35 resultados para Readout durability
em Universidad Politécnica de Madrid
Resumo:
Experimental research has been performed to relate specific cement characteristics to deterioration due to sulfate and sea water attack after five year exposure, and to study different test method suitability for sulfate and marine resistance. Sulfate resistance testing have been performed on mortar specimens made with fifteen cement types of statistically diverse chemical composition according to European standard EN 197-1, most of them with sulfate resistant properties according to Spanish regulations. Chemical and mechanical characteristics were studied to determine the variation in properties of selected cements. SO3 content, type and amount of additions, C3A, and C4AF content were used to examine relationships between these characteristics and the results of sulfate resistance. Mortar specimens testing using Na2SO4 as the aggressive medium according to ASTM 1012 (with w/c ratio adapted to prENV 196-X:1995) was performed using each type of cement; identical specimens were also stored in sea water, and in lime saturated water (blank condition), up to five year age. Additionally these cements were tested conforming ASTM 452 and Koch and Steinegger test. Recommended acceptance limits for sulfate resistance of cements concerning to each used test method were evaluated in order to explore their suitability. Relationships between cement characteristics, degradation, expansive products obtained by X-ray diffraction techniques and maximum expansion after applied storage treatments, were correlated at final age, to redefine cement characteristics for sulfate resistant and marine resistant Portland cement
Resumo:
Residual stresses developed during wire drawing influence the mechanical behavior and durability of steel wires used for prestressed concrete structures, particularly the shape of the stress–strain curve, stress relaxation losses, fatigue life, and environmental cracking susceptibility. The availability of general purpose finite element analysis tools and powerful diffraction techniques (X-rays and neutrons) has made it possible to predict and measure accurately residual stress fields in cold-drawn steel wires. Work carried out in this field in the past decade, shows the prospects and limitations of residual stress measurement, how the stress relaxation losses and environmentally-assisted cracking are correlated with the profile of residual stresses and how the performance of steel wires can be improved by modifying such a stress profile
Resumo:
In many university courses such as Building Engineering or Technical Architectural, the high density of the contents included in the curriculum, make the student, after graduation, unable to develop the skills already acquired and evaluated in the disciplines of the first courses. From the Group of Educational Innovation at the Polytechnic University of Madrid (UPM) "Teaching of Structural Concrete" (GIEHE) we have conducted a study in which are valued specific skills acquired by students after the first courses of career. We have worked with students from UPM fourth-year career and with Technical Architecture students who have completed their studies and also have completed the Adaptation Course of Technical Architecture to the Building Engineer. The work is part of the Educational Innovation Project funded by the UPM "Integration of training and assessment of generic and specific skills in structural concrete" We have evaluated specific skills learned in the areas of durability and control of structural concrete structures. The results show that overall, students are not able to fully develop the skills already acquired earlier, even being these essential to their professional development. Possibly, the large amount of content taught in these degrees together with a teaching and assessment of "flat profile", ie, which are presented and evaluated with the same intensity as the fundamental and the accessory, are causes enough to cause these results.
Resumo:
Several dielectric fluids that might be used for immersing optics are analyzed in this paper. Their transmittances, both before and after an accelerated exposure to ultraviolet (UV) radiation equivalent to several years under real sun, are presented. In addition, the photocurrent losses caused by the decrease in transmittance experienced by each fluid are estimated for current III?V multijunction (MJ) solar cells. The most stable fluids were found to be paraffin and silicone oils whose transmittances remained practically unaltered after a UV dosage equivalent to 3 years of AM1.5D radiation.
Resumo:
A special Working Group, to study and develop standars related to Building Restoration, Rehabilitation and Maintenance, was formed in January 2001 in AENOR (Spanish Association for Codes and Standars) under the management of the Department of Building Construction of the School of Architecture of Madrid (DCTA-UPM). Three groups were organized to deal with different topics: Diagnosis, Techiques and Materials, and Maintenance. In this paper the differents topics in which the Diagnosis Subgroup is working are described: historical studies, constructive description of the building and building pathology. These will be basic to carry out a correct diagnosis of any type of building, whether it is historic or not. In the development of such topics, the recognizable architectural values are justified as they are prior to the diagnosis stage. As an example of the subgroup work, several pathology cards are shown which include: longitudinal cracks of mechanical origin in beams of concrete structures, façade closings and claddings, and general symptoms of installation services.
Resumo:
La fisuración iniciada en la superficie de los pavimentos asfálticos constituye uno de los más frecuentes e importantes modos de deterioro que tienen lugar en los firmes bituminosos, como han demostrado los estudios teóricos y experimentales llevados a cabo en la última década. Sin embargo, este mecanismo de fallo no ha sido considerado por los métodos tradicionales de diseño de estos firmes. El concepto de firmes de larga duración se fundamenta en un adecuado seguimiento del proceso de avance en profundidad de estos deterioros y la intervención en el momento más apropiado para conseguir mantenerlos confinados como fisuras de profundidad parcial en la capa superficial más fácilmente accesible y reparable, de manera que pueda prolongarse la durabilidad y funcionalidad del firme y reducir los costes generalizados de su ciclo de vida. Por lo tanto, para la selección de la estrategia óptima de conservación de los firmes resulta esencial disponer de metodologías que posibiliten la identificación precisa in situ de la fisuración descendente, su seguimiento y control, y que además permitan una determinación fiable y con alto rendimiento de su profundidad y extensión. En esta Tesis Doctoral se presentan los resultados obtenidos mediante la investigación sistemática de laboratorio e in situ llevada a cabo para la obtención de datos sobre fisuración descendente en firmes asfálticos y para el estudio de procedimientos de evaluación de la profundidad de este tipo de fisuras empleando técnicas de ultrasonidos. Dichos resultados han permitido comprobar que la metodología no destructiva propuesta, de rápida ejecución, bajo coste y sencilla implementación (principalmente empleada hasta el momento en estructuras metálicas y de hormigón, debido a las dificultades que introduce la naturaleza viscoelástica de los materiales bituminosos) puede ser aplicada con suficiente fiabilidad y repetibilidad sobre firmes asfálticos. Las medidas resultan asimismo independientes del espesor total del firme. Además, permite resolver algunos de los inconvenientes frecuentes que presentan otros métodos de diagnóstico de las fisuras de pavimentos, tales como la extracción de testigos (sistema destructivo, de alto coste y prolongados tiempos de interrupción del tráfico) o algunas otras técnicas no destructivas como las basadas en medidas de deflexiones o el georradar, las cuales no resultan suficientemente precisas para la investigación de fisuras superficiales. Para ello se han realizado varias campañas de ensayos sobre probetas de laboratorio en las que se han estudiado diferentes condiciones empíricas como, por ejemplo, distintos tipos de mezclas bituminosas en caliente (AC, SMA y PA), espesores de firme y adherencias entre capas, temperaturas, texturas superficiales, materiales de relleno y agua en el interior de las grietas, posición de los sensores y un amplio rango de posibles profundidades de fisura. Los métodos empleados se basan en la realización de varias medidas de velocidad o de tiempo de transmisión del pulso ultrasónico sobre una única cara o superficie accesible del material, de manera que resulte posible obtener un coeficiente de transmisión de la señal (mediciones relativas o autocompensadas). Las mediciones se han realizado a bajas frecuencias de excitación mediante dos equipos de ultrasonidos diferentes dotados, en un caso, de transductores de contacto puntual seco (DPC) y siendo en el otro instrumento de contacto plano a través de un material especialmente seleccionado para el acoplamiento (CPC). Ello ha permitido superar algunos de los tradicionales inconvenientes que presenta el uso de los transductores convencionales y no precisar preparación previa de las superficies. La técnica de autocalibración empleada elimina los errores sistemáticos y la necesidad de una calibración local previa, demostrando el potencial de esta tecnología. Los resultados experimentales han sido comparados con modelos teóricos simplificados que simulan la propagación de las ondas ultrasónicas en estos materiales bituminosos fisurados, los cuales han sido deducidos previamente mediante un planteamiento analítico y han permitido la correcta interpretación de dichos datos empíricos. Posteriormente, estos modelos se han calibrado mediante los resultados de laboratorio, proporcionándose sus expresiones matemáticas generalizadas y gráficas para su uso rutinario en las aplicaciones prácticas. Mediante los ensayos con ultrasonidos efectuados en campañas llevadas a cabo in situ, acompañados de la extracción de testigos del firme, se han podido evaluar los modelos propuestos. El máximo error relativo promedio en la estimación de la profundidad de las fisuras al aplicar dichos modelos no ha superado el 13%, con un nivel de confianza del 95%, en el conjunto de todos los ensayos realizados. La comprobación in situ de los modelos ha permitido establecer los criterios y las necesarias recomendaciones para su utilización sobre firmes en servicio. La experiencia obtenida posibilita la integración de esta metodología entre las técnicas de auscultación para la gestión de su conservación. Abstract Surface-initiated cracking of asphalt pavements constitutes one of the most frequent and important types of distress that occur in flexible bituminous pavements, as clearly has been demonstrated in the technical and experimental studies done over the past decade. However, this failure mechanism has not been taken into consideration for traditional methods of flexible pavement design. The concept of long-lasting pavements is based on adequate monitoring of the depth and extent of these deteriorations and on intervention at the most appropriate moment so as to contain them in the surface layer in the form of easily-accessible and repairable partial-depth topdown cracks, thereby prolonging the durability and serviceability of the pavement and reducing the overall cost of its life cycle. Therefore, to select the optimal maintenance strategy for perpetual pavements, it becomes essential to have access to methodologies that enable precise on-site identification, monitoring and control of top-down propagated cracks and that also permit a reliable, high-performance determination of the extent and depth of cracking. This PhD Thesis presents the results of systematic laboratory and in situ research carried out to obtain information about top-down cracking in asphalt pavements and to study methods of depth evaluation of this type of cracking using ultrasonic techniques. These results have demonstrated that the proposed non-destructive methodology –cost-effective, fast and easy-to-implement– (mainly used to date for concrete and metal structures, due to the difficulties caused by the viscoelastic nature of bituminous materials) can be applied with sufficient reliability and repeatability to asphalt pavements. Measurements are also independent of the asphalt thickness. Furthermore, it resolves some of the common inconveniences presented by other methods used to evaluate pavement cracking, such as core extraction (a destructive and expensive procedure that requires prolonged traffic interruptions) and other non-destructive techniques, such as those based on deflection measurements or ground-penetrating radar, which are not sufficiently precise to measure surface cracks. To obtain these results, extensive tests were performed on laboratory specimens. Different empirical conditions were studied, such as various types of hot bituminous mixtures (AC, SMA and PA), differing thicknesses of asphalt and adhesions between layers, varied temperatures, surface textures, filling materials and water within the crack, different sensor positions, as well as an ample range of possible crack depths. The methods employed in the study are based on a series of measurements of ultrasonic pulse velocities or transmission times over a single accessible side or surface of the material that make it possible to obtain a signal transmission coefficient (relative or auto-calibrated readings). Measurements were taken at low frequencies by two short-pulse ultrasonic devices: one equipped with dry point contact transducers (DPC) and the other with flat contact transducers that require a specially-selected coupling material (CPC). In this way, some of the traditional inconveniences presented by the use of conventional transducers were overcome and a prior preparation of the surfaces was not required. The auto-compensating technique eliminated systematic errors and the need for previous local calibration, demonstrating the potential for this technology. The experimental results have been compared with simplified theoretical models that simulate ultrasonic wave propagation in cracked bituminous materials, which had been previously deduced using an analytical approach and have permitted the correct interpretation of the aforementioned empirical results. These models were subsequently calibrated using the laboratory results, providing generalized mathematical expressions and graphics for routine use in practical applications. Through a series of on-site ultrasound test campaigns, accompanied by asphalt core extraction, it was possible to evaluate the proposed models, with differences between predicted crack depths and those measured in situ lower than 13% (with a confidence level of 95%). Thereby, the criteria and the necessary recommendations for their implementation on in-service asphalt pavements have been established. The experience obtained through this study makes it possible to integrate this methodology into the evaluation techniques for pavement management systems.
Resumo:
Los paneles sándwich de madera son un producto de creciente aplicación en la edificación de nuestro país. Este ascendente uso del material debe estar acompañado de las garantías necesarias avaladas por un estudio previo de sus prestaciones. Como es preceptivo y entre otros, se evalúa su durabilidad frente a las condiciones climatológicas, clave en los productos derivados de la madera, acorde a la normativa actual definida con tal fin, la Guía ETAG 016. Sin embargo, debido a la clase de uso del material, se ha detectado que dicha normativa tal y como está concebida no es capaz de valorar su envejecimiento adecuadamente. En este trabajo se proponen ensayos alternativos al establecido tras exhaustivos aná- lisis que recrean las condiciones reales de uso y más acordes a los productos de madera. Se concluye que la incorporación de una lámina impermeable, pero permeable al vapor de agua hacia el exterior, como las utilizadas en el montaje, aportan el mejor procedimiento de ensayo. Composite lightweight wood panels are being increasingly used in construction in Spain. Their growing use should be accompanied by necessary guarantees based on studies of their properties. As it is prescriptive and in addition to others tests, in the present work is examinated the durability of these panels when exposed to the climatic conditions, a characteristic of great importance for wood products, according to Guide ETAG 016, the current standard defining the ageing tests to be used. However, due to the use class of this material, there are indications that the testing outlined in this Guide is inappropriate for assessing the ageing of wood-based sandwich panels. Alternative tests are here proposed that recreate rather better the real conditions under which these products are used. Covering the samples in a waterproof sheeting permeable to the outward movement of water vapour, which is in fact used in the installation, provided the best procedure for testing these panels.
Resumo:
The European construction industry is supposed to consume the 40% of the natural European resources and to generate the 40% of the European solid waste. Conscious of the great damage being suffered by the environment because of construction activity, this work tries to provide the building actors with a new tool to improve the current situation. The tool proposed is a model for the comprehensive evaluation of construction products by determining their environmental level. In this research, the environmental level of a construction product has been defined as its quality of accomplishing the construction requirements needed by causing the minimum ecological impact in its surrounding environment. This information allows building actors to choose suitable materials for building needs and also for the environment, mainly in the project stage or on the building site, contributing to improve the relationship between buildings and environment. For the assessment of the environmental level of construction products, five indicators have been identified regarding their global environmental impact through the product life cycle: CO2 emissions provoked during their production, volume and toxicity of waste generated on the building site, durability and recycling capacity after their useful life. Therefore, the less environmental impact one construction product produces, the higher environmental level performs. The model has been tested in 30 construction products that include environmental criteria in their description. The results obtained will be discussed in this article. Furthermore, this model can lay down guidelines for the selection of ecoefficient construction products and the design of new eco-competitive and eco-committed ones
Resumo:
Under the 12th International Conference on Building Materials and Components is inserted this communication related to the field of management of those assets that constitute the Spanish Cultural Heritage and maintenance. This work is related to the field of management of those assets that constitute the Spanish Cultural Heritage which share an artistic or historical background. The conservation and maintenance become a social demand necessary for the preservation of public values, requiring the investment of necessary resources. The legal protection involves a number of obligations and rights to ensure the conservation and heritage protection. The duty of maintenance and upkeep exceeds the useful life the property that must endure more for their cultural value for its usability. The establishment of the necessary conditions to prevent deterioration and precise in order to fulfill its social function, seeking to prolong the life of the asset, preserving their physical integrity and its ability to convey the values protected. This obligation implies a substantial financial effort to the holder of the property, either public or private entity, addressing a problem of economic sustainability. Economic exploitation, with the aim of contributing to their well-maintained, is sometimes the best way to get resources. The work will include different lines of research with the following objectives. - Establishment of processes for assessing total costs over the building life cycle (LCC), during the planning stages or maintenance budgets to determine the most advantageous operating system. - Relationship between the value of property and maintenance costs, and establishing a sensitivity analysis.
Resumo:
High performance materials are needed for the reconstruction of such a singular building as a cathedral, since in addition to special mechanical properties, high self compact ability, high durability and high surface quality, are specified. Because of the project’s specifications, the use of polypropylene fiber-reinforced, self-compacting concrete was selected by the engineering office. The low quality of local materials and the lack of experience in applying macro polypropylene fiber for structural reinforcement with these components materials required the development of a pretesting program. To optimize the mix design, performance was evaluated following technical, economical and constructability criteria. Since the addition of fibers reduces concrete self-compactability, many trials were run to determine the optimal mix proportions. The variables introduced were paste volume; the aggregate skeleton of two or three fractions plus limestone filler; fiber type and dosage. Two mix designs were selected from the preliminary results. The first one was used as reference for self-compactability and mechanical properties. The second one was an optimized mix with a reduction in cement content of 20 kg/m3and fiber dosage of 1 kg/m3. For these mix designs, extended testing was carried out to measure the compression and flexural strength, modulus of elasticity, toughness, and water permeability resistance
Resumo:
Cold-drawn steel rods and wires retain significant residual stresses as a consequence of the manufacturing process. These residual stresses are known to be detrimental for the mechanical properties of the wires and their durability in aggressive environments. Steel makers are aware of the problem and have developed post-drawing processes to try and reduce the residual stresses on the wires. The present authors have studied this problem for a number of years and have performed a detailed characterization of the residual stress state inside cold-drawn rods, including both experimental and numerical techniques. High-energy synchrotron sources have been particularly useful for this research. The results have shown how residual stresses evolve as a consequence of cold-drawing and how they change with subsequent post-drawing treatments. The authors have been able to measure for the first time a complete residual strain profile along the diameter in both phases (ferrite and cementite) of a cold-drawn steel rod.
Resumo:
Heart valve prostheses are used to replace native heart valves which that are damaged because of congenital diseases or due to ageing. Biological prostheses made of bovine pericardium are similar to native valves and do not require any anticoagulation treatment, but are less durable than mechanical prostheses and usually fail by tearing. Researches are oriented in improving the resistance and durability of biological heart valve prostheses in order to increase their life expectancy. To understand the mechanical behaviour of bovine pericardium and relate it to its microstructure (mainly collagen fibres concentration and orientation) uniaxial tensile tests have been performed on a model material made of collagen fibres. Small Angle Light Scattering (SALS) has been also used to characterize the microstructure without damaging the material. Results with the model material allowed us to obtain the orientation of the fibres, relating the microstructure to mechanical performance
Resumo:
The presented study is related to the EU 7 th Framework Programme CODICE (COmputationally Driven design of Innovative CEment-based materials). The main aim of the project is the development of a multi-scale model for the computer based simulation of mechanical and durability performance of cementitious materials. This paper reports results of micro/nano scale characterisation and mechanical property mapping of cementitious skeletons formed by the cement hydration at different ages. Using the statistical nanoindentation and micro-mechanical property mapping technique, intrinsic properties of different hydrate phases, and also the possible interaction (or overlapping) of different phases (e.g. calcium-silcate-hydrates) has been studied. Results of the mapping and statistical indentation testing appear to suggest the possible existence of more hydrate phases than the commonly reported LD and HD C-S-H and CH phases
Resumo:
In the Standard EHE 08, for the first time, durability acquires the status of Limit State. Article 8 provides that the term Durability limit state, produced by physical and chemical actions, different loads and actions of structural analysis, which can degrade the concrete and reinforcement to unacceptable limits. The verification of this limit state can be done through a procedure set out in the provisions of the Standard. This procedure is based on the use of tables that, depending on the aggressiveness of the environment in which the structure is the concrete strength and the life of the project, setting the quality of the concrete cover (minimum thickness and maximum water cement ratio of concrete used) and the maximum crack width. This procedure, simple in its application, provides highly secure solutions. In addition, on Annex 9, the Standard EHE 08 offers models for testing the durability limit state in cases of corrosion of reinforcement due to carbonation of concrete or entry of chloride ions. The results obtained with these models are tighter than those obtained with the procedure of the articles. In this paper we use both methods in the study of reinforced concrete structures with potential problems of corrosion of reinforcement due to carbonation of concrete. Later checking the results obtained by both procedures. Results demonstrate that the use of the models listed in Annex 9 of Standard EHE 08 offer cheaper solutions than those obtained using the procedure of the articles
Resumo:
La mayoría de las estructuras de hormigón pretensadas construidas en los últimos 50 años han demostrado una excelente durabilidad cuando su construcción se realiza atendiendo las recomendaciones de un buen diseño así como una buena ejecución y puesta en obra de la estructura. Este hecho se debe en gran parte al temor que despierta el fenómeno de la corrosión bajo tensión típico de las armaduras de acero de alta resistencia. Menos atención se ha prestado a la susceptibilidad a la corrosión bajo tensión de los anclajes de postensado, posiblemente debido a que se han reportado pocos casos de fallos catastróficos. El concepto de Tolerancia al Daño y la Mecánica de la Fractura en estructuras de Ingeniería Civil ha empezado a incorporarse recientemente en algunas normas de diseño y cálculo de estructuras metálicas, sin embargo, aún está lejos de ser asimilado y empleado habitualmente por los ingenieros en sus cálculos cuando la ocasión lo requiere. Este desconocimiento de los aspectos relacionados con la Tolerancia al Daño genera importantes gastos de mantenimiento y reparación. En este trabajo se ha estudiado la aplicabilidad de los conceptos de la Mecánica de la Fractura a los componentes de los sistemas de postensado empleados en ingeniería civil, empleándolo para analizar la susceptibilidad de las armaduras activas frente a la corrosión bajo tensiones y a la pérdida de capacidad portante de las cabezas de anclajes de postensado debido a la presencia de defectos. Con este objeto se han combinado tanto técnicas experimentales como numéricas. Los defectos superficiales en los alambres de pretensado no se presentan de manera aislada si no que existe una cierta continuidad en la dirección axial así como un elevado número de defectos. Por este motivo se ha optado por un enfoque estadístico, que es más apropiado que el determinístico. El empleo de modelos estadísticos basados en la teoría de valores extremos ha permitido caracterizar el estado superficial en alambres de 5,2 mm de diámetro. Por otro lado la susceptibilidad del alambre frente a la corrosión bajo tensión ha sido evaluada mediante la realización de una campaña de ensayos de acuerdo con la actual normativa que ha permitido caracterizar estadísticamente su comportamiento. A la vista de los resultados ha sido posible evaluar como los parámetros que definen el estado superficial del alambre pueden determinar la durabilidad de la armadura atendiendo a su resistencia frente a la corrosión bajo tensión, evaluada mediante los ensayos que especifica la normativa. En el caso de las cabezas de anclaje de tendones de pretensado, los defectos se presentan de manera aislada y tienen su origen en marcas, arañazos o picaduras de corrosión que pueden producirse durante el proceso de fabricación, transporte, manipulación o puesta en obra. Dada la naturaleza de los defectos, el enfoque determinístico es más apropiado que el estadístico. La evaluación de la importancia de un defecto en un elemento estructural requiere la estimación de la solicitación local que genera el defecto, que permite conocer si el defecto es crítico o si puede llegar a serlo, si es que progresa con el tiempo (por fatiga, corrosión, una combinación de ambas, etc.). En este trabajo los defectos han sido idealizados como grietas, de manera que el análisis quedara del lado de la seguridad. La evaluación de la solicitación local del defecto ha sido calculada mediante el empleo de modelos de elementos finitos de la cabeza de anclaje que simulan las condiciones de trabajo reales de la cabeza de anclaje durante su vida útil. A partir de estos modelos numéricos se ha analizado la influencia en la carga de rotura del anclaje de diversos factores como la geometría del anclaje, las condiciones del apoyo, el material del anclaje, el tamaño del defecto su forma y su posición. Los resultados del análisis numérico han sido contrastados satisfactoriamente mediante la realización de una campaña experimental de modelos a escala de cabezas de anclaje de Polimetil-metacrilato en los que artificialmente se han introducido defectos de diversos tamaños y en distintas posiciones. ABSTRACT Most of the prestressed concrete structures built in the last 50 years have demonstrated an excellent durability when they are constructed in accordance with the rules of good design, detailing and execution. This is particularly true with respect to the feared stress corrosion cracking, which is typical of high strength prestressing steel wires. Less attention, however, has been paid to the stress corrosion cracking susceptibility of anchorages for steel tendons for prestressing concrete, probably due to the low number of reported failure cases. Damage tolerance and fracture mechanics concepts in civil engineering structures have recently started to be incorporated in some design and calculation rules for metallic structures, however it is still far from being assimilated and used by civil engineers in their calculations on a regular basis. This limited knowledge of the damage tolerance basis could lead to significant repair and maintenance costs. This work deals with the applicability of fracture mechanics and damage tolerance concepts to the components of prestressed systems, which are used in civil engineering. Such concepts have been applied to assess the susceptibility of the prestressing steel wires to stress corrosion cracking and the reduction of load bearing capability of anchorage devices due to the presence of defects. For this purpose a combination of experimental work and numerical techniques have been performed. Surface defects in prestressing steel wires are not shown alone, though a certain degree of continuity in the axial direction exist. A significant number of such defects is also observed. Hence a statistical approach was used, which is assumed to be more appropriate than the deterministic approach. The use of statistical methods based in extreme value theories has allowed the characterising of the surface condition of 5.2 mm-diameter wires. On the other hand the stress corrosion cracking susceptibility of the wire has been assessed by means of an experimental testing program in line with the current regulations, which has allowed statistical characterisasion of their performances against stress corrosion cracking. In the light of the test results, it has been possible to evaluate how the surface condition parameters could determine the durability of the active metal armour regarding to its resistance against stress corrosion cracking assessed by means of the current testing regulations. In the case of anchorage devices for steel tendons for prestressing concrete, the damage is presented as point defects originating from dents, scratches or corrosion pits that could be produced during the manufacturing proccess, transport, handling, assembly or use. Due to the nature of these defects, in this case the deterministic approach is more appropriate than the statistical approach. The assessment of the relevancy of defect in a structural component requires the computation of the stress intensity factors, which in turn allow the evaluation of whether the size defect is critical or could become critical with the progress of time (due to fatigue, corrosion or a combination of both effects). In this work the damage is idealised as tiny cracks, a conservative hypothesis. The stress intensity factors have been calculated by means of finite element models of the anchorage representing the real working conditions during its service life. These numeric models were used to assess the impact of some factors on the rupture load of the anchorage, such the anchorage geometry, material, support conditions, defect size, shape and its location. The results from the numerical analysis have been succesfully correlated against the results of the experimental testing program of scaled models of the anchorages in poly-methil methacrylate in which artificial damage in several sizes and locations were introduced.