853 resultados para 330506 Ingeniería civil


Relevância:

80.00% 80.00%

Publicador:

Resumo:

El presente trabajo estudia el comportamiento de dos hormigones frente al ensayo de resistencia al hielo-deshielo de hormigones endurecidos. La incorporación de un aditivo aireante mejora de forma sensible el comportamiento del hormigón frente a este ensayo. Sin embargo, en hormigón pretensado con cordón adherente está prohibido el uso de aditivos aireantes. Una estrategia adecuada es emplear humo de sílice para mejorar la impermeabilidad del hormigón. En este trabajo se compara el comportamiento de un hormigón con aditivo aireante y otro con humo de sílice frente al ensayo de resistencia al hielo-deshielo. Además, estudia la viabilidad de emplear técnicas alternativas de medida del deterioro superficial: modificación de la velocidad de pulso ultrasónico y medida de la deformación superficial con galgas extensométricas. Ambas técnicas se muestran viables y aportan ventajas frente al peso de la masa superficial desprendida por descascarillamiento

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The traditional teaching methods used for training civil engineers are currently being called into question as a result of the new knowledge and skills now required by the labor market. In addition, the European Higher Education Area is requesting that students be given a greater say in their learning. In the subject called Construction and Building Materials at the Civil Engineering School of the Universidad Politécnica de Madrid, a path was set three academic years ago to lead to an improvement in traditional teaching by introducing active methodologies. The innovations are based on cooperative learning, new technologies, and continuous assessment. The writers’ proposal is to offer their experience as a contribution to the debate on how students can be encouraged to acquire the skills currently demanded from a civil engineer, though not overlooking solid, top-quality training. From the outcomes obtained, it can be concluded that using new teaching techniques to supplement a traditional approach provides more opportunities for students to learn while boosting their motivation. In our case, the introduction of these changes has resulted in an increased pass rate of 29% on average, when such a figure is considered in the light of the mean value of passes during the last decade.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Es para mí un honor presentar esta publicación que recoge las comunicaciones presentadas en las IX Jornadas Iberoamericanas de Materiales de Construcción, que se han celebrado en Quito, Ecuador, los días 9 y 10 de agosto de 2011. En esta ocasión fue nuestra anfitriona la Escuela Politécnica Nacional, radicada en la bellísima ciudad de Quito, con el auspicio de diversas instancias ecuatorianas, tanto públicas como privadas. Por este motivo, mis primeras palabras quieren ser de agradecimiento por la hospitalidad brindada y la excelente organización local. Asimismo, quisiera reiterar mi gratitud a las entidades que todos los años apoyan decididamente la celebración de estas Jornadas y que este año no han faltado a la cita, como son: La Universidad Politécnica de Madrid (España), y muy especialmente su Escuela Técnica Superior de Ingenieros de Minas. La Asociación Española de Fabricantes de Áridos (ANEFA). La Cámara de la Piedra de la Provincia de Buenos Aires (Argentina) La empresa ERAL, Equipos y Procesos, S.L. Confiamos en que progresivamente otras entidades de nuestro entorno profesional, tanto académico como empresarial, se vayan vinculando de forma permanente a dicha organización. El lema que se eligió para este año fue: "Los materiales de construcción como pilares del desarrollo de la sociedad del siglo XXI". Creo que constituye toda una declaración de intenciones, además de enraizarse profundamente con la aún corta, pero ya intensa historia de nuestras Jornadas. Éstas nacen precisamente con el tercer milenio, y así todas las ediciones celebradas hasta ahora (Madrid 2001, La Habana 2002, San Juan 2003, Tegucigalpa 2004, Panamá 2007, Mar del Plata 2008, Valencia 2009 y Lima 2010) han tratado de poner un granito de arena (y nunca el símil fue más oportuno) para conseguir desarrollar la cooperación científica y técnica entre los países de Iberoamérica, Portugal y España, a través del intercambio de conocimiento y la transferencia tecnológica. Nuestras reuniones no han de verse únicamente como un punto de encuentro en el que presentar nuestros trabajos y experiencias, compartiéndolas con los colegas de otros lugares, tal vez lejanos en lo geográfico pero cercanos en la cultura y la sensibilidad. Con ser éste un fin no sólo loable, sino esencial a nuestra actividad, sería insuficiente para colmar nuestras expectativas. Las Jornadas han de ser un foro que constituya la semilla de futuras actuaciones conjuntas de todo tipo, académicas o empresariales, bilaterales o multilaterales, siempre con el objetivo de fomentar las relaciones basadas en compartir nuestros saberes y, en la medida de lo posible, la movilidad de nuestros técnicos, profesores o alumnos. Precisamente en un momento como el actual, en el que las incógnitas y graves preocupaciones que la crisis financiera mundial ha sembrado en nuestro ánimo no se han despejado todavía, es cuando este tipo de actividades son más necesarias, ya que es generalmente reconocido que para salir de esta situación se precisa mejorar la competitividad de nuestras economías y sólo a través de la innovación científica y tecnológica esto será posible, siempre que las políticas laborales y regulatorias lo apoyen. Los materiales de construcción constituyen un caso destacable en este sentido, ya que generalmente su producción está ligada a la extracción próxima de sus materias primas, dados los volúmenes que se mueven. Esto también es así muy frecuentemente con su utilización, de lo que es un ejemplo paradigmático la industria del hormigón (o concreto). Esto implica que pueden suponer un aporte fundamental en el desarrollo de las comunidades locales, gracias a la generación de tejido industrial y la consiguiente de puestos de trabajo, además de contribuir en calidad de componente imprescindible a la implantación de infraestructuras de todo tipo (residenciales, viarias o de transporte en general, entre otras) que son la base en la que otros sectores económicos han de apoyarse de modo ineludible. Por supuesto, este desarrollo ha de ser sostenible. Soy consciente de que ésta es ya una frase hecha, que por tanto ha perdido ya parte de su impacto, al utilizarse tantas veces con poco o ningún fundamento. Pero los que nos dedicamos a la ciencia y la tecnología sabemos de la importancia de su profundo significado, ya que el desarrollo o es sostenible o no será desarrollo, sino a lo sumo especulación para beneficio de unos pocos. Creo que el verdadero sentido del término está en que permita un desarrollo que beneficie de forma general a toda la sociedad, y no sólo a la presente, sino a la futura. Éste es el reto que los técnicos tenemos. Traducir este concepto en términos de aseguramiento de la calidad, seguridad e higiene en el trabajo, cuidado de los aspectos ambientales, I+D+i, cualificación académica y profesional y, por qué no, rentabilidad económica, entre otros aspectos fundamentales de nuestras actividades. Creo sinceramente que los trabajos que aquí se presentan suponen una contribución en este sentido, tanto por su calidad como por la diversidad de sus temáticas dentro del campo de los materiales de construcción. Espero y deseo que constituyan el germen de futuros encuentros y otras actividades de colaboración científica, tecnológica o educativa entre las entidades de nuestro entorno iberoamericano. José-Luis Parra y Alfaro Presidente del Comité Científico

Relevância:

80.00% 80.00%

Publicador:

Resumo:

En este estudio se aplica una metodología de obtención de las leyes de frecuencia derivadas (de caudales máximo vertidos y niveles máximos alcanzados) en un entorno de simulaciones de Monte Carlo, para su inclusión en un modelo de análisis de riesgo de presas. Se compara su comportamiento respecto del uso de leyes de frecuencia obtenidas con las técnicas tradicionalmente utilizadas.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

La gestión de presiones en las redes de distribución de agua urbana, a pesar de tratarse de una operación habitual y de suma importancia para la explotación de este tipo de infraestructuras, carece hoy día de una metodología generalizable. Así, su instauración y posterior control generalmente vienen determinados por un diseño particularizado para cada caso y basado en la experiencia de la empresa operadora y los ingenieros correspondientes. La presente investigación propone, a partir de un estudio cualitativo de estructura propia, fundamentado en el análisis y estudio comparativo de casos, una metodología integral de implantación aplicable al conjunto de este tipo de sistemas. La elaboración de esta metodología se basa en la selección y propuesta de una serie de indicadores tanto de diseño de los factores más importantes a considerar, como de control de resultados de acuerdo a las diferentes finalidades a alcanzar. Asimismo se ha establecido una categorización de los tipos de regulación más convenientes para cada sistema según las distintas finalidades para las que ha podido ser diseñada la operación de gestión de presiones

Relevância:

80.00% 80.00%

Publicador:

Resumo:

High performance materials are needed for the reconstruction of such a singular building as a cathedral, since in addition to special mechanical properties, high self compact ability, high durability and high surface quality, are specified. Because of the project’s specifications, the use of polypropylene fiber-reinforced, self-compacting concrete was selected by the engineering office. The low quality of local materials and the lack of experience in applying macro polypropylene fiber for structural reinforcement with these components materials required the development of a pretesting program. To optimize the mix design, performance was evaluated following technical, economical and constructability criteria. Since the addition of fibers reduces concrete self-compactability, many trials were run to determine the optimal mix proportions. The variables introduced were paste volume; the aggregate skeleton of two or three fractions plus limestone filler; fiber type and dosage. Two mix designs were selected from the preliminary results. The first one was used as reference for self-compactability and mechanical properties. The second one was an optimized mix with a reduction in cement content of 20 kg/m3and fiber dosage of 1 kg/m3. For these mix designs, extended testing was carried out to measure the compression and flexural strength, modulus of elasticity, toughness, and water permeability resistance

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The aim of this work is to relate the curing conditions of concrete and the addition of an air-entraining admixture with the damage caused by freeze–thaw cycles. In countries with a continental climate, the curing of concrete in summer is performed under climatic conditions of high temperature and low humidity, and during the winter the concrete suffers conditions of freeze–thaw, often accompanied by the use of de-icing salts. This paper shows the experimental results of the behaviour of concrete specimens cured under climatic summer conditions (high temperature and low humidity) and then subjected to freeze–thaw cycles. Curing of the specimens includes conditions of good and bad practice in relation to wetting and protection of the concrete. It also examines the effectiveness of using an air-entraining admixture in both cases. The experimental programme includes an evaluation of the mechanical properties of the concrete, the study of the cement hydration and the measurement of the volume and pore sizes of the concrete. These tests were performed before and after the application of the freeze–thaw cycles. The results obtained showed that the specimens without air-entraining admixture show a deterioration of mechanical properties after the freeze–thaw test. However, the inclusion of air bubbles benefits the behaviour of concrete against freeze–thaw cycles so even better mechanical properties after the test were observed. This anomalous behaviour is because the cement hydration process continues over the freeze–thaw tests, closing the pore structure. This aspect has been confirmed with the DTA and TG tests performed

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The initial curing of concrete specimens for quality assurance is addressed in different ways in testing standards, which often specify requirements that are difficult to meet in practice unless very costly initial curing chambers are available. The failure to meet these requirements in many areas of the world does not appear to result in adverse consequences. This study analyzed six initial curing temperature schemes, all with cycles similar to natural conditions to avoid the simplifications inherent in constant temperature curing. Three strengths of concrete and two initial curing times (24 and 72 hours) were used in this study. The findings showed that initial curing time had no effect on 28-day strength. The 28-day strength also proved to be resilient to maximum and minimum initial curing temperatures outside the limits stated in the standards considered in this study

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Es una realidad cada vez más aceptada que la durabilidad del hormigón es una propiedad igual de importante que la resistencia mecánica o la estabilidad de volumen. No es el objeto del presente trabajo ahondar en las causas de esta evidencia sino en contribuir a hacer del diseño de la durabilidad una materia incorporada al quehacer diario de los técnicos y especialistas. Solo si la durabilidad de una estructura se puede proyectar y verificar, será posible conseguir vidas útiles con una cierta garantía o seguridad en que se alcanzarán los periodos de servicio que se especifiquen. En el diseño de la durabilidad se ha dedicado mucho tiempo en el pasado a aclarar los mecanismos de ataque (por ejemplo: por sulfatos o por reacción árido-álcali) o como realizar ensayos acelerados en estos casos y también en el caso concreto de la corrosión de la armadura. En el caso de la corrosión, la envergadura de los costes de reparaciones ha estimulado la publicación de modelos y ensayos que, si bien necesitan todavía calibración, al menos suponen una cierta ayuda para el proyectista.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

La norma UNE-EN 13374 “Sistemas provisionales de protección de borde. Especificaciones del producto, métodos de ensayo” (1) clasifica los sistemas provisionales de protección de borde (SPPB) en tres clases (A, B y C), en función del ángulo de la superficie de trabajo y de la altura de caída de la persona a proteger. Los sistemas clase A son los indicados cuando la inclinación de la superficie de trabajo es menor de 10º. La norma establece los requisitos de flecha y de resistencia de los SPPB. Los requisitos se pueden comprobar tanto analítica como experimentalmente. El objetivo del trabajo ha sido la evaluación del comportamiento de los SPPB utilizados habitualmente en las obras y establecer los cambios necesarios para que cumplan con la norma UNE-EN 13374. Para ello se han evaluado analítica y experimentalmente tres SPPB clase A, fabricados con acero S235. Los resultados obtenidos muestran que, el sistema empleado de forma habitual en obras no supera los requisitos de la norma ni analítica ni experimentalmente. El tercer sistema supera los requisitos con las dos metodologías de análisis. El segundo sistema supera los requisitos cuando la evaluación se realiza analíticamente pero no cuando la vía utilizada es la experimental.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

En este trabajo se presentan los diagramas tensióndeformación de un nuevo acero inoxidable con bajo contenido en níquel, un inoxidable convencional AISI 304 y un acero al carbono de uso común en estructuras de hormigón armado. Dicha ductilidad se ha estudiado determinando la tensión máxima (fmax), la tensión en el límite elástico (fy) y la deformación bajo carga máxima (εmax). Los tres materiales se han evaluado utilizando criterios aceptados internacionalmente, como son el índice p (capacidad de rotación plástica), el índice A* (área plástica de endurecimiento) y el índice de tenacidad Id (energía total absorbida en el punto de alargamiento bajo carga máxima), los resultados obtenidos se han comparado con los aceros convencionales de armaduras 500SD, 500N y 500H (EC-2).

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Los efectos de la corrosión sobre las armaduras se manifiestan por la pérdida de sección y la variación de las propiedades mecánicas relacionadas con la ductilidad. En este trabajo se han ensayado a tracción 96 barras de acero B500SD que previamente se han sometido a niveles variables de corrosión. Los resultados muestran que los alargamientos de las barras disminuyen y el cociente entre la tensión máxima y el límite elástico aumenta conforme el nivel de corrosión avanza. A partir del estudio del efecto de entalla y de la distinta constitución metalográfica del acero a nivel de sección debido a su procedimiento de fabricación se pueden explicar los fenómenos anteriores.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

This study includes an analysis of the applicability of current models used for estimating the mechanical properties of conventional concrete to self-compacting concrete. The mechanical properties evaluated are: modulus of elasticity, tensile strength, and modulus of rupture. An extensive database which included the dosifications and the mechanical properties of 627 mixtures from 138 different references, was used. The models considered are: ACI, EC-2, NZS 3101:2006 (New Zealand code) and the CSA A23.3-04 (Canadian code). The precision in estimating the modulus of elasticity and tensile strength is acceptable for all models; however, all models are less precise in estimating the modulus of rupture.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

El objetivo principal de este trabajo ha sido estudiar el comportamiento de vigas de hormigón, reforzadas a cortante con tejidos de fibra de carbono pegados con resinas epoxi. Para conseguir este objetivo se han planteado objetivos parciales como el análisis de la fisuración y de los movimientos en las vigas reforzadas. La metodología empleada ha sido principalmente experimental, realizándose una serie de diez vigas de hormigón en masa o armado. Se han comparado los resultados experimentales con los teóricos, obtenidos mediante la formulación analítica existente, como la recomendada por el fib Bulletin 14. Los resultados obtenidos demuestran que las vigas reforzadas ofrecen un comportamiento significativamente superior al de las vigas sin refuerzo, tanto en el valor de las cargas últimas como en la ductilidad de las piezas. Además se puede concluir que en todos los casos estudiados la rigidez prevista hasta la fisuración de las vigas es superior a la obtenida experimentalmente. Además las vigas reforzadas a cortante con tejido de fibra de carbono poseen una ductilidad superior a la de las vigas sin reforzar

Relevância:

80.00% 80.00%

Publicador:

Resumo:

El objetivo principal ha sido estudiar el comportamiento de vigas de hormigón reforzadas a cortante con tejidos de fibra de carbono o basalto pegados con resinas epoxi. Se han planteado objetivos parciales como el análisis de la fisuración y de los movimientos en las vigas y la comparación del comportamiento mecánico de los sistemas de refuerzo estudiados. La metodología empleada ha sido experimental, realizándose vigas de hormigón en masa reforzadas inferiormente con tejido de fibra de carbono. Las vigas se han reforzado a cortante con tejidos de fibra de carbono o basalto. Se han comparado los resultados experimentales con los teóricos, obtenidos mediante la formulación analítica existente. Los resultados demuestran que las vigas reforzadas ofrecen un comportamiento significativamente superior al de las vigas sin refuerzo, tanto en el valor de las cargas últimas como en la ductilidad de las piezas. Además la rigidez prevista hasta fisuración es superior a la obtenida experimentalmente. Los resultados obtenidos nos permiten concluir que de la formulación aditiva propuesta por el Fib Bulletin 14 no se obtienen buenos resultados y que la formulación existente en diversas normativas vigentes para el cálculo de la resistencia a cortante del hormigón resulta conservadora.