo, se definen los conceptos de curvatura última de rotura y ductilidad de la sección en rotura, que tienen en cuenta las altas deformaciones alcanzadas por las armaduras de acero inoxidable. Los resultados a nivel de pieza permiten identificar el comportamiento estructural del hormigón armado con barras corrugadas de acero inoxidable y compararlo con el de las estructuras de hormigón armado convencionales, verificando los resultados experimentales con los teóricos obtenidos con la formulación recogida en la instrucción EHE- 08. Los ensayos de resistencia a la corrosión por cloruros demuestran, durante el primer año y medio de vida de las probetas, un comportamiento muy similar entre el nuevo acero inoxidable dúplex bajo en níquel y el austenítico y el dúplex utilizados para la comparación, incluso para las probetas carbonatadas. Por último, se añade una comparativa económica, realizada sobre dos edificaciones tipo, para cuantificar el sobrecoste que supone la utilización de armaduras de acero inoxidable respecto a las de acero al carbono. El alto coste inicial de las armaduras de acero inoxidable se ve compensado en el coste final de la estructura de muy diferentes formas, principalmente dependiendo del grado de acero elegido y de si se emplean en el total de la estructura o solamente en los elementos más expuestos. The durability of the concrete structures is limited, especially in certain environments. The attack of aggressive agents in the concrete, mainly carbon dioxide and chloride ions, penetrating the thickness of concrete cover and reaching the reinforcements, reduce the high pH of concrete to the point of reaching a critical threshold, under which, the steel despasivates. Therefore, if there is enough humidity and oxygen, the steel corroes, causing drastic reductions in the service life of these structures and its inevitable repair. Despite the high initial cost compared to carbon steel, the usage of stainless steel reinforcements is an alternative with a major consideration nowadays. Its resistance to corrosion in the most aggressive atmospheres, including chlorides attack, makes the stainless steel a suitable material to extend considerably its lifetime. In this study, it’s been evaluated the mechanical and structural behaviour, and the corrosion resistance, of a new low-nickel duplex stainless steel EN 1.4482 (AISI 2001), and it has been compared with the most widely used austenitic type EN 1.4301 (AISI 304), with duplex steel EN 1.4362 (AISI 2304) and with the traditional carbon steel B-500-SD. The mechanical and structural study has been carried out in three different levels: bar level, studying mechanical properties and ductility of the four steels; section level, studying its behaviour when blending with different amounts of reinforcement through the moment-curvature diagrams; and structural element level, testing a series of reinforced beams with different steels and amounts, and checking its sag and resistance through the load-deflection diagrams. The corrosion resistance study was performed by embedding ribbed bars, using the three stainless steel listed, on mortar specimens contaminated with different amounts of chlorides, and taking electrochemical measurements over a period of at least one year. Mortar specimens have been prepared for two different comparisons. The first, keeping the specimens at 95% of relative humidity during the measurement period. The second, immersing the specimens partially in a carbonate buffer solution. The results of those tests have proved two different aspects. Firstly, that stainless steel reinforcements show a very similar behaviour to carbon steel, according to the reached levels of mechanical resistance, yield stress and steel strength, but a different behaviour in Young’s modulus, which value is clearly lower than the carbon steel. Therefore, when using in concrete structures it is need to consider on that point the existing calculus of linear analysis. The second aspect is that stainless steel reinforcement manufactured by hot-rolling process show a very higher ductility than carbon steel, offering a better security on cracks or structure collapse, which it has to be taken into account on plastic calculus analysis. However, the stainless steel reinfor9 cement cold-rolled bars only meet the minimum thresholds of ductility established by EHE-08 for welded steel, and not for steels with special ductility. The results at the section level reflect the paradox of getting less ductile sections with hot rolled stainless steel reinforcement than with carbon steel reinforcements. To overcome that, the concepts of last break curvature and break ductility section have been defined, which take into account the high deformation value achieved by stainless steel reinforcements. The results at the structural element level allow to identify the structural behaviour of reinforced concrete with stainless steel reinforcements and compared with that of conventional steel reinforcement, contrasting the experimental with the theoretical results obtained from the formulation contained in the instruction EHE-08. Tests on resistance of chloride corrosion show during the first year and a half of specimens life, a similar behaviour between the new low nickel duplex stainless steel and austenitic and duplex used for comparison, even for carbonated specimens. Finally, it has been included an economic comparison on two differents building types, to quantify the additional cost involved on the use of stainless steel reinforcement compared to that of carbon steel. The high initial cost of stainless steel reinforcements is offset in the final cost of the structure in many different ways, mainly depending on the chosen steel grade and whether the reinforcement is used in the total structure or only in risky structural elements.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Corrosion of reinforcing steel in concrete due to chloride ingress is one of the main causes of the deterioration of reinforced concrete structures. Structures most affected by such a corrosion are marine zone buildings and structures exposed to de-icing salts like highways and bridges. Such process is accompanied by an increase in volume of the corrosión products on the rebarsconcrete interface. Depending on the level of oxidation, iron can expand as much as six times its original volume. This increase in volume exerts tensile stresses in the surrounding concrete which result in cracking and spalling of the concrete cover if the concrete tensile strength is exceeded. The mechanism by which steel embedded in concrete corrodes in presence of chloride is the local breakdown of the passive layer formed in the highly alkaline condition of the concrete. It is assumed that corrosion initiates when a critical chloride content reaches the rebar surface. The mathematical formulation idealized the corrosion sequence as a two-stage process: an initiation stage, during which chloride ions penetrate to the reinforcing steel surface and depassivate it, and a propagation stage, in which active corrosion takes place until cracking of the concrete cover has occurred. The aim of this research is to develop computer tools to evaluate the duration of the service life of reinforced concrete structures, considering both the initiation and propagation periods. Such tools must offer a friendly interface to facilitate its use by the researchers even though their background is not in numerical simulation. For the evaluation of the initiation period different tools have been developed: Program TavProbabilidade: provides means to carry out a probability analysis of a chloride ingress model. Such a tool is necessary due to the lack of data and general uncertainties associated with the phenomenon of the chloride diffusion. It differs from the deterministic approach because it computes not just a chloride profile at a certain age, but a range of chloride profiles for each probability or occurrence. Program TavProbabilidade_Fiabilidade: carries out reliability analyses of the initiation period. It takes into account the critical value of the chloride concentration on the steel that causes breakdown of the passive layer and the beginning of the propagation stage. It differs from the deterministic analysis in that it does not predict if the corrosion is going to begin or not, but to quantifies the probability of corrosion initiation. Program TavDif_1D: was created to do a one dimension deterministic analysis of the chloride diffusion process by the finite element method (FEM) which numerically solves Fick’second Law. Despite of the different FEM solver already developed in one dimension, the decision to create a new code (TavDif_1D) was taken because of the need to have a solver with friendly interface for pre- and post-process according to the need of IETCC. An innovative tool was also developed with a systematic method devised to compare the ability of the different 1D models to predict the actual evolution of chloride ingress based on experimental measurements, and also to quantify the degree of agreement of the models with each others. For the evaluation of the entire service life of the structure: a computer program has been developed using finite elements method to do the coupling of both service life periods: initiation and propagation. The program for 2D (TavDif_2D) allows the complementary use of two external programs in a unique friendly interface: • GMSH - an finite element mesh generator and post-processing viewer • OOFEM – a finite element solver. This program (TavDif_2D) is responsible to decide in each time step when and where to start applying the boundary conditions of fracture mechanics module in function of the amount of chloride concentration and corrosion parameters (Icorr, etc). This program is also responsible to verify the presence and the degree of fracture in each element to send the Information of diffusion coefficient variation with the crack width. • GMSH - an finite element mesh generator and post-processing viewer • OOFEM – a finite element solver. The advantages of the FEM with the interface provided by the tool are: • the flexibility to input the data such as material property and boundary conditions as time dependent function. • the flexibility to predict the chloride concentration profile for different geometries. • the possibility to couple chloride diffusion (initiation stage) with chemical and mechanical behavior (propagation stage). The OOFEM code had to be modified to accept temperature, humidity and the time dependent values for the material properties, which is necessary to adequately describe the environmental variations. A 3-D simulation has been performed to simulate the behavior of the beam on both, action of the external load and the internal load caused by the corrosion products, using elements of imbedded fracture in order to plot the curve of the deflection of the central region of the beam versus the external load to compare with the experimental data.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The aim of this paper is to explain the chloride concentration profiles obtained experimentally from control samples of an offshore platform after 25 years of service life. The platform is located 12 km off the coast of the Brazilian province Rio Grande do Norte, in the north-east of Brazil. The samples were extracted at different orientations and heights above mean sea level. A simple model based on Fick’s second law is considered and compared with a finite element model which takes into account transport of chloride ions by diffusion and convection. Results show that convective flows significantly affect the studied chloride penetrations. The convection velocity is obtained by fitting the finite element solution to the experimental data and seems to be directly proportional to the height above mean sea level and also seems to depend on the orientation of the face of the platform. This work shows that considering solely diffusion as transport mechanism does not allow a good prediction of the chloride profiles. Accounting for capillary suction due to moisture gradients permits a better interpretation of the material’s behaviour.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The aim of this paper is to explain the chloride concentration profiles obtained experimentally from control samples of an offshore platform after 25 years of service life. The platform is located 12 km off the coast of the Brazilian province Rio Grande do Norte, in the north-east of Brazil. The samples were extracted at different orientations and heights above mean sea level. A simple model based on Fick’s second law is considered and compared with a finite element model which takes into account transport of chloride ions by diffusion and convection. Results show that convective flows significantly affect the studied chloride penetrations. The convection velocity is obtained by fitting the finite element solution to the experimental data and seems to be directly proportional to the height above mean sea level and also seems to depend on the orientation of the face of the platform. This work shows that considering solely diffusion as transport mechanism does not allow a good prediction of the chloride profiles. Accounting for capillary suction due to moisture gradients permits a better interpretation of the material’s behaviour

Relevância:

80.00% 80.00%

Publicador:

Resumo:

En esta Tesis Doctoral se aborda un tema poco estudiado en el ámbito de los túneles y cuya problemática está basada en los riesgos e incertidumbres que representa el diseño y ejecución de túneles en macizos calizos karstificados. Mediante un estudio profundo del comportamiento de distintos casos reales de túneles en macizos kársticos calizos, aportando la realización de modelos y la experiencia constructiva del autor, se pretende proponer un procedimiento que permita sistematizar las actuaciones, investigación, evaluación y tratamiento en los túneles en karst, como herramienta básica para la toma de decisiones primarias correctas. Además, se proponen herramientas que pueden ayudar a mejorar el diseño y a decidir las medidas más eficientes para afrontar los problemas que genera el karst en los túneles, minimizando los riesgos para todos los actores, su probabilidad e impacto. Se profundiza en tres fases principales (que son referidas en la tesis en cuatro Partes): La INVESTIGACIÓN del macizo rocoso: La investigación engloba todas las actuaciones observacionales encaminadas a obtener el IK (Índice de Karstificación), así como las investigaciones necesarias mediante recopilación de datos superficiales, hidrogeológicos, climáticos, topográficos, así como los datos de investigaciones geofísicas, fotointerpretación, sondeos y ensayos geotécnicos que sean posibles. Mediante la misma, se debe alcanzar un conocimiento suficiente para llevar a cabo la determinación de la Caracterización geomecánica básica del macizo rocoso a distintas profundidades, la determinación del Modelo o modo de karstificación del macizo rocoso respecto al túnel y la Zonificación del índice de karstificación en el ámbito de actuación en el que se implantará el túnel. En esta primera fase es necesaria la correcta Definición geométrica y trazado de la obra subterránea: En función de las necesidades que plantee el proyecto y de los condicionantes externos de la infraestructura, se deben establecer los requisitos mínimos de gálibo necesarios, así como las condiciones de máximas pendientes para el trazado en alzado y los radios mínimos de las curvas en planta, en función del procedimiento constructivo y motivación de construcción del túnel (ferrocarril, carretera o hidráulico, etc...). Estas son decisiones estratégicas o primerias para las que se ha de contar con un criterio y datos adecuados. En esta fase, son importantes las decisiones en cuanto a las monteras o profundidades relativas a la karstificación dominante e investigación de las tensiones naturales del macizo, tectónica, así como las dimensiones del túnel en función de las cavidades previstas, tratamientos, proceso de excavación y explotación. En esta decisión se debe definir, conocida ya de forma parcial la geotecnia básica, el procedimiento de excavación en función de las longitudes del túnel y la clasificación geomecánica del terreno, así como sus monteras mínimas, accesos y condicionantes medioambientales, pero también en función de la hidrogeología. Se establecerá la afección esperable en el túnel, identificando en la sectorización del túnel, la afección esperable de forma general para las secciones pésimas del túnel. Con todos estos datos, en esta primera aproximación, es posible realizar el inventario de casos posibles a lo largo del trazado, para poder, posteriormente, minimizar el número de casos con mayores riesgos (técnicos, temporales o económicos) que requieran de tratamiento. Para la fase de EVALUACIÓN de la matriz de casos posibles en función del trazado inicial escogido (que puede estar ya impuesto por el proyecto, si no se ha podido intervenir en dicha fase), es necesario valorar el comportamiento teórico del túnel en toda su longitud, estudiando las secciones concretas según el tipo y el modo de afección (CASOS) y todo ello en función de los resultados de los estudios realizados en otros túneles. Se debe evaluar el riesgo para cada uno de los casos en función de las longitudes de túnel que se esperan que sean afectadas y el proceso constructivo y de excavación que se vaya a adoptar, a veces varios. Es importante tener en cuenta la existencia o no de agua o relleno arcilloso o incluso heterogéneo en las cavidades, ya que los riesgos se multiplican, así mismo se tendrá en cuenta la estabilidad del frente y del perímetro del túnel. En esta segunda fase se concluirá una nueva matriz con los resultados de los riesgos para cada uno de los casos que se presentarán en el túnel estudiado. El TRATAMIENTO, que se debe proponer al mismo tiempo que una serie de actuaciones para cada uno de los casos (combinación de tipos y modos de afección), debiendo evaluar la eficacia y eficiencia, es decir la relevancia técnica y económica, y como se pueden optimizar los tratamientos. Si la tabla de riesgos que se debe generar de nuevo introduciendo los factores técnicos y económicos no resulta aceptable, será necesaria la reconsideración de los parámetros determinados en fases anteriores. Todo el desarrollo de estas tres etapas se ha recogido en 4 partes, en la primera parte se establece un método de estudio e interpretativo de las investigaciones superficiales y geotécnicas, denominado índice de karstificación. En la segunda parte, se estudia la afección a las obras subterráneas, modelos y tipos de afección, desde un punto de vista teórico. La tercera parte trata de una recopilación de casos reales y las consecuencias extraídas de ellos. Y finalmente, la cuarta parte establece los tratamientos y actuaciones para el diseño y ejecución de túneles en macizos kársticos calizos. Las novedades más importantes que presenta este trabajo son: El estudio de los casos de túneles realizados en karst calizo. Propuesta de los tratamientos más efectivos en casos generales. La evaluación de riesgos en función de las tipologías de túnel y afecciones en casos generales. La propuesta de investigación superficial mediante el índice de karstificación observacional. La evaluación mediante modelos del comportamiento teórico de los túneles en karst para casos muy generales de la influencia de la forma, profundidad y desarrollo de la karstificación. In this doctoral thesis is studied the recommended investigation, evaluation and treatment when a tunnel is planed and constructed in karstic calcareous rock masses. Calcareous rock masses were selected only because the slow disolution produces stable conduct and caves instead the problems of sudden disolutions. Karstification index (IK) that encompasses various aspects of research karstic rock mass is presented. The karst rock masses are all unique and there are no similarities between them in size or density cavities ducts, but both their formation mechanisms, like, geological and hydrogeological geomorphological evidence allow us, through a geomechanical survey and geological-photo interpretation in the surface, establish a karst evaluation index specific for tunnelling, which allows us to set a ranking of the intensity of karstification and the associated stadistic to find caves and its risk in tunnelling. This index is estimated and useful for decision-making and evaluation of measures to be considered in the design of a tunnel and is set in degrees from 0 to 100, with similar to the RMR degrees. The sectorization of the tunnel section and the types of condition proposed in this thesis, are estimated also useful to understand the different effects that interception of ducts and cavities may have in the tunnel during construction and service life. Simplified calculations using two-dimensional models contained in the thesis, have been done to establish the relationship between the position of the cavities relative to the section of the tunnel and its size in relation to the safety factors for each ground conditions, cover and natural stresses. Study of over 100 cases of tunnels that have intercepted cavities or karst conduits have been used in this thesis and the list of risks found in these tunnels have been related as well. The most common and effective treatments are listed and finally associated to the models and type of affection generated to give the proper tool to help in the critical decision when the tunnels intercept cavities. Some existing studies from Marinos have been considered for this document. The structure of the thesis is mainly divided 4 parts included in 3 steps: The investigation, the evaluation and the treatments, which match with the main steps needed for the critical decisions to be made during the design and construction of tunnels in karstic rockmasses, very important to get a successfully project done.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Los sismos afectan a las estructuras en función de su intensidad. Normalmente se espera de las estructuras daños irreparables por motivos de ductilidad en los sismos nominales o de diseño, para protección de las personas y sus bienes. No obstante, las estructuras en zonas sísmicas sufren terremotos de baja o media intensidad de manera continuada y éstos pueden afectar a la capacidad resistente residual de las mismas, es por eso que en el presente trabajo se plantea lo siguiente: a) Identificar cuál es la estrategia o nivel de protección, que consideran las diferentes Normativas y Reglamentos frente a sismos de baja o mediana intensidad, puesto que durante la vida útil de una estructura, esta puede verse afectada por sismos de intensidad baja o moderada, los cuales también provocan daños; es por ello que es de mucha importancia conocer y estudiar el aporte, estrategias y demás parámetros que consideran las Normas, esto mediante la técnica de revisión de documentación o Literatura. b) Identificar la manera con que un terremoto de baja o media intensidad afecta a la capacidad resistente de las estructuras, sus señales, sus síntomas de daño, etc. Esto a través de tres técnicas de Investigación : Revisión en Literatura, Tormenta de ideas con un grupo de expertos en el tema, y mediante la Técnica Delphi; para finalmente aplicar una método de refinamiento para elaborar un listado y un mapa de síntomas esperables en las estructuras, consecuencia de eventos sísmicos de baja o mediana intensidad. Los cuales se podrían controlar con sistemas inteligentes y así monitorizar las construcciones para prever su comportamiento futuro. Earthquakes affect structures depending on its intensity. Normally it expected of the irreparable damage structures. It due to ductility in nominal earthquakes to protect people and property. Structures in seismic areas suffer earthquakes of low to medium intensity continually, and it may affect the residual resistant ability, therefore posed in this investigation is the following: (a) Identifying what is the strategy or level of protection, which consider different guidelines and regulations against earthquakes of low to medium intensity. Since during the service life of a structure may be affected by low or moderate intensity earthquakes, which also cause damage. For this reason it is very important also to meet and study the contribution, strategies and other parameters considered by the Guidelines by reviewing the documentation or literature technique. b) Identifying the way an earthquake of low to medium intensity affects the resistant ability of structures, their signs, their symptoms of injury, etc. Through three research techniques: review of documentation or literature, brainstorming technique with a group of experts, and using the Delphi technique. Finally applying a method of refining to produce a list and a map of symptoms expected in structures, consequence of low to medium intensity earthquakes. It could be controlled with intelligent systems and thus to monitor structures to predict its future behavior

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Arch bridge structural solution has been known for centuries, in fact the simple nature of arch that require low tension and shear strength was an advantage as the simple materials like stone and brick were the only option back in ancient centuries. By the pass of time especially after industrial revolution, the new materials were adopted in construction of arch bridges to reach longer spans. Nowadays one long span arch bridge is made of steel, concrete or combination of these two as "CFST", as the result of using these high strength materials, very long spans can be achieved. The current record for longest arch belongs to Chaotianmen bridge over Yangtze river in China with 552 meters span made of steel and the longest reinforced concrete type is Wanxian bridge which also cross the Yangtze river through a 420 meters span. Today the designer is no longer limited by span length as long as arch bridge is the most applicable solution among other approaches, i.e. cable stayed and suspended bridges are more reasonable if very long span is desired. Like any super structure, the economical and architectural aspects in construction of a bridge is extremely important, in other words, as a narrower bridge has better appearance, it also require smaller volume of material which make the design more economical. Design of such bridge, beside the high strength materials, requires precise structural analysis approaches capable of integrating the combination of material behaviour and complex geometry of structure and various types of loads which may be applied to bridge during its service life. Depend on the design strategy, analysis may only evaluates the linear elastic behaviour of structure or consider the nonlinear properties as well. Although most of structures in the past were designed to act in their elastic range, the rapid increase in computational capacity allow us to consider different sources of nonlinearities in order to achieve a more realistic evaluations where the dynamic behaviour of bridge is important especially in seismic zones where large movements may occur or structure experience P - _ effect during the earthquake. The above mentioned type of analysis is computationally expensive and very time consuming. In recent years, several methods were proposed in order to resolve this problem. Discussion of recent developments on these methods and their application on long span concrete arch bridges is the main goal of this research. Accordingly available long span concrete arch bridges have been studied to gather the critical information about their geometrical aspects and properties of their materials. Based on concluded information, several concrete arch bridges were designed for further studies. The main span of these bridges range from 100 to 400 meters. The Structural analysis methods implemented in in this study are as following: Elastic Analysis: Direct Response History Analysis (DRHA): This method solves the direct equation of motion over time history of applied acceleration or imposed load in linear elastic range. Modal Response History Analysis (MRHA): Similar to DRHA, this method is also based on time history, but the equation of motion is simplified to single degree of freedom system and calculates the response of each mode independently. Performing this analysis require less time than DRHA. Modal Response Spectrum Analysis (MRSA): As it is obvious from its name, this method calculates the peak response of structure for each mode and combine them using modal combination rules based on the introduced spectra of ground motion. This method is expected to be fastest among Elastic analysis. Inelastic Analysis: Nonlinear Response History Analysis (NL-RHA): The most accurate strategy to address significant nonlinearities in structural dynamics is undoubtedly the nonlinear response history analysis which is similar to DRHA but extended to inelastic range by updating the stiffness matrix for every iteration. This onerous task, clearly increase the computational cost especially for unsymmetrical buildings that requires to be analyzed in a full 3D model for taking the torsional effects in to consideration. Modal Pushover Analysis (MPA): The Modal Pushover Analysis is basically the MRHA but extended to inelastic stage. After all, the MRHA cannot solve the system of dynamics because the resisting force fs(u; u_ ) is unknown for inelastic stage. The solution of MPA for this obstacle is using the previously recorded fs to evaluate system of dynamics. Extended Modal Pushover Analysis (EMPA): Expanded Modal pushover is a one of very recent proposed methods which evaluates response of structure under multi-directional excitation using the modal pushover analysis strategy. In one specific mode,the original pushover neglect the contribution of the directions different than characteristic one, this is reasonable in regular symmetric building but a structure with complex shape like long span arch bridges may go through strong modal coupling. This method intend to consider modal coupling while it take same time of computation as MPA. Coupled Nonlinear Static Pushover Analysis (CNSP): The EMPA includes the contribution of non-characteristic direction to the formal MPA procedure. However the static pushovers in EMPA are performed individually for every mode, accordingly the resulted values from different modes can be combined but this is only valid in elastic phase; as soon as any element in structure starts yielding the neutral axis of that section is no longer fixed for both response during the earthquake, meaning the longitudinal deflection unavoidably affect the transverse one or vice versa. To overcome this drawback, the CNSP suggests executing pushover analysis for governing modes of each direction at the same time. This strategy is estimated to be more accurate than MPA and EMPA, moreover the calculation time is reduced because only one pushover analysis is required. Regardless of the strategy, the accuracy of structural analysis is highly dependent on modelling and numerical integration approaches used in evaluation of each method. Therefore the widely used Finite Element Method is implemented in process of all analysis performed in this research. In order to address the study, chapter 2, starts with gathered information about constructed long span arch bridges, this chapter continuous with geometrical and material definition of new models. Chapter 3 provides the detailed information about structural analysis strategies; furthermore the step by step description of procedure of all methods is available in Appendix A. The document ends with the description of results and conclusion of chapter 4.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

La presente tesis doctoral surge ante la necesidad de completar el estudio sobre la corrosión en el hormigón armado expuesto al ambiente marino iniciado por D. Miguel Ángel Bermúdez Odriozola en 2007 con la tesis doctoral con título “Corrosión de las armaduras del hormigón armado en ambiente marino: zona de carrera de mareas y zona sumergida”. Una vez realizado el estudio bibliográfico, se ha planteado un estudio experimental en el que se analizan cuatro muelles de distintas edades y localizados en distintos lugares de la geografía española. Uno de ellos contiene adiciones en el hormigón. Una vez inspeccionados, se extraen testigos de cada uno de ellos con el fin de realizar ensayos de caracterización y se analizan sus resultados en paralelo con los coeficientes de difusión. Uno se los objetivos ha sido comprobar el mejor método de ensayo que permita controlar la durabilidad del hormigón en ambiente IIIa. La tesis que se presenta ha demostrado la efectividad del ensayo de penetración de agua para discriminar los hormigones que presentarán un buen comportamiento frente a la difusión de cloruros y por tanto para predecir la vida útil de la estructura. Asimismo, otro objetivo ha sido valorar el uso de adiciones en el hormigón y cómo afectan a la mejora del comportamiento del hormigón expuesto al ambiente marino. Se han obtenido valores del coeficiente de eficacia de cenizas volantes y humo de sílice frente a la difusión de cloruros, muy superiores a los actualmente considerados en términos de resistencia. El ambiente marino aéreo engloba estructuras situadas en primera línea de costa así como aquellas que se sitúan hasta 5km de distancia de la línea del mar. La investigación realizada ha demostrado la necesidad de establecer una nueva subdivisión en este ambiente introduciendo la zona Spray, siguiendo criterios internacionales, que permita diferenciar la zona más desfavorable del mismo que comprende las estructuras ubicadas sobre el nivel del mar tal como los tableros de pantalanes portuarios estudiados. Se han analizado en profundidad los valores del contenido de cloruros en superficie de hormigón en los diferentes tipos de ambiente marino recogidos por la Instrucción EHE- 08 contrastando los requisitos normativos. Como conclusión se han hecho nuevas propuestas normativas que afectan al ambiente sumergido y al ambiente marino aéreo (zona spray). Asimismo se ha realizado un análisis en profundidad de la concentración crítica de cloruros recogida por la Instrucción EHE-08, a partir de los datos obtenidos en estructuras reales. Se ha evaluado el ensayo de resistividad para estimar el valor del coeficiente de difusión de cloruros. Este ensayo ha demostrado su efectividad para discriminar hormigones con adiciones y con muy baja penetración de agua, si bien no resulta sensible para detectar hormigones con elevada permeabilidad. Finalmente en la tesis se ha obtenido un modelo de difusión de cloruros (a/c-D) en ambiente marino aéreo a fin de poder estimar la difusión de cloruros en el hormigón a partir de un requisito normativo como es la relación a/c. This Thesis is focussed to complete the previous study on the corrosion of reinforced concrete exposed to marine environment, carried out by Dr. Miguel Ángel Bermúdez Odrizola in 2007. That Thesis title was “Corrosion of concrete reinforcement located in marine environment: tidal zone and submerged zone”. After the literature review presented in the State of the Art, an experimental programme was carried out. Four docks of different ages and locations have been studied, one of them was a fly ash concrete. The structures were inspected on site and several cores extracted in order to develop characterization tests and obtain diffusion profiles at the laboratory. One of the objectives has been to check the best laboratory test method to control concrete durability when exposed to atmospheric marine environment. This Thesis has proven the effectiveness of the water penetration test to differentiate concretes well behaved against chloride diffusion and also to predict the structure service life. Another objective has been to study the effect of mineral additions in concrete and how they improve the durability of concrete in this environment. Efficiency factors have been obtained for fly ashes and silica fume, much higher than those consider for strength. According to the Spanish Concrete Code EHE 08, the atmospheric marine environment includes structures located at the cost, from the sea line up to 5km inland. The research conducted has shown the need to consider a spray zone which is the most unfavourable area of the atmospheric environment, affecting structures over the sea level as the decks of the wharves here studied. Surface chloride contents of structures in the different marine environments have been deeply analysed, checking the actual standard limits. As a conclusion, new normative values have been proposed for submerged and atmospheric zone (spray zone). A complete analysis of the chloride threshold concentration from the data obtained in real structures has also been performed. It has been evaluated the resistivity test as a tool to estimate the chloride diffusion coefficient. This test has proven effectiveness to discriminate concrete with mineral additions and low water penetration values, while it is not sensitive to detect concretes with high permeability. Finally, a chloride diffusion model (w/c) has been obtained in atmospheric marine environment in order to estimate the chloride diffusion of the concrete knowing a normative requirement as w/c.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

El desarrollo de nuevas estructuras aeroespaciales optimizadas, utilizan materiales compuestos, para los componentes críticos y subsistemas, principalmente polímeros reforzados con fibra de carbono (CFRP). Un conocimiento profundo del estado de daño por fatiga de estructuras de CFRP avanzado, es esencial para predecir la vida residual y optimizar los intervalos de inspección estructural, reparaciones y/o sustitución de componentes. Las técnicas actuales se basan principalmente en la medición de cargas estructurales a lo largo de la vida útil de la estructura mediante galgas extensométricas eléctricas. Con esos datos, se estima la vida a fatiga utilizando modelos de acumulación de daño. En la presente tesis, se evalúa la metodología convencional para la estimación de la vida a fatiga de un CFRP aeronáutico. Esta metodología está basada en la regla de acumulación de daño lineal de Palmgren-Miner, y es aplicada para determinar la vida a fatiga de estructuras sometidas a cargas de amplitud variable. Se ha realizado una campaña de ensayos con cargas de amplitud constante para caracterizar un CFRP aeronáutico a fatiga, obteniendo las curvas clásicas S-N, en diferentes relaciones de esfuerzo. Se determinaron los diagramas de vida constante, (CLD), también conocidos como diagramas de Goodman, utilizando redes neuronales artificiales debido a la ausencia de modelos coherentes para materiales compuestos. Se ha caracterizado la degradación de la rigidez debido al daño por fatiga. Se ha ensayado un segundo grupo de probetas con secuencias estandarizadas de cargas de amplitud variable, para obtener la vida a fatiga y la degradación de rigidez en condiciones realistas. Las cargas aplicadas son representativas de misiones de aviones de combate (Falstaff), y de aviones de transporte (Twist). La vida a fatiga de las probetas cicladas con cargas de amplitud variable, se comparó con el índice de daño teórico calculado en base a la regla de acumulación de daño lineal convencional. Los resultados obtenidos muestran predicciones no conservativas. Esta tesis también presenta el estudio y desarrollo, de una nueva técnica de no contacto para evaluar el estado de daño por fatiga de estructuras de CFRP por medio de cambios de los parámetros de rugosidad. La rugosidad superficial se puede medir fácilmente en campo con métodos sin contacto, mediante técnicas ópticas tales como speckle y perfilómetros ópticos. En el presente estudio, se han medido parámetros de rugosidad superficial, y el factor de irregularidad de la superficie, a lo largo de la vida de las probetas cicladas con cargas de amplitud constante y variable, Se ha obtenido una buena tendencia de ajuste al correlacionar la magnitud de la rugosidad y el factor de irregularidad de la superficie con la degradación de la rigidez de las probetas fatigadas. Estos resultados sugieren que los cambios en la rugosidad superficial medida en zonas estratégicas de componentes y estructuras hechas de CFRP, podrían ser indicativas del nivel de daño interno debido a cargas de fatiga. Los resultados también sugieren que el método es independiente del tipo de carga de fatiga que ha causado el daño. Esto último hace que esta técnica de medición sea aplicable como inspección para una amplia gama de estructuras de materiales compuestos, desde tanques presurizados con cargas de amplitud constante, estructuras aeronáuticas como alas y colas de aeronaves cicladas con cargas de amplitud variable, hasta aplicaciones industriales como automoción, entre otros. ABSTRACT New optimized aerospace structures use composite materials, mainly carbon fiber reinforced polymer composite (CFRP), for critical components and subsystems. A strong knowledge of the fatigue state of highly advanced (CFRP) structures is essential to predict the residual life and optimize intervals of structural inspection, repairs, and/or replacements. Current techniques are based mostly on measurement of structural loads throughout the service life by electric strain gauge sensors. These sensors are affected by extreme environmental conditions and by fatigue loads in such a way that the sensors and their systems require exhaustive maintenance throughout system life. In the present thesis, the conventional methodology based on linear damage accumulation rules, applied to determine the fatigue life of structures subjected to variable amplitude loads was evaluated for an aeronautical CFRP. A test program with constant amplitude loads has been performed to obtain the classical S-N curves at different stress ratios. Constant life diagrams, CLDs, where determined by means of Artificial Neural Networks due to the absence of consistent models for composites. The stiffness degradation due to fatigue damage has been characterized for coupons under cyclic tensile loads. A second group of coupons have been tested until failure with a standardized sequence of variable amplitude loads, representative of missions for combat aircraft (Falstaff), and representative of commercial flights (Twist), to obtain the fatigue life and the stiffness degradation under realistic conditions. The fatigue life of the coupons cycled with variable amplitude loads were compared to the theoretical damage index calculated based on the conventional linear damage accumulation rule. The obtained results show non-conservative predictions. This thesis also presents the evaluation of a new non-contact technique to evaluate the fatigue damage state of CFRP structures by means of measuring roughness parameters to evaluate changes in the surface topography. Surface roughness can be measured easily on field with non-contact methods by optical techniques such as speckle and optical perfilometers. In the present study, surface roughness parameters, and the surface irregularity factor, have been measured along the life of the coupons cycled with constant and variable amplitude loads of different magnitude. A good agreement has been obtained when correlating the magnitude of the roughness and the surface irregularity factor with the stiffness degradation. These results suggest that the changes on the surface roughness measured in strategic zones of components and structures made of CFRP, could be indicative of the level of internal damage due to fatigue loads. The results also suggest that the method is independent of the type of fatigue load that have caused the damage. It makes this measurement technique applicable for a wide range of inspections of composite materials structures, from pressurized tanks with constant amplitude loads, to variable amplitude loaded aeronautical structures like wings and empennages, up to automotive and other industrial applications.