We present a combined magnetooptic and ferromagnetic resonance study of a series of arrays of single-crystalline Fe stripes fabricated by electron beam lithography on epitaxial Au(001)/Fe(001)/MgO(001) films grown by pulsed laser deposition. The analysis of the films revealed a clear fourfold magnetocrystalline anisotropy, with no significant presence of other anisotropy sources. The use of a large series of arrays, with stripe widths between 140 and 1000 nm and separation between them of either 200 nm or 500 nm, allowed studying their magnetization processes and resonance modes as well as the effects of the dipolar interactions on both. The magnetization processes of the stripes were interpreted in terms of a macrospin approximation, with a good agreement between experiments and calculations and negligible influence of the dipolar interactions. The ferromagnetic resonance spectra evidenced two types of resonances linked to bulk oscillation modes, essentially insensitive to the dipolar interactions, and a third one associated with edge-localized oscillations, whose resonance field is strongly dependent on the dipolar interactions. The ability to produce a high quality, controlled series of stripes provided a good opportunity to achieve an agreement between the experiments and calculations, carried out by taking into account just the Fe intrinsic properties and the morphology of the arrays, thus evidencing the relatively small role of other extrinsic factors.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

We report on an experimental study on the spin-waves relaxation rate in two series of nanodisks of diameter ϕ=300 , 500, and 700 nm, patterned out of two systems: a 20 nm thick yttrium iron garnet (YIG) film grown by pulsed laser deposition either bare or covered by 13 nm of Pt. Using a magnetic resonance force microscope, we measure precisely the ferromagnetic resonance linewidth of each individual YIG and YIG|Pt nanodisks. We find that the linewidth in the nanostructure is sensibly smaller than the one measured in the extended film. Analysis of the frequency dependence of the spectral linewidth indicates that the improvement is principally due to the suppression of the inhomogeneous part of the broadening due to geometrical confinement, suggesting that only the homogeneous broadening contributes to the linewidth of the nanostructure. For the bare YIG nano-disks, the broadening is associated to a damping constant α=4 × 10−4 . A threefold increase of the linewidth is observed for the series with Pt cap layer, attributed to the spin pumping effect. The measured enhancement allows to extract the spin mixing conductance found to be G↑↓=1.55 × 1014 Ω−1 m−2 for our YIG(20nm)|Pt interface, thus opening large opportunities for the design of YIG based nanostructures with optimized magnetic losses.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

One of the key steps to achieve high efficiencies in amorphous/crystalline silicon photovoltaic structures is to design low-ohmic-resistance backcontacts with good passivation in the rear part of the cell. A well known approach to achieve this goal is to use laser-fired contact (LFC) processes in which a metal layer is fired through the dielectric to define good contacts with the semiconductor. However, and despite the fact that this approach has demonstrated to be extremely successful, there is still enough room for process improvement with an appropriate optimization. In this paper, a study focused on the optimal adjustment of the irradiation parameters to produce laser-fired contacts in a-Si:H/c-Si heterojunctionsolarcells is presented. We used samples consisting of crystalline-silicon (c-Si) wafers together with a passivation layer of intrinsic hydrogenated amorphous silicon (a-Si:H(i)) deposited by plasma-enhanced chemical deposition (PECVD). Then, an aluminum layer was evaporated on both sides, the thickness of this layer varied from 0.2 to 1 μm in order to identify the optimal amount of Al required to create an appropriate contact. A q-switched Nd:YVO4laser source, λ = 532 nm, was used to locally fire the aluminum through the thin a-Si:H(i)-layers to form the LFC. The effects of laser fluences were analyzed using a comprehensive morphological and electrical characterization.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Crystallization and grain growth technique of thin film silicon are among the most promising methods for improving efficiency and lowering cost of solar cells. A major advantage of laser crystallization and annealing over conventional heating methods is its ability to limit rapid heating and cooling to thin surface layers. Laser energy is used to heat the amorphous silicon thin film, melting it and changing the microstructure to polycrystalline silicon (poly-Si) as it cools. Depending on the laser density, the vaporization temperature can be reached at the center of the irradiated area. In these cases ablation effects are expected and the annealing process becomes ineffective. The heating process in the a-Si thin film is governed by the general heat transfer equation. The two dimensional non-linear heat transfer equation with a moving heat source is solve numerically using the finite element method (FEM), particularly COMSOL Multiphysics. The numerical model help to establish the density and the process speed range needed to assure the melting and crystallization without damage or ablation of the silicon surface. The samples of a-Si obtained by physical vapour deposition were irradiated with a cw-green laser source (Millennia Prime from Newport-Spectra) that delivers up to 15 W of average power. The morphology of the irradiated area was characterized by confocal laser scanning microscopy (Leica DCM3D) and Scanning Electron Microscopy (SEM Hitachi 3000N). The structural properties were studied by micro-Raman spectroscopy (Renishaw, inVia Raman microscope).