5 resultados para Metal-work

em Universidad Politécnica de Madrid


Relevância:

30.00% 30.00%

Publicador:

Resumo:

The Bienaventurada mine operates a polymetallic Ag-Pb-Zn (Cu, Au) vein system of the low sulphidation epithermal type. Fluid inclusions, FI, are abundant in quartz, sphalerite and adularia. FI petrography demonstrates typical primary growth zoning which occurs frequently in crystalline quartz, and defines the most common primary FI. These are usually very small, but several types of primary, P, and secondary, S, FI Assemblages (FIAs) comprising FI of measurable size (3 to > 100 μm) can also be identified through careful petrographic work. The fluids are aqueous and undersaturated, and no evidence of CO2 was found; the degree of fill is usually high (~70-80 %) in the L-rich inclusions, but extremely low in V-rich inclusions. The measured microthermometric values are very consistent in the FIAs selected; they are for the most part roughly similar in the P and S assemblages: the median is typically ~258ºC for total homogenization temperatures, Th, and -1.5 ºC for ice melting temperatures, Tm (corresponding to 2.57 wt% NaCl eq). The widespread occurrence of L-rich and V-rich FI in the same FIA and the consistent Th values point to an extensive boiling system along the vein. In these conditions, Th equals T of trapping, and the ores are assumed to have been precipitated from an aqueous low salinity boiling fluid, of likely meteoric origin, at some 250-280º C, under ~500 m hydrostatic head.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The extraction of metal impurities during phosphorus diffusion gettering (PDG) is one of the crucial process steps when fabricating high-efficiency solar cells using low-cost, lower-purity silicon wafers. In this work, we show that for a given metal concentration, the size and density of metal silicide precipitates strongly influences the gettering efficacy. Different precipitate size distributions can be already found in silicon wafers grown by different techniques. In our experiment, however, the as-grown distribution of precipitated metals in multicrystalline Si sister wafers is engineered through different annealing treatments in order to control for the concentration and distribution of other defects. A high density of small precipitates is formed during a homogenization step, and a lower density of larger precipitates is formed during extended annealing at 740º C. After PDG, homogenized samples show a decreased interstitial iron concentration compared to as-grown and ripened samples, in agreement with simulations.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The adhesives used for applications in marine environments are subject to particular chemical conditions, which are mainly characterised by an elevated chlorine ion content and intermittent wetting/drying cycles, among others.These conditions can limit the use of adhesives due to the degradation processes that they experience. In this work, the chemical degradation of two different polymers, polyurethane and vinylester, was studied in natural seawater under immersion for different periods of time.The diffusion coefficients and concentration profiles of water throughout the thickness of the adhesiveswere obtained.Microstructural changes in the polymer due to the action of water were observed by SEM, and the chemical degradation of the polymer was monitored with the Fourier transform infrared spectroscopy (FTIR) and differential scanning calorimetry (DSC). The degradation of the mechanical properties of the adhesive was determined by creep tests withMixed Cantilever Beam (MCB) specimens at different temperatures. After 180 days of immersion of the specimens, it was concluded that the J-integral value (depending on the strain) implies a loss of stiffness of 51% and a decrease in the failure load of 59% for the adhesive tested.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A colloidal deposition technique is presented to construct long-range ordered hybrid arrays of self-assembled quantum dots and metal nanoparticles. Quantum dots are promising for novel opto-electronic devices but, in most cases, their optical transitions of interest lack sufficient light absorption to provide a significant impact in their implementation. A potential solution is to couple the dots with localized plasmons in metal nanoparticles. The extreme confinement of light in the near-field produced by the nanoparticles can potentially boost the absorption in the quantum dots by up to two orders of magnitude. In this work, light extinction measurements are employed to probe the plasmon resonance of spherical gold nanoparticles in lead sulfide colloidal quantum dots and amorphous silicon thin-films. Mie theory computations are used to analyze the experimental results and determine the absorption enhancement that can be generated by the highly intense near-field produced in the vicinity of the gold nanoparticles at their surface plasmon resonance. The results presented here are of interest for the development of plasmon-enhanced colloidal nanostructured photovoltaic materials, such as colloidal quantum dot intermediate-band solar cells.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

El objetivo principal de este trabajo es profundizar en el conocimiento del fenómeno de la corrosión subpelicular inducida por contaminantes hidrosolubles en la intercara metal/pintura. La contaminación salina del substrato es una situación común en la práctica: la superficie metálica suele estar expuesta a atmósferas contaminadas antes de ser recubierta, limpieza previa del metal con abrasivos contaminados, etc. La eliminación total de estos contaminantes resulta muy difícil de conseguir incluso con las técnicas más sofisticadas de limpieza. Esta investigación se centra en la determinación del efecto de la naturaleza del contaminante y la naturaleza y espesor del recubrimiento en el proceso de corrosión subpelicular del acero. En la investigación se utilizaron dos barnices de naturaleza diferente: poliuretano y vinílico; y se aplicaron a tres espesores diferentes. Los contaminantes empleados en este trabajo fueron: NaCl, NH4C1, CaCl2, Na2S04, (NH4)2S04, NaN03, NH4N03, Ca(N03)2. Los ensayos se realizaron en una cámara de condensación de humedad permanente. Los tiempos de exposición fueron 100, 300 y 600 horas. La velocidad de corrosión se evaluó gravimétricamente, mediante la técnica de pérdida de peso. Se realizaron estudios de permeabilidad al oxígeno y al agua de películas libres de substrato, evaluación de la velocidad de corrosión de probetas sin pintar inmersas en soluciones salinas de los contaminantes seleccionados, conductividad de dichas soluciones salinas, solubilidad del oxígeno en las soluciones salinas, adherencia en seco y en húmedo a diferentes tiempos de exposición. Se aporta evidencia respecto al control ejercido en el proceso corrosivo por el oxígeno que permea a través de la película, mientras que la permeación de agua controla la pérdida de adherencia del recubrimiento. Ambas permeabilidades dependen de la naturaleza del recubrimiento y de su espesor. Se ha investigado la influencia de la naturaleza del contaminante en la intercara metal/pintura. La naturaleza del catión parece quedar enmascarada por el efecto definitivo del anión. La concentración salina ejerce asimismo un efecto importante en la corrosión subpelicular. ABSTRACT The main aim of this work is to study in depth the knowledge of underfilm corrosión induced by hydrosoluble contaminants at the metal/paint Ínterface. The saline contamination of the substrate is a common situation in practice: metallic surfaces use to be exposed to polluted atmospheres, previous cleaning of the metal with contaminated abrasives, etc. Total elimination of these contaminants is hard to obtain even with modern cleaning techniques. This research is focused in determining the effect of contaminant nature, coating nature and its thickness on the steel underfilm corrosión process. In this work we used two varnishes with different nature: polyurethane and vinyl; they were applied in three different thicknesses. The saline contaminants employed were: NaCl, NH4C1, CaCl2, Na2S04, (NH4)2S04, NaN03, NH4N03/ Ca(N03)2. The tests were carried out in a condensation humidity chamber. The period of exposure were 100, 300 and 600 hours. Corrosión rate was assessed by weight loss. Simultaneously, studies on oxygen and water permeability of free films, assessing on corrosión rate of uncoated samples immersed in saline solutions of the selected contaminants, conductivity of these solutions, oxygen solubility in saline solutions, wet and dry adhesión of the polyurethane varnish at different periods of exposure, were carried out. There is clear evidence about control on corrosión process of oxygen that passes through the coating, while the passing of water controls the loss of adhesión of the coating. Both, water and oxygen permeation, depend on the nature and thickness of the coating. It has been researched the inf luence of the nature of contaminant at the metal/paint interface. The nature of the catión seems to be "masked" by the definitive effect of the nature of anión. The saline concentration also exerts an important effect on underfilm corrosión.